Daxun 304 stainless steel plate and sheet China supplier
As China’s leading stainless steel plate supplier and exporter, Daxun provides stainless steel plates to the world.
- Grade: AISI 304/S30400
- Manufaktur: pelat canai dingin, pelat canai panas, pelat tempa
- Standar: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Jenis: pelat tipis canai dingin, pelat tebal canai panas
- Permukaan: 2B, NO.1, NO.4, HL, BA, 8K, dll.
- Panjang: 2438mm3048mm6000mm dapat disesuaikan
- Asal TISCO, Baosteel, Posco, Tsingshan, Delong
Pemimpin global dalam layanan fabrikasi lembaran baja tahan karat
304 is one of the most popular grades of stainless steel because of its high strength, excellent corrosion resistance, and excellent formability. This grade has a low carbon content and excellent ductility. It can be cold worked by roll forming, deep drawing, and bending. This grade is suitable for forming complex shapes. You will see this grade in the oil and gas industry and the food service industry.Our 304 series is a standout product available in thicknesses from 0.4mm to 20mm. Available in 2B and 2D finishes, these stainless steel products offer excellent corrosion resistance, strength and a wide range of surface finish options to suit different project requirements.
Daxun is your trusted stainless steel sheet supplier.By choosing our 304stainless steel plates, you are investing in a material that guarantees long life, reliability and superior performance. Don’t compromise on quality – choose our stainless steel solutions and experience the difference they can make in your projects. Contact us today for more details or to order your required specifications and quantities.
Data
- Parameter
- Bahan dan properti
- Sifat mekanik
- SIFAT FISIK
| Stainless Plate and sheet Type | Pelat, Lembaran, Strip, Gulungan, Foil, Flat, Pelat Berpakaian, Lembaran Polos, Lembaran Bergulir, Pelat Bergulir, Shim Datar, Lembaran Datar, Lembaran Shim, Gulungan, Kosong (Lingkaran), dicukur, dianil, dianil lunak, kerak, pelat tapak, Pelat Pemeriksa |
| Standar | ASTM A240 / ASME SA240 ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2JIS, AISI, ASTM, GB, DIN, EN, etc |
| Stainless Steel Plate and sheet Length | 1000mm-13000mm atau sesuai kebutuhan |
| 304 Stainless Plate Width | 1000mm-1219mm-1500mm-1800mm-2000mm-2500mm atau sesuai kebutuhan |
| UNS 304 Plate Thickness | 0,3 hingga 120mm atau sesuai kebutuhan |
| ASTM A240 Stainless Steel 304 Plate Process | Canai Panas / Dingin / penempaan |
| UNS 304 Plate surface | No.1, No. 2D, No. 2B, BA, No.3, No.4, No.6, No.7, 2B, 2D, BA NO(8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled ASTM A240Stainless Steel 304 Plate, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc. |
| Stainless 304 Sheet ASTM | ASTM A240 |
| Stainless 304 Sheet AMS | AMS 240 |
| Toleransi lebar dan ketebalan | ASTM-ASME-GB-EN-DIN-JIS |
| 304 Stainless Plate standards and approvals | EN ISO 18286 EN 10051 EN 10088-1 ISO 15510 EN ISO 9445 ASTM A 480 ASTM A 959 ASME IID |
| 304 Plate & Sheet Sizes | 1000 x 2000 mm, 1220 x 2440 mm, 1500 x 3000 mm, 2000 x 2000 mm, 2000 x 4000 mm,1500*6000,Cold rolled 304 Stainless Plate 0.5-6.4 mm,Hot rolled 304 Stainless Plate 3.0–60.0 mm |
| UNS 304 Plate Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard ASTM A240Stainless Steel 304 Sheet suppliers |
| Pemotongan | To provide a comprehensive service, we use a variety of cutting methods, including:Laser Plate Cutting,Plasma Plate Cutting,Oxy-propane Flame Cutting |
| Profil plasma | As per customer’s drawings |
| Value added services for 304 Stainless Plate | Pemotongan laser, pemotongan waterjet, pemotongan plasma, pembengkokan dan pemrosesan mekanis, persiapan tepi, pengelasan, penggergajian dan pemotongan. |
| Produsen | POSCO, Aperam, ATI, ThyssenKrupp, Baosteel, TISCO, ArcelorMittal, VDM, Nippon Metal, Outokumpu, Tsingshan, Delong. |
| China 304 Stainless Plate Manufacturer | ASTM A240Stainless Steel 304 Plate: material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width;304 Stainless Sheet: material under 3/16″ [5.00 mm] in thickness and 24″ [600 mm] and over in width;Steel Stainless 304 Clad plate: Steel Stainless 304 Clad plate is a composite steel plate made by bonding 304 Stainless 304 Plate, etc.ASTM A240Stainless Steel 304 Strip: cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width. |
