Daxun is an excellent manufacturer of CP-2-grade titanium rods
As China’s leading supplier of titanium and titanium alloy rods, Daxun provides high-performance titanium rods to the world.
- Titanium Rod Grade:CP-2(Grade 2)- UNS R50400-3.7035-TA2
- Types: Hot rolled rod, forged rod, cold drawn rod, extruded rod etc
- Shape: Titanium round bar, titanium square bar、Ti hexagonal bar
- Density of Titanium Rod: Density of Grade 2 Titanium Rod is 4.51g/cm3
- Standards: ASTM B 348,ASME SB348,DIN 17862,ASTM F67,ASTM 265
- Dimensions: GB, GJB, EN, ASTM, JIS, ASME, BS, AISI, DIN, ISO, etc.
The global leader in commercially pure titanium rod manufacturing services
Grade 2 Titanium Rod is the workhorse among titanium alloy rods, offering an excellent balance of strength and weight for weight-sensitive applications. As a commercially pure (CP) titanium alloy, it achieves an ideal combination of strength and ductility, making it suitable for a wide range of demanding uses. It provides high impact strength, is easily weldable, and is extremely corrosion-resistant in oxidizing conditions, alkaline media, brine solutions, weakly reducing environments, nitric acid, and wet chlorine. Additionally, its excellent resistance to seawater and saline solutions further enhances its versatility.
The Grade 2 Titanium Rod stands out for its lightweight nature, impressive strength-to-weight ratio, and outstanding resistance to corrosion, making it highly versatile and ideal for numerous industrial uses. From general industrial uses to military and aerospace applications, this material delivers reliable performance in challenging environments.
Daxun Alloys stocks Grade 2 Titanium Rods in a variety of diameters to meet the specific requirements of different projects. Our inventory includes sizes ranging from 1 mm to 300 mm, with the ability to accommodate custom orders for larger dimensions. All rods are certified to ASTM B348 and ASTM B381 standards.
For those seeking reliable suppliers, Daxun Alloys offers a comprehensive range of Grade 2 Titanium products, including ASTM B348 Titanium Grade 2 Round Bars, UNS R50400 Bright Bars, and WERKSTOFF NR. 3.7035 Round Bars. Whether you need round, forged, or square bars, we ensure consistent quality and competitive pricing.
Feel free to contact Daxun Alloys for inquiries or to request a quote. Our team is committed to providing high-quality Grade 2 Titanium Rods and is happy to assist with any questions or project-specific needs.
Данные
- Параметр
- Ingredient
- Механические свойства
- Физические свойства
- Hot searches
| Specification | Details |
| Материал | Titanium rod and bar Grade 2 (UNS R50400) |
| Стандарт | ASTM B348, ASTM SB348, AMS 4921, AMS 4902 |
| Dimensions | EN, ASTM, JIS, ASME, BS, AISI |
| Diameter Range | 0.125″ – 14″ (3.175mm – 355.6mm), custom |
| Length Range | Up to 240″ (6096mm), custom |
| Finish | Cold (bright) drawn, centreless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centreless Ground & Black |
| Отделка поверхности | Cold drawn, Centerless Ground, Polished, Or Rough Turned, Black, NO.4 Finish, BA Finish, Matt Finish, etc. |
| Condition | Hardened & tempered, annealed |
| Толерантность | Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm) |
| Form | Titanium square bars, titanium ingots, titanium round bars, rectangular titanium bars, triangular titanium bars, forged titanium bars, titanium hexagonal bars, etc. |
