Daxun is an experienced manufacturer of CP-2 grade titanium tubes
중국에서 티타늄 및 티타늄 합금 튜브의 선도적인 공급업체인 Daxun은 전 세계에 고성능 티타늄 튜브를 공급합니다.
- Titanium pipe/tube Grade:CP-2(2등급)- UNS R50400-3.7035
- Titanium tube types: Seamless Ti tube, Ti welded tube, forged Ti tube
- Titanium tubes density The density of grade 2 titanium is 4.51 g/cm3
- Standards: ASTM B861、B862、B338 / ASME SB861、SB862、SB338
- High strength, very corrosion resistant, good cold formability
----다순은 중국에서 티타늄 튜브를 생산하여 고객의 다양하고 -- 까다로운 요구를 충족합니다!.
A global leader in commercially pure titanium tubes fabrication services
Buy Grade 2 Titanium Tubes from Daxun; we can offer you a wide range of sizes, starting from 1.0 mm diameter, in a wide variety, either directly from stock or custom made to your specifications. We can immediately provide drawn, seamless rolled or longitudinally welded tubes for a variety of applications from stock. We sell welded or seamless tubes made of Grade 2 Titanium to typical specifications for heat exchangers such as ASTM B 338, ASME SB 338, DIN and VD TÜV.
Our CP Grade 2 tubes have a density of 4.51 g/cm3, which is 45% lower than ferrous alloys. It is a medium-strength alloy with a typical yield strength of 352 MPa. The alloy has good ductility, formability and welding properties. The addition of iron and oxygen improves strength and formability. CP Grade 2 exhibits similar performance qualities to Grade 1, including excellent corrosion resistance under oxidizing conditions. However, this titanium tube is stronger than Grade 1 titanium tube.
Grade 2 Titanium Tubes are commercially pure titanium with a good balance between strength and ductility. The material has good toughness. It is the most commonly used titanium alloy due to its high strength, weldability and corrosion resistance. Its high ductility and formability make it the alloy of choice for piping systems, heat exchangers, reaction and pressure vessels, and flue gas desulfurization systems. Grade 2 titanium alloys are used in a variety of industries, including chemical processing, petrochemical processing, aerospace and marine.
Are you looking to purchase titanium tubes for your project or order a range of tubes? Daxun produces a wide range of titanium tubes including Grade 1 (3.7025), Grade 2 (3.7035), Grade 3 (3.7055), Grade 7 (3.7235), Grade 9 (3.7195) and Grade 12 (3.7105).
Buy titanium tubes at Daxun Alloys.
We offer a wide range of sizes starting from 1.0 mm in diameter with multiple variations, available directly from stock or custom made to your specifications through our network. We have wrought titanium tubes, seamless titanium tubes and longitudinally welded titanium tubes immediately available from stock for a wide range of applications.
We offer heat exchanger tubing in standard specifications such as ASTM B 338, ASME SB 338, DIN 17866 and VD TÜV welded titanium tubes or seamless titanium tubes. When it comes to titanium tubes, we have a large supply of titanium welded tubes and titanium seamless tubes in China in standard sizes up to 100 mm thick. We will supply welded titanium tubes for larger pipe sizes. The most common specifications used in the industry are ASTM B 861, ASFM B 862, NACE and NORSOK and VD TÜV Tube 230/2, depending on the specifications of the plant designer.
Titanium tube surface treatment options include bright annealing, pickling and grinding. Material parameters vary depending on the application and product requirements. The corrosion and mechanical properties of titanium alloy tubes vary. We are happy to assist you in evaluating your needs. If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee price and quantity for a specified period.
