Duplex 2205 (UNS S32205 / S31803) Stainless Steel Pipe Manufacturers and Stockists

Являясь ведущим китайским поставщиком и экспортером труб и трубок из нержавеющей стали, компания Daxun поставляет трубы из нержавеющей стали по всему миру.
  • Grade: AISI 2205/S32205-S31803
  • Manufacturing: hot-rolled, cold-rolled, forged, welded
  • Стандарты: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Type: general seamless steel pipe
  • Диаметр: от труб малого диаметра до труб большого диаметра
  • Thickness: thin-walled pipe and thick-walled pipe
  • Surface: pickled AP, polished, bright EP, annealed BA, etc.
  • Длина: 3000 мм, 6000 мм, 9000 мм и т.д.

Global leader in stainless steel tube fabrication services

Duplex 2205 stainless steel is a versatile and widely used alloy that offers a unique combination of high strength, good corrosion resistance, and excellent weldability. Its high chromium content and balanced austenitic-ferritic structure make it an ideal choice for various applications, including chemical processing, oil and gas, and marine environments. The alloy’s superior performance in high chloride and oxidizing environments, along with its resistance to pitting, ensures long-lasting durability and reliability, making it a preferred material for demanding industrial applications.

Global leader in stainless steel tube fabrication services

Your Trusted Partner in Stainless Steel Tubing Solutions

Daxun Alloy specializes in producing high-quality stainless steel and titanium tubing. Among our products is Alloy 2205, a duplex stainless steel enhanced with nitrogen to provide exceptional corrosion resistance, especially in welding applications. In its annealed state, Alloy 2205 offers twice the strength of standard austenitic stainless steels and performs better than Alloy 316 in many environments. Commonly referred to as UNS S31803 or UNS S32205, Alloy 2205 contains 22% chromium, 3% molybdenum, and 5-6% nickel, making it highly resistant to stress corrosion cracking, pitting, and harsh chloride conditions.

At Daxun Alloy, we supply Duplex 2205 tubing in various types, including seamless, welded, precision, and capillary forms. All our products meet international standards like ASTM, ASME, ISO, UNS, and EN, ensuring superior quality and reliability.

We have been a trusted manufacturer of Duplex 2205 stainless steel pipes since 1999. Our inventory includes over 25,000 tonnes of pipes in a wide range of shapes, sizes, and finishes. This makes us one of the largest stockholders of ASTM A789 UNS S32205 pipes in China. As an ISO 9001-certified company, we offer Duplex 2205 seamless and welded pipes, polished and electro-polished pipes, and square, rectangular, and round options.

In addition to manufacturing, we also distribute pipes sourced from leading SAF 2205 producers in the United States and Europe. We provide Duplex 2205 pipes in specifications such as SCH 40, SCH 80, SCH 160, SCH 10, SCH XS, and SCH XXS, ensuring we meet diverse customer requirements.

With competitive prices and consistent stock availability, Daxun Alloy is proud to be your go-to supplier for premium-quality Duplex 2205 stainless steel pipes.

