x
Отправьте запрос сегодня
Быстрая цитата

Труба из нержавеющей стали

– Stainless steel pipe and tube supplier from China
– OD 3mm to 2000mm, wall thickness 0.3mm to 100mm
– Seamless, welded, and welded-and-drawn tube in a full range of grades

Труба из нержавеющей стали

Welded Tube
Made from strip that is roll formed and fusion welded along a longitudinal seam. Daxun’s welding process uses no filler metal, keeping the seam consistent with the base material.

Welded & Drawn Tubing
Welded tube redrawn to final size — the way to get heavy wall-to-diameter ratios that can’t be welded directly, at a lower cost than seamless. All Daxun welded and drawn tube is bright annealed.

Seamless Tubing
Drawn from hollows made by piercing a billet or hot extrusion. Best suited for heavy diameter-to-wall ratios and tight outside-diameter tolerances.

Daxun is located in China

Product Parameters:   Stainless Steel Pipe/Tube
OD 3mm~2000mm thickness 0.3mm~100mm
Стандарт ASTM A312 A249 A213 A269 A268 etc
Тип Seamless Tube, Welded Tube, Precision Tube, Polished Tube, Pickled Tube, Hairline Tube, etc.
shape Round square rectangle Hexagonal Special-shaped etc
Класс 304 304L 304H 309S 310S 316L 316TI 317L 321 347 347H 430 410 410S 420 430  439 441 443

444  904L 2205 2507 S32750 S32760

Daxun is a China-based manufacturer of precision seamless tube, produced to
standard specifications with tight tolerances, including thin-walled tube.
Materials supplied include stainless steel, titanium alloy, high-strength steel
and nickel-based alloy.

Daxun supplies seamless and welded stainless steel pipe for large-diameter
applications in the power generation, petrochemical, and marine engineering
industries. Specifications and certification requirements are confirmed per
order.

Читать далее

Brands and characteristics of various stainless steel pipes

Our unparalleled resources, technical expertise and highly skilled workforce produce consistently high quality stainless steel pipe

Duplex stainless steel pipe, with higher strength and corrosion resistance

Stainless steel pipe

We produce seamless, high-strength tubing in diameters from 1″ to 50″

Stainless steel pipe

Stainless steel pipes made of this material have good high temperature resistance.

Stainless steel pipe

317L is a stainless steel pipe produced in accordance with American ASTM standards

Stainless steel pipe

Duplex stainless steel pipe, with higher strength and corrosion resistance

Stainless steel pipe

Duplex stainless steel pipe, with higher strength and corrosion resistance

Stainless steel pipe

904L stainless steel tube and pipe Have good corrosion resistance and performance

Stainless steel pipe
Труба из нержавеющей стали

Stainless steel square tubes are often used in the construction field and structural parts.

Найдено 16 товаров.

Manufacturing Methods

Each tube is manufactured to the strictest regulatory and internal specifications. Daxun’s proprietary forming, welding and finishing processes produce pipe and Tube with superilnconelor performance. Some of the stages of manufacturing are randomly listed below.

Main features of stainless steel pipes

Preservative

Excellent corrosion resistance in extreme environments

Высокая прочность

Many types of stainless steel pipe offer very high strength for demanding structural and pressure applications.

Немагнитный

Подходит для ситуаций, когда необходимо избегать вмешательства магнитного поля

Temperature Resistant

The ability to withstand very high temperatures makes nickel alloys perfect for onshore, offshore and power generation applications.

Daxun stainless steel pipe manufacturing capabilities

Daxun works with established mills and finishing partners to supply seamless,welded, and welded-and-drawn stainless steel pipe and tube across a widerange of diameters and wall thicknesses, in round, square, rectangular, andspecial-shaped profiles. Surface finishes include mill, pickled, polished,and hairline.Every order is confirmed against the applicable standard — ASTM, EN, JIS, orGB — with dimensions, tolerances, and delivery condition matched to yourproject requirements. A mill test certificate is provided with each shipment.Send your OD, wall thickness, length, grade, and standard, and we’ll confirmfeasibility, pricing, and lead time.

