Daxun is an experienced manufacturer of CP-Grade 2 titanium plates

As China’s leading supplier of titanium, Daxun provides high-performance titanium plates to the world.
  • Titanium plate Grade:CP-2(2 класс)- UNS R50400
  • Titanium plate Production type: cold rolling, hot rolling, forging.
  • Titanium plate density Grade 2 has a density of 4.51 g/cm3
  • Standard: ASTM B265 Gr 2, ASME SB265, ASTM F67 AMS 4919
  • Features:High specific strength Lightweight Corrosion resistance

————Daxun produces titanium sheets in China to meet the diverse needs of customers!

A global leader in commercially pure titanium sheet supplies

DAXUN produces commercially pure titanium Grade 2 (UNS R50400) in thicknesses ranging from 0.5mm to 120mm. Grade 2 Titanium Plate (UNS R50400) is the “workhorse” of the commercially pure series. It combines high strength, and ductility, and is corrosion resistant for many industrial applications.

The Grade 2 Plate is a commercially pure titanium plate. It offers an excellent balance between strength and ductility. It has good impact strength and good weldability. It is corrosion resistant in highly oxidizing environments, alkaline media, brine solutions, weakly reducing environments, nitric acid, and wet chlorine. It also has excellent resistance to seawater and salt solutions.

Titanium’s low density, high strength-to-weight ratio, and corrosion resistance make it an ideal material for a wide range of applications, and it effectively resists stress corrosion cracking, pitting, and crevice corrosion in chloride solutions below 70°C. With a melting point of 1660°C, the plate is the alloy of choice for most industrial applications requiring good ductility and corrosion resistance.

