x
Sorgunuzu Bugün Gönderin
Hızlı Alıntı

Ti 15333 Ti-15V-3O-3Sn-3Al Alloy Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:Ti 15333 – UNS R58153
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of Ti 15333 titanium is approximately 4.76 g/cm3
  • Standards:ASTM B337
  • Softest Ti,High ductility, Very corrosion resistant, good cold formability

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

Ti 15333 Titanium Alloy Pipe Manufacturer

Ti-15-3-3-3, also known by its alloy designation Ti-15333, is a high-strength, metastable beta titanium alloy. Its chemical composition is approximately 15% Vanadium, 3% Chromium, 3% Aluminum, and 3% Tin, with the remainder being titanium. This unique composition gives it a distinct set of properties that differentiate it from the more common alpha-beta alloys like Ti-6Al-4V.

The primary advantage of Ti-15-3-3-3 lies in its excellent cold formability. In its solution-treated (annealed) condition, it is quite ductile and can be readily formed into complex shapes, including tubing, sheets, and wires, at room temperature. This is a significant benefit for manufacturing, as it reduces the need for high-temperature forming processes.

After forming, Ti-15-3-3-3 can be precipitation hardened (aged) to achieve very high tensile strength, often exceeding 1200 MPa (175 ksi). This combination of formability and high strength makes it a preferred material for demanding aerospace applications.

Key Characteristics of Ti-15-3-3-3 Tubing:

  • High Strength-to-Weight Ratio: Like all titanium alloys, it offers exceptional strength for its weight, which is critical in aerospace and high-performance motorsports.
  • Excellent Cold Formability: It can be easily manipulated into tubular and other structural components in its annealed state.
  • Good Weldability: The alloy can be welded using standard techniques, though post-weld heat treatment is often required to restore optimal mechanical properties.
  • Superior Corrosion Resistance: It exhibits excellent resistance to corrosion in many environments, including seawater and various chemical atmospheres.

Common Applications for Ti-15-3-3-3 Tubing:

Due to its specific property profile, Ti-15-3-3-3 tubing is predominantly used in high-performance sectors:

  • Havacılık ve uzay: Used for structural components, airframe parts, and high-strength fasteners.
  • Sporting Goods: High-end bicycle frames, golf club heads, and other performance equipment where strength and lightness are paramount.
  • Medical Devices: Occasionally used for surgical implants and instruments that benefit from its combination of strength, biocompatibility, and formability.

Veri

Element Content (%)
Titanium(Ti) 75
Vanadium(V) 15
Chromium(Cr) 3
Aluminum(Al) 3
Tin(Sn) 3
Iron(Fe) ≤ 0.25
Oxygen(O) ≤ 0.13
Carbon(C) ≤ 0.05
Nitrogen(N) ≤ 0.05
Hydrogen(H) ≤ 0.015

 

Mülkiyet Değer
Density (g/cm³) 4.8
Melting Point (°C) 1600-1650
Termal İletkenlik (W/m-K) 6.7-8.0
Specific Heat (J/kg·K) 510
Electrical Resistivity (μΩ·m) 1.30
Coefficient of Thermal Expansion (10^-6/K) 8.6-9.4

 

Mülkiyet Değer
Çekme Dayanımı (MPa) 1100-1200
Yield Strength (MPa) 950-1050
Uzama (%) 10-15
Reduction of Area (%) 25-35
Hardness (HB) 350-400
Fatigue Strength (MPa) 550-650
Shear Strength (MPa) 670-770
Impact Toughness (J) 40-60

Projenizin yükselmesine yardımcı olmak için Daxun'u seçin.

Daxun ile şimdi iletişime geçin

Advanced Production:Titanium seamless pipe

  • Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.
  • (The above is agreed upon by the manufacturer and the customer based on the specific situation)
Daxun ile şimdi iletişime geçin

Ti 15333 Titanium Tube Features

Ti 15333 Titanium Tube is the softest form of titanium and has the highest ductility. It has good cold forming characteristics and offers excellent corrosion resistance. It also has excellent welding properties and high impact toughness.

  • Softest Titanium
  • Highest Ductility
  • Excellent Corrosion Resistance
  • Good Cold Formability
Daxun ile şimdi iletişime geçin

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

Daxun ile şimdi iletişime geçin

Test Raporları

The test reports we provide include: Factory test certificate for Ti 15333 titanium welded pipe and Ti 15333 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

Daxun ile şimdi iletişime geçin

Applications and standards

Titanium 15333 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
Daxun ile şimdi iletişime geçin

Kalite, teslimat, denetim

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Ti 15333 Titanium Welded Pipe and Ti 15333 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • Teslimat süremiz kesinlikle sözleşmeye uygundur.
  • Müşterinin üçüncü taraf acentelerinin denetim için fabrikaya gitmesine destek olun
  • Müşteri testleri için ücretsiz numune desteği
  • Yerinde veya video fabrika denetimini destekleyin
Daxun ile şimdi iletişime geçin

Paketleme

Daxun Alloy, malların nihai varış noktasına ulaşmak için çeşitli kanallardan geçtiği uluslararası taşımacılıkta önemli bir rol oynadığı için en iyi ambalaj kalitesini sağlar, bu nedenle ambalajlamaya özel önem veririz. Ürünlerimizi ürüne bağlı olarak birçok şekilde paketliyoruz. Ürünlerimizi aşağıdaki gibi birçok şekilde paketliyoruz:
- Kutular ve kasalar
- Shrink ambalaj
- Ahşap paletler
- Ahşap kutular

Daxun ile şimdi iletişime geçin

Teknik Destek

Herhangi bir ek teknik yardıma ihtiyacınız olursa, yerleşik metalürji uzmanımız ve bilgili personelimiz size yardımcı olmaktan memnuniyet duyacaktır. Ayrıca Daxun, çoklu metal ve plastik envanter endüstrisinde bir ilk olan sertifikalı bir test laboratuvarına sahiptir. Bu, bize göre, kaliteye olan sarsılmaz bağlılığımızı ve tam hizmet tedarikçisi olarak felsefemizi göstermektedir.

