  • Titanium tube Grade:Grade 5 -Ti6Al 4V- UNS R56400-3.7165-TC4
  • Ti tube types:Seamless titanium tube, drawn tube, forged titanium tube
  • Titanium tube density The density of grade 5 titanium is 4.51 g/cm3
  • Main standards: ASTM  ASME GB GJB EN JIS DIN ISO ATP BS  etc.
  • High strength, high temperature resistance, corrosion resistance, lightweight

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

A global leader in commercially pure titanium tube fabrication services

Daxun Alloy, as a leading titanium alloy tube manufacturer and supplier in China, provides high-quality Grade 5 titanium pipes to the world and has been well received by many projects.

Ti 6Al-4V (Grade 5 Titanium) is the most widely used of all titanium alloy tubes, accounting for more than 50% of the total titanium usage. It is usually used in the annealed state and has an operating temperature of up to 400°C (750°F). Ti 6Al/4V is welded with matching or ELI filler wire. Ti 6Al/4V has significantly higher strength than commercial pure titanium tubes, while having better stiffness and thermal properties (excluding thermal conductivity), and the thermal conductivity of Grade 5 titanium tube is about 60% lower than CP titanium. Among its many advantages, it can be heat treated. Thus, more ideal strength and performance are obtained. The advantages of using Grade 5 titanium seamless tubes include not only strong formability and low density, but also excellent corrosion resistance.

This grade is a perfect combination of strength, corrosion resistance, weldability and machinability. Therefore, it is widely used, such as in military aircraft or aviation industry, rocket parts, precision-guided components, armor parts, ship equipment, military vacuum equipment and other parts. The close version of 6-4, 6-4ELI, is also used in surgical implants. Typically, it is used in applications up to 400°C to improve ductility and toughness in cold working conditions. It also has excellent specific strength. It is usually provided in the annealed state and is easy to heat treat to increase strength for a variety of applications. As a general-purpose titanium alloy, Ti 6Al-4V titanium seamless tube has a wide range of ideal properties at temperatures around -210°C – 400°C. Grade 5 titanium alloy tube is the most commercialized of all titanium alloys. It combines high strength and toughness. Grade 5 titanium alloy tube has good welding and processing characteristics.

Titanium Alloy Grade 5 Seamless Pipe, Titanium Gr 5 High Pressure Pipe, ASTM B338 Titanium Alloy Gr 5 Seamless Pipe, Titanium Gr 5 Thick Wall Pipe. China Titanium Grade 5 ERW Pipe Supplier. Titanium Alloy Gr 5 Pipe, Titanium Gr 5 Electropolished Pipe, Anti-corrosion Titanium Pipe, Titanium Tube, ASTM B338 Titanium Grade 5 Welded Pipe, ASTM B861 / ASME SB861 Titanium Grade 5 Seamless Pipe China Titanium Gr-5 Seamless Pipe Manufacturer. Ti-6al-4v Pipe Dealer, ASTM B338 Titanium Grade 5 Pipe, Titanium Gr 5 Bright Annealed Pipe, Ti-6al-4v Pipe, Gr 5 Pipe, Titanium Gr 5 Pipe, Titanium WERKSTOFF NR 3.7165 Pipe

 

Are you looking to purchase titanium tubes for your project or order a range of titanium tubes? Daxun produces a wide range of titanium tubes including Grade 1 (3.7025), Grade 2 (3.7035), Grade 3 (3.7055), Grade 5 (3.7165), Grade 7 (3.7235), Grade 9 (3.7195) and Grade 12 (3.7105).

Buy titanium tubes at Daxun Alloys.
We offer a wide range of sizes starting from 1.0 mm in diameter with multiple variations, available directly from stock or custom made to your specifications through our network. We have wrought titanium tubes, seamless titanium tubes and longitudinally welded titanium tubes immediately available from stock for a wide range of applications.

We offer heat exchanger tubing in standard specifications such as ASTM B 338, ASME SB 338, DIN 17866 and VD TÜV welded titanium tubes or seamless titanium tubes. When it comes to titanium tubes, we have a large supply of titanium welded tubes and titanium seamless tubes in China in standard sizes up to 100 mm thick. We will supply welded titanium tubes for larger pipe sizes. The most common specifications used in the industry are ASTM B 861, ASFM B 862, NACE and NORSOK and VD TÜV Tube 230/2, depending on the specifications of the plant designer.

Titanium tube surface treatment options include bright annealing, pickling and grinding. Material parameters vary depending on the application and product requirements. The corrosion and mechanical properties of titanium alloy tubes vary. We are happy to assist you in evaluating your needs. If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee price and quantity for a specified period.

