Daxun is a 316/316L stainless steel angle steel supplier in China
As a leading stainless steel angle steel supplier and exporter in China, Daxun supplies stainless steel angle steel to all over the world.
- Grade: S31600(316)-S31603(316L)
- Equal Angle Steel/Unequal Angle Steel
- Process: hot rolling and laser welding
- Easy to weld and process
- Length can be cut to size
- Daxun specializes in custom stainless steel angles with fast delivery and competitive prices. Contact Daxun today.
Global leader in stainless steel angle fabrication services
304/304L and 316/316L Stainless Steel Angles
As China’s premier supplier of specialty metals, you can trust Daxun for all of your stainless steel angle needs. Our stainless steel angle selection includes 304/304L and 316/316L stainless steel angles. Our extensive product line offers durability and versatility, making it the perfect solution for your structural and fabrication needs.
Our stainless steel angles are available in 304/304L and 316/316L, all from fully certified factories. Our comprehensive product line is both durable and adaptable, ideal for structural and fabrication applications. As a leading stainless steel angle manufacturer, we offer a wide range of specialty angles and L-shaped angles. Daxun offers stainless steel angles in any length, up to 6 meters. The following stainless steel grades are also available: 304/304L and 316/316L. Stainless steel angles are most commonly used for supports or frames, but are also used in food equipment, building supports, structural supports, and medical equipment.
Can be welded and processed using simple procedures, 304/304L stainless steel angles are suitable for many environments, such as general industrial projects, chemical projects. While 316/316L angles are marine grade and have strong corrosion resistance in more demanding conditions.
The surface treatment we use on our stainless steel angles is hot rolling, annealing, and pickling. This surface treatment maximizes corrosion resistance and gives the angles a unique “stainless” appearance.
The two manufacturing methods are laser melting and hot rolling. Hot rolling produces stainless steel angles at a lower price. They usually have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also have a sandblasted, smoother surface. Laser melted stainless steel angles have a smoother surface quality than hot rolled stainless steel angles.
Daxun Alloy manufactures laser melted and hot rolled stainless steel angles in metric and imperial sizes. We can ship them all over the world.
데이터
- 매개변수
- 요소
- 기계적 특성
- 물리적 속성
- 모두 동일
| 표준 | ASTM、EN、DIN、JIS,ASME, BS, GBetc, |
| 치수 | ∠20*20*3mm-∠200*200*24mm |
| 합금 | 201, 310, 304, 304L, 316, 316L |
| 유형 | Equal, Unequal |
| 길이 | 1.0-12.0m |
| 두께 | 3mm-25mm |
| Custom Options | Yes |
| 허용 오차 | ± ¼”, ± 1/16” |
| 완료 | Mill, brush, mirror, polished |
| CHEMICAL COMPOSITION: ASTM A240, A666 | ||
| 요소 | Type 316 | Type 316L |
| 탄소 | 최대 0.08. | 최대 0.030. |
| 망간 | 2.00 max. | 2.00 max. |
| 유황 | 최대 0.030. | 최대 0.030. |
| Phosphorus | 0.045 max. | 0.045 max. |
| 실리콘 | 0.75 max. | 0.75 max. |
| 크롬 | 16.0 – 18.0 | 16.0 – 18.0 |
| 니켈 | 10.00 – 14.00 | 10.00 – 14.00 |
| 몰리브덴 | 2.00 – 3.00 | 2.00 – 3.00 |
| 질소 | 최대 0.10. | 최대 0.10. |
| 유형 | Yield Strength 0.2% offset (KSI) | Tensile Strength (KSI) | % Elongation (2″ Gauge length) |
| 316 | 30 min. | 75 min. | 40 min. |
| 316L | 25 min. | 70 min. | 40 min. |
| 밀도(파운드/인치^2) @ RT | 0.29 | |
| 장력 탄성 계수(psi x 10^6) | 28 | |
| 비열(BTU/o F/lb.) | 32~212oF | 0.12 |
| 열 전도성(BTU/hr/ft^2/ft) | 212oF | 9.4 |
| 932oF | 12.4 | |
| 평균 열팽창 계수(인치 x 10^-6 o F당) | 32~212oF | 8.9 |
| 32 to 600oF | 9 | |
| 32 to 1,000oF | 9.7 | |
| 32~1,200oF | 10.3 | |
| 전기 저항률(마이크로옴 - cm) | 70oF에서 | 29.4 |
| Melting Point Range (oF) | 2500 – 2550 |
| 등급 | 유엔 아니요 | 올드 브리티시 | 유로노름 | Swedish SS | Japanese JIS | ||
| BS | En | 아니요 | 이름 | ||||
| 316l | S31603 | 316S11 | – | 1.4404 | X2CrNiMo17-12-2 | 2348 | SUS 316L |
Daxun을 선택하고 고객을 만족시키세요.