Daxun’s pipe processing capabilities

Daxun’s pipe processing capabilities Beyond supplying raw pipe and tube, Daxun coordinates downstream processing to deliver parts closer to finished condition:Precision machining — straightening, boring, turning, and machining to tighter dimensional tolerances than mill-standard product.Surface and joint work — honing,trepanning, polishing, and laser weldingfor applications requiring specific surface finish or fabricated assemblies.Cutting and testing — cutting to length and non-destructive testing (eddy current, ultrasonic, or per the applicable ASTM standard) beforeshipment.Whether you need a single machining job or processing across a full order,send your drawing or specification and we’ll confirm what’s achievable.

Bigger, Better Pipe Solutions

Large-diameter and heavy-wall pipe brings tighter constraints on roundness,wall uniformity, and weld integrity — especially for welded and welded-and-drawn product. Daxun confirms production method, tolerance class,and testing requirements for each large-diameter project individually,rather than applying a single standard spec across all sizes.Send your OD, wall thickness, length, grade, and standard, and we’ll confirmfeasibility, tolerance, and lead time for your project.

4628cac1

Powerful Pipe Solutions

Daxun supplies the power generation market with ductwork, boiler tubes, main steam tubes, thermal reheat tubes, flue gas desulfurization units and other products for nuclear, coal-fired, renewable energy and combined cycle applications.

Техническая информация

Daxun supplies pipe and tubing for demanding mechanical and structural applications, including sour service environments and high-pressure,high-temperature conditions. High-alloy nickel casing and mechanical tubeproducts are available for these applications.

Chemical processing applications include pipe and tube for ethylene production, caustic soda production, and heat exchanger tube. Daxun also supplies tube products for the medical and general industrial sectors, including X-ray equipment, thermocouple sheathing tube for industrial furnaces, and boiler tube.

Фактический вес и хорошее качество

Actual Weight & Good Quality Daxun maintains an in-house testing laboratory to verify that every shipment meets the specified weight and quality standard before delivery. Our quality control team performs 100% inspection at every production stage.

Отличное послепродажное обслуживание

Our support doesn’t end when your order ships. Daxun continues to provide after-sales assistance and warranty support for every order.

Application cases of stainless steel pipes in different industries

5ff7292d-1af6-473d-b0d9-bfd49aed751f.jpg_560xaf
Coal chemical industry

Daxun Stainless has developed R&D and manufacturing technology for N08825 alloy pipes for high-pressure hydrogen applications. The product and various mechanical, physical and chemical properties have reached the international advanced level, meeting the requirements for the use of alloy seamless pipes for high-pressure hydrogen applications, and realizing high-pressure hydrogen applications. The engineering development of alloy seamless pipe products has formed independent intellectual property rights and industrialization capabilities. It meets the pipe requirements for petroleum hydrogenation units, and also meets the needs of special pipes for nuclear power, petrochemical, coal-to-liquids, chemical industry, aerospace and other major equipment and high-end equipment manufacturing.

dianzhanguolu
Power station boiler

In thermal power generation, the use of supercritical units and ultra-supercritical units has increased. The supercritical unit improves the thermal efficiency of the unit by increasing the pressure and temperature of the steam in the boiler. Its steam and water pipelines include reheater tubes, superheater tubes, water wall tubes, economizer tubes, air preheating tubes, heat transfer tubes, and downcomers. And various header pipes are exposed to high temperature and high pressure conditions for a long time, so the steel pipes are required to have high lasting strength, high resistance to oxidation and corrosion and good structural stability. Usually, the number of high-pressure boiler tubes such as Super304H and HR3C consumed per million kilowatts of super (super)critical units is about 1,250 tons.

hanyangogngxheng
marine pipeline

Daxun developed the manufacturing technology of large-diameter super duplex stainless steel seamless pipes, realized the transformation of scientific and technological achievements into high-tech products for marine engineering, and served as a demonstration for the industrialization of key equipment and systems in high-end ship and marine engineering manufacturing.

hedian
nuclear power

Daxun joined the ranks of qualified suppliers and developed the core technology of N08367 seamless and welded steel pipe manufacturing for third-generation nuclear power AP1000, achieving major industrialization goals. Reaching the international advanced and leading level, the implementation of the project will effectively promote the independence of the nuclear power industry, meet the development needs of domestic and foreign advanced nuclear power equipment manufacturing, and ensure the safe operation of nuclear power plants.

lng
СПГ

Focusing on the performance requirements of welded pipes for LNG, Daxun broke through the key technologies of welding and heat treatment during product processing and manufacturing, and developed large-diameter stainless steel welded pipes for LNG with excellent corrosion resistance, low-temperature toughness and good low-temperature strength.