| Физические свойства | Density: 0.163 lb/in³ (4.51 g/cm³), Melting Point: 3,020°F (1,660°C), Elongation: 20-30%, Modulus of Elasticity: 16.5 x 10⁶ psi (114 GPa) |
| Химический состав | Titanium (min): 99.2%, Oxygen (max): 0.25%, Carbon (max): 0.08%, Iron (max): 0.30%, Nitrogen (max): 0.03%, Hydrogen (max): 0.015% |
| Элемент | Weight % |
| C | ≤0.08 |
| O | ≤0.25 |
| N | ≤0.03 |
| H | ≤0.015 |
| Fe | ≤0.30 |
| *OEE | ≤0.10 |
| *OET | ≤0.40 |
| Ti | Remaining |
| Hardness, Knoop | 170 | 170 | |
| Hardness, Rockwell B | 80 | 80 | |
| Hardness, Vickers | 145 | 145 | |
| Tensile Strength, Ultimate | 344 MPa | 49900 psi | |
| Tensile Strength, Yield | 275 – 410 MPa | 39900 – 59500 psi | |
| Elongation at Break | 20 % | 20 % | |
| Reduction of Area | 35 % | 35 % | |
| Modulus of Elasticity | 105 GPa | 15200 ksi | In Tension |
| Compressive Modulus | 110 GPa | 16000 ksi | |
| Poisson’s Ratio | 0.37 | 0.37 | |
| Izod Impact | 114 – 171 J | 84.1 – 126 ft-lb | |
| Fatigue Strength | 300 MPa | 43500 psi | 1E+7 cycles, Unnotched |
| Fatigue Strength | 425 MPa | 61600 psi | 30,000 cycles, Unnotched |
| Fracture Toughness | 66 MPa-m½ | 60.1 ksi-in½ | K(Q); annealed |
| Shear Modulus | 45 GPa | 6530 ksi |
| Плотность | Melting Range | Modulus of Elasticity (Tension) | Specific Heat | Mean Coefficient of Expansion | Thermal conductivity | Электрическое сопротивление |
| kg/m3 | °C | GPa | J/kg. °C | x10 -6 / °C | W / m. °C | micro-ohm.m |
| 4,507 | 1668± 10 | 103 | 519 | 8.41 | 11.4 | 0.42 |
| ASTM B348 Alloy Gr 2 Hex Bar Polished | grade 2 titanium Hexagonal Bar |
| ASTM B348 Alloy Gr 2 Rectangular Bar | Titanium WERKSTOFF NR. 3.7035 Threaded Bar Black |
| Titanium UNS R50400 Round Bar | grade 2 titanium Din 3.7035 Flat Bar |
| Titanium Grade 2 Bar | Alloy grade 2 titanium Flat Bar Black |
| Alloy Gr 2 Rounds | ASME SB 338 gr 2 Flat Bar Bright |
| Titanium Alloy Grade 2 Bright Bar | Alloy Gr 2 Flat Bar Polished |
| Alloy grade 2 titanium Hex Bar Annealed | Titanium WERKSTOFF NR. 3.7035 Cold Drawn Round Bar |
| ASTM B348 grade 2 titanium Round Bars | Titanium Grade 2 Flat Bar stock |
| Titanium WERKSTOFF NR. 3.7035 Hex Bar | Alloy Gr 2 Threaded Bar |
| Titanium Grade 2 Square Bar Polished | Titanium UNS R50400 Bright Bar Hot Rolled |
| 3.7035 grade 2 titanium Hex Bar Bright | Alloy Gr 2 Alloy Hollow Bar |
| Gr 2 Titanium Rectangular Bar Annealed | Alloy grade 2 titanium Polished Hex Bar |
| ASME SB 338 gr 2 Forged Bar | Gr 2 Titanium Polished Bar |
| Alloy Gr 2 Alloy Rods | UNS R50400 Titanium Flat Bar Cold Drawn |
| Alloy Gr 2 Square Bar Cold Drawn | Titanium Grade 2 Bright Bar material |
| grade 2 titanium Rod | Titanium UNS R50400 Flat Bar Annealed |
Выберите Daxun, чтобы помочь вашему проекту взлететь.
DAXUN® Grade 2 Titanium Rod Features
DAXUN® Ti Grade 2 is a commercially pure (CP) titanium bar known for its standout features:
- Excellent general corrosion resistance in seawater
- Resistant to stress corrosion cracking in chloride and sour gas environments
- Excellent resistance to pitting, crevice, and erosion-corrosion
- High heat transfer efficiency
- Good formability and weldability
- Extremely low thermal expansion
- Moderate strength
Daxun Factory Advantages
Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.
Grade 2 Titanium Rod Production Method
Daxun specializes in producing high-quality titanium bars known for their exceptional performance. Additionally, we offer customized manufacturing services to meet specific requirements as outlined in the customer’s agreement.
- Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
Отчеты о тестировании
The test reports we provide include: Grade 2 Titanium Rod and Grade 2 Titanium Round Bar Factory Test Certificate, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, NABL Approved Laboratory Report, Destructive Test Report, Non-destructive Testing Report. (Daxun will provide according to customer requirements)
Grade 2 Rods Applications and Standards
Grade 2 Titanium Rods are widely used in the following industries under extreme corrosive conditions:
- Aerospace, military, oil and gas industry, marine engineering, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
- Specifications: ASTM B861, B862, B338 / ASME SB861, SB862, SB338
- Standards: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
Качество, доставка, проверка
Daxun ensures the reliability of Grade 2 Titanium Rods and Round Bars through rigorous quality assurance tests. These include tensile testing, chemical analysis, PMI for material consistency, micro and macro testing, IGC testing for corrosion resistance, ultrasonic flaw detection, and hardness and expansion evaluations.
Throughout production, Daxun carefully measures diameter, thickness, and surface quality, guaranteeing materials meet the highest standards and application requirements.
- Сроки доставки строго соответствуют договору.
- Поддержка сторонних агентств клиентов для посещения завода для проверки
- Поддержка бесплатных образцов для тестирования клиентов
- Поддержка инспекции на месте или видеоинспекции на заводе
Упаковка
Daxun Alloy обеспечивает наилучшее качество упаковки, поскольку она играет важную роль в международных перевозках, где товары проходят через различные каналы, чтобы достичь конечного пункта назначения, поэтому мы уделяем особое внимание упаковке. Мы упаковываем наши товары различными способами в зависимости от продукта. Мы упаковываем наши товары различными способами, такими как:
- Коробки и ящики
• Shrinkwrap
- Деревянные поддоны
- Деревянные ящики
Техническая поддержка
If you require additional technical assistance, our resident metallurgist and knowledgeable staff are ready to support you. At Daxun, we take pride in our certified testing laboratory, a first in the multi-metal and plastic inventory industry. This reflects our unwavering commitment to quality and reinforces our philosophy as a full-service supplier dedicated to meeting your needs.
Grade 2 bar and rod features
Daxun Grade 2 Titanium Rods help your brand improve quickly
- Titanium rod/bar
- Types of Grade 2 Titanium Rods
- Tolerances for Grade 2 Titanium Round Bars (BS EN ISO 286-2)
| Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of rod/bar, Bar and Tube. | |
| Products/Processing Standard | Grade/Size |
| Titanium rod/bar— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Thickness:( 0.0197”-6”)Max Width: 12 feet,Max Length: 50 feet) |
| AMS-T-9046 | |
| Titanium and Titanium alloy rod/bar | |
| Commercially pure titanium (CP) | |
| Code designation | Yield strength |
| minimum, ksi 1 / | |
| CP-1 | 70 |
| CP-2 | 55 |
| CP-3 | 40 |
| CP-4 | 25 |
| Alpha titanium alloys(A) | |
| Code designation | Composition |
| A-1 | 5A1-2.5Sn |
| A-2 | 5A1-2.5Sn(ELI) 2 / |
| A-3 | 6A1-2Cb-1Ta-0.8Mo |
| A-4 | 8A1-1Mo-1V |
| Alpha-beta titanium alloys(AB) | |
| Code designation | Composition |
| AB-1 | 6A1-4V |
| AB-2 | 6A1-4V(ELI) |
| AB-3 | 6A1-6V-2Sn |
| AB-4 | 6A1-2Sn-4Zr-2Mo |
| AB-5 | 3A1-2.5V |
| AB-6 | 8Mn |
| Beta titanium alloys(B) | |
| Code designation | Composition |
| B-1 | 13V-11Cr-3A1 |
| B-2 | 11.5Mo-6Zr-4.5Sn |
| B-3 | 3A1-8V-6Cr-4Mo-4Zr |
| B-4 | 8Mo-8V-2Fe-3A1 |
| Processing: | |
| Горячая прокатка | Холодная прокатка |
| Available Grades: | |
| CP Класс 1 | Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2) |
| CP Класс 2 | Grade 6Al-4V ELI (Formerly Grade 23) |
| Grade 7 | Grade 6Al-6V-2Sn (6-62) |
| Grade 19 | Grade 8Al-1Mo-1V (8-1-1) |
| Grade 5 (6Al-4V) | Grade 9 (3Al-2.5V) |
| Grade 6 (5Al-2.5Sn) | CP 3 класс |