데이터
- 매개변수
- 성분
- 기계적 특성
- Hot searches
| Grade 2 Titanium pipe & Tubes Specification | ASTM B338 / ASTM B861 / ASTM B862 / ASME SB338 / ASME SB861 / ASME SB862 |
| Grade 2 Titanium pipe & Tubes Grades | Commercially pure titanium Grade 2- TA2- USN 50400 |
| Grade 2 Titanium pipe & Tubes Type | ot Rolled / Cold Drawn / Welded / ERW |
| Grade 2 Titanium pipe & Tubes Outer Diameter Size | Titanium seamless pipe – φ1.0mm to φ508.3mm |
| Titanium welded pipe – φ1.0mm to φ1219mm | |
| Grade 2 Titanium pipe & Tubes Wall Thickness | 1.0mm—50mm (customizable wall thickness) |
| Grade 2 Titanium pipe & Tubes Length | 5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size. |
| Titanium pipe Form TA2 | ‘ Hollow, U’ bent, LSAW, Hydraulic, Straight Tube, Boiler, Round, Tube Coil, Square, Rectangular Etc |
| Marking TA2 3.7035 | All Titanium Tubes Tubing are marked as follows: Grade, Standard, Thickness, OD, Heat No., Length (Or according to the customer’s request.) |
| Uses of Titanium Alloy Tubes | Gas pipes, oil pipes, heat exchanger tubes, boiler tubes, fluid pipes, titanium exhaust pipes. |
| Grade 2 Titanium pipe & Tubes Pipe Ends | Plain Ends / Beveled Ends |
| Grade 2 Titanium pipe & Tubes Delivery Conditions | As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered |
| Grade 2 Titanium pipe & Tubes Coating | Electropolish, Mechanical Polish, Satin Finish, Passivated |
| Grade 2 Titanium pipe & Tubes Other Testing | ardness Test, Hydrostatic Test, Eddy Current test, Eddy Current, Tensile Test, Flattening, Flare Test, Annealed, Hydrostatic Test, Tempered, Stress Relieved etc. |
| Grade 2 Titanium pipe & Tubes Dimension | All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME |
| Grade 2 Titanium pipe & Tubes Value Added Services | Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment |
| Grade 2 Titanium pipe & Tubes Packaging | Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector |
| Grade 2 Titanium pipe & Tubes Shipment & Transportation | By Road – Truck / Train, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes |
| Grade 2 Titanium pipe & Tubes Material Test Certificate | Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS ETC |
| 요소 | Weight % |
| C | ≤0.08 |
| O | ≤0.25 |
| N | ≤0.03 |
| H | ≤0.015 |
| Fe | ≤0.30 |
| *OEE | ≤0.10 |
| *OET | ≤0.40 |
| Ti | Remaining |
| 합금 | 유엔 지정 | 사양. | Tensile Strength (min.) | Yield Strength 0.2% Offset (min.) | Elongation in 2 inches (min.) | Grain Size Requirement | Max Hardness | 탄성 계수(x106 psi) | Mean Coefficient of Thermal Expansion IN./IN./°F x 10-6) | Thermal Conductivity (BTU-in/ft2-h-°F) | ||||
| psi | MPa | ksi | psi | MPa | ksi | % | ||||||||
| Grade 2 Titanium | R50400 | B338 | 50,000 | -345 | 50 | 40,000- | (276-448) | 40-65 | 20 | — | — | 16 | 5.1 | 144 |
| 50,000 | ||||||||||||||
| 3.7035 Ti Grade 2 Tubes | R50400 titanium alloy Tubes |
| Ti Grade 2 tubing | Tube Ti Grade 2 |
| R50400 alloy tubing | R50400 alloy tube |
| Ti Grade 2 Tube | Ti Grade 2 Tubing |
| SB338 R50400 Seamless Tubing | SB338 UNS R50400 Tubes |
| R50400 tubing | Nickel alloy uns R50400 Exhaust Tubing |
| Ti Grade 2 tubing | Ti Grade 2 tube |
| Ti Grade 2 Seamless Tubing | Ti Grade 2 Seamless Tube |
| Grade 2 Alloy Tubes | Cp Grade 2 Ti tubing |
| Inconel R50400 Tubes | UNS 50400 Tubes |
| Ti Grade 2 uns R50400 Tubes | 3.7035 Grade 2 Ti Tubing |
| SB 338 R50400 Round Tubes | SB-338 R50400 Tubes |
| ASME SB338 Cp Grade 2 Ti Tubes | ASTM B338 Seamless Tube |
| Grade 2 Ti alloy Tubes | WERKSTOFF Nr 3.7035 tubing |
| ASTM B338 Ti Grade 2 Tubes | SB338 Grade 2 Ti Tubes |
| ASTM B338 R50400 Tubes | B338 R50400 Tubes |
| ASTM B337 Grade 2 Ti Tubing | Ti gr 2 Tubing |
| Grade 2 Ti Chemical process Tube | Ti Grade 2 Medical Tube |
| SB-338 tube material | SB-338 material |