Daha fazla bilgi edinin

Veri

Ti-6Al-4V Grade 5 Titanium pipe & Tubes Specification ASTM B338 / ASTM B861 / ASTM B862 / ASME SB338 / ASME SB861 / ASME SB862
Grade 5 Titanium pipe & Tubes Grades Commercially pure titanium Grade 5-Ti-6Al4V- TC4- USN 56400
Grade 5 Titanium pipe & Tubes Type ot Rolled / Cold Drawn / Welded / ERW
Grade 5 Titanium pipe & Tubes Outer Diameter Size Titanium seamless pipe – φ1.0mm to φ508.3mm
Titanium welded pipe – φ6.0mm to φ1219mm
Grade 5 Titanium pipe & Tubes Wall Thickness 1.0mm—50mm (customizable wall thickness)
Grade 5 Titanium pipe & Tubes Length 5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size.
Titanium pipe Form Ti-6Al-4V ‘ Hollow, U’ bent, LSAW, Hydraulic, Straight Tube, Boiler, Round, Tube Coil, Square, Rectangular Etc
Marking  TC4 1.37165 All Titanium Tubes Tubing are marked as follows: Grade, Standard, Thickness, OD, Heat No., Length (Or according to the customer’s request.)
Uses of Titanium Alloy Tubes Gas pipes, oil pipes, heat exchanger tubes, boiler tubes, fluid pipes, titanium exhaust pipes.
Grade 5 Titanium pipe & Tubes Pipe Ends Plain Ends / Beveled Ends
Grade 5 Titanium pipe & Tubes Delivery Conditions As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered
Grade 5 Titanium pipe & Tubes Coating Electropolish, Mechanical Polish, Satin Finish, Passivated
Grade 5 Titanium pipe & Tubes Other Testing ardness Test, Hydrostatic Test, Eddy Current test, Eddy Current, Tensile Test, Flattening, Flare Test, Annealed, Hydrostatic Test, Tempered, Stress Relieved etc.
Grade 5 Titanium pipe & Tubes Dimension All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME
Grade 5 Titanium pipe & Tubes Value Added Services Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment
Grade 5 Titanium pipe & Tubes Packaging Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector
Grade 5 Titanium pipe & Tubes Shipment & Transportation By Road – Truck / Train, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes
Grade 5 Titanium pipe & Tubes Material Test Certificate Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS ETC
Kimyasal Bileşim:
Sembol Element Min % Maksimum %
Al Alüminyum 5.50% 6.75%
V Vanadyum 3.50% 4.50%
Fe Demir 0.30%
O Oksijen 0.20%
C Karbon 0.08%
N Azot 0.05%
H Hidrojen 0.01%
Y İtriyum 0.01%
Diğer, her biri 0.10%
Diğer, toplam 0.40%
Ti Titanyum Kalan
Fiziksel Özellikler Metrik İngilizce Yorumlar
Yoğunluk 4,43 g/cc 0,16 lb/in³
Mekanik Özellikler
Sertlik, Brinell 334 334  Rockwell C.'den tahmin edilmiştir.
Sertlik, Knoop 363 363  Rockwell C.'den tahmin edilmiştir.
Sertlik, Rockwell C 36 36
Sertlik, Vickers 349 349  Rockwell C.'den tahmin edilmiştir.
Çekme mukavemeti min. 895MPa 129810 psi
Akma dayanımı min. 828MPa 120090 psi
Kopma Uzaması min.10 % 10 %
Alanın Azaltılması min.25 % 25 %
Elastisite Modülü 113,8 GPa 16500 ksi
Basınçlı Akma Dayanımı 970 MPa 141000 psi
Çentikli Çekme Dayanımı 1450 MPa 210000 psi  Kt (stres konsantrasyon faktörü) = 6,7
Nihai Taşıma Gücü 1860 MPa 270000 psi  e/D = 2
Yatak Akma Dayanımı 1480 MPa 215000 psi  e/D = 2
Poisson Oranı 0.342 0.342
Charpy Darbe 17 J 12,5 ft-lb  V-notch
Yorulma Dayanımı 240 MPa 34800 psi  1E+7 döngüde. Kt (gerilim yoğunlaşma faktörü) = 3,3
Yorulma Dayanımı 510 MPa 74000 psi  Çentiksiz 10.000.000 Döngü
Kırılma Tokluğu 75 MPa-m½ 68,3 ksi-in½
Kayma Modülü 44 GPa 6380 ksi
Kesme Dayanımı 550 MPa 79800 psi  Nihai kesme mukavemeti
Elektriksel Özellikler
Elektriksel Dirençlilik 0.000178 ohm-cm 0.000178 ohm-cm
Manyetik Geçirgenlik 1.00005 1.00005  1,6kA/m'de
Manyetik Duyarlılık 3.30E-06 3.30E-06  cgs/g
Termal Özellikler
CTE, doğrusal 20°C 8,6 µm/m-°C 4,78 µin/in-°F  20-100ºC
CTE, doğrusal 250°C 9,2 µm/m-°C 5,11 µin/in-°F  20-315ºC aralığında ortalama
CTE, doğrusal 500°C 9,7 µm/m-°C 5,39 µin/in-°F  20-650ºC aralığında ortalama
Özgül Isı Kapasitesi 0,5263 J/g-°C 0,126 BTU/lb-°F
Termal İletkenlik 6,7 W/m-K 46,5 BTU-in/hr-ft²-°F
Erime Noktası 1604 - 1660 °C 2920 - 3020 °F
Solidus 1604 °C 2920 °F
Liquidus 1660 °C 3020 °F
Beta Transus 980 °C 1800 °F
Beta Transus (K ± 25) 1830
Termal Genleşme Katsayısı (10-6in./in./F) 32-212 5
32-600 5.3
32-1000 5.6
32-1200 5.9
32-1500 6.1
Yoğunluk (lbs./cu. in.) 0.16
Erime Noktası, Yaklaşık (F) 3200
