x
Отправьте запрос сегодня
Быстрая цитата

Stainless steel bar

  • Round stainless steel bar, round steel
  • Rectangular stainless steel square bar
  • Special shaped stainless steel bar

Daxun Stainless steel rod and bar

Hot rolled rod

Stainless steel rod and bar is heated and rolled through multiple passes in a rolling mill. It has complete specifications and its performance meets standards and requirements.

Cold drawn bright Stainless steel rods

Cold-drawn Stainless steel rods are Stainless steel rods drawn under cold working conditions. They have a smooth surface and can also be polished and ground.

Forged Stainless steel rod and bar

Forged Stainless steel rods are forged multiple times to improve the mechanical properties and higher strength of the Stainless steel rods.

Daxun Stainless steel rod and bar

Product Parameters:   Stainless Steel rod
Specifications ASTM A276, ASME SA276 / ASTM A479  ASME SA479
Dimensions EN, DIN, JIS, ASTM, BS, ASME, AISI
Stainless Round Bars Outside Diameter in the range of 4mm to 500mm
Stainless Bright Bars Outside Diameter in the range of 4mm to 100mm
Stainless Hex Bars 18mm – 57mm (11/16″ to 2-3/4″)
Finish Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish
Длина 1 to 6 Meters, Custom Cut Lengths
Form Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc.

 

Daxun has a complete stainless steel round bar production technology cycle: from raw material processing to finished product production with a high degree of mechanical processing.

Читать далее

Materials and characteristics of various stainless steel rods

Each stainless steel rod material has its different usage scenarios.

Нажмите на изображение, чтобы увидеть дополнительную информацию об этом продукте

Нажмите на изображение, чтобы увидеть дополнительную информацию об этом продукте

Нажмите на изображение, чтобы увидеть дополнительную информацию об этом продукте

Нажмите на изображение, чтобы увидеть дополнительную информацию об этом продукте

Нажмите на изображение, чтобы увидеть дополнительную информацию об этом продукте

Нажмите на изображение, чтобы увидеть дополнительную информацию об этом продукте

Нажмите на изображение, чтобы увидеть дополнительную информацию об этом продукте

Нажмите на изображение, чтобы увидеть дополнительную информацию об этом продукте

Найдено 20 товаров.

Stainless Steel Rod Small Diameter

stainless steel rods and bar 10
3mm stainless steel rod

Bright surface, precise dimensions

Найдено 12 товаров.

Stainless steel rod production process

With our reliable stainless steel rods, their performance can be customized to suit your application.

Main Features of Stainless Steel Rod

Работоспособность
Ценный металл
Недорогие
Устойчивость к коррозии

Daxun’s Stainless steel rods manufacturing capabilities

Forming capabilities include radial forging machines, heat treatment furnaces, melting furnaces, and rolling mills for manufacturing stainless steel rod and bar. Radial forging refines grain structure and improves mechanical properties in larger-diameter bar, while rolling mills handle the volume production of standard round, square, and hex sections. Equipment is matched to the product form and grade — forged bar for higher-strength applications, hot rolled bar for standard structural and mechanical grades — so send your specification and we’ll confirm the right production route for your order.

Печь для термообработки Daxun

Stainless steel rod heat treatment uses advanced heat treatment furnace equipment to ensure the stability and high performance of the material. Heat treatment relieves internal stress from forging and rolling, restores corrosion resistance in the heat-affected zone, and stabilizes grain structure to the properties specified for the grade. Solution annealing is standard for austenitic grades like 304 and 316L, while precipitation-hardening grades such as 17-4PH require a controlled aging cycle to reach the specified strength and hardness. Confirm the required condition with your order and we’ll match the heat treatment cycle to it.

Плавильная способность Даксуна

Daxun uses vacuum induction melting, vacuum consumable electrode melting, and electroslag remelting to reduce impurities during the smelting process, improving the consistency and performance of the finished stainless steel bar. Each melting method is selected based on the grade and application — vacuum induction melting for tighter composition control on specialty grades, and electroslag remelting for improved internal cleanliness on bar destined for high-stress or corrosion-critical service. This is combined with in-process testing at each stage to confirm the material meets the specified chemistry and mechanical properties before it moves to forming.

Powerful Stainless steel rod solutions

inventory
services-

Daxun is a vertically coordinated supplier of stainless steel rod and rolled products, from smelting through finished bar.

Техническая информация

Сертификация по результатам тестирования материалов

Daxun’s quality management system is certified to ISO 9001:2015. Every shipment includes a mill test certificate, and material is traceable from source to delivery.

Отличное послепродажное обслуживание

Our support doesn’t end when your order ships. Daxun continues to provide after-sales assistance and warranty support for every order.

All our stainless steel round bars and rods are packed as per international standards to prevent any possible damage or loss. By default, we bundle finished pipes together in bulk using thick woven plastic bags. However, for some specialty pipes that are susceptible to dirt, scratches, pressure, or rough handling, we use wooden crates for protection.

We offer three shipping methods — sea, land, and air. Quotes are based on sea freight by default (FOB, CFR, CIF), with land or air transportation available on request for urgent orders.

Application cases of stainless steel rods in different industries.

Аэрокосмическая промышленность

Stainless steel rod and bar offers strength, toughness, and corrosion resistance suited to demanding structural applications.

Нефтехимия

Serving the petrochemical industry for electrolyzers, blowers, reaction towers, heat exchangers, pressure shafts, distillation towers, valves, and pumps. Send your specifications for a quote.

Судовое поле

Stainless steel rods are used to manufacture ship pumps, valves, drive shafts, propellers, whip antennas, acoustic devices, fire-fighting equipment and other components.