Читать далее

Данные

Titanium Plate and sheet Type Plate, Sheet, Strip, Coils, Foils, Flats, Clad Plate, Plain Sheet, Rolling Sheet, Rolling Plate, Flat Shim, Flat Sheet, Shim Sheet, Rolls, Blank (Circle), sheared, annealed, soft annealed, descaled, tread plate, Checker Plate
Класс ASME SB265、AMS 4911、AMS 4919、AMS 4914、ASTM F67、ASTM F136, MSRR, AMS, BS
Titanium Alloy Gr 2 Plate Length 1000mm-13000mm or as required
Gr 2 Titanium Plate Width 1000mm-1219mm-1500mm-1800mm-2000mm-2500mm or as required
UNS R50400 Plate Thickness 0.3 to 120mm or as required
ASTM B265 Titanium Alloy Gr 2 Plate Process Hot/ Cold Rolled/forging
UNS R50400 Plate surface No.1, No. 2D, No. 2B, BA, No.3, No.4, No.6, No.7, 2B, 2D, BA NO(8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled ASTM B265 Titanium Alloy Gr 2 Plate, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc.
ASTM B265 Titanium Alloy Gr 2 Plate, Sheet and Strip JIS: N0, N2, N1, NW2200, NW2201, NW4400, NW5500, NW6002, etc
DIN:H-Ni99.96, H-Ni99.95, H-Ni99.92, H-Ni99.90, H-Ni99.5, H-Ni99, etc
Titanium grade 2 Sheet ASTM ASTM B265
Titanium grade 2 Sheet AMS AMS 4902
Tolerances of width and thickness EN 10258 (formerly DIN 59381),EN 10151 ASTM B265 Titanium Alloy Gr 2 strip for springs,EN 10088 ASTM B265 Titanium Alloy Gr 2 strip (general)
Cp Grade 2 Titanium Plate standards and approvals EN ISO 18286 EN 10051 EN 10088-1 ISO 15510 EN ISO 9445 ASTM A 480 ASTM A 959 ASME IID
Standard 3.7035 Plate & Sheet Sizes 1000 x 2000 mm, 1220 x 2440 mm, 1500 x 3000 mm, 2000 x 2000 mm, 2000 x 4000 mm
Cold rolled Gr 2 Titanium Plate 0.5-6.4 mm
Hot rolled Gr 2 Titanium Plate 3.0–60.0 mm
UNS R50400 Plate Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard ASTM B265 Titanium Alloy Gr 2 Sheet suppliers
Availability of Titanium Alloy Gr 2 Foil sizes Thickness : 8-100 microns (0.00031-0.004 in)
Width: Up to 500 mm (19.5 in)
Weight (in rolls) : Up to 50 kg (110 lb); e.g. approxi- mately 1400 m at 8 microns and ap- proximately 112 m at 100 microns.
Cutting To provide a comprehensive service, we use a variety of cutting methods, including:
Laser Plate Cutting,Plasma Plate Cutting,Oxy-propane Flame Cutting
Plasma profiles As per customer’s drawings
Value added services for Cp Grade 2 Titanium Plate Laser cutting, Waterjet cutting, Plasma cutting, Bending and mechanical processing, edge preparation, welding, sawing and shearing.
China Grade 2 Titanium Plate Manufacturer ASTM B265 Titanium Alloy Gr 2 Plate: material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width;Gr 2 Titanium Sheet: material under 3/16″ [5.00 mm] in thickness and 24″ [600 mm] and over in width;Alloy Titanium Grade 2 Clad plate: Alloy Titanium Grade 2 Clad plate is a composite steel plate made by bonding UNS R50400 Titanium Grade 2 Plate, etc.ASTM B265 Titanium Alloy Gr 2 Strip: cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width.
UNS R50400 Plate Origin КИТАЙ
Packing of DIN 3.7035 plate Bundles with waterproof cloth outside or plywood box
Test UT, SGS testing, TUV etc
Why buy UNS R50400 Sheet from DAXUN? Free quote、Free sample、EN 10204 3.1、Mill Test Certificate is supplied with shipment.、NABL Approved Lab Reports、Any third party inspection is accepted.、Tested to ASTM A923 Method “C” or ASTM G48 Method “A”.Minimum Nitrogen content and Ferrite Count Test
Typical Analysis (Weight %)
Элемент Grade 2/2H
Oxygen 0.25 max.
Азот 0.03 max.
Углерод 0.08 max.
Iron 0.030 max.
Hydrogen 0.015 max.
Residual Elements, Each 0.10 max.
Residual Elements, Total 0.40 max.
Титан Баланс
Недвижимость Annealed Temper
0.2% Yield (Rp = 0.2) 40 ksi (275 MPa) minimum
Tensile (Rm) 50 ksi (345 MPa) minimum
Elongation (2”gl) 20% minimum
Твердость 200 HV maximum
Плотность Магнитная проницаемость
0.163 lbs/in-3 Nonmagnetic
4.51 g/cm-3 Электрическое сопротивление
Beta Transus (+/- 25°F, +/- -3.9°C) 21 µΩ/in
1680°F 0.53 µΩ/m
915°C Модуль упругости
Теплопроводность 15.2 – 17.4 Msi
12.60 BTU hr-1 ft-1 °F-1 105 – 120 GPa
21.79 W m-1 °C-1 Typical values at room temperature of about 68 – 78°F (20 – 25°C)
alloy Grade 2 Hot Rolled Plate ASTM B265 Alloy Gr 2 Perforated Plate
ASTM B265 Alloy Gr 2 Plate 2b Finish CP Gr 2 Plate
alloy Grade 2 Plate Mill Finish Ti Grade 2 Din 3.7035 Thin Plate
UNS R50400 Grade 2 Cold Rolled Plate alloy Grade 2  Plate SHEET
Cp Grade 2 Titanium Plate UNS R50400 Grade 2 Rolling Plate
ASTM B265 Alloy Gr 2 Chequered Plate alloy Grade 2 Quarto Plate
Grade 2 Alloy Checker Plate 3.7035 Alloy Gr 2 Polished Plate
UNS R50400 Alloy Gr 2 Plate Mirror Finish Ti Grade 2 Grade Chequered Plate
Ti Grade 2 Din 3.7035 Chequer Plate UNS R50400 Alloy Gr 2 Tread Plate
Alloy Gr 2 Nickel Clad Plate Grade 2 Alloy Tisco Plate
3.7035 Checkered Plate ASTM B265 Alloy Gr 2 Laser Cut Plate
Alloy Gr 2 Custom Cut Plate Gr 2 Titanium Sheet
Gr 2 Titanium Embossed Plate Cp Grade 2 Titanium Plasma Cutting Plate
3.7035 Alloy Gr 2 Plate Brushed Finish Ti Grade 2 Superalloy Hot Rolled Sheet
Ti Grade 2 Superalloy 1/4 Inch Plate 3.7035 Perforated Sheet
Ti Grade 2 Grade 10mm Plate Alloy Gr 2 Cold Rolled Sheet

Выберите Daxun, чтобы помочь вашему проекту взлететь.

