CE Certification 2205 Stainless Steel Round Bar
As a leading stainless steel supplier and exporter in China, Daxun supplies stainless steel barsRod (Round Bar)to all over the world.
- Grade: AISI 2205-S32205-S31803
- Manufacturing: hot rolled, cold drawn, forged
- Standards: ASTM, ASME, GB, DIN, JIS, ISO
- High resistance to stress corrosion cracking, fatigue and erosion
- Higher thermal conductivity and lower thermal expansion than austenitic steels
- Excellent and uniform resistance to pitting and crevice corrosion
- Good resistance to sulfide stress corrosion cracking
Global leader in stainless rod and Round Bar fabrication services
Product Specifications
- ASTM A479 UNS S32205 Bar
- ASTM A276 F60 Duplex Round Bar
- ASTM A479 UNS S32205 Round Bar
- UNS S32205 Duplex Round Bar
- Duplex Steel S32205 Bar Manufacturer from China
Overview
Duplex Steel S32205 rods are used in many industries because of their great properties and versatility. S32205 is a duplex stainless steel that has both austenitic and ferritic characteristics. This gives it high strength, excellent corrosion resistance, and cost efficiency.
Composition and Properties
Duplex Steel S32205 has about 22% chromium, 5-6% nickel, 3% molybdenum, and high nitrogen. This combination makes it very resistant to corrosion and very strong. Its structure has both austenite and ferrite, which makes it stronger and better than regular austenitic or ferritic stainless steels.
Устойчивость к коррозии
One of the main features of S32205 rods is their resistance to different types of corrosion. They are highly resistant to pitting and crevice corrosion in chloride environments, which makes them perfect for use in corrosive areas like chemical processing, marine settings, and the offshore oil and gas industry.
Our network of service centers stock stainless steel bar products for fast, ready supply of bar in common sizes and alloys.We also produce custom-sized stainless steel rods and can arrange inventory schedules for quick turnaround in a timely manner if quantities are below factory minimums.Daxun Alloys stocks stainless steel round bars with diameters ranging from 1/16″ to 26″. Round bars are available in nearly every grade of stainless steel, including 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205, and Alloy 20. Heat treated stainless steel round bars are offered in 17-4PH, H900 temper (on request), H1025, H1150, Double H1150, and H1150M. Other heat-treated tempers can be manufactured upon request. We stock the following 400 series stainless steels: 410, 430, and 416. We also carry 303, 304, and 316/L precision and bearing quality stainless steel round bars. The majority of our inventory consists of our unique machined bar grades: stainless steel round bars that are melted to consistent standards to increase machinability and lower total cost per component. Our stainless steel bar processing machinery allows Daxun Alloys to produce to our customers’ exact specifications.
Данные
- Параметр
- Ingredients
- Механические свойства
- ФИЗИЧЕСКИЕ СВОЙСТВА
- Все эквиваленты
- Типы
| Product Parameters: Stainless Steel rod | |
| Specifications | ASTM A276, ASME SA276 / ASTM A479 ASME SA479 |
| Dimensions | EN, DIN, JIS, ASTM, BS, ASME, AISI |
| SS 2205/S32205 Round Bars | Outside Diameter in the range of 4mm to 500mm |
| SS 2205/S32205 Bright Bars | Outside Diameter in the range of 4mm to 100mm |
| SS 2205/S32205 Hex Bars | 18mm – 57mm (11/16″ to 2-3/4″) |
| Finish | Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
| Длина | 1 to 6 Meters, Custom Cut Lengths |
| Form | Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc. |