Oda Sıcaklığında Elektriksel Direnç (Microhms cm) 171
Elastisite Modülü - Gerilim (106 psi) 16.5
Elastisite Modülü - Burulma (106 psi) 6.1
Termal İletkenlik Oda Sıcaklığında 3,9
(Btu/saat/metrekare ft./F/ft.)
Oda Sıcaklığında Özgül Isı (Btu/lb./F). 0.135
Kaynaklanabilirlik Adil
Tavlama Sıcaklığı (F) Tam 1300 - 1525°/15 Dk. - 2 Saat,; Hava Soğutmalı
Stres Giderici 900 - 1200°/1 -4 Saat; Hava Soğutmalı
Dövme* Sıcaklık (F) Engelleme 1750 - 1800°
Bitirme 1650 - 1750°
Tipik Uygulama Kompresör kanatları, diskler, uçak bileşenleri, basınçlı kaplar, roket motoru kasaları;
en çok yönlü titanyum alaşımıdır.
Titanium Grade 5 Pipes 4 inch Ti Alloy Grade 5 Seamless Pipes
Ti Alloy Grade 5 Pipes Titanium gr 5 Welded Pipes
Grade 5 Titanium Seamless Steel Pipes Titanium UNS R56400 Cold Drawn Welded Pipes
Ti Alloy Grade 5 Welded Pipes Grade 5 Pure Titanium Cold Drawn Pipes
Titanium gr 5 ERW Pipes Schedule 5S Grade 5 Titanium Seamless Pipe
Grade 5 Pure Titanium EFW Pipes Schedule 40 Titanium 3.7165 Pipes
Grade 5 Titanium Cold Drawn Seamless Pipes Titanium gr 5 Precision Pipes
Alloy Grade 5 Seamless Steel Precision Pipes High pressure ASTM B337 Titanium Grade 5 Pipes
Titanium 3.7165 Cold Drawn Seamless Pipes Titanium Alloy Grade 5 Electropolished Pipes
Ti Alloy Grade 5 Custom Pipes Titanium Grade 5 Cold Drawn Pipes
UNS R56400 Round Pipes Gr 5 Ti Exhaust Pipes
Gr 5 Titanium Rectangular Pipes Small diameter Titanium Alloy Grade 5 Pipes
Grade 5 Titanium Hexagonal Pipe Ti Alloy Grade 5 Pipe material
UNS R56400 Welded Pipe Grade 5 Titanium Hexagonal Pipe
Ti Alloy Grade 5 Welded Pipe Titanium Alloy Gr 5 Pipe
Titanium Gr 5 EFW Pipe Grade 5 Titanium Seamless Pipe
Alloy Grade 5 Bush Hex Pipe DIN 3.7165 Precision Steel Pipes
Grade 5 Pure Titanium Fabricated Pipe UNS R56400 Annealed pipe
Ti Grade 5 Beveled End Pipe Grade 5 Pure Titanium Rectangle Pipe
ASTM B337 Titanium Grade 5 Cold Drawn Pipe Cold Drawn Alloy Grade 5 Welded Pipe
Titanium Grade 5 Seamless Tubes Titanium Alloy Gr 5 Welded Tubes
Titanium Gr 5 High Pressure Tube Titanium UNS R56400 Welded Tube
ASTM B338 Titanium Alloy Gr 5 Seamless Tubing Ti. Alloy WERKSTOFF NR. 3.7165 Welded Tubes
Titanium Alloy Gr 5 Tubes ASTM B338 Gr.5 Titanium Welded Tubes
Titanium Gr 5 Santiary Tube Grade 5 Alloy Round Tube
Titanium Gr 5 Cold Rolled Coiled Tube Grade 5 Titanium Alloy Round Tubes
Gr 5 Titanium Welded Tubes Titanium Grade 5 Round Tube
Dealer of ASTM B338 Titanium Grade 5 Tube UNS R56400 Round Tubes
Titanium Gr 5 Decorative Tube Titanium Alloy Gr 5 Round Tube
Gr 5 Titanium Bright Annealed Tube ASME SB338 Gr 5 Titanium Round Tubes
Ti. Alloy Grade 2 ERW Tubes UNS R56400 Gr5 Ti Alloy Tubing
Titanium UNS R56400 Tubing Grade 5 Ti Tubing
Titanium NCF Gr 5 Tubes ASTM B558 Titanium Alloy Welded Tubes
Titanium Gr 5 Tubing WERKSTOFF NR. 3.7165 Gr5 Titanium Tubes
Titanium WERKSTOFF NR. 3.7165 Tubing Ti-6Al-4V Tube
Titanium Alloy Gr 5 Tubing Titanium Alloy Grade 5 Seamless Tubes
Titanium Gr 5 Electropolish Tube Titanium Alloy Grade 5 Round Tube
ASTM B338 Titanium Grade 5 Welded Tubing Titanium Grade 5 Elliptical and Oval Tubes
Grade 5 Titanium Alloy Seamless Tubing Titanium Grade 5 Rectangular Tube
Titanium Grade 5 Welded Tubes0 Titanium Grade 5 Sighting Tube
Gr 5 Titanium Heat Exchanger Tube Titanium Grade 5 Polish Tubes
ASTM B338 Titanium Gr 5 Tube Titanium Grade 5 Aerospace tubes
Gr 5 Titanium Tubing Titanium Grade 5 High Pressure Tube
Titanium Grade 5 Tube Titanium Alloy Grade 5 Coiled Tubing
Grade 5 Titanium Alloy Seamless Tubes Grade 5 Titanium Capillary Tubing
Titanium Grade 5 Welded Tube Titanium Alloy Grade 5 Seamless Tubing
Titanium Alloy Grade 5 Tubing Titanium Grade 5 Condenser Tubes
Grade 5 Ti. Alloy Tubing Titanium Grade 5 Aero engine tubes
Ti. Alloy Gr 5 Seamless Tubes Titanium Alloy Grade 5 Straight Tube boiler
Gr 5 Alloy Seamless Tube Titanium Grade 5 Furnace Tube
Titanium Alloy Gr.5 Seamless Tubes Grade 5 Titanium Seamless Tube
UNS R56400 Seamless Tube Grade 5 Titanium Tube
WERKSTOFF NR. 3.7165 Seamless Tubes Titanium Grade 5 Tubing
ASME SB338 Gr.5 Titanium Seamless Tube Grade 5 Alloy Welded Tube
Titanium Alloy Grade 5 Welded Tubes Titanium Grade 5 Seamless Tubes