빠른 응답
긴급한 니즈가 있는 고객에게 스테인리스 스틸 제품을 적시에 신속하게 배송합니다. 속도 뒤에는 정보 흐름에서 물류 및 자본 흐름에 이르는 시스템 지원이 있습니다. 예를 들어, 정보 흐름 측면에서 Daxun의 주문 데이터는 실시간으로 물류 시스템에 푸시되고 데이터가 원활하게 연결되며 물류 측면에서 처리 센터는 고속도로와 강과 바다에 가깝고 합리적인 일정, 신속한 대응, 보관 및 운송 연계, 효율적인 적재를 통해 작업이 일정대로 완료되도록 보장합니다.Daxun의 스테인리스 스틸 재료는 신뢰할 수있는 품질이며 품종, 사양 및 배송 무게는 표준을 엄격하게 준수합니다.
닥순의 장점
Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of each angle steel, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.


패키징
상품이 다양한 경로를 거쳐 최종 목적지에 도착하는 국제화물에서 포장은 중요한 역할을 하기 때문에 대순합금은 포장에 각별한 주의를 기울이고 있으며 최고의 품질을 보장합니다. 제품에 따라 다양한 방법으로 상품을 포장합니다. 다음과 같은 다양한 방법으로 제품을 포장합니다:
- 상자 및 상자
- 수축 포장
- 목재 팔레트
- 나무 상자
품질, 배송, 검사
- Daxun은 또한 여러 가지 품질 보증 테스트를 수행합니다. 이러한 테스트에는 평탄화 테스트, 피팅 및 저항 테스트, 기계적 테스트, 경도 테스트, 재료 양성 식별, 팽창 테스트 등이 포함됩니다. 이러한 모든 테스트를 통해 재료가 필요한 용도에 적합한지 확인합니다.
- 생산 과정에서 제품의 직경, 두께, 표면을 측정합니다. 표준 배송 기간은 7~15일이며, 일부 특수 사이즈 제품을 제외하고는 배송 기간이 20일로 늘어납니다.
배송 시간은 엄격하게 계약에 따릅니다. - 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
- 고객에게 테스트용 무료 샘플 지원
- 현장 또는 비디오 공장 검사 지원


주문 정보
구매 주문서에는 수량, 등급, 유형 또는 카테고리, API5L 기준, 두께, 너비, 길이 및 화학 성분, 기계적 특성, 열처리, 추가 테스트, 제조 공정, 표면 코팅 또는 최종 마감과 관련된 모든 해당 부착물 또는 추가 요구 사항이 포함되어야 합니다. 지금 Daxun에 문의하시면 최대한 빨리 답변해 드리겠습니다.
기술 지원
추가 기술 지원이 필요한 경우 금속 전문가와 지식이 풍부한 직원이 기꺼이 도와드릴 것입니다. 또한 Daxun은 다중 금속 및 플라스틱 재고 업계 최초로 인증된 테스트 실험실을 보유하고 있습니다. 이는 품질에 대한 변함없는 헌신과 풀서비스 공급업체로서의 철학을 보여주는 것이라고 생각합니다.

SS 316-316L Stainless Steel angle Features
Daxun 합금으로 브랜드를 빠르게 향상 시키십시오.