Читать далее

Данные

Stainless Steel S32205/S31803 Tube Standards SA 789 alloy 2205, astm a790 duplex 2205, a790 gr 2205ASTM A213, ASTM A249, ASTM A269, ASME SA213, ASME SA249, ASME SA269, EN 10216-5 TC1 / TC2, PED 97/23/EC, AD 2000, NACE MR0175/ISO 15156
S32205/S31803 SEAMLESS Stainless Steel Aerospace Tubing AMS 5557, AMS 5897 (Canceled & non-current specs include MIL-T-8808, MIL-T-8973)
S32205/S31803 WELDED & DRAWN Stainless Steel Aerospace Tubing AMS 5556, AMS 5575 (Canceled & non-current specs include MIL-T-6737, MIL-T-8606, MIL-T-8808)
Stainless Steel S32205/S31803 Seamless Tube Size От 3,35 мм OD до 101,6 мм OD
Stainless Steel S32205/S31803 Welded Tube Size 6,35 мм наружный диаметр До 152 мм наружный диаметр
Swg & Bwg 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg.
Stainless Steel S32205/S31803 tubing wall thickness 0.020″ –0.220″, (special wall thicknesses available)
SS S32205/S31803 tube Length Одинарная случайная, двойная случайная, стандартная и обрезанная длина
S32205/S31803 Stainless Steel Tube Finish Полированный, AP (отожженный и травленый), BA (яркий и отожженный), MF
Stainless Steel S32205/S31803 tube Form Round, Coil, Square, Rectangular, Boiler, Hydraulic, Straight or ‘U’ bent Tubes, Hollow, LSAW Tubes Etc.
Stainless Steel S32205/S31803 Tube Type Бесшовные, ERW, EFW, сварные, изготовленные
Electropolished (EP) Электрополированный для систем сверхвысокой чистоты
Non-Electropolished (BA) Отожженный или (AP) Отожженный и травленый для высокой чистоты, (CFOS) Очищенный для работы с кислородом или коррозионными системами
I.D. Surface Finish Options 5, 7 и 10 мкн. Ra
JIS 8A - 250A
Допуски В соответствии с: ASTM: A269 & A632, JIS: G 3459
S32205/S31803 stainless steel tubing End Плоский конец, скошенный конец, резьбовой конец, концы подходят для орбитальной сварки
Marking All S32205/S31803 Stainless Steel tubes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.)
S32205/S31803 stainless steel tubing Application Нефтяные трубки, газовые трубки, жидкостные трубки, трубки для котлов и теплообменников
Value Added Service Чертеж и расширение в соответствии с требуемым размером и длиной, полировка (электро- и коммерческая), отжиг и травление, гибка, механическая обработка и т.д.
Specialize in Stainless Steel S32205/S31803 Capillary Tube & Other Odd Size
Stainless Steel S32205/S31803 Heat Exchanger & Condenser Tubes
Stainless Steel S32205/S31803 Hydraulic tubing with OD up to 50.8 mm (2.0 in.) are delivered in bright annealed condition
Stainless Steel S32205/S31803 hydraulic tube with OD larger than 50.8 mm are supplied in the annealed and pickled condition, Or in polished condition
Marking & Traceability Each Stainless Steel S32205/S31803 Tubing is traceable to its producing mill and heat by an identification number etched within 24″ (610mm) of one end.
S32205/S31803 stainless steel tubing Test Certificate Сертификат испытаний изготовителя в соответствии с EN 10204 3.1 B
Сертификат лабораторных испытаний из утвержденной правительством лаборатории.
Под контролем третьей стороны
S32205/S31803 stainless steel tubing Testing & Inspection Визуальный осмотр - Измерение шероховатости поверхности - Испытание на утечку гелия - Сканирующая электронная микроскопия (SEM) - Оже-электронная микроскопия (AES) - Избирательная спектроскопия для химического анализа (ESCA или XPS) - Испытание частиц - Испытание на влажность
Класс C Mn Si P S Cr Mo Ni N
2205 0.03 2 1 0.03 0.02 min: 21.0 min: 2.5 min: 4.5 min: 0.08
(S31803) max max max max max max: 23.0 max: 3.5 max: 6.5 max: 0.20
2205 0.03 2 1 0.03 0.02 min: 22.0 min: 3.0 min: 4.5 min: 0.14
(S32205) max max max max max max: 23.0 max: 3.5 max: 6.5 max: 0.20
Класс Прочность на разрыв Предел текучести Удлинение Твердость
(МПа) мин 0.2% Доказательство (% в 50 мм) мин
(МПа) мин Rockwell C (HR C) Brinell (HB)
UNS S31803 / 2205 621 448 25 31 max 293 max
UNS S32205 / 2205 621 448 25 31 max 293 max
Grade 2205 Плотность Elastic Mean Co-eff of Thermal Thermal Specific Electrical
(kg/m3) Modulus(GPa) Expansion (μm/m/°C) Conductivity (W/m.K) Heat Resistivity
0-100°C 0-315°C 0-538°C at 100°C at 500°C 0-100°C( J/kg.K) (nΩ.m)
UNS S32205 / UNS S31803 782 190 13.7 14.2 19 418 850
Класс КИТАЙ UNS Старая Британия Евронорм Swedish SS Japanese JIS
Нет BS En Нет Имя
2205 022Cr23Ni5Mo3N S31803 / S32205 318S13 1.4462 X2CrNiMoN22-5-3 2377 SUS 329J3L
Welded Duplex 2205 Stainless Steel pipe Seamless Duplex Stainless Steel 2205 pipe
Tuberia Duplex 2205 saf 2205 pipe
Duplex 2205 Steel Pipe Tubo Duplex 2205
Duplex Stainless Steel 2205 Custom Pipe 2205 Stainless Steel Round Pipe Price
6 Inch Welded 2205 Duplex Steel pipe Welded polished annealed Duplex Stainless Steel 2205 pipe
Duplex 2205 Stainless Steel flex pipe supplier Duplex SS 2205 Polished Pipe
2205 Stainless Steel Thick Wall Pipe 2205 Duplex Welded Pipe stockist
2205 Stainless Steel lined pipe 2205 Stainless Steel Thin Wall Pipe
2205 Duplex Steel Custom Pipe SCH40 2205 Stainless Steel pipe
2205 Stainless Steel Rectangular Pipe 2205 Duplex Stainless Steel EFW Pipe
Duplex SS 2205 Seamless Round Pipes 2205 Duplex Steel ERW Pipe
SCH20 Duplex 2205 Pipe Distributors SCH80 2205 Duplex Stainless Steel pipe
Duplex 2205 Stainless Steel Square Pipe (Radius Corners) Duplex 2205 Pipe Supplier
Hot Rolled 2205 Duplex Steel Welded Pipe Cold Drawn 22 Cr Duplex Steel Pipes
Hot Rolled 22 Cr Duplex Steel Pipe Hot Rolled 22 Cr Duplex Steel Seamless Pipe
2205 Duplex Steel Fabricated Pipe 22 Cr Duplex Steel Annealed pipes
Cold Drawn 22 Cr Duplex Steel Welded Pipes Cold Drawn 2205 Duplex Stainless Steel Seamless Pipes
2205 Duplex Steel Hollow Pipe 2205 Duplex Stainless Steel High Pressure Tube
Duplex 2205 Stainless Steel small diameter pipe 22 Cr Super Duplex Capillary Pipe
2205 Duplex 1.4462 Elliptical and Oval Tubes 22 Cr Super Duplex Rectangular Tube
2205 Duplex Stainless Steel Sighting Tube 2205 Duplex Steel Polish Tubes
2205 Duplex 1.4462 straight tube boiler 22 Cr Super Duplex furnace tube
22 Cr Super Duplex Condenser Tubes 2205 Duplex Steel Aero engine tubes
2205 Duplex SS Extruded Seamless Tube Duplex 2205 AISI Precision tube
22 Cr Super Duplex Protection tube 2205 Duplex Steel Cold Drawn Seamless tube
2205 Stainless Steel Round Tubing 2205 Stainless Steel ERW Tube
2205 Stainless Steel Gas Tube  Duplex 2205  Tube
Duplex 2205 AISI Tubing bends 2205 Duplex Steel Capillary tube