| Класс | C | Mn | Si | P | S | Cr | Mo | Ni | N |
| 2205 | 0.03 | 2 | 1 | 0.03 | 0.02 | min: 21.0 | min: 2.5 | min: 4.5 | min: 0.08 |
| (S31803) | max | max | max | max | max | max: 23.0 | max: 3.5 | max: 6.5 | max: 0.20 |
| 2205 | 0.03 | 2 | 1 | 0.03 | 0.02 | min: 22.0 | min: 3.0 | min: 4.5 | min: 0.14 |
| (S32205) | max | max | max | max | max | max: 23.0 | max: 3.5 | max: 6.5 | max: 0.20 |
| Класс | Прочность на разрыв | Предел текучести | Удлинение | Твердость | |
| (МПа) мин | 0.2% Доказательство | (% в 50 мм) мин | |||
| (МПа) мин | Rockwell C (HR C) | Brinell (HB) | |||
| UNS S31803 / 2205 | 621 | 448 | 25 | 31 max | 293 max |
| UNS S32205 / 2205 | 621 | 448 | 25 | 31 max | 293 max |
| Grade 2205 | Плотность | Elastic | Mean Co-eff of Thermal | Thermal | Specific | Electrical | |||
| (kg/m3) | Modulus(GPa) | Expansion (μm/m/°C) | Conductivity (W/m.K) | Heat | Resistivity | ||||
| 0-100°C | 0-315°C | 0-538°C | at 100°C | at 500°C | 0-100°C( J/kg.K) | (nΩ.m) | |||
| UNS S32205 / UNS S31803 | 782 | 190 | 13.7 | 14.2 | – | 19 | – | 418 | 850 |
| Класс | КИТАЙ | UNS | Старая Британия | Евронорм | Swedish SS | Japanese JIS | ||
| Нет | BS | En | Нет | Имя | ||||
| 2205 | 022Cr23Ni5Mo3N | S31803 / S32205 | 318S13 | – | 1.4462 | X2CrNiMoN22-5-3 | 2377 | SUS 329J3L |
| Stainless Steel 2205/S32205/S31803 Bright Bar | SS 2205/S32205/S31803 Bright Bar |
| 2205/S32205/S31803 SS Bright Bar | |
| Stainless Steel 2205/S32205/S31803 Bright Bar | |
| UNS S2205/S32205/S3180300 SS Bright Bar | |
| WERKSTOFF NR. 1.4462 Bright Bar | |
| ASTM A276 2205/S32205/S31803 Stainless Steel Bright Bar | |
| Stainless Steel 2205/S32205/S31803 Hex Bar | SS 2205/S32205/S31803 Hex Bar |
| 2205/S32205/S31803 SS Hexagonal Bar | |
| 2205/S32205/S31803 Stainless Steel Hex Bar | |
| UNS S2205/S32205/S3180300 SS Hexagonal Bar | |
| ASTM A276 2205/S32205/S31803 Stainless Steel Hex Bar | |
| Stainless Steel 2205/S32205/S31803 Square Bar | SS 2205/S32205/S31803 Square Bar |
| 2205/S32205/S31803 SS Square Bars | |
| 2205/S32205/S31803 Stainless Steel Square Bar | |
| UNS S2205/S32205/S3180300 SS Square Bar | |
| WERKSTOFF NR. 1.4462 Square Bar | |
| ASTM A479 2205/S32205/S31803 Stainless Steel Square Bars | |
| Stainless Steel 2205/S32205/S31803 Rectangular Bar | SS 2205/S32205/S31803 Rectangular Bar |
| 2205/S32205/S31803 SS Rectangular Bars | |
| 2205/S32205/S31803 Stainless Steel Rectangular Bar | |
| UNS S2205/S32205/S3180300 SS Rectangular Bars | |
| WERKSTOFF NR. 1.4462 Rectangular Bar | |
| ASTM A276 2205/S32205/S31803 Stainless Steel Rectangular Bar | |
| Stainless Steel 2205/S32205/S31803 Flat Bars | SS 2205/S32205/S31803 Flat Bar |
| 2205/S32205/S31803 SS Flat Bars | |
| 2205/S32205/S31803 Stainless Steel Flat Bars | |
| UNS S2205/S32205/S3180300 SS Flat Bars | |
| WERKSTOFF NR. 1.4462 Flat Bars | |
| ASTM A276 2205/S32205/S31803 Stainless Steel Flat Bars | |
| Stainless Steel 2205/S32205/S31803 Polished Bar | SS 2205/S32205/S31803 Polished Bar |
| 2205/S32205/S31803 SS Polished Bars | |
| 2205/S32205/S31803 Stainless Steel Polished Bar | |
| UNS S2205/S32205/S3180300 SS Polished Bars | |
| WERKSTOFF NR. 1.4462 Polished Bar | |
| ASTM A476 2205/S32205/S31803 Stainless Steel Polished Bar | |
| Stainless Steel 2205/S32205/S31803 Threaded Bar | SS 2205/S32205/S31803 Threaded Bar |
| 2205/S32205/S31803 SS Threaded Bars | |
| 2205/S32205/S31803 Stainless Steel Threaded Bar | |
| UNS S2205/S32205/S3180300 SS Threaded Bar | |
| WERKSTOFF NR. 1.4462 Threaded Bar | |
| ASTM A276 2205/S32205/S31803 Stainless Steel Threaded Bar |
Выберите Daxun и сделайте своих клиентов довольными.