- Specification Table
| Angle – Steel Data | |||||||||||||
| EQUAL AND UNEQUAL ANGLE | |||||||||||||
| ANGLE is available in other sizes on request | |||||||||||||
| 설명 | Width (W) | Depth (D) | 두께 | 표준 | Weight per | Surface | |||||||
| (mm) | (mm) | (T) (mm) | 길이 | Metre | Area per | ||||||||
| (kg/m) | Metre | ||||||||||||
| (m²/m) | |||||||||||||
| ANGLE 20 X 20 X 3.0mm | 20 | 20 | 3 | 6.0 metres | 0.98 | 0.0897 | |||||||
| ANGLE 25 X 25 X 3.0mm | 25 | 25 | 3 | 7.5 metres | 1.12 | 0.0953 | |||||||
| ANGLE 25 X 25 X 5.0mm | 25 | 25 | 5 | 7.5 metres | 1.65 | 0.0953 | |||||||
| ANGLE 25 X 25 X 6.0mm | 25 | 25 | 6 | 7.5 metres | 2.08 | 0.0953 | |||||||
| ANGLE 30 X 30 X 2.5mm | 30 | 30 | 2.5 | 6.0 metres | 1.06 | 0.117 | |||||||
| ANGLE 30 X 30 X 3.0mm | 30 | 30 | 3 | 7.5 metres | 1.35 | 0.115 | |||||||
| ANGLE 30 X 30 X 5.0mm | 30 | 30 | 5 | 7.5 metres | 2.01 | 0.115 | |||||||
| ANGLE 30 X 30 X 6.0mm | 30 | 30 | 6 | 7.5 metres | 2.56 | 0.115 | |||||||
| ANGLE 40 X 40 X 2.5mm | 40 | 40 | 2.5 | 6.0 metres | 1.43 | 0.157 | |||||||
| ANGLE 40 X 40 X 3.0mm | 40 | 40 | 3 | 7.5 metres | 1.83 | 0.155 | |||||||
| ANGLE 40 X 40 X 4.0mm | 40 | 40 | 4 | 6.0 metres | 2.2 | 0.155 | |||||||
| ANGLE 40 X 40 X 5.0mm | 40 | 40 | 5 | 9.0 metres | 2.73 | 0.155 | |||||||
| ANGLE 40 X 40 X 6.0mm | 40 | 40 | 6 | 9.0 metres | 3.5 | 0.155 | |||||||
| ANGLE 45 X 45 X 3.0mm | 45 | 45 | 3 | 9.0 metres | 2.06 | 0.175 | |||||||
| ANGLE 45 X 45 X 5.0mm | 45 | 45 | 5 | 9.0 metres | 3.1 | 0.175 | |||||||
| ANGLE 45 X 45 X 6.0mm | 45 | 45 | 6 | 9.0 metres | 3.97 | 0.175 | |||||||
| ANGLE 50 X 50 X 2.5mm | 50 | 50 | 2.5 | 9.0 metres | 1.81 | 0.197 | |||||||
| ANGLE 50 X 50 X 3.0mm | 50 | 50 | 3 | 7.5 metres | 2.31 | 0.195 | |||||||
| ANGLE 50 X 50 X 4.0mm | 50 | 50 | 4 | 9.0 metres | 2.79 | 0.195 | |||||||
| ANGLE 50 X 50 X 5.0mm | 50 | 50 | 5 | 9.0 metres | 3.48 | 0.195 | |||||||
| ANGLE 50 X 50 X 6.0mm | 50 | 50 | 6 | 9.0 metres | 4.46 | 0.195 | |||||||
| ANGLE 50 X 50 X 8.0mm | 50 | 50 | 8 | 9.0 metres | 5.68 | 0.195 | |||||||
| ANGLE 55 X 55 X 5.0mm | 55 | 55 | 5 | 9.0 metres | 3.84 | 0.215 | |||||||
| ANGLE 55 X 55 X 6.0mm | 55 | 55 | 6 | 9.0 metres | 4.93 | 0.215 | |||||||
| ANGLE 65 X 50 X 5.0mm | 65 | 50 | 5 | 9.0 metres | 4.02 | 0.225 | |||||||
| ANGLE 65 X 50 X 6.0mm | 65 | 50 | 6 | 9.0 metres | 5.16 | 0.225 | |||||||
| ANGLE 65 X 50 X 8.0mm | 65 | 65 | 8 | 9.0 metres | 6.59 | 0.225 | |||||||
| ANGLE 65 X 65 X 4.0mm | 65 | 65 | 4 | 9.0 metres | 3.69 | 0.255 | |||||||