Выберите Daxun и сделайте своих клиентов довольными.

Quick response 2205 Stainless Steel pipe

  • High resistance to stress corrosion cracking, fatigue and erosion
  • Higher thermal conductivity and lower thermal expansion than austenitic steels
  • Excellent and uniform resistance to pitting and crevice corrosion
  • Good resistance to sulfide stress corrosion cracking
  • Usable up to 600°F
  • High yield strength
  • Good fatigue strength
  • Excellent corrosion resistance superior

Daxun Advantages: Superior Performance Across Applications

Устойчивость к коррозии
Alloy 2205 stands out for its exceptional resistance to chloride-induced pitting and stress corrosion cracking, making it an ideal choice for environments exposed to chlorides. Its high chromium, molybdenum, and nitrogen content ensures superior protection against pitting and crevice corrosion, especially in demanding industries like oil and gas extraction or processes involving corrosive media. It also performs well in seawater and other harsh conditions.

Elevated Temperature Resistance
Alloy 2205 is designed to perform under elevated temperatures, with an upper limit of 600°F (315°C) as per the ASME Boiler and Pressure Vessel Code. Prolonged exposure to temperatures beyond this range may lead to embrittlement, so it is best suited for controlled temperature applications.

Механическая прочность
With a yield strength approximately twice that of conventional austenitic stainless steels in its annealed state, Alloy 2205 delivers outstanding durability. It can also be cold-worked to achieve even higher strength levels, exceeding 160 ksi. Additionally, it maintains good toughness at temperatures as low as -50°F (-10°C), making it a versatile material for both high-strength and low-temperature applications.

Работоспособность
Alloy 2205 can be easily cold-formed, though its high work-hardening rate may require intermediate annealing during the process. For optimal stress corrosion resistance, annealing is recommended after both hot and cold forming. This ensures the alloy retains its excellent mechanical and corrosion-resistant properties.

2205 Stainless Steel pipe packagingWoven bag bale cargo (hexagonal)

  1. Специальные ящики для труб с U-образным изгибом, (сталь/дерево) разделены
  2. Каждый тюк завернут в полиэтилен для защиты от ветра и дождя.
  3. SS 2205 seamless pipes are protected by plastic covers.
  4. Для крепления тюка используются пластиковые ленты.
  5. Экспортная упаковка в деревянные ящики без фумигации.
  6. Ламинированный упаковочный лист, прикрепленный к тюку или ящику.
  7. Индивидуальная упаковка в соответствии с требованиями заказчика.