Морская техника

Deep-sea exploration equipment Deep-sea exploration is one of the important directions in the field of marine engineering. Stainless steel rods have become an ideal material for various deep-sea exploration equipment due to their corrosion resistance and high strength. Drill pipes, deep-sea buoys, detectors, sonar equipment, etc. can all use stainless steel rods to ensure long-term reliable operation in harsh marine environments.

Фармацевтические, биологические

Daxun supplies stainless steel rod and bar for pharmaceutical and biopharmaceutical equipment, with high-purity and ultra-high-purity material available on request.

Электрическое силовое поле

Daxun supplies stainless steel rod for power generation equipment components, drawing on smelting and processing capability from raw material through finished bar.

about-feature3
Let us be your trustworthy Stainless steel Rod supplier

Every shipment includes a mill test certificate and is traceable from source to delivery, backed by our ISO 9001:2015-certified quality management system. Daxun supplies stainless steel rod and bar to a range of industries, including industrial equipment, medical, marine, and power generation.

Техническая информация

Диаметр (мм) Durface Длина (мм) Комментарий
φ3.0-12.0 bright 3000 AAA
φ14.0-25.0 bright 6000 AAA
φ25.0-50.0 bright 6000 AAA
>80 ~ ≤120 Bright/primary color 6000 AAA
>120 ~ ≤140 Bright/primary color 6000 AAA
>140 ~ ≤180 Bright/primary color 6000 AAA
>180 ~ ≤200 Bright/primary color 6000 AAA
>200 ~ ≤220 Bright/primary color 6000 AAA
>220 ~ ≤240 Bright/primary color 6000 AAA
>240 ~ ≤250 Bright/primary color 6000 AAA
>250 ~ ≤300+

 

Bright/primary color

 

6000

 

AAA

 

Если вам нужно узнать больше о размере, пожалуйста, свяжитесь с Daxun

Tolerance for Hot Rolled Round Bars
Размер Рейтинг толерантности
Группа 1 Группа 2 Группа 3
>7 ~ ≤20 ±0.25 ±0.35 ±0.40
>20 ~ ≤30 ±0.30 ±0.40 ±0.50
>30 ~ ≤50 ±0.40 ±0.50 ±0.60
>50 ~ ≤80 ±0.60 ±0.70 ±0.80
>80 ~ ≤110 ±0.90 ±1.00 ±1.10
>110 ~ ≤150 ±1.20 ±1.30 ±1.40
Tolerance for Hot Forging Round Bars
Размер Рейтинг толерантности
Группа 1 Группа 2
>50 ~ ≤60 0.5 1
>60 ~ ≤80 1 1.5
>80 ~ ≤100 1.5 2
>100 ~ ≤120 1 1.5
>120 ~ ≤140 1.5 2
>140 ~ ≤160 1 2
>160 ~ ≤180 2 3
>180 ~ ≤200 3 4
>200 ~ ≤220 2 3
>220 ~ ≤240 3 4
>240 ~ ≤250 4 5
>250 ~ ≤300 5 6
Tolerance for Cold Drawn Round Bars
Размер Рейтинг толерантности
H8 H9 H10 H11 H12 H13
3 0 ~ -0.014 0 ~ -0.025 0 ~ -0.040 0 ~ -0.060 0 ~ -0.100 0 ~ -0.140
>3 ~ ≤6 0 ~ -0.018 0 ~ -0.030 0 ~ -0.048 0 ~ -0.075 0 ~ -0.120 0 ~ -0.180
>6 ~ ≤10 0 ~ -0.022 0 ~ -0.036 0 ~ -0.058 0 ~ -0.090 0 ~ -0.150 0 ~ -0.220
>10 ~ ≤18 0 ~ -0.027 0 ~ -0.043 0 ~ -0.070 0 ~ -0.110 0 ~ -0.180 0 ~ -0.270
>18 ~ ≤30 0 ~ -0.033 0 ~ -0.052 0 ~ -0.084 0 ~ -0.130 0 ~ -0.210 0 ~ -0.330
>30 ~ ≤50 0 ~ -0.039 0 ~ -0.062 0 ~ -0.100 0 ~ -0.160 0 ~ -0.250 0 ~ -0.390
>50 ~ ≤80 0 ~ -0.046 0 ~ -0.074 0 ~ -0.120 0 ~ -0.190 0 ~ -0.300 0 ~ -0.460
Выбор государства доставки Состояние поверхности
Кованые Black
Полированный
Горячекатаный Black
Полированный
Яркий
Маринованные
Холодная вытяжка Полированный
Яркий
Примечание:
1. Если вам требуется другое состояние доставки, чем перечисленные выше, пожалуйста, подтвердите с нами.
2. В случае запроса или заказа, пожалуйста, сообщите нам о любых дополнительных требованиях, не указанных здесь.
  • Customer references and project case studies available on request.

Сплав Даксунь

Regarding Stainless Steel rods, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.

Есть ли у вас в наличии?

Да, у нас есть полные спецификации и инвентарь, и мы можем быстро удовлетворить ваши потребности.

Можно ли его настроить?

Да, он может быть настроен. Вы можете связаться с нами и отправить нам настроенные спецификации и количество.

Как вы отправляете товары?

Наши способы транспортировки обычно включают морские перевозки, наземные перевозки и морские перевозки. Мы доставим вам груз быстро и безопасно.

Какова ваша цена?

Поскольку наша производительность высока, затраты будут гораздо ниже, поэтому цена низкая.

Как у вас обстоят дела с качеством?

Мы придаем большое значение качеству продукции и прошли различные испытания системы качества.

Отправьте запрос сегодня
Быстрая цитата