| ANGLE 65 x 65 x 5.0mm | 65 | 65 | 5 | 9.0 metres | 4.56 | 0.255 | |||||||
| ANGLE 65 X 65 X 6.0mm | 65 | 65 | 6 | 9.0 metres | 5.87 | 0.255 | |||||||
| ANGLE 65 X 65 X 8.0mm | 65 | 65 | 8 | 9.0 metres | 7.51 | 0.255 | |||||||
| ANGLE 65 X 65 X 10.0mm | 65 | 65 | 10 | 9.0 metres | 9.02 | 0.255 | |||||||
| ANGLE 75 X 50 X 5.0mm | 75 | 50 | 5 | 9.0 metres | 4.4 | 0.244 | |||||||
| ANGLE 75 X 50 X 6.0mm | 75 | 50 | 6 | 9.0 metres | 5.66 | 0.244 | |||||||
| ANGLE 75 X 50 X 8.0mm | 75 | 50 | 8 | 9.0 metres | 7.23 | 0.244 | |||||||
| ANGLE 75 X 75 X 4.0mm | 75 | 75 | 4 | 9.0 metres | 4.29 | 0.295 | |||||||
| ANGLE 75 X 75 X 5.0mm | 75 | 75 | 5 | 9.0 metres | 5.27 | 0.292 | |||||||
| ANGLE 75 X 75 X 6.0mm | 75 | 75 | 6 | 9.0 metres | 6.81 | 0.292 | |||||||
| ANGLE 75 X 75 X 8.0mm | 75 | 75 | 8 | 9.0 metres | 8.73 | 0.292 | |||||||
| ANGLE 75 X 75 X 10.0mm | 75 | 75 | 10 | 9.0 metres | 10.5 | 0.292 | |||||||
| ANGLE 90 X 90 X 6.0mm | 90 | 90 | 6.0 | 9.0 metres | 8.22 | 0.352 | |||||||
| ANGLE 90 X 90 X 8.0mm | 90 | 90 | 8.0 | 9.0 metres | 10.6 | 0.352 | |||||||
| ANGLE 90 X 90 X 10.0mm | 90 | 90 | 10.0 | 9.0 metres | 12.7 | 0.352 | |||||||
| ANGLE 100 X 75 X 6.0mm | 100 | 75 | 6.0 | 9.0 metres | 7.98 | 0.342 | |||||||
| ANGLE 100 X 75 X 8.0mm | 100 | 75 | 8.0 | 9.0 metres | 10.3 | 0.342 | |||||||
| ANGLE 100 X 75 X 10.0mm | 100 | 75 | 10.0 | 9.0 metres | 12.4 | 0.342 | |||||||
| ANGLE 100 X 100 X 10.0mm | 100 | 100 | 10.0 | 9.0 metres | 14.2 | 0.392 | |||||||
| ANGLE 100 X 100 X 12.0mm | 100 | 100 | 12.0 | 9.0 metres | 17.7 | 0.392 | |||||||
| ANGLE 100 X 100 X 4.0mm | 100 | 100 | 4.0 | 9.0 metres | 5.78 | 0.395 | |||||||
| ANGLE 100 X 100 X 6.0mm | 100 | 100 | 6.0 | 9.0 metres | 9.16 | 0.392 | |||||||
| ANGLE 100 X 100 X 8.0mm | 100 | 100 | 8.0 | 9.0 metres | 11.8 | 0.392 | |||||||
| ANGLE125 X 75 X 6.0mm | 125 | 75 | 6.0 | 9.0 metres | 9.16 | 0.392 | |||||||
| ANGLE 125 X 75 X 8.0mm | 125 | 75 | 8.0 | 9.0 metres | 11.8 | 0.392 | |||||||
| ANGLE 125 X 75 X 10.0mm | 125 | 75 | 10.0 | 9.0 metres | 14.2 | 0.392 | |||||||
| ANGLE 125 X 75 X 12.0mm | 125 | 75 | 12.0 | 9.0 metres | 17.7 | 0.392 | |||||||
| ANGLE 125 X 125 X 8.0mm | 125 | 125 | 8.0 | 9.0 metres | 14.9 | 0.491 | |||||||
| ANGLE 125 X 125 X 10.0mm | 125 | 125 | 10.0 | 9.0 metres | 18 | 0.491 | |||||||
| ANGLE 125 X 125 X 12.0mm | 125 | 125 | 12.0 | 9.0 metres | 22.5 | 0.491 | |||||||
| ANGLE 125 X 125 X 16.0mm | 125 | 125 | 16.0 | 9.0 metres | 29.1 | 0.491 | |||||||