2205 Stainless Steel pipe Ordering Information

Duplex 2205 Stainless Steel Pipe The purchase order shall include quantity, PSL grade, type or class, API5L reference, outside diameter, wall thickness, length and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Pipe is solution bright annealed.

Quality, Delivery, and Inspection at Daxun

  • At Daxun, we prioritize quality at every step of production. To ensure our products meet the highest standards, we perform a variety of quality assurance tests, including flattening tests, pitting and resistance tests, mechanical tests, hardness tests, material positive identification, and expansion tests. These tests assess the mechanical properties of our materials, guaranteeing that they are reliable and suitable for their intended applications.

    Throughout the manufacturing process, we carefully measure the diameter, thickness, and surface quality of each product to maintain precision. Our standard delivery time is 7-15 days, with an extended timeline of up to 20 days for special sizes. We strictly adhere to contract timelines to ensure timely delivery.

Additional Customer Support Services

  • We welcome third-party agencies to conduct factory inspections on-site.
  • Free product samples are available for customer testing.
  • On-site or video inspections of our facilities are fully supported.

Техническая поддержка

Если вам потребуется дополнительная техническая помощь, наш постоянный металлург и компетентный персонал будут рады помочь. Кроме того, Daxun может похвастаться сертифицированной испытательной лабораторией - впервые в отрасли производства инвентаря из нескольких металлов и пластика. Это, по нашему мнению, демонстрирует нашу неизменную приверженность качеству и философию поставщика полного цикла.

2205/S31803 Stainless Steel pipe and tube Features

Высокая прочность
Устойчивость к коррозии
Термостойкость
Устойчивость к низким температурам
Защита окружающей среды
Производительность сварки