Свяжитесь с Daxun прямо сейчас

Custom Cutting

Daxun Alloy offers customized cutting solutions to minimize size loss, saving you time and processing costs. Cutting methods include:

  • Water jet cutting
  • Laser cutting
  • Sawing
  • Wire cutting, etc.
Свяжитесь с Daxun прямо сейчас

Advanced Production

Titanium Grade like #2 comes in cold rolled thicknesses from 0.3 mm to 6.0 mm. Hot-rolled thicknesses range from 4.76 mm to 155 mm. Plates can be heat treated or creep flattened. They are available in cut blank form, with further processing as per customer needs.

Свяжитесь с Daxun прямо сейчас

Quality, Inspection

Daxun performs multiple quality tests, including flattening, pitting, mechanical, hardness, and material identification tests. These ensure suitability for the required application. Diameter, thickness, and surface are measured during production.

Свяжитесь с Daxun прямо сейчас

Applications and Standards

Titanium grade 2 plate is lightweight and suited for industries like medical, aerospace, and chemical equipment. Its strength and corrosion resistance make it ideal for marine, chemical processing, and desalination. Common uses include oil and gas components, vessels, piping, heat exchangers, and more. It meets standards like ASTM B265 and AMS4911.

Свяжитесь с Daxun прямо сейчас

Техническая поддержка

Daxun offers technical support through its metallurgist and knowledgeable staff. We also have a certified testing laboratory, the first in the multi-metal and plastic inventory industry, reflecting our strong commitment to quality and full-service supply.

Свяжитесь с Daxun прямо сейчас

Быстрая доставка

We offer fast delivery, supported by seamless data integration, real-time logistics updates, and efficient scheduling. With processing centers near highways and waterways, we ensure quick responses, coordinated storage and transportation, and timely order fulfillment.

Свяжитесь с Daxun прямо сейчас

Быстрый ответ

Daxun saves customers time, materials, and costs by offering cost-optimized material suggestions and reducing expenses through continuous and nesting processing, leveraging its professional expertise.

Свяжитесь с Daxun прямо сейчас

Упаковка

Daxun titanium alloys prioritize quality packaging for international freight. Goods pass through various channels, so careful packaging is essential. We pack products using methods like boxes, crates, shrink wrap, wooden pallets, and wooden boxes, tailored to the product forms.

Grade 2 Titanium Plate Features

Высокая прочность
Устойчивость к коррозии
Термостойкость
Устойчивость к низким температурам
Защита окружающей среды
Легкий

Daxun Grade 2 Titanium sheet Let your brand improve rapidly

Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube.
Products/Processing Standard Grade/Size
Titanium Plate, Sheet, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Thickness:( 0.0197”-6”)Max Width: 12 feet,Max Length: 50 feet)
AMS-T-9046
Titanium and Titanium alloy sheet, plate
Commercially pure titanium (CP)
Code designation Yield strength
minimum, ksi 1 /
CP-1 70
CP-2 55
CP-3 40
CP-4 25
Alpha titanium alloys(A)
Code designation Composition
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
Alpha-beta titanium alloys(AB)
Code designation Composition
AB-1 6A1-4V
AB-2 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
Beta titanium alloys(B)
Code designation Composition
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
Processing:
Горячая прокатка Холодная прокатка
Available Grades:
CP Класс 1 Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP Класс 2 Grade 6Al-4V ELI (Formerly Grade 23)
Grade 7 Grade 6Al-6V-2Sn (6-62)
Grade 19 Grade 8Al-1Mo-1V (8-1-1)
Grade 5 (6Al-4V) Grade 9 (3Al-2.5V)
Grade 6 (5Al-2.5Sn) CP 3 класс
Application
Химическая промышленность Desalination Of Sea Water
Petrochemical Industry Аэрокосмическая промышленность
Machining Field, Automobile Field Mobile Phone Component Field.