Projenizin yükselmesine yardımcı olmak için Daxun'u seçin.

Daxun ile şimdi iletişime geçin

Advanced Production:Titanium seamless pipe

  • Grade 5 steel seamless pipes are processed by hot turning or hot pressing, straightening, inner and outer diameter processing, and can be provided in heat treatment or non-heat treatment forms. / Hot rolled seamless pipe: outer diameter 1.0mm to 325mm, wall thickness 0.3mm to 50mm, length up to 12000mm. Cold rolled seamless pipe: cold processed pipes are heat treated, surface engraved, water pressure tested or ultrasonically tested according to the manufacturing standards of outer diameter 6mm to 102mm, wall thickness 0.5mm to 20mm, and length up to 9000mm.
    (The above is determined according to the specific situation of the manufacturer and the customer)
Daxun ile şimdi iletişime geçin

Grade 5 Titanium Tube Features

Ti-6Al4V Grade 5 Titanium Alloy Tube is the most commercially available of all Titanium alloys. It combines high strength and toughness. Grade 5 Titanium alloy has good welding and processing characteristics:

  • High Strength Titanium Alloy
  • Heat Treatable
  • Good Ductility
  • Good Machinability
  • Good Weldability

We stock and sell Grade 5 Titanium Alloy Seamless Tubes, Forged Seamless Tubes, Welded Tubes, etc.

Daxun ile şimdi iletişime geçin

Advanced Production: Forged Titanium Alloy Tube

Forged Titanium Seamless Tubes: Diameters range from 100mm to 1219mm, wall thickness ranges from 5mm to 100mm (depending on diameter), lengths up to 2000mm, made from Grade 5 Titanium. Forged Titanium alloy tubes undergo multiple forgings to achieve more uniform grains and metallographic structures, better performance and stability, and are finally heat treated. Before the finished products are packaged according to customer specifications, they undergo mechanical testing, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing. Manufacturing technology as well as inspection and testing equipment ensure that forged 6-4 titanium tubes meet ASTM and ASME specifications.

Daxun ile şimdi iletişime geçin

Test Raporları

The test reports we provide include: Factory test certificate for Grade 5 Titanium Seamless Pipe and Ti-6al-4v Titanium Seamless Pipe, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, NABL Approved Laboratory Report, Destructive Test Report, Non-destructive Testing Report. (DaXun will provide according to customer requirements)

Daxun ile şimdi iletişime geçin

Applications and standards

Grade 5 titanium tubes are widely used in the following industries under extreme corrosive conditions:

  • Chemical processing parts, military industry, aerospace, chemical energy, marine engineering, oil and gas industry, rockets and missiles, military armor, ships and vessels, industrial machinery, power industry, paper and pulp industry, pharmaceutical and food processing equipment, etc.
  • Specifications: ASTM B861, B862, B338 / ASME SB861, SB862, SB338
  • Standards: ASTM, GB, GJB, ASME and API
Daxun ile şimdi iletişime geçin

Kalite, teslimat, denetim

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 1 Titanium Welded Pipe and Grade 1 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • Teslimat süremiz kesinlikle sözleşmeye uygundur.
  • Müşterinin üçüncü taraf acentelerinin denetim için fabrikaya gitmesine destek olun
  • Müşteri testleri için ücretsiz numune desteği
  • Yerinde veya video fabrika denetimini destekleyin
Daxun ile şimdi iletişime geçin

Paketleme

Daxun Alloy ensures the best quality of titanium tube packaging, because it plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Kutular ve kasalar
- Shrink ambalaj
- Ahşap paletler
- Ahşap kutular

Daxun ile şimdi iletişime geçin

Teknik Destek

Herhangi bir ek teknik yardıma ihtiyacınız olursa, yerleşik metalürji uzmanımız ve bilgili personelimiz size yardımcı olmaktan memnuniyet duyacaktır. Ayrıca Daxun, çoklu metal ve plastik envanter endüstrisinde bir ilk olan sertifikalı bir test laboratuvarına sahiptir. Bu, bize göre, kaliteye olan sarsılmaz bağlılığımızı ve tam hizmet tedarikçisi olarak felsefemizi göstermektedir.

Grade 5 Titanium TUBE Features

Yüksek mukavemetli
Korozyon direnci
Isı direnci
Düşük sıcaklık direnci
Çevre koruma
Hafif