Сплав Daxun Пусть ваш бренд быстро улучшается

NPS Наружный диаметр Толщина стенок Вес Вес
в мм в мм Расписание кг/метр фунт/фунт
1/2″ 0.84 21 0.109 2.769 40 STD 1.268 0.851
0.147 3.734 80 СТД 1.621 1.088
3/4″ 1.05 27 0.113 2.87 40 STD 1.684 1.131
0.154 3.912 80 СТД 2.195 1.474
1″ 1.315 33 0.133 3.378 40 STD 2.501 1.679
0.179 4.547 80 СТД 3.325 2.172
1 1/4″ 1.66 42 0.14 3.556 40 STD 3.385 2.273
0.191 4.851 80 СТД 4.464 2.997
1 1/2″ 1.9 48 0.145 3.683 40 STD 4.048 2.718
0.2 5.08 80 СТД 5.409 3.361
2″ 2.375 60 0.154 3.912 40 STD 5.441 3.653
0.218 5.537 80 СТД 7.48 5.022
2 1/2″ 2.875 73 0.203 5.516 40 STD 8.629 5.793
0.276 7.01 80 СТД 11.411 7.661
3″ 3.5 89 0.216 5.486 40 STD 11.284 7.576
0.3 7.62 80 СТД 15.272 10.253
4″ 4.5 114 0.237 6.02 16.073 10.79
0.337 8.56 22.318 14.983
6″ 6.625 168 0.188 4.775 19.252 12.924
0.203 5.516 20.739 13.923
0.219 5.563 22.318 14.983
0.25 6.35 25.354 17.021
0.28 7.112 40 STD 58.263 18.974
0.312 7.925 31.334 21.036
0.375 9.525 37.285 25.031
0.432 10.973 80 XHY 42.561 28.573
0.5 12.7 48.719 32.708
8″ 8.625 219 0.188 4.775 25.233 16.94
0.203 5.156 27.198 18.259
0.219 5.563 29.286 19.661
0.25 6.35 20 33.308 22.361
0.277 7.036 30 36.786 24.696
0.322 8.179 40 42.352 28.554
0.375 9.525 49.216 33.041
0.406 10.312 60 53.085 35.638
0.5 12.7 80 XHY 64.627 43.388
10″ 10.75 273 0.188 4.775 31.588 21.207
0.219 5.563 36.689 24.631
0.25 6.35 20 41.759 28.035
0.307 7.798 30 51.002 34.24
0.344 8.738 56.946 38.231
0.365 9.271 40 STD 63.301 40.483
0.438 11.125 71.852 48.238
0.5 12.7 60 XHY 81.53 54.735
0.594 15.088 80 95.969 64.429
12″ 12.75 324 0.188 4.775 37.57 25.222
0.219 5.563 43.657 29.309
0.25 6.35 49.713 33.375
0.281 7.137 55.739 37.42
0.312 7.925 61.735 41.445
0.375 9.525 73.824 49.562
0.406 10.312 79.727 53.525
0.5 12.7 97.438 65.415
0.562 14.275 108.966 73.154
14″ 14 356 0.188 4.775 41.308 27.732
0.219 5.563 48.012 32.233
0.25 6.35 20 54.685 36.713
0.281 7.137 61.327 41.172
0.312 7.925 67.939 45.611
0.375 9.525 STD 81.281 54.568
0.438 11.125 40 94.498 63.441
0.5 12.7 XHY 107.381 72.09
0.625 15.875 132.983 89.278
16” 16 406 0.188 4.775 47.29 21.748
0.219 5.563 54.98 36.91
0.25 6.35 10 62.639 42.053
0.281 7.137 70.268 47.174
0.312 7.925 20 77.866 52.275
0.344 8.738 85.677 57.519
0.375 9.525 30 93.213 62.578
STD
0.438 11.125 108.433 72.797
0.5 12.7 40 123.289 82.77
XHY
18″ 18 457 0.219 5.563 61.948 41.588
0.25 6.35 70.593 47.393
0.281 7.137 79.208 53.176
0.312 7.925 20 87.792 58.939
0.375 9.525 STD 105.144 70.588
0.438 11.125 30 122.369 82.152
0.5 12.7 XHY 139.198 93.45
0.562 14.275 40 155.904 104.666
0.625 15.875 172.754 115.978
20″ 20 508 0.25 6.35 78.547 52.733
0.282 7.163 88.458 59.386
0.312 7.925 97.719 65.604
0.375 9.525 20 СТД 117.075 78.598
0.438 11.125 136.305 91.508
0.5 12.7 30 XHY 155.106 104.13
0.594 15.088 40 183.378 123.11
0.625 15.875 192.64 129.328
0.688 17.475 211.368 141.901
24″ 24 610 0.25 6.35 94.456 63.413
0.281 7.137 106.029 71.183
0.312 7.925 117.573 18.932
0.375 9.525 20 СТД 140.938 64.618
0.438 11.125 164.176 110.219
0.5 12.7 XHY 186.923 125.49
0.625 15.875 232.41 156.028
0.688 17.475 40 255.148 171.293
0.75 19.05 277.401 186.233
30″ 30 762 0.25 6.35 118.318 79.433
0.281 7.137 132.851 89.189
0.312 7.925 10 147.353 98.925
0.375 9.525 STD 176.731 118.648
0.438 11.125 205.983 138.286
0.5 12.7 20 XHY 234.647 157.53
0.625 15.875 30 292.066 196.078
0.688 17.475 320.817 215.38