| 304 Plate Origin | CHINA |
| Packing of 304 plate | Bundel dengan kain tahan air di luar atau kotak kayu lapis |
| Tes | UT, pengujian SGS, TUV dll |
| Why buy 304 Sheet from DAXUN? | Free quote、Free sample、EN 10204 3.1、Mill Test Certificate is supplied with shipment、NABL Approved Lab Reports、Any third party inspection is accepted、Tested to ASTM A923 Method “C” or ASTM G48 Method “A”.Minimum Nitrogen content and Ferrite Count TestGrade: AISI 304/S30400 Manufaktur: pelat canai dingin, pelat canai panas, pelat tempa Standar: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS Jenis: pelat tipis canai dingin, pelat tebal canai panas Permukaan: 2B, NO.1, NO.4, HL, BA, 8K, dll. Panjang: 2438mm3048mm6000mm dapat disesuaikan Asal TISCO, Baosteel, Posco, Tsingshan, Delong |
| Standar | Werkstoff Nr. | UNS | JIS | BS | GOST | AFNOR | EN | CN |
| SS 304 | 1.4301 | S30400 | SUS 304 | 304S31 | 08Х18Н10 | Z7CN18‐09 | X5CrNi18-10 | 06Cr19Ni10 |
| Kelas | C | Mn | Si | P | S | Cr | Ni | N |
| 304 | ≤0.08% | ≤2.0% | ≤ 0.75% | ≤0.045% | ≤0.030% | 18%-20% | 8.0%-10.5% | ≤0.10% |
| Jenis | Kekuatan Hasil 0,2% offset (KSI) | Kekuatan Tarik (KSI) | % Elongation(2″ Gauge length) |
| 304 Ann | 30 min. | 75 menit. | 40 min. |
| 304 ¼ Hard | 75 menit. | 125 menit. | 12 min. |
| 304 ½ Hard | 110 menit. | 150 menit. | 7 min. |
| 304L Ann | 25 menit. | 70 min. | 40 min. |
| 304L ¼ Hard | 75 menit. | 125 menit. | 12 min. |
| 304L ½ Hard | 110 menit. | 150 menit. | 6 min. |
| 304 & 304L | ||
| Kepadatan (lb./ in^2) @ RT | 0.29 | |
| Modulus Elastisitas dalam Ketegangan (psi x 10^6) | 28 | |
| Panas Spesifik (BTU/o F/lb.) | 32 hingga 212 oF | 0.12 |
| Konduktivitas Termal (BTU/jam/ft^2/ft) | 212oF | 9.4 |
| 932oF | 12.4 | |
| Koefisien Ekspansi Termal Rata-rata (dalam. x 10^-6 per o F) | 32 hingga 212oF | 9.2 |
| 32 hingga 600oF | 9.9 | |
| 32 hingga 1.000oF | 10.2 | |
| 32 to 1,200oF | 10.4 | |
| Resistivitas Listrik (mikro ohm - cm) | pada suhu 70oF | 72 |
| Rentang Titik Leleh (oF) | 2550 to 2650 | |
| Ketahanan Oksidasi - Layanan Berkelanjutan (oF) | 1,650 | |
| Ketahanan Oksidasi - Layanan Terputus-putus (oF) | 1,500 |
Pilih Daxun dan buat pelanggan Anda puas.

Pengiriman cepat
Daxun provides customers with timely and fast delivery of stainless steel plate products. Behind the speed is the system support from production capacity, information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Respon cepat
Daxun saves customers time, materials and stress, and ultimately saves them costs. With its professional advantages, Daxun can provide the most cost-optimized material recommendations based on customer needs, and can also reduce costs for customers through continuous processing, nesting processing, etc.

Pemesinan tingkat lanjut
Our advanced nesting processing method improves material utilization and cutting utilization. At the same time, Daxun can also achieve continuous cost reduction and efficiency improvement by promoting lean improvement activities, and return the benefits to customers. In addition, Daiming also has a complete product traceability system and rapid handling of quality objections, which makes customers worry-free.
304 stainless steel plate packaging
Daxun Alloy ensures the best quality of 304 stainless steel sheet packaging, because packaging plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Kotak dan peti
- Kertas kraft + palet kayu
- Kecilkan bungkus
- Palet kayu bebas fumigasi
- Kotak kayu bebas fumigasi

304 Stainless Steel Sheet Processing:
- Pemrosesan etsa
- Pemrosesan pengelasan
- Pemrosesan pembengkokan
- Pemrosesan timbul
- Pemrosesan sandblasting
- Pemrosesan pemolesan
- Pemrosesan meninju
- Pemrosesan stamping
SS 304 Plate Surface Treatment
1D: Permukaannya matte dengan bentuk partikel yang terputus-putus.
2D: Putih dengan nada keperakan.
2B: Abu-abu perak dengan kilap dan kerataan yang lebih baik daripada permukaan 2D.
Ba: Dekat dengan permukaan cermin dengan kilap dan daya pantul yang istimewa.
No.3: Kilauan yang bagus dan permukaan yang kasar.
No.4: Permukaannya memiliki garis-garis halus dan kilap yang bagus.
HL: Abu-abu perak dengan rambut keemasan.
8K: Permukaan cermin.