Daxun Grade 5 Titanium TUBE Let your brand improve rapidly

Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of pipe/tube Bar and Tube.
Ürünler/İşleme Standardı Sınıf / Boyut
Titanium pipe/tube, — ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7, GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3 (Kalınlık: ( 0.0197”-6”) Maksimum Genişlik: 12 fit, Maksimum Uzunluk: 50 fit)
AMS-T-9046
Titanium and Titanium alloy pipe/tube
Ticari olarak saf titanyum (CP)
Kod tanımı Akma dayanımı
minimum, ksi 1 /
CP-1 70
CP-2 55
CP-3 40
CP-4 25
Alfa titanyum alaşımları(A)
Kod tanımı Kompozisyon
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0,8Mo
A-4 8A1-1Mo-1V
Alfa-beta titanyum alaşımları (AB)
Kod tanımı Kompozisyon
AB-1 6A1-4V
AB-2 6A1-4V (ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
Beta titanyum alaşımları (B)
Kod tanımı Kompozisyon
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
İşleniyor:
Sıcak Haddeleme Soğuk Haddeleme
Mevcut Sınıflar:
CP Sınıf 1 Sınıf 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP Sınıf 2 Sınıf 6Al-4V ELI (Eski Sınıf 23)
7. Sınıf Sınıf 6Al-6V-2Sn (6-62)
19. Sınıf Sınıf 8Al-1Mo-1V (8-1-1)
5. Sınıf (6Al-4V) 9. Sınıf (3Al-2,5V)
Sınıf 6 (5Al-2,5Sn) CP Sınıf 3
Uygulama
Kimya Endüstrisi Deniz Suyunun Tuzdan Arındırılması
Petrokimya Endüstrisi Havacılık ve Uzay
Talaşlı İmalat Alanı, Otomobil Alanı Cep Telefonu Bileşen Alanı.
urface Finish İç Yüzey (ID) Dış Yüzey (OD)
Pürüzlülük Ortalaması (RA) Pürüzlülük Ortalaması (RA)
μ inç μm μ inç μm
BA Beight Tavlı 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
EP Elektro Cila 15,10,7,5 0.38,0.25,0.20;0.13 32 0.8
MP Mekanik Cila 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
AP Tavlanmış & Salamura Tanımlanmamış Tanımlanmamış 40 veya Tanımlanmamış 1.0 veya Tanımlanmamış
Titanium Grade 5 Seamless Pipe Titanium DIN 3.7165 Seamless Pipe
Titanium UNS R56400 Seamless Pipe
Titanium Grade 5 Seamless Pipes
Titanium Alloy Gr.5 Seamless Pipe
ASTM B337 Titanium Grade 5 Seamless Pipe
ASME SB337 Ti Alloy Gr.5 Seamless Pipes
Titanium Grade 5 Welded Pipe Titanium DIN 3.7165 Welded Pipe
Titanium UNS R56400 Welded Pipe
Titanium Grade 5 Welded Pipes
Titanium Alloy Gr.5 Welded Pipe
ASTM B337 Titanium Grade 5 Welded Pipes
ASME SB337 Ti Alloy Gr.5 Welded Pipes
Titanium Grade 5 Round Pipe Titanium DIN 3.7165 Round Pipe
Titanium UNS R56400 Round Pipes
Titanium Grade 5 Round Pipes
Titanium Alloy Gr.5 Round Pipe
Titanium Grade 5 Round Pipe
Ti Alloy Gr.5 Round Pipes
Titanium Gr.5 Seamless Tubes Titanium DIN 3.7165 Seamless Tubes
Titanium UNS R56400 Seamless Tubes
Titanium Grade 5 Seamless Tubing
Titanium Alloy Gr.5 Seamless Tubes
ASTM B338 Titanium Gr.5 Seamless Tubing
ASME SB338 Ti Alloy Grade 5 Seamless Tubes
Titanium Grade 5 Welded Tubes Titanium DIN 3.7165 Welded Tubes
Titanium UNS R56400 Welded Tubes
Titanium Grade 5 Welded Tubing
Titanium Alloy Gr.5 Welded Tubes
ASTM B338 Titanium Grade 5 Welded Tubing
ASME SB338 Ti Alloy Gr.5 Welded Tubes
Titanium Grade 5 Round Tubes Titanium DIN 3.7165 Round Tubes
Titanium UNS R56400 Round Tubes
Titanium Grade 5 Round Tubing
Titanium Alloy Gr.5 Round Tubes
Titanium Grade 5 Round Tubing
Ti Alloy Gr.5 Round Tubes
Titanium Grade 5 Pipe Titanium DIN 3.7165 Pipe
Titanium UNS R56400 Pipes
Titanium Grade 5 Pipe
Titanium Alloy Gr.5 Pipes
Titanium Grade 5 Pipes
Ti Alloy Gr.5 Pipe
Titanium Grade 5 Tube Titanium DIN 3.7165 Tubes
Titanium UNS R56400 Tube
Titanium Grade 5 Tubing
Titanium Alloy Gr.5 Tubes
Titanium Grade 5 Tubes
Ti Alloy Gr.5 Tubes

 