0.75 19.05 348.988 234.293
36″ 36 914 0.25 6.35 142.18 95.453
0.281 7.137 159.672 107.196
0.312 7.925 10 177.133 118.918
0.375 9.525 STD 215.525 142.678
0.438 11.125 247.79 166.353
0.5 12.7 20 XHY 282.372 198.57
0.625 15.875 351.723 236.128
0.688 17.475 386.487 259.467
0.75 19.05 420.576 282.353
42″ 42 1067 0.312 7.925 206.914 138.911
0.375 9.525 STD 248.319 166.708
0.5 12.7 XHY 33.097 221.61
0.75 19.05 492.163 330.413
48″ 48 1219 0.375 9.525 STD 284.112 190.738
0.438 11.125 331.404 222.487
0.5 12.7 XHY 377.822 253.65
0.75 19.05 563.75 378.473
0.875 22.225 655.969 440.383
НОМИНАЛЬНОЕ ДАВЛЕНИЕ (PSIG)
РАЗМЕРЫ СХЕМА (SCH) СНАРУЖИ СТЕНА ТЕМПЕРАТУРА (ИЗ)
(ДЮЙМЫ) DIA. ТОЛСТЫЙ. 100 200 300 400 500 600 650 700 750
(IN) (IN) ДОПУСТИМОЕ НАПРЯЖЕНИЕ (PSI)
16700 16700 16700 15500 14400 13500 13200 12900 12600
1″ 40 1.315 0.133 2205 2205 2205 2047 1902 1783 1743 1703 1664
80 1.315 0.179 3061 3061 3061 2841 2640 2475 2420 2365 2310
160 1.315 0.25 4493 4493 4493 4170 3874 3632 3552 3471 3390
1 1/2″ 40 1.9 0.145 1629 1629 1629 1512 1404 1317 1287 1258 1229
80 1.9 0.2 2303 2303 2303 2138 1986 1862 1821 1779 1738
160 1.9 0.281 3362 3362 3362 3120 2899 2717 2657 2597 2536
2″ 40 2.375 0.154 1371 1371 1371 1272 1182 1108 1083 1059 1034
80 2.375 0.218 1985 1985 1985 1843 1712 1605 1569 1534 1498
160 2.375 0.344 3283 3283 3283 3047 2831 2654 2595 2536 2477
3″ 40 3.5 0.216 1301 1301 1301 1208 1122 1052 1028 1005 982
80 3.5 0.3 1844 1844 1844 1712 1590 1491 1458 1425 1391
160 3.5 0.438 2787 2787 2787 2587 2403 2253 2203 2153 2103
4″ 40 4.5 0.237 1102 1102 1102 1023 950 891 871 851 831
80 4.5 0.337 1596 1596 1596 1482 1377 1291 1262 1233 1204
160 4.5 0.531 2611 2611 2611 2424 2552 2111 2064 2017 1970
5″ 40 5.563 0.258 965 965 965 896 832 780 763 746 728
80 5.563 0.375 1428 1428 1428 1325 1231 1154 1129 1103 1077
160 5.563 0.625 2474 2474 2474 2296 2133 2000 1955 1911 1866
6″ 40 6.625 0.28 877 877 877 814 756 709 693 677 661
80 6.625 0.432 1379 1379 1379 1280 1189 1115 1090 1065 1040
160 6.625 0.719 2382 2382 2382 2211 2054 1925 1883 1840 1797
8″ 40 8.625 0.322 771 771 771 716 665 623 610 596 582
80 8.625 0.5 1218 1218 1218 1131 1050 985 963 941 919
160 8.625 0.906 2298 2298 2298 2133 1982 1858 1817 1775 1734
10″ 40 10.75 0.365 699 699 699 649 603 565 553 540 528
80 10.75 0.594 1159 1159 1159 1075 999 937 916 895 874
160 10.75 1.125 2289 2289 2289 2124 1974 1850 1809 1768 1727
Типы Наружный диаметр Размеры Длина
Размеры NB (в наличии) .0035” ~ 20” 1/8″, 1/4″, 3/8″, 1/2″, 5/8″, 3/4″, 1″, 1,25″, 1,5″, 2″, 2,5″, 3″, 4″, 5″, 6″ и т.д. Отрежьте по длине
Stainless Steel 2205/S31803 Seamless Tube (Custom Sizes) Наружный диаметр 6,35 мм До наружного диаметра 508 мм В соответствии с требованиями Отрежьте по длине
Stainless Steel 2205/S31803 Welded Tube (ERW Tube) (in Stock + Custom Sizes) Наружный диаметр 6,35 мм До наружного диаметра 1219 мм В соответствии с требованиями Отрежьте по длине
Отделка поверхности Внутренняя поверхность (ID) Внешняя поверхность (OD)
Средняя шероховатость (RA) Средняя шероховатость (RA)
мк дюйм мкм мк дюйм мкм
AP Отожженные и маринованные Не определено Не определено 40 или Не определено 1,0 или Не определено
BA Отжиг 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
MP Механическая полировка 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
EP Электрополировка 15,10,7,5 0.38,0.25,0.20;0.13 32 0.8