| Application | |
| Химическая промышленность | Desalination Of Sea Water |
| Petrochemical Industry | Аэрокосмическая промышленность |
| Machining Field, Automobile Field | Mobile Phone Component Field. |
| Titanium Grade 2 Hex Bar | Titanium Gr 2 Hex Bar |
| Grade 2 Titanium Hexagonal Bar | |
| Gr 2 Titanium Alloy Hex Bar | |
| UNS R50400 Titanium Hexagonal Bar | |
| ASTM B348 Grade 2 Titanium Hex Bar | |
| Titanium Alloy Grade 2 Square Bar | Titanium Grade 2 Square Bar |
| Grade 2 Titanium Square Bars | |
| Gr 2Titanium Alloy Square Bar | |
| UNS R50400 Titanium Square Bar | |
| WERKSTOFF NR. 3.7035 Square Bar | |
| ASTM B348 Gr 2 Titanium Square Bars | |
| Titanium Grade 2 Rectangular Bar | Titanium Grade 2 Rectangular Bar |
| Ti. Alloy Gr2 Rectangular Bars | |
| Gr 2 Titanium Alloy Rectangular Bar | |
| UNS R50400 Titanium Rectangular Bars | |
| WERKSTOFF NR. 3.7035 Rectangular Bar | |
| ASTM B348 Gr 2 Titanium Rectangular Bar | |
| Titanium Grade 2 Flat Bars | Titanium Grade 2 Flat Bar |
| Gr 2Titanium Alloy Flat Bars | |
| Titanium Gr 2Flat Bars | |
| UNS R50400 Titanium Flat Bars | |
| WERKSTOFF NR. 3.7035 Flat Bars | |
| ASTM B348 Gr 2 Titanium Flat Bars | |
| Titanium Grade 2 Polished Bar | Titanium Grade 2 Polished Bar |
| Grade 2Titanium Polished Bars | |
| Gr 2Titanium Alloy Polished Bar | |
| UNS R50400 Titanium Polished Bars | |
| WERKSTOFF NR. 3.7035 Polished Bar | |
| ASTM B348 Gr 2 Titanium Polished Bar | |
| Titanium Grade 2 Threaded Bar | Titanium Gr 2 Threaded Bar |
| Grade 2Titanium Threaded Bars | |
| Ti. Alloy Grade 2 Threaded Bar | |
| UNS R50400 Titanium Threaded Bar | |
| WERKSTOFF NR. 3.7035 Threaded Bar | |
| ASTM B348 Gr 2 Titanium Threaded Bar |
| NOMINAL SIZE | h5 | h6 | h7 | h8 | h9 | H10 | H11 | h12 |
|---|---|---|---|---|---|---|---|---|
| DIAMETER mm | ||||||||
| ~ to 3 | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| over 3 to 6 | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| over 6 to 10 | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| over 10 to 18 | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| over 18 to 30 | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| over 30 to 50 | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| over 50 to 80 | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| over 80 to 120 | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| over 120 to 180 | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| over 180 to 250 | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
2nd grade bar type (3)
Информация доступна для ознакомления и скачивания
Титановый стержень
Daxun is a trustworthy titanium rod and bar manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium bars are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the Titanium rod have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
Последние проекты и продукты для горячих случаев
Сопутствующие товары (8)
What are Grade 2 Titanium rods?
Ti CP Grade 2 has greater tolerated levels of iron and oxygen and is frequently utilized due to its outstanding formability, moderate strength, and superior corrosion resistance. It has a minimum yield strength of 275 Mpa (40 ksi) and relatively low amounts of impurity elements, placing it in the strength range of Grades 1 to 3.
Grade 2 Titanium Rod Equivalent Grade
| nation | name | usually |
| Russia | VT1-0 (VT1-0) | Gorst 19807-91 |
| Germany | 3.7035 | Job Number (3.7035) |
| Europe | Titanium Grade 2 | ZH-10204 3.1 |
| Japan | Titanium Grade 2 | JIS H 4600 |
| People’s Republic of China | TA2 | GB/T 3621-2007 / GB/T 13810-2007 |
| USA | Titanium Grade 2 | ASTM B348 / B265 / B337,UNS R50400 |
Устойчивость к коррозии
Commercially pure (CP) titanium offers remarkable resistance to crevice corrosion in salt solutions, outperforming stainless steel. It retains its integrity against crevice corrosion at temperatures under 80 °C (176 °F), regardless of pH levels, even in environments with high chlorine concentrations.