304 plate stainless steel Features
Let your brand improve rapidly
- Galeri
- TOLERANCE
- DELIVERY STATE
- Seri produk lainnya
| Toleransi untuk Lembar 2B | |||
| Ukuran | Peringkat Toleransi | ||
| Kelompok 1 | Kelompok 2 | Kelompok 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Toleransi untuk Pelat Canai Panas No.1 | |||
| Ukuran | Peringkat Toleransi | ||
| Kelompok 1 | Kelompok 2 | Kelompok 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Pilihan Status Pengiriman | Kondisi Permukaan |
| Digulung Dingin | 2B |
| 2D | |
| BA | |
| Garis rambut | |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Catatan: | |
| 1. Jika Anda memerlukan status pengiriman yang berbeda dari yang tercantum di atas, mohon konfirmasi dengan kami. | |
| 2. Jika ada pertanyaan atau pesanan, mohon beritahukan kepada kami persyaratan tambahan yang tidak disebutkan di sini. | |
| Status Pengiriman | |
| Pilihan Status Pengiriman | Kondisi Permukaan |
| Canai Panas | No.1 |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Acar | |
| Catatan: | |
| 1. Jika Anda memerlukan status pengiriman yang berbeda dari yang tercantum di atas, mohon konfirmasi dengan kami. | |
| 2. Jika ada pertanyaan atau pesanan, mohon beritahukan kepada kami persyaratan tambahan yang tidak disebutkan di sini. | |
| Kelas | Jenis | Ketebalan | Permukaan |
| Austenitik | 304/304H/304L/304J1 | 0,25-150mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0,3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferit | 430 | 0.4-3.0mm | 2B/BA/NO.4/8K/SB/HL |
| Ferit Ultra Murni | 443 | 0.4-2.0mm | 2B |
| 436L/439/444/441 | 0.5-3.0mm | 2B 、 2D | |
| 409L | 0,4-2,5 mm | 2B 、 2D | |
| Kelas | Jenis | Ketebalan | Asli |
| Baja tahan panas | 309S | 0,5-40mm | CHN |
| 310S | 0,5-40mm | CHN | |
| Baja Dupleks | 2101 | 1,5-50mm | CHN |
| 2304 | 3.0-50mm | CHN | |
| 2205 | 0,5-60mm | CHN | |
| 2507 | 1.0-60mm | SWE / JPN / CHN | |
| Baja Austenitik Super | N08904 | 0,6-50mm | SWE / JPN / CHN |
| S31254 | 0,5-50mm | SWE / JPN / CHN | |
| N08926 | 0,5-50mm | SWE / JPN / CHN | |
| N08367 | 0,5-50mm | SWE / JPN / CHN | |
| Paduan Dasar Nikel | N08031 | 1.0-50mm | AS / JPN / GER |
| N08810 / N08800 | 0,8-50mm | AS / JPN / CHN | |
| N08028 | 1.0-20mm | AS / JERMAN / JPN | |
| N08020 | 1.0-20mm | AS / JERMAN / JPN | |
| N08825 | 0,8-40mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0,5-50mm | AS / JERMAN / JPN | |
| N06022 | 1.0-50mm | AS / JERMAN / JPN | |
| N06625 | 0,8-20mm | AS / GER / CHN | |
| N04400 | 1.0-20mm | AS / JERMAN / JPN | |
| N06600 | 1.0-50mm | US / GER / JPN / CHN | |
| N02201 | 0,5-20mm | AS / JPN | |
| Titanium | TA1/Gr1 | 0,5-50mm | JPN / CHN |
| TA2/Gr2 | 0,5-50mm | JPN / CHN | |
| Bahan Pengelasan | ERNiCrMo-13 | 1.2 、 2.4mm | GER |
| ERNiCrMo-3 | 2.4mm | GER | |
| ERNiCrMo-4 | 2.4mm | AS |
The surface and shape of 304 stainless steel plate (6)
Informasi yang tersedia untuk referensi dan diunduh
Daxun adalah produsen pelat baja tahan karat yang dapat dipercaya
Sebagai produsen profesional, Daxun memastikan bahwa semua produk yang kami hasilkan berkualitas tinggi. Oleh karena itu, kami memastikan bahwa semua pelat baja tahan karat disertifikasi oleh ISO9001, SGS, CE, OQC, dan lebih banyak standar kualitas internasional, serta memiliki kontrol kualitas yang ketat untuk memastikan bahwa pelat baja tahan karat memiliki lebih sedikit cacat. Di Daxun, yakinlah bahwa semua produk tahan lama, berkualitas tinggi, dan berkinerja tinggi.
Proyek dan produk hot case terbaru
Produk Terkait (13)
Kami dapat menyediakan sampel lembaran baja tahan karat untuk Anda periksa kualitasnya. Sampel gratis dan Anda hanya membayar ongkos kirim.
Kami telah mengekspor ke lebih dari 42 negara, seperti Kanada, Chili, Kuwait, Jerman, Korea Selatan, Arab Saudi, Singapura, dll.
MOQ kami adalah 1 ton untuk lembaran baja tahan karat.
Pesanan percobaan dapat dikirim dalam waktu satu minggu. Untuk pesanan reguler, kira-kira membutuhkan waktu dua minggu.