The surface and shape of 2205 stainless steel tube (6)

Информация доступна для ознакомления и скачивания

axun is a trustworthy stainless steel pipe and tube manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also have strict quality control to ensure that the 2205 Stainless Steel pipes have less defects. At Daxun, rest assured that all products are durable, high quality, high performance, and include ferritic options.

Последние проекты и продукты для горячих случаев

бесшовная труба из нержавеющей стали
труба из нержавеющей стали большого диаметра
Полированная труба из нержавеющей стали
Труба из нержавеющей стали
Труба из нержавеющей стали BA
Труба из нержавеющей стали / труба
Сварная труба из нержавеющей стали
Прецизионная труба из нержавеющей стали
Leading stainless steel tube and pipe Suppliers in China

General Properties of Duplex 2205 Stainless Steel Pipe

Duplex 2205 stainless steel is a duplex ferritic-austenitic alloy containing 22% chromium, 3% molybdenum, and 5-6% nickel. It is the most widely used grade of duplex stainless steel, offering twice the yield strength of standard austenitic grades. Known for its excellent fatigue strength, it provides outstanding resistance to stress corrosion cracking, crevice corrosion, pitting, erosion, and general corrosion, even in harsh environments.

Химический состав

Duplex 2205 stainless steel boasts a well-balanced chemical composition that includes:

  • Chromium: 21-23%
  • Molybdenum: 2.5-3.5%
  • Nickel: 4.5-6.5%
  • Nitrogen: 0.8-2.0%
  • Manganese: <2%
  • Silicon: <1%
  • Phosphorus: <0.03%
  • Sulfur: <0.02%
  • Iron: Balance

The high chromium content in Duplex 2205 is a key factor in its excellent corrosion resistance. Chromium forms a passive layer on the steel surface, protecting it from oxidation and corrosion. Molybdenum and nitrogen further enhance this resistance, particularly against pitting and crevice corrosion, making Duplex 2205 a robust choice for challenging environments.

Механические свойства

Duplex 2205 stainless steel is renowned for its impressive mechanical properties:

  • Yield strength: 448 MPa (65,000 psi) min
  • Tensile strength: 621 MPa (90,000 psi) min
  • Elongation at break: 25% min
  • Reduction of area: 50% min
  • Hardness: 31 max Rockwell C (HR C)

Compared to austenitic stainless steels, Duplex 2205 offers significantly higher yield and tensile strength. This makes it an excellent option for applications that demand both high strength and good corrosion resistance. Its mechanical properties ensure durability and reliability, even in the most demanding conditions.

ФИЗИЧЕСКИЕ СВОЙСТВА

The physical properties of Duplex 2205 stainless steel are as follows:

  • Плотность: 7.8 g/cm³
  • Melting point: 1450°C (2642°F)
  • Thermal expansion: 13.7 x 10^-6 K^-1 (7.6 x 10^-6 °F^-1)
  • Thermal conductivity: 14.2 W/m-K (8.2 Btu/h-ft-°F)
  • Specific heat capacity: 500 J/kg-K (0.12 Btu/lb-°F)
  • Electrical resistivity: 80 x 10^-8 Ωm (50 x 10^-8 Ωin)

These properties contribute to the alloy’s excellent performance in various industrial applications, ensuring stability and efficiency under different thermal and mechanical conditions.

Heat Resistance

Duplex 2205 stainless steel exhibits good heat resistance, but it is not designed for high-temperature applications. The maximum recommended temperature for Duplex 2205 is 300°C (572°F). Beyond this temperature, the material may undergo precipitation, which can adversely affect its corrosion resistance and mechanical properties. Therefore, it is crucial to use Duplex 2205 within its specified temperature range to maintain its integrity and performance.

APPLICATIONS IN HIGH CHLORIDE ENVIRONMENTS

  • Chemical processing, transport and storage – pressure vessels, tanks, piping, and heat exchangers
  • Oil and gas exploration and processing equipment – piping, tubing, and heat exchangers
  • Marine and other high chloride environments
  • Effluent scrubbing systems
  • Pulp and paper industry – digesters, bleaching equipment, and stock-handling systems
  • Cargo tanks for ships and trucks
  • Food processing equipment
  • Biofuels plants

STANDARDS

  • ASTM/ASME: A240 UNS S32205/S31803
  • EURONORM: 1.4462 X2CrNiMoN 22.5.3
  • AFNOR: Z3 CrNi 22.05 AZ
  • DIN: W.Nr 1.4462

Good Corrosion Resistance

Duplex 2205 offers excellent resistance to corrosion due to its high chromium, molybdenum, and nitrogen content. It outperforms 316 and 316L stainless steels in most environments, especially in oxidizing and acidic solutions. Its resistance to pitting and crevice corrosion is outstanding, even in harsh chloride-containing environments. Additionally, it can withstand chloride stress corrosion cracking at temperatures up to 302°F (150°C). The ferritic structure also enhances its performance in caustic conditions.

Heat Resistance
Duplex 2205 provides good oxidation resistance at elevated temperatures. However, it may become brittle when exposed to temperatures above 572°F (300°C), even for short durations. Therefore, it is not recommended for use in applications exceeding this temperature.

Welding Characteristics
Duplex 2205 demonstrates good weldability. However, welding without filler metal is generally not recommended as it may result in excessive ferrite content, compromising the material’s properties.

Heat Treatment
The recommended annealing temperature for Duplex 2205 is between 1868°F and 2012°F (1020°C to 1100°C). While it cannot be hardened through heat treatment, the alloy does work-harden. Special precautions are required to manage its higher coefficient of thermal expansion, which can lead to warping or distortion.

Processing – Hot Forming
For hot forming, the maximum recommended temperature is between 2010°F and 2100°F (1100°C to 1150°C). Uneven cooling, such as cooler edges compared to the bulk, can increase the risk of cracking. Careful handling is essential.

Processing – Cold Forming
Duplex 2205 has good formability but requires careful consideration due to its high strength. The higher springback characteristic of this material must be accounted for during cold forming processes.