Stress Corrosion Cracking (SCC)
Grade 2 titanium exhibits remarkable resistance to stress corrosion cracking. It performs exceptionally well in hot chloride solutions and is entirely immune to SCC in seawater, making it a dependable material for harsh environments.
Erosion Corrosion
Titanium exhibits exceptional durability in flowing seawater, withstanding velocities as high as 130 ft/sec (40 m/sec) without significant degradation. Even in the presence of abrasive particles like sand, its corrosion resistance remains largely unaffected, highlighting its reliability in demanding environments.
Hydrogen Embrittlement
When exposed to seawater, titanium absorbs minimal hydrogen, even at higher temperatures. However, absorption typically takes place only under certain specific conditions:
- pH levels below 3 or above 12
- Temperatures exceeding 80 °C (176 °F)
- A mechanism for hydrogen generation, such as galvanic coupling or an impressed current.
Bio-Corrosion
Titanium alloys exhibit complete immunity to microbiologically influenced corrosion. However, because they are non-toxic to marine organisms, biofouling can develop in seawater. This can be effectively managed through chlorination or by increasing the flow rate of water through heat exchangers.
Corrosion Fatigue
Unlike many materials, titanium maintains its fatigue performance in seawater. Fatigue endurance limits and crack growth rates are consistent, whether tested in air or seawater, making it a reliable choice for marine applications.
Galvanic Corrosion
Titanium ranks among the noble materials in the galvanic series, positioned near stainless steels, and generally serves as the cathode when paired with other metals. As a result, titanium remains resistant to galvanic corrosion but can increase corrosion in less noble metals. When paired with more noble substances, such as graphite, its passive properties become even stronger.
Fatigue Properties
Grade 2 Titanium Rod maintains its exceptional fatigue properties even in seawater. Its fatigue endurance limits and crack growth rates remain unchanged regardless of whether testing occurs in air or seawater, highlighting its consistent performance under varied conditions.
Свариваемость
CP2 Grade Titanium Rod is highly weldable when appropriate precautions are observed. Given its reactive nature, an inert gas shield must protect both the outer diameter (OD) and inner diameter (ID) during welding. Additionally, the rod should be completely free of grease or oil to ensure optimal weld integrity.
Grade 2 Titanium Rod is most often welded using either manual or automatic TIG methods, with or without filler wire. A low heat input is advised to limit the size of the heat-affected zone. Post-weld heat treatment is generally not required, simplifying the process while maintaining the rod’s key properties.
This revised version maintains the technical depth and original structure while improving clarity, readability, and flow. Let me know if you’d like further refinements!
| Working material: | 3.7035 / UNS R50400 |
| Diameter: | 3 – 400 mm |
| Lengths: | 2.000 – 4.000 mm |
| Versions: | Rolled, forged, annealed |
| Surfaces: | Turned, peeled, polished |
| Standards: | ASTM B 348, ASME SB 348, DIN 17862, ASTM F 67, NACE MR 0175, ISO 1515156-3, ISO 5832-2 |
Buy Grade 2 Titanium Rods/Rounds at Daxun
Are you in need of round rod material made from Grade 2 Titanium Alloy Rod-3.7035? At Daxun, we specialize in providing customized titanium rods tailored to your project’s specifications. As an experienced supplier, we are committed to supporting your needs with precision and reliability.
Our Grade 2 Titanium bars are available in diameters ranging from 2.0 mm to 400 mm. Tolerances and execution may vary based on the size of the bar. Smaller diameters are provided centerless ground with h7 tolerances, while larger sizes come with h9 or h11 tolerances. Contact Daxun to discuss your requirements or to request a customized project quote.
Buy Grade 2 Titanium Bars: Features and Specifications.
- Forged bars can be peeled or pre-machined. The material is available in a variety of specifications depending on the application and market needs.