NPS Dış Çap Duvar Kalınlığı Ağırlık Ağırlık
içinde mm içinde mm Sched kg/Mtr Lb/ft
1/2″ 0.84 21 0.109 2.769 40 STD 1.268 0.851
0.147 3.734 80 STD 1.621 1.088
3/4″ 1.05 27 0.113 2.87 40 STD 1.684 1.131
0.154 3.912 80 STD 2.195 1.474
1″ 1.315 33 0.133 3.378 40 STD 2.501 1.679
0.179 4.547 80 STD 3.325 2.172
1 1/4″ 1.66 42 0.14 3.556 40 STD 3.385 2.273
0.191 4.851 80 STD 4.464 2.997
1 1/2″ 1.9 48 0.145 3.683 40 STD 4.048 2.718
0.2 5.08 80 STD 5.409 3.361
2″ 2.375 60 0.154 3.912 40 STD 5.441 3.653
0.218 5.537 80 STD 7.48 5.022
2 1/2″ 2.875 73 0.203 5.516 40 STD 8.629 5.793
0.276 7.01 80 STD 11.411 7.661
3″ 3.5 89 0.216 5.486 40 STD 11.284 7.576
0.3 7.62 80 STD 15.272 10.253
4″ 4.5 114 0.237 6.02 16.073 10.79
0.337 8.56 22.318 14.983
6″ 6.625 168 0.188 4.775 19.252 12.924
0.203 5.516 20.739 13.923
0.219 5.563 22.318 14.983
0.25 6.35 25.354 17.021
0.28 7.112 40 STD 58.263 18.974
0.312 7.925 31.334 21.036
0.375 9.525 37.285 25.031
0.432 10.973 80 XHY 42.561 28.573
0.5 12.7 48.719 32.708
8″ 8.625 219 0.188 4.775 25.233 16.94
0.203 5.156 27.198 18.259
0.219 5.563 29.286 19.661
0.25 6.35 20 33.308 22.361
0.277 7.036 30 36.786 24.696
0.322 8.179 40 42.352 28.554
0.375 9.525 49.216 33.041
0.406 10.312 60 53.085 35.638
0.5 12.7 80 XHY 64.627 43.388
10″ 10.75 273 0.188 4.775 31.588 21.207
0.219 5.563 36.689 24.631
0.25 6.35 20 41.759 28.035
0.307 7.798 30 51.002 34.24
0.344 8.738 56.946 38.231
0.365 9.271 40 STD 63.301 40.483
0.438 11.125 71.852 48.238
0.5 12.7 60 XHY 81.53 54.735
0.594 15.088 80 95.969 64.429
12″ 12.75 324 0.188 4.775 37.57 25.222
0.219 5.563 43.657 29.309
0.25 6.35 49.713 33.375
0.281 7.137 55.739 37.42
0.312 7.925 61.735 41.445
0.375 9.525 73.824 49.562
0.406 10.312 79.727 53.525
0.5 12.7 97.438 65.415
0.562 14.275 108.966 73.154
14″ 14 356 0.188 4.775 41.308 27.732
0.219 5.563 48.012 32.233
0.25 6.35 20 54.685 36.713
0.281 7.137 61.327 41.172
0.312 7.925 67.939 45.611
0.375 9.525 STD 81.281 54.568
0.438 11.125 40 94.498 63.441
0.5 12.7 XHY 107.381 72.09
0.625 15.875 132.983 89.278
16” 16 406 0.188 4.775 47.29 21.748
0.219 5.563 54.98 36.91
0.25 6.35 10 62.639 42.053
0.281 7.137 70.268 47.174
0.312 7.925 20 77.866 52.275
0.344 8.738 85.677 57.519
0.375 9.525 30 93.213 62.578
STD
0.438 11.125 108.433 72.797
0.5 12.7 40 123.289 82.77
XHY
18″ 18 457 0.219 5.563 61.948 41.588
0.25 6.35 70.593 47.393
0.281 7.137 79.208 53.176
0.312 7.925 20 87.792 58.939
0.375 9.525 STD 105.144 70.588
0.438 11.125 30 122.369 82.152
0.5 12.7 XHY 139.198 93.45
0.562 14.275 40 155.904 104.666
0.625 15.875 172.754 115.978
20″ 20 508 0.25 6.35 78.547 52.733
0.282 7.163 88.458 59.386
0.312 7.925 97.719 65.604
0.375 9.525 20 STD 117.075 78.598
0.438 11.125 136.305 91.508
0.5 12.7 30 XHY 155.106 104.13
0.594 15.088 40 183.378 123.11
0.625 15.875 192.64 129.328
0.688 17.475 211.368 141.901
24″ 24 610 0.25 6.35 94.456 63.413
0.281 7.137 106.029 71.183
0.312 7.925 117.573 18.932
0.375 9.525 20 STD 140.938 64.618
0.438 11.125 164.176 110.219
0.5 12.7 XHY 186.923 125.49
0.625 15.875 232.41 156.028
0.688 17.475 40 255.148 171.293
0.75 19.05 277.401 186.233
30″ 30 762 0.25 6.35 118.318 79.433
0.281 7.137 132.851 89.189
0.312 7.925 10 147.353 98.925
0.375 9.525 STD 176.731 118.648
0.438 11.125 205.983 138.286
0.5 12.7 20 XHY 234.647 157.53
0.625 15.875 30 292.066 196.078
0.688 17.475 320.817 215.38
0.75 19.05 348.988 234.293
36″ 36 914 0.25 6.35 142.18 95.453
0.281 7.137 159.672 107.196
0.312 7.925 10 177.133 118.918
0.375 9.525 STD 215.525 142.678
0.438 11.125 247.79 166.353
0.5 12.7 20 XHY 282.372 198.57
0.625 15.875 351.723 236.128
0.688 17.475 386.487 259.467
0.75 19.05 420.576 282.353
42″ 42 1067 0.312 7.925 206.914 138.911
0.375 9.525 STD 248.319 166.708
0.5 12.7 XHY 33.097 221.61
0.75 19.05 492.163 330.413
48″ 48 1219 0.375 9.525 STD 284.112 190.738
0.438 11.125 331.404 222.487
0.5 12.7 XHY 377.822 253.65
0.75 19.05 563.75 378.473
0.875 22.225 655.969 440.383

Grade 2 titanium tube form (4)

  • Titanium seamless pipe is made by perforating and drawing solid titanium rod, and the hollow part of the pipe is made by perforation or hot extrusion process. Titanium seamless pipe is an ideal choice for very large diameter to wall thickness ratio and has very good external dimension tolerance.

  • Titanium welded pipe is a tubular product made of strip titanium that is roll formed and fusion welded along the longitudinal seam. The welding process used by Daxun Alloy does not use any filler metal during the welding process.

  • Titanium square tubes are drawn from round tubes or round tube billets and can be formed into right angles or rounded corners. They can also be cold extruded, which is efficient and low cost. The only disadvantage is that the tolerance will gradually increase.