Быстрый ответ
We provide timely and fast delivery of 2205 stainless steel bar products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading to ensure that the task is completed on time.
Преимущества Daxun
- Varieties: We offer a wide range of sizes and grades, including 300 series, 400, 600 series, and more.
- Flexibility: Whether you need hot-rolled or cold-drawn bars, our stainless steel bar lengths are designed to meet your specific project requirements.
- Quality Standards: Our stainless steel tubes meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
- Custom Orders: Looking for special sizes of stainless steel bars? We offer a variety of stainless steel bar customization options with competitive prices and convenient online ordering.
2205 Stainless Steel Rod packaging
We pay attention to every process to ensure quality. The packaging we usually adopt is to pack 2205 stainless steel round bars in environmentally friendly plastic bags and then put them into fumigation-free wooden boxes or wooden pallets. Customized packaging, such as OEM, can also be negotiated. We provide almost everything to meet your round bar packaging requirements. We attach great importance to packaging. The round bars are packed in wooden corrugated boxes, wrapped with plastic packaging and bubble film on the outside.
Качество, доставка, проверка
- Daxun conducts several quality assurance tests, including flattening tests, pitting resistance tests, mechanical tests, hardness tests, material identification, and expansion tests. These tests ensure that the materials meet all required standards for their intended applications.
- We support customer inspections by third-party agencies, provide free samples for testing, and offer both on-site and video factory inspections.
Техническая поддержка
Если вам потребуется дополнительная техническая помощь, наш постоянный металлург и компетентный персонал будут рады помочь. Кроме того, Daxun может похвастаться сертифицированной испытательной лабораторией - впервые в отрасли производства инвентаря из нескольких металлов и пластика. Это, по нашему мнению, демонстрирует нашу неизменную приверженность качеству и философию поставщика полного цикла.
2205 Stainless Steel Rod Ordering Information
When placing an order for 2205 Stainless Steel Round Bars, please include the following details:
- Quantity
- PSL grade
- Type or category
- API5L reference
- Diameter
- Отделка поверхности
- Длина
- Any other specific requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish, or end treatment.
- Payment terms, including deposit requirements and available options such as T/T and L/C.
All bars are solution bright annealed.
2205-S32205-S31803 Stainless Steel Rod Features
Сплав Daxun Пусть ваш бренд быстро улучшается
- Галерея
- Состояние доставки
- Age Hardening
| Выбор государства доставки | Состояние поверхности |
| Кованые | Black |
| Полированный | |
| Горячекатаный | Black |
| Полированный | |
| Яркий | |
| Маринованные | |
| Холодная вытяжка | Полированный |
| Яркий | |
| Примечание: | |
| 1. Если вам требуется другое состояние доставки, чем перечисленные выше, пожалуйста, подтвердите с нами. | |
| 2. В случае запроса или заказа, пожалуйста, сообщите нам о любых дополнительных требованиях, не указанных здесь. | |
| Material in the solution annealed condition may be age hardened as follows:-*Denotes Double Overaged | ||||||||||||
| Condition | H900 (H480) | H925 (H495) | H1025 (H550) | H1075 (H580) | H1100 (H595) | H1150 (H620) | H1150M (H620M)* | Plus | H1150D (H620D)* | Plus | ||
| Heat to | ±15oF | 900oF | 925 oF | 1025oF | 1075oF | 1100oF | 1150oF | 1400oF | 1150oF | 1150oF | 1150oF | |
| ±9oC | 480oC | 495oC | 550oC | 580oC | 595oC | 620oC | 760oC | 620oC | 620oC | 620oC | ||
| Hold for Hours | 1 | 4 | 4 | 4 | 4 | 4 | 2 | 4 | 4 | 4 | ||
| Cool to Below | Air | Air | Air | Air | Air | Air | Air | Air | Air | Air | ||
| 90oF (32oC) | ||||||||||||
Информация доступна для ознакомления и скачивания
Stainless Steel Rod Production
Daxun is a trustworthy stainless steel rod and bar manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless rod are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 2205 Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
Последние проекты и продукты для горячих случаев





Сопутствующие товары (12)
2205 Duplex Stainless Steel Round Bar is a strong type of steel that contains 22% chromium, 3% molybdenum, and 5-6% nickel. It has both ferritic and austenitic properties, which makes it stronger than regular stainless steels. 2205 has twice the yield strength of standard stainless steels and is very resistant to corrosion in tough environments. It also has good fatigue strength and resists stress cracking, pitting, crevice corrosion, and erosion, making it useful for challenging applications.
