Manufacturing of titanium welded pipes and seamless titanium pipes

The Foundation: Extracting Pure Titanium Before any pipe can be made, titanium must be extracted from its ores, primarily rutile and ilmenite. This is achieved through the Kroll process, a complex and energy-intensive procedure that produces the foundational material for all titanium products. Chlorination:The ore is first reacted with chlorine