Информация доступна для ознакомления и скачивания

Daxun is a trustworthy metal manufacturer

Daxun ensures high-quality alloy products, certified by ISO9001, SGS, CE, and OQC standards. Strict quality control minimizes defects, guaranteeing durability, excellent performance, and reliability in every product. As a professional manufacturer, we are committed to producing high-quality goods you can trust.

Titanium plate and sheet Grade 2 / UNS R50400

Why Us ?

  • We are adaptable and can customize hundreds of of specific product forms, and we handle every step of the process. This may include planning, budgeting, raw material preparation, inspection, and finished product delivery.
  • Our technological advantages ensure that our customers have access to high-quality materials that meet their specific project needs.
  • We have established supply chains, research laboratories, and subsidiaries to ensure that every order is produced and delivered to the highest standards of relevant industries.
  • When you buy from us, you get more than just raw material products, but also excellent service and technical support.

Description 

  • Grade 2 Titanium Plate, commonly known as Ti-CP (Commercially Pure Titanium Grade #2), is a non-alloyed metal plate known for its high corrosion resistance, formability, and mild strength. It is one of the commercially pure titanium grades, which are classed according to their composition and mechanical characteristics.

Обрабатываемость

  • The Grade 2 is easily machinable using conventional processes. Machinability is similar to that of austenitic stainless steel. Just like stainless steel, it has limited thermal conductivity and poor heat dissipation, hence a substantial amount of coolant is needed. Sharp tools are essential. Cuts should be deep and continuous, with slow cutting speeds.

 

Свариваемость

  • Grade 2 titanium plates can be easily welded using GMAW and GTAW processes. Preheat and post-weld heat treatment are not required. The area around the weld must be clean and free of oil and shop dirt, including pencil marks. Abrasive cleaning, solvent cleaning, or pickling with nitric and hydrofluoric acid solutions are options.
  • Use AWS ERTi-2 compatible filler metal. The gas barrier should be low in hydrogen, oxygen, and nitrogen, all of which readily dissolve in titanium and cause embrittlement.
Industries & Applications
  • Grade 2 titanium alloys have a lower density, making them ideal for applications where weight is a concern. This grade of the alloys are industrial components that are commonly used in oil and gas components, reaction and pressure vessels, piping systems, heat exchangers, linings, flue gas desulfurization systems and a variety of other industrial applications. Continuous service temperatures can reach 800°F, while intermittent service temperatures can reach 1000°F.
Качество

  • Industrial and aerospace quality titanium plates are available in a wide range of specifications and tolerances for applications ranging from ballistic armor to structural components to engineered hollow fan blade systems where exceptional flatness and specification control are critical.
Устойчивость к коррозии
  • The corrosion resistance of C.P. titanium grade is due to the formation of a strongly adherent, stable, protective oxide film in the presence of oxygen. Titanium grade 2 is highly corrosion-resistant to seawater and marine atmospheric corrosion. The plate is resistant to attack from wet chlorides and metal chlorides, chlorite and hypochlorite solutions, nitric and chromic acids, organic acids, and many gaseous industrial uses.
Heat Treatment
  • Titanium Grade 2 sheet has excellent ductility and may be cold-produced. To eliminate cold forming issues, use a minimum bend radius of 2T for material less than 0.070 inches thick and 2.5T for material larger than 0.070 inches.
  • The material is also simple to machine, post heat treatments and has good weldability. Hot work should be done between 400°F and 600°F.
  • Welding Grade 2 titanium can be done using a variety of techniques, including MIG and TIG. Inert gas shielding can prevent oxygen pickup and embrittlement in the weld region.
How to get a quote or understand the market information ASAP?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email ([email protected]) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week.

Могу я получить несколько образцов?

We can provide samples for you to check the quality. The sample is free and you just pay the freight.

В какие страны вы уже экспортировали свою продукцию?

Мы экспортировали продукцию в более чем 42 страны, такие как Канада, Чили, Кувейт, Германия, Южная Корея, Саудовская Аравия, Сингапур и др.

Какова ваша MOQ?

Our MOQ is 1 ton for titanium sheet.

Как долго длится доставка?

Пробные заказы могут быть доставлены в течение недели. Для обычных заказов требуется примерно две недели.

Отправьте запрос сегодня
Быстрая цитата