- Chemical processing, transport and storage – pressure vessels, tanks, piping, and heat exchangers
- Oil and gas exploration and processing equipment – piping, tubing, and heat exchangers
- Marine and other high chloride environments
- Effluent scrubbing systems
- Pulp and paper industry – digesters, bleaching equipment, and stock-handling systems
- Cargo tanks for ships and trucks
- Food processing equipment
- Biofuels plants
- ASTM/ASME: A240 UNS S32205/S31803
- EURONORM: 1.4462 X2CrNiMoN 22.5.3
- AFNOR: Z3 CrNi 22.05 AZ
- DIN: W.Nr 1.4462
We can provide 2205 Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.
КОРРОЗИОННАЯ СТОЙКОСТЬ
- High amounts of chromium, molybdenum, and nitrogen make Duplex 2205 Stainless Steel more corrosion-resistant than 316 and 316L grades.
- Provides protection against pitting and crevice corrosion, even in tough or acidic environments.
- Resistant to chloride stress corrosion cracking.
- Handles temperatures up to 302°F (150°C).
- Ferrite in its structure helps it work well in caustic conditions.
- Suitable for challenging environments.
HEAT RESISTANCE
- Duplex 2205 has good oxidation resistance at high temperatures, similar to other duplex stainless steels.
- Becomes brittle when exposed to temperatures above 572°F (300°C), even for short periods.
- Not recommended for use at temperatures above 572°F (300°C).
Welding Characteristics
- Duplex 2205 has good weldability.
- Should not be welded without filler metal, as this can lead to excessive ferrite content.
Heat Treatment
- Annealing temperature range is between 1868 to 2012°F (1020 to 1100°C).
- Cannot be hardened by heat treatment but does work-harden.
- Special attention is needed to handle a higher thermal expansion rate to avoid warping and distortion.
PROCESSING – HOT FORMING
Most producers suggest keeping the hot forming temperature for Duplex 2205 between 2010 and 2100°F (1100 to 1150°C). If the shape isn’t compact, the edges can cool faster than the center, which might cause cracking.
PROCESSING – COLD FORMING
Duplex 2205 can be formed in different ways, but its high strength makes it more challenging. Even with strong equipment, you need to account for extra spring-back because of its strength.
MACHINABILITY
Duplex 2205 stainless steel is a bit harder to machine than 300 series stainless steels. It needs more cutting force, which makes tools wear out faster. Here are some machining tips:
- Use a strong, rigid machine with solid tool and workpiece mounts.
- Keep tool extensions short to reduce vibration.
- Avoid a large tool nose radius to keep the carbide sharp but strong.
- Plan the machining so the cut depth stays below the hardened layer from previous passes.
Тестирование
- Here are the tests we conduct for Duplex 2205 Stainless Steel:
- Positive material identification test
- Intergranular corrosion test
- Pitting resistance test
- Mechanical test
- Chemical test
- Macro/micro test
- Flattening/flaring test
Documents provided
- Heart treatment chart, quality assurance plan, commercial invoice, certificate of origin, raw material test report, material traceability report etc are a few essential documents provided to the buyers. Additionally, the other documents like MTC as per EN 10204/3.1B, TC like radiography test report and the third party test report are provided.
2205-s32205-S31803 grade stainless steel round bars
We provide important documents such as:
- Heat treatment chart
- Quality assurance plan
- Commercial invoice
- Certificate of origin
- Raw material test report
- Material traceability report
Documents Provided
We provide important documents such as:
- Heat treatment chart
- Quality assurance plan
- Commercial invoice
- Certificate of origin
- Raw material test report
- Material traceability report
We also provide other documents like Material Test Certificate (MTC) according to EN 10204/3.1B, radiography test report, and third-party test report.
Our stainless steel round bars come in many sizes. You can choose the grade you need, with lengths from 500mm to 6 meters and diameters from 3mm to 500mm. We offer both metric and imperial sizes. If you need custom sizes, we provide free cuts using advanced bandsaws to make sure it’s done right.
Our MOQ is 1 ton for 2205 Stainless Steel Rod.