| ANGLE 150 X 90 X 8.0mm | 150 | 90 | 8.0 | 9.0 metres | 14.3 | 0.471 | |||||||
| ANGLE 150 X 90 X 12.0mm | 150 | 90 | 12.0 | 9.0 metres | 21.6 | 0.471 | |||||||
| ANGLE 150 X 90 X 16.0mm | 150 | 90 | 16.0 | 9.0 metres | 27.9 | 0.471 | |||||||
| ANGLE 150 X 100 X 10.0mm | 150 | 100 | 10.0 | 9.0 metres | 18 | 0.491 | |||||||
| ANGLE 150 X 100 X 12.0mm | 150 | 100 | 12.0 | 9.0 metres | 22.5 | 0.491 | |||||||
| ANGLE 150 X 150 X 10.0mm | 150 | 150 | 10.0 | 9.0 metres | 21.9 | 0.59 | |||||||
| ANGLE 150 X 150 X 12.0mm | 150 | 150 | 12.0 | 9.0 metres | 27.3 | 0.59 | |||||||
| ANGLE 150 X 150 X 16.0mm | 150 | 150 | 16.0 | 9.0 metres | 35.4 | 0.59 | |||||||
| ANGLE 150 X 150 X 19.0mm | 150 | 150 | 19.0 | 9.0 metres | 42.1 | 0.59 | |||||||
| ANGLE 150 X 90 X 10.0mm | 150 | 90 | 10.0 | 9.0 metres | 17.3 | 0.471 | |||||||
| ANGLE 200 x 200 x 13.0mm | 200 | 200 | 13.0 | 9.0 metres | 40 | 0.788 | |||||||
| ANGLE 200 X 200 X 16.0mm | 200 | 200 | 16.0 | 9.0 metres | 48.7 | 0.788 | |||||||
| ANGLE 200 X 200 X 20.0mm | 200 | 200 | 20.0 | 9.0 metres | 60.1 | 0.788 | |||||||
| ANGLE 200 X 200 X 26.0mm | 200 | 200 | 26.0 | 9.0 metres | 76.8 | 0.788 | |||||||
SS 316/316L Stainless Steel Angle Surface Type (3)
참조 및 다운로드 가능한 정보
Daxun is a trustworthy stainless steel Angle manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel angles have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
최근 인기 있는 사례 프로젝트 및 제품
관련 제품 (8)
Leading stainless steel angle Suppliers in China
Daxun has been engaged in international business for more than ten years. In 2023, the export volume exceeded 100 million US dollars, and the export volume ranked among the top Chinese stainless steel manufacturers. Daxun continuously improves its service skills. To serve the global market, it has established three export service facilities in China, cooperating with engineering companies, steel mills, and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relations with dozens of well-known steel mills around the world. The inventory includes 50,000 tons of conventional stainless steel and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of stable quality, and the varieties, specifications, and delivery weights strictly meet the standards.
316 Stainless Steel Angle
- 316 Stainless Steel Angle is an austenitic chromium nickel angle shape containing molybdenum which provides superior corrosion resistance and increased strength at elevated temperatures when compared to 304 Stainless.