Аэрокосмическая промышленность

Can be used in fuselage parts, aerospace equipment, rockets, artificial satellites, missiles, spacecraft shells, pipeline systems, etc.

Нефтехимия

Serving the petrochemical industry for reaction towers, heat exchangers, pressure vessels, distillation towers, valves, pumps, and pipeline systems. Send your specifications for a quote.

Судовое поле

Stainless steel pipes are used in the manufacture of ship piping systems, whip antennas, seawater pipes, condensers, heat exchangers, acoustic devices, fire piping, etc.

Морская техника

Deep-sea exploration equipment is one of the important directions in the field of marine engineering, and stainless steel pipes have become an ideal material for various deep-sea exploration equipment due to their corrosion resistance, high strength and other advantages. Deep-sea pipelines, detectors, sonar equipment, etc. can all be made of stainless steel pipes to ensure long-term reliable operation in harsh marine environments.

Фармацевтические, биологические

Serving the pharmaceutical and biopharmaceutical industries has been a welcome challenge for Daxun. From raw material selection to delivery, we have developed high purity and ultra-high purity services to meet and exceed industry standards. When only the best stainless steel tubing and stainless steel pipes can meet the demand, more and more pharmaceutical and biopharmaceutical companies trust Daxun.

Электрическое силовое поле

Serving the power generation industry with pipe and tube for boiler, turbine, and pipeline applications. Send your specifications for a quote.

about-feature3
Let us be your trustworthy stainless steel pipe supplier

Customers from different industries trust Daxun for fast delivery of high-quality products. Seamless, welded and drawn tubing are produced at our factory in Wuxi, China. Strict production processes produce pipes that are homogeneous throughout their outer diameter and wall microstructure.

Техническая информация

Диаметр (мм) Thickness(mm) Длина (мм) Комментарий
φ3.0-12.0 0.3-1.0 6000 AAA
φ19.0-22.0 0.6-3.0 6000 AAA
φ25.0-27.2 0.8-10.0 6000 AAA
φ32.0-60.3 0.8-15.0 36000 AAA
φ76.3-102.1 0.8-20.0 36000 AAA
φ114.3-168.3 0.8-20.0 6000 AAA
φ180.0-219.2 3.0-20.0 6000 AAA
φ273.1-325.3 4.0-30.0 6000 AAA
φ377.2-426.3 5.0-30.0 6000 AAA
φ508.1-711.0 5.0-30.0 6000 AAA
711.0+

 

5.0-30.0

 

6000

 

AAA

 