Daxun Ti 15333 Titanium TUBE Let your brand improve rapidly

Ti 15333 titanium tube form (4)

  • Titanium seamless tubes are made by piercing and drawing solid titanium bars, and the hollow part of the tube is made by piercing or hot extrusion. Titanium seamless tubes are ideal for very large diameter to wall thickness ratios and have very good external dimensional tolerances.

  • Titanium welded pipe is a tubular product made of strip titanium that is roll formed and fusion welded along the longitudinal seam. The welding process used by Daxun Alloy does not use any filler metal during the welding process.

  • Titanium square tubes are drawn from round tubes or round tube billets and can be formed into right angles or rounded corners. They can also be cold extruded, which is efficient and low cost. The only disadvantage is that the tolerance will gradually increase.

  • Tubular products are welded and then re-drawn to final size. Welding and drawing is ideal for producing thick walled, large diameter tubes that cannot be welded directly to size but still offer cost savings over seamless tubes. All Daxun welded and drawn tubes are bright annealed.

Güncel sıcak vaka projeleri ve ürünleri

Ti 15333 Titanium pipe and tube
Ti 15333 Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
What is Ti-15-3-3-3 titanium alloy, and how is it different from Ti-6Al-4V?

Ti-15-3-3-3 (or Ti-15333) is a beta-rich titanium alloy known for its exceptional cold formability. Unlike the more common Ti-6Al-4V (an alpha-beta alloy), Ti-15-3-3-3 can be easily formed into complex shapes, like tubing, at room temperature. After forming, it can be heat-treated to achieve very high strength, making it ideal for applications that require both intricate manufacturing and high performance.

Can Ti-15-3-3-3 tubing be welded?

Yes, Ti-15-3-3-3 has good weldability. However, to achieve the best mechanical properties in the welded joint, a post-weld heat treatment (solution treating and aging) is typically recommended. This process restores the high strength that the alloy is known for.

What sizes and specifications of Ti-15-3-3-3 tubing does Daxun Alloys Co., Ltd. offer?

At Daxun Alloys Co., Ltd., we supply Ti-15-3-3-3 tubing in a wide range of outer diameters, wall thicknesses, and lengths to meet your specific project requirements. We offer tubing in both the annealed (easily formable) and aged (high-strength) conditions. Please contact us with your detailed specifications for a custom quote.

Titanyum sınıfı maliyeti etkiler mi?

Titanyum sınıfı maliyeti biraz artırsa da, toplam maliyet öncelikle ihtiyacınız olan titanyum şekli ve formu tarafından belirlenir.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

Ne yazık ki, projeniz ve titanyumun ne için kullanılacağı hakkında çok fazla bilgi sahibi olmadan çevrimiçi bir fiyat bulmak zordur.

Neyse ki, uzman ekibimiz titanyum ihtiyaçlarınız konusunda size yardımcı olmak ve tavsiyelerde bulunmak için her zaman burada. [email protected] adresine bir e-posta göndererek, size bazı tavsiyeler ve doğru bir fiyat teklifi ile geri dönebileceğiz.

İhtiyaçlarınızı daha iyi anlamak için ihtiyacınız olan titanyum sınıfı, şekli ve miktarı hakkında mümkün olduğunca fazla bilgi eklediğinizden emin olun.

Fiyat teklifi nasıl alınır veya piyasa bilgileri en kısa sürede nasıl anlaşılır?

Lütfen “Bize Ulaşın” sayfasındaki formu doldurun veya “+86 13382898899” adresinden satış müdürümüzü arayın, en kısa sürede sizinle iletişime geçeceğiz. WhatsApp'ımız çevrimiçidir ve e-posta ([email protected]) 6 saat içinde kontrol edilecektir. Her soruya veya mesaja derhal yanıt verilecektir. Ayrıca, her hafta müşterilerimizle pazar bilgilerini paylaşıyoruz

Biraz örnek alabilir miyim?

Kaliteyi kontrol etmeniz için paslanmaz çelik sac örnekleri sağlayabiliriz. Numune ücretsizdir ve siz sadece navlunu ödersiniz.

Şimdiye kadar hangi ülkelere ihracat yaptınız?

Kanada, Şili, Kuveyt, Almanya, Güney Kore, Suudi Arabistan, Singapur gibi 42'den fazla ülkeye ihracat yaptık.

MOQ'unuz nedir?

Paslanmaz çelik sac için MOQ'umuz 1 tondur.

Teslimat süreniz ne kadar?

Deneme siparişleri bir hafta içinde teslim edilebilir. Normal siparişler için bu süre yaklaşık iki haftadır.

Sorgunuzu Bugün Gönderin
Hızlı Alıntı