| ASME SB337 Cp Grade 2 Ti Tubing | ASTM B337 Gr. 600 Tubing |
| ASME Grade 2 Ti Seamless Tube | Grade 2 Ti Nuclear Tube |
| SB337 Grade 2 Ti Tubing | ASTM B337 Cp Grade 2 Ti Tubing |
| Ti Grade 2 Heat exchanger Tube | Grade 2 Alloy Control lines |
| Ti Grade 2 Aerospace Tube | Cp Grade 2 Ti Alloy Oil and gas Tube |
| Grade 2 Ti Umbilicals | Ti Grade 2 Polish Tube |
| WERKSTOFF NR. 3.7035 Hydraulic Tube | Grade 2 Alloy High pressure Tube |
| Ti Grade 2 Nuclear Fuel Tube | ASTM B337 Weld Tube |
| Cp Grade 2 Ti Alloy SCH 40 Tube | Grade 2 Ti SCH 80 Tube |
| Ti Grade 2 elliptical and Oval Tube | Ti Grade 2 Rectangular Tube |
| Ti Grade 2 Seamless Hollow Tube | Grade 2 Ti Electropolished Tube |
| Grade 2 Ti Instrumentation Tube | WERKSTOFF NR. 3.7035 Electropolished Tube |
| Ti Grade 2 SCH 40 Tube | Ti Grade 2 SCH 80 Tube |
| Ti Grade 2 Condenser Tube | ASTM B337 Cp Grade 2 Ti Oil & Gas Tubing |
| Ti Grade 2 Tubing | Ti Grade 2 Oil Tube |
| Ti Grade 2 Alloy Tube | ASTM Ti Grade 2 Decorative Tube |
| ASTM B337 Cp Grade 2 Ti Capillary Tube | Grade 2 Ti U Shaped Tube |
| ASME SB337 Cp Grade 2 Ti Instrumentation Tube | Grade 2 Ti Triangle Tube |
| Ti Grade 2 High-strength capillary tubing | Ti Grade 2 Bellows Tube |
| ASME SB338 Cp Grade 2 Ti precision Tube | Grade 2 Ti Transmission Tube |
| Cp Grade 2 Ti Alloy Pitot Tube | WERKSTOFF NR. 3.7035 encapsulated coiled tubing |
| Ti Grade 2 high precision Tube | Grade 2 Ti Nuclear Control Rod Tube |
| WERKSTOFF NR. 3.7035 Seamless Tubing | Ti Grade 2 Gas Tube Ar 15 |
| Ti Grade 2 Gas Tubing | Ti Grade 2 Furnace Tube |
| Ti Grade 2 cold drawn seamless Tube | Grade 2 Ti Aero engine Tube |
| Grade 2 Ti Bourdon Tube | ASME SB338 Cp Grade 2 Ti Capillary Tubing |
| Cp Grade 2 Ti Alloy Precision Tubing | Ti Grade 2 High Pressure Tube |
| Ti Grade 2 Aerospace Engine Tube | Ti Grade 2 Furnace Tube |
| Ti Grade 2 Drawn over mandrel (DOM) | Ti Grade 2 Finned Tube |
| Ti Grade 2 seamless coil tubing | Grade 2 Ti seamless straight tubing |
| Ti Grade 2 Hot finished seamless tubing (HFS) | Ti Grade 2 Cold drawn seamless tubing (CDS) |
| Grade 2 Ti Tube for Precision Components | Grade 2 Ti Sighting Tube |
| Seamless Ti Grade 2 Tubing | 600 Nickel Chromium Tubing |
| High Quality Ti Grade 2 Seamless Tube | Grade 2 Ti Square Tube |
| ASME SB338 Cp Grade 2 Ti Cold Drawn Tube | UNS R50400 ERW Tube |
| Grade 2 Ti Round Tube | Ti Grade 2 Rectangular Tube |
| Cp Grade 2 Ti Alloy thermocouple Tube | ASME SB337 Cp Grade 2 Ti Polish Tube |
| Ti Grade 2 Hexagonal Tube | Ti Grade 2 Hollow Tube |
| Ti Grade 2 Chemical Process Tube | Ti Grade 2 Welded coiled tubing |
| ASME SB337 Cp Grade 2 Ti Round Tube | Ti Grade 2 Triangle Tube |
| Grade 2 Ti Colour Coated Tube | Grade 2 Ti Welded Tube |
| ASTM B337 Cp Grade 2 Ti Capillary Tube | Grade 2 Ti EFW Tube |
| UNS R50400 U Shaped Tube | Grade 2 Alloy exhaust tubing |
| Ti Grade 2 Secondary & Surplus Tube | WERKSTOFF NR. 3.7035 Outside Polished Tube |
| WERKSTOFF Nr 3.7035 seam-welded tubing | UNS R50400 cold-drawn coiled tubing |
| Cp Grade 2 Ti Alloy Welded Tube | Ti Grade 2 redrawn tubing |
| Ti Grade 2 Boiler Tube | ASME SB338 Cp Grade 2 Ti Cold Drawn Tube |
| Grade 2 Ti Condensers Tube | WERKSTOFF NR. 3.7035 Super Heaters |
| Titanium Grade 2 Aerospace Pipe suppliers | Titanium Grade 2 Seamless Hollow Pipes |
| Titanium Grade 2 Oil and gas Pipe distributor | Stockist of Titanium Grade 2 Electropolished Pipes |
| ASME SB163 Titanium Grade 2 Seamless Pipe | ASTM/ASME B167 Titanium Grade 2 Capillary Pipes |
| Titanium Grade 2 Nuclear Pipe suppliers | Titanium Grade 2 U Shaped Pipe distributor |
| Titanium Grade 2 Chemical process Pipe traders | Titanium Grade 2 Alloy Pipe suppliers |
| Titanium Grade 2 Medical Pipe manufacturers | ASTM B163 