AMS4930M vs AMS4931H Grade 23 Titanium Bar
AMS4930M vs AMS4931H Grade 23 Titanium Bar Direct answer: AMS4930M and AMS4931H both cover Ti-6Al-4V ELI bar, but they are not interchangeable. AMS4930M is an annealed product route, while AMS4931H is duplex annealed and specifically includes fracture-toughness control. The engineering drawing must select the route, size range, test orientation, ultrasonic