- Because of the 4% molybdenum concentration, the 316 material is resistant to chloride ion stress corrosion. Stainless Steel 304 Unequal Angle Sizes vary depending on the application needs. Angles are used to hold components together using a grip. There are also angles with bolt holes for screws and bolts. The 316 Stainless Steel Unequal Angle is suitable for more corrosive applications than the 304 angles. The Stainless Steel Unequal Angle is just as frequent as the Equal Angle. They are utilized in a variety of applications, including brackets, trim, and reinforcements. Please contact us for more information about the angles and their costs.
Characteristics
- Cold Working: Good
- Corrosion Resistance: Excellent
- Heat Resistance: Good
- Heat Treatment: Poor
- Hot Working: Fair
- Machinability: Good
- Weldability: Very Good
Why should you buy stainless steel angles from Daxun?
Daxun’s objective is to supply you with the highest quality and most durable stainless steel angles and steel. We provide hundreds of stainless steel angles in various leg lengths, thicknesses, and material grades. Our 316/316L and 304/304L stainless steel angles are made at our well-equipped production facility using high-quality raw materials and cutting-edge technology, overseen by qualified workers. Some other significant benefits of partnering with us include:
- When you purchase any steel products from us, you get the products directly from the manufacturer.
- Our employees are dedicated to providing the lowest prices and fastest shipping times so that you can start your project right away!
- We have a skilled, capable workforce for quality checks, packaging, and shipping.
- We follow multiple quality check levels, which helps ensure that the products are of the highest standards.
- We have a qualified and dedicated support team available 24×7 to help you out if any issues arise.
Suppliers from China Make Stainless Steel Angles to Size
- Daxun is a leading supplier of stainless steel products in China. With high-quality products and customized services, we can meet all your stainless steel angle needs. Order online or by phone and get it delivered in as fast as 15 days.
304 and 316 Grade Stainless Steel Angles
- This versatile right angle steel has a wide range of applications and is available in grades 304 /30L and 316 /316L. Grade 304 is the most versatile and commonly used grade of stainless steel angle steel and is suitable for most general applications. It is easy to weld and has good formability and corrosion resistance. Sometimes called 18/8 stainless steel because its composition includes 18% chromium and 8% nickel, grade 304 is well suited to most applications.
- Grade 316 is more suitable for harsh environments, such as exposure to salt water and areas with high industrialization. Due to the higher nickel content and the addition of molybdenum to the metal, it has higher corrosion resistance than grade 304, especially to chlorides and chlorinated solutions. It also has good weldability, but is more difficult to process than grade 304.
There are two basic processes for manufacturing stainless steel angles:
- laser melting and hot rolling. Hot rolled stainless steel angles are less expensive. They typically have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also include sandblasting and a smoother finish. The surface of laser melted stainless steel angles is smoother than that of hot rolled stainless steel angles.
Choose Your Size and Size
- We offer a wide variety of stainless steel angles, so whatever your needs, we have you covered. Grade 304 stainless steel angles come in a variety of sizes with thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m.
- Our grade 316 angles come in thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m. Angles are available in a variety of sizes.
Talk to Your Preferred Stainless Steel Angle Supplier
- It couldn’t be easier to buy the stainless steel angles you need, as well as all of our other products, through our website. Alternatively, you can call our sales team in China at +8613382898899 to place your order and they will be happy to process your order. If you have any questions, you can even send an email to [email protected] and our team will get back to you as soon as possible.
“문의하기” 페이지의 양식을 작성하거나 영업 관리자(+86 13382898899)에게 전화하시면 최대한 빨리 연락드리겠습니다. WhatsApp은 온라인 상태이며 이메일([email protected])은 6시간 이내에 확인합니다. 모든 문의나 메시지는 신속하게 답변해 드립니다. 또한 매주 고객과 시장 정보를 공유합니다.
샘플은 무료로 제공될 수 있지만 운임은 고객 부담이며, 협조 후 환불해 드립니다.
캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.
Our MOQ is 1 ton for 316L Stainless Steel Angle.
우리는 원자재 구매에서 가공 및 선적 준비에 이르기까지 완벽한 조직을 갖추고 있습니다. 전체 체인에서 다큐멘터리 사람들 광고 QC는 정확한 요구 사항에 따라 찾고 확인하며 타사 검사를 환영합니다.
체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.