Если вам нужно узнать больше о размере, пожалуйста, свяжитесь с Daxun

ASTM A269
Group Size, Outside Diameter, in. Permissible Variations in Outside Diameter, in. (mm) Permissible Variations in Wall Thickness, % Permissible Variations in Cut Length, in. (mm) Thin Walled Tubes
Over Under
1 Up to ½ ±0.005(0.13) ±15 ⅛(3.2) 0 …
2 ½ to 1½, excl ±0.005(0.13) ±10 ⅛(3.2) 0 less than 0.065 in. (1.65 mm) nominal
3 1½ to 3½, excl ±0.010(0.25) ±10 3/16(4.8) 0 less than 0.095 in. (2.41 mm) nominal
4 3½ to 5½, excl ±0.015(0.38) ±10 3/16(4.8) 0 less than 0.150 in. (3.81 mm) nominal
5 5½ to 8, excl ±0.030(0.76) ±10 3/16(4.8) 0 less than 0.150 in. (3.81 mm) nominal
6 8 to 12, excl ±0.040(1.01) ±10 3/16(4.8) 0 less than 0.200 in. (5.08 mm) nominal
7 12 to 14, excl ±0.050(1.26) ±10 3/16(4.8) 0 less than 0.220 in. (5.59 mm) nominal
ASTM A554
OD Size, in. (mm) Толщина стенок OD, ±
in. мм in. мм
Under ½ (12.7) 0.020 to 0.049 0.51 to 1.24 0.004 0.1
½ to 1 (12.7 to 25.4) 0.020 to 0.065 0.51 to 1.65 0.005 0.13
½ to 1 (12.7 to 25.4) over 0.065 to 0.134 over 1.65 to 3.40 0.01 0.25
Over 1 to 1½ (25.4 to 38.1), incl 0.025 to 0.065 0.64 to 1.65 0.008 0.2
Over 1 to 1½ (25.4 to 38.1), incl over 0.065 to 0.134 over 1.65 to 3.40 0.01 0.25
Over 1½ to 2 (38.1 to 50.8), incl 0.025 to 0.049 0.64 to 1.24 0.01 0.25
Over 1½ to 2 (38.1 to 50.8), incl over 0.049 to 0.083 over 1.24 to 2.11 0.011 0.28
Over 1½ to 2 (38.1 to 50.8), incl over 0.083 to 0.149 over 2.11 to 3.78 0.012 0.3
Over 2 to 2½ (50.8 to 63.5), incl 0.032 to 0.065 0.81 to 1.65 0.012 0.3
Over 2 to 2½ (50.8 to 63.5), incl over 0.065 to 0.109 over 1.65 to 2.77 0.013 0.33
Over 2 to 2½ (50.8 to 63.5), incl over 0.109 to 0.165 over 2.77 to 4.19 0.014 0.36
Over 2½ to 3½ (63.5 to 88.9), incl 0.032 to 0.165 0.81 to 4.19 0.014 0.36
Over 2½ to 3½ (63.5 to 88.9), incl over 0.165 over 4.19 0.02 0.51
Over 3½ to 5 (88.9 to 127.0), incl 0.035 to 0.165 0.89 to 4.19 0.02 0.51
Over 3½ to 5 (88.9 to 127.0), incl over 0.165 over 4.19 0.025 0.64
Over 5 to 7½ (127.0 to 190.5), incl 0.049 to 0.250 1.24 to 6.35 0.025 0.64
Over 5 to 7½ (127.0 to 190.5), incl over 0.250 over 6.35 0.03 0.76
Over 7½ to 16 (190.5 to 406.4), incl all all 0.00125 in./in. or mm/mm of circumference
ASTM A312
NPS Designator Tolerance, % from Nominal
Over Under
⅛ to 2½ incl., all t/D ratios 20 12.5
3 to 18 incl., t/D up to 5% incl. 22.5 12.5
3 to 18 incl., t/D > 5% 15 12.5
20 and larger, welded, all t/D ratios 17.5 12.5
20 and larger, seamless, t/D up to 5% incl. 22.5 12.5
20 and larger, seamless, t/D > 5% 15 12.5
Состояние доставки
Выбор государства доставки Состояние поверхности
Горячекатаный Silver Bright
Polished (320#, 400#, 600#, Mirror finish)
Холодная прокатка Silver Bright
Polished (320#, 400#, 600#, Mirror finish)
Примечание:
1. Если вам требуется другое состояние доставки, чем перечисленные выше, пожалуйста, подтвердите с нами.
2. В случае запроса или заказа, пожалуйста, сообщите нам о любых дополнительных требованиях, не указанных здесь.
  • Customer references and project case studies available on request.

Сплав Даксунь

Regarding stainless steel pipes, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.

Есть ли у вас в наличии?

Yes — we maintain stock across common specifications and can typically ship quickly from inventory.

Можно ли его настроить?

Да, он может быть настроен. Вы можете связаться с нами и отправить нам настроенные спецификации и количество.

Как вы отправляете товары?

Наши способы транспортировки обычно включают морские перевозки, наземные перевозки и морские перевозки. Мы доставим вам груз быстро и безопасно.

How is pricing determined?

Pricing depends on grade, dimensions, quantity, and delivery condition. Send your specifications for a quote.

How is your quality controlled?

Every order goes through in-process and final inspection before shipment. Our quality management system is certified to ISO 9001.

Отправьте запрос сегодня
Быстрая цитата