  • Tubular products are welded and then re-drawn to final size. Welding and drawing is ideal for producing thick walled, large diameter tubes that cannot be welded directly to size but still offer cost savings over seamless tubes. All Daxun welded and drawn tubes are bright annealed.

Referans ve indirme için mevcut bilgiler

Daxun is a reliable manufacturer of grade 5 titanium tubes

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel plates have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

Güncel sıcak vaka projeleri ve ürünleri

Grade 5 Titanium pipe and tube
Grade 5 Titanium pipe and tube
6al 4v Titanium pipe and tube
Titanium pipe and tube 6al 4v
6al 4v Titanium pipe and tube
6al 4v Titanium pipe and tube
Titanium pipe and tube 6al 4v
Titanium pipe and tube 6al 4v
Titanium pipe and tube 6al 4v
Commercially Pure Titanium Tube Grade 5/UNS R56400/Ti-6AL-4V

Ti-6Al-4V- Grade 5 Titanium tube

  • Titanium Alloy-(UNS R56400)

INTRODUCTION

  • DAXUN Ti-6Al-4V, Grade 5 Alloy Tube (UNS R56400) is the most popular titanium alloy. It is a duplex alpha+beta titanium alloy that uses aluminium as an alpha stabiliser and vanadium as a beta stabiliser. This high-strength alloy can be employed at cryogenic temperatures of around 800°F (427°C). ATI Ti-6Al-4V, Grade 5 alloy is used in annealing, solution treatment, and ageing. Compressor blades, discs, and rings for jet engines; fuselage and space capsule components; pressure containers; rocket engine cases; helicopter rotor hubs; fasteners; and crucial forgings with a high strength-to-weight ratio.
  • The alloy is initially melted using vacuum arc (VAR), electron beam (EB) or plasma arc hearth melting (PAM). Remelting is achieved in one or two vacuum arc steps.

ÖZELLİKLER

•ASTE B338 – Tubes Titanium tubes standard heat treatable
• AMS 4928 – Forgings and forging stock (annealed)
• AMS 4965 – Forgings (solution treated and aged)
• AMS 4967 – Forgings (annealed, heat treatable)

FİZİKSEL ÖZELLİKLER

  • Melting Range: 2,800-3,000°F (1,538 – 1,649°C)
  • Density: 0.160 lbs/cu. in.; 4.47 gm/cc
  • Beta Transus Temperature: 1830°F (± 25°); 999°C (± 14°)

ISI TEDAVİSİ

  • Annealing at 1,700-1,900°F (927 – 1,038°C) is done where high hardness, tensile and fatigue strength are desired.
  • DAXUN 6-4™, Grade 5 Alloy can be heat treated in several ways.
  • 1. Tavlama: 1.275 -1.400°F; (691 - 760°C), ½ ila 2 saat, hava veya fırın soğutması
  • 2. Gerilim Giderme Tavlaması: 1.000 -1.200°F; (538 - 649°C), 1 ila 8 saat, hava veya fırın soğutması
  • 3. Solution Heat Treatment: 1,675 -1,750°F; (913 – 954°C), 1 hour, water quench
  • 4. Aging Treatment: 975 -1,025°F; (524 – 552°C), 4 to 8 hours – air cool
  • The very best of properties In the solution treated and aged condition, small cross sections are obtained that are rapidly
    quenched. Larger sections sizes and/or a quench delay may cause properties to be lower than the optimum values.

SERTLİK

Tavlanmış durumda tipik sertlik Rockwell C 30-34 ve çözelti ve yaşlandırılmış durumda yaklaşık Rockwell C 35-39'dur.

FORGEABILITY/ FORMABILITY

  • DAXUN Ti-6Al-4V, Grade 5 alloy tubes are forged at 1,750°F (954°C), with an end forging temperature of 1,450°F (788°C). For optimal results, a reduction of at least 35% is recommended.
  • DAXUN Ti-6Al-4V, Grade 5 alloy is difficult to form at room temperature, even when annealed. As a result, harsh forming operations like bending or stretching can be conducted on annealed material at temperatures as high as 1,200°F (649°C) without altering its mechanical qualities. Creep forming can be used for hot sizing or forming at temperatures ranging from 1,000 to 1,200°F (538 to 649°C).

MACHINABILITY

  • DAXUN  Ti-6Al-4V, Grade 5 alloy can be machined using practices for austenitic stainless steels with slow speeds, heavy feeds, rigid
    tooling, and large amounts of non-chlorinated cutting fluid.

WELDABILITY

  • DAXUN Ti-6Al-4V Grade 5 Alloy Titanium Tube is easily welded in the annealed or solution and partially aged form, with ageing.
  • done during the post-weld heat treatment. Precautions must be made to avoid contamination by oxygen, nitrogen, and hydrogen. Fusion welding can be performed in an inert gas-filled chamber or with an inert gas tail shield applied to the molten metal and nearby hot zone. Spot welding, seam welding, and flash welding can all be performed without the use of a protective environment.

SPECIAL PRECAUTIONS

  • DAXUN Ti-6Al-4V, Grade 5 alloy may be contaminated with hydrogen as a result of incorrect pickling, as well as the absorption of oxygen, nitrogen, and carbon during forging, heat treatment, brazing, and so on. This contamination may reduce ductility, compromising notch sensitivity and forming properties.
Hangi titanyum sınıfı en iyisidir?

İhtiyacınız olan titanyum alaşımı sınıfı, üzerinde çalıştığınız projeye bağlıdır, çünkü her sınıfın farklı faydaları vardır.

Titanyum alaşımının tüm sınıfları son derece güçlü ve korozyona dayanıklıdır, bu da en zorlu koşullarda bile iyi çalışmaya devam edecekleri anlamına gelir.