- Our titanium bars typically meet various requirements and certifications, including ASTM B348 and ASTM F 67, DIN 17860, VD TÜV Table 230-3, and Nace MR 0175.
- Titanium round bars are often used where they have excellent corrosion resistance and good mechanical properties.
- Grade 2 titanium bars (3,7035) are therefore suitable for use as a construction material for equipment and devices, as they are easy to process.
Our Titanium Bar Material Services
- As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.
- We will be happy to provide you with a consultation and explain everything you need to know about obtaining titanium bar material, including which standards require greater attention for the components to be manufactured.
- If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.
- Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about the Grade 2 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.
Информация для заказа
When placing a purchase order, make sure to include the quantity, grade, type or category, API5L reference, as well as the thickness, width, and length of the product. If you have any specific requirements, like chemical composition, mechanical properties, heat treatment, additional testing, manufacturing methods, surface coatings, or end finishes, let us know so we can meet your needs.
Feel free to contact Daxun with your order details. We are committed to responding to your inquiry promptly.
The grade of titanium alloy you need depends on the project you are working on, as each grade has different benefits.
All grades of titanium alloy are extremely strong and corrosion resistant, which means they will continue to work well in the harshest conditions.
The higher grades of titanium alloy (5-12) are alloys designed for specific benefits. For example, grade 12 titanium alloy has excellent heat resistance, making it a perfect choice for shell and tube heat exchangers, hydraulic piping, and chemical industry equipment.
Grades 1-4 are pure titanium alloys, and they are a perfect choice if you need a weldable, ductile material for piping systems and tubing. You will find lower grades used in the marine and industrial industries.
If you are starting a project and are unsure which grade of titanium alloy is best for you, contact us today; we are more than happy to help you.
At DAXUN, we offer a wide range of titanium alloy grades from grade 1 to grade 12.
Grades 1-4 are pure titanium, while higher grades are alloys.
Alloy grades are popular for their high strength-to-weight ratio.
The most commonly used titanium alloy grade we find is grade 5. While still high in titanium, this grade is one of the most reliable because it can withstand temperatures up to 600°F and withstand extreme conditions.
Higher grades are favored by industries such as aerospace and marine industries for their wear and corrosion resistance.
Conversely, lower grades are primarily used for welding due to their lower strength.
To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.
Хотя марка титана несколько повышает стоимость, общая стоимость в основном определяется формой и видом титана, который вам нужен.
At DAXUN, we offer a wide range of titanium products, including rod/bars, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.
К сожалению, сложно назвать цену в интернете, не зная подробностей вашего проекта и того, для чего будет использоваться титан.
К счастью, наша команда экспертов всегда готова помочь и проконсультировать вас по вопросам, связанным с титаном. Отправив письмо по адресу [email protected], мы сможем ответить вам советом и точным предложением.
Обязательно укажите как можно больше информации о сорте, форме и количестве титана, который вам требуется, чтобы лучше понять ваши потребности.
The team at DAXUN is experienced, knowledgeable, and friendly. With years of experience in the industry, they know all about titanium, including its uses, benefits, and grades.
For regular updates on titanium, its uses, and its applications across industries, be sure to check out our blog. Our experts have written easy-to-follow guides that you can always refer to when you have questions.
If you’re still having trouble, feel free to contact us; we’ll be happy to help.
By sending an email to [email protected], you’ll receive a quick response. Make sure to include as much detail as possible in your question so we can recommend a suitable solution.
Пожалуйста, заполните форму на странице “Контакты” или позвоните нашему менеджеру по продажам по телефону “+86 13382898899”, мы свяжемся с вами в кратчайшие сроки. Наш WhatsApp работает в режиме онлайн, а электронная почта ([email protected]) будет проверена в течение 6 часов. На каждый запрос или сообщение мы ответим незамедлительно. Кроме того, каждую неделю мы делимся с нашими клиентами информацией о рынке
We can provide Titanium rod. samples for you to check the quality. Sample is free and you just pay the freight.
Мы экспортировали продукцию в более чем 42 страны, такие как Канада, Чили, Кувейт, Германия, Южная Корея, Саудовская Аравия, Сингапур и др.
Our MOQ is 1 ton for Titanium rod.
Пробные заказы могут быть доставлены в течение недели. Для обычных заказов требуется примерно две недели.