Обрабатываемость
Duplex 2205 is slightly more challenging to machine compared to 300 series austenitic stainless steels. It requires higher cutting forces, which result in faster tool wear. To optimize machining:

  • Use a rigid, powerful machine with strong tool and workpiece mounts.
  • Minimize tool extension to reduce vibration.
  • Keep the tool nose radius short to maintain a sharp cutting edge while ensuring strength.
  • Plan machining sequences so the depth of each cut avoids the work-hardened layer from prior operations.

FABRICATION

Duplex 2205 stainless steel can be fabricated using various techniques, including hot and cold forming, machining, and welding. However, its high strength and hardness require specialized equipment and techniques to avoid damage and ensure optimal results.

  • Hot forming: Duplex 2205 can be hot formed at temperatures between 1000°C (1832°F) and 1150°C (2102°F). However, temperatures above 1150°C (2102°F) can cause precipitation of chromium carbides, leading to reduced corrosion resistance. Proper temperature control is crucial to maintain the alloy’s integrity and performance.
  • Cold forming: Duplex 2205 can be cold formed using various techniques, including bending, spinning, and drawing. However, its high strength and hardness require higher forces and more powerful equipment compared to austenitic stainless steels. Intermediate annealing may be required to relieve stress and prevent cracking.
  • Machining: Duplex 2205 is more difficult to machine than austenitic stainless steels due to its high hardness and strength. Cutting speeds should be reduced by 20-30% to avoid tool wear and damage. Using a powerful, rigid machine with strong tool and workpiece mounts is essential to achieve precise results.
  • Сварка: Duplex 2205 can be welded using various techniques, including shielded metal arc welding (SMAW), gas metal arc welding (GMAW), and gas tungsten arc welding (GTAW). However, welding requires careful control of heat input and shielding gas to avoid precipitation of chromium carbides and ensure optimal corrosion resistance. Proper post-weld heat treatment may be necessary to restore the alloy’s properties.

By following these guidelines, manufacturers can ensure that Duplex 2205 stainless steel retains its superior properties and performs reliably in demanding applications.

Welding and Joining

Duplex 2205 stainless steel can be effectively welded using various techniques, including shielded metal arc welding (SMAW), gas metal arc welding (GMAW), and gas tungsten arc welding (GTAW). However, welding Duplex 2205 requires meticulous control of welding parameters to prevent precipitation and ensure good corrosion resistance. Proper heat input and shielding gas are essential to maintain the alloy’s properties and achieve optimal weld quality.

2205/31803/S32205 grade austenitic stainless steels pipe

Comparison with Other Grades

When compared to austenitic stainless steels like 316L and 317L, Duplex 2205 stands out due to its higher strength and superior resistance to pitting and crevice corrosion. This makes it particularly suitable for applications in marine environments, oil and gas, and chemical processing. Its high chromium content provides better corrosion resistance in oxidizing environments, while its high chloride resistance makes it ideal for high-chloride environments such as seawater and brine.

Overall, Duplex 2205 stainless steel offers a unique combination of high strength, good corrosion resistance, and weldability, making it a preferred choice for a wide range of demanding applications.

Wide choice of dimensions and free cutting

  • Whatever your needs, Daxun Alloys has the perfect stainless steel tube for you. We offer 3m and 6m lengths, with diameters from 3mm to 2000mm (Grade 2205) and ¾” to 20″ (Grade S31803).
  • If you require a specific length, we offer a free unlimited cutting service with every purchase. Using state-of-the-art bandsaws and optimized cutting speeds, our precision cutting service can cut the tube to the exact length you require. Just let us know when ordering. It’s another reason why we are a leading stainless steel tube supplier to our domestic and international customers.

Contact your stainless steel tube suppliers

  • You can easily order stainless steel pipes online, in any size, in any quantity.
  • Кроме того, наш дружелюбный отдел продаж будет рад принять ваш заказ. Просто позвоните по телефону +86 13382898899 или напишите по электронной почте Daxunhejin@gmail, и мы свяжемся с вами как можно скорее.
Могу я получить несколько образцов?

Мы можем предоставить вам образцы листов из нержавеющей стали для проверки качества. Образец бесплатен, и вы просто оплачиваете перевозку.

В какие страны вы уже экспортировали свою продукцию?

Мы экспортировали продукцию в более чем 42 страны, такие как Канада, Чили, Кувейт, Германия, Южная Корея, Саудовская Аравия, Сингапур и др.

Какова ваша MOQ?

Наш MOQ составляет 1 тонну для листов из нержавеющей стали.

Как долго длится доставка?

Пробные заказы могут быть доставлены в течение недели. Для обычных заказов требуется примерно две недели.

Отправьте запрос сегодня
Быстрая цитата