Titanyum alaşımının daha yüksek dereceleri (5-12) belirli faydalar için tasarlanmış alaşımlardır. Örneğin, 12. sınıf titanyum alaşımı mükemmel ısı direncine sahiptir, bu da onu kabuk ve borulu ısı eşanjörleri, hidrolik borular ve kimya endüstrisi ekipmanları için mükemmel bir seçim haline getirir.

1-4. Sınıflar saf titanyum alaşımlarıdır ve boru sistemleri ve borular için kaynaklanabilir, sünek bir malzemeye ihtiyacınız varsa mükemmel bir seçimdir. Denizcilik ve endüstriyel endüstrilerde kullanılan daha düşük kaliteler bulacaksınız.

Bir projeye başlıyorsanız ve hangi titanyum alaşımının sizin için en iyisi olduğundan emin değilseniz, bugün bizimle iletişime geçin; size yardımcı olmaktan mutluluk duyarız.

Daha yüksek titanyum sınıfları daha düşük sınıflardan nasıl farklıdır?

DAXUN'da, 1. sınıftan 12. sınıfa kadar çok çeşitli titanyum alaşım kaliteleri sunuyoruz.

1-4. sınıflar saf titanyumdur, daha yüksek sınıflar ise alaşımlardır.

Alaşım kaliteleri, yüksek mukavemet/ağırlık oranları nedeniyle popülerdir.

Bulduğumuz en yaygın kullanılan titanyum alaşım sınıfı 5. sınıftır. Titanyum oranı hala yüksek olsa da, bu sınıf en güvenilir olanlardan biridir çünkü 600 ° F'ye kadar sıcaklıklara dayanabilir ve aşırı koşullara dayanabilir.

Daha yüksek kaliteler, aşınma ve korozyon dirençleri nedeniyle havacılık ve denizcilik endüstrileri gibi endüstriler tarafından tercih edilmektedir.

Buna karşılık, daha düşük kaliteler daha düşük mukavemetleri nedeniyle öncelikle kaynak için kullanılır.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

Titanyum sınıfı maliyeti etkiler mi?

Titanyum sınıfı maliyeti biraz artırsa da, toplam maliyet öncelikle ihtiyacınız olan titanyum şekli ve formu tarafından belirlenir.

DAXUN'da, plakalar, tüpler, bobinler ve çubuklar dahil olmak üzere çok çeşitli titanyum ürünleri sunuyoruz. İhtiyacınız olan her bir ürünün uzunluğu, genişliği ve miktarı, ödeme sırasında ödeyeceğiniz tutarı etkileyecektir.

Ne yazık ki, projeniz ve titanyumun ne için kullanılacağı hakkında çok fazla bilgi sahibi olmadan çevrimiçi bir fiyat bulmak zordur.

Neyse ki, uzman ekibimiz titanyum ihtiyaçlarınız konusunda size yardımcı olmak ve tavsiyelerde bulunmak için her zaman burada. [email protected] adresine bir e-posta göndererek, size bazı tavsiyeler ve doğru bir fiyat teklifi ile geri dönebileceğiz.

İhtiyaçlarınızı daha iyi anlamak için ihtiyacınız olan titanyum sınıfı, şekli ve miktarı hakkında mümkün olduğunca fazla bilgi eklediğinizden emin olun.

Titanyum kaliteleri hakkında daha fazla bilgiyi nereden edinebilirim?

DAXUN'daki ekip deneyimli, bilgili ve arkadaş canlısıdır. Sektördeki yılların tecrübesiyle, kullanımları, faydaları ve kaliteleri de dahil olmak üzere titanyum hakkında her şeyi biliyorlar.

Titanyum, kullanım alanları ve sektörlerdeki uygulamaları hakkında düzenli güncellemeler için blogumuza göz atmayı unutmayın. Uzmanlarımız, sorularınız olduğunda her zaman başvurabileceğiniz, takip etmesi kolay kılavuzlar yazdı.

Hala sorun yaşıyorsanız, bizimle iletişime geçmekten çekinmeyin; size yardımcı olmaktan memnuniyet duyarız.

[email protected] adresine bir e-posta göndererek hızlı bir yanıt alabilirsiniz. Uygun bir çözüm önerebilmemiz için sorunuza mümkün olduğunca fazla ayrıntı eklediğinizden emin olun.

Fiyat teklifi nasıl alınır veya piyasa bilgileri en kısa sürede nasıl anlaşılır?

Lütfen “Bize Ulaşın” sayfasındaki formu doldurun veya “+86 13382898899” adresinden satış müdürümüzü arayın, en kısa sürede sizinle iletişime geçeceğiz. WhatsApp'ımız çevrimiçidir ve e-posta ([email protected]) 6 saat içinde kontrol edilecektir. Her soruya veya mesaja derhal yanıt verilecektir. Ayrıca, her hafta müşterilerimizle pazar bilgilerini paylaşıyoruz

Biraz örnek alabilir miyim?

We can provide stainless steel pipe/tube samples for you to check the quality. Sample is free and you just pay the freight.

Şimdiye kadar hangi ülkelere ihracat yaptınız?

Kanada, Şili, Kuveyt, Almanya, Güney Kore, Suudi Arabistan, Singapur gibi 42'den fazla ülkeye ihracat yaptık.

MOQ'unuz nedir?

Our MOQ is 1 ton for stainless steel pipe/tube

Teslimat süreniz ne kadar?

Deneme siparişleri bir hafta içinde teslim edilebilir. Normal siparişler için bu süre yaklaşık iki haftadır.

Sorgunuzu Bugün Gönderin
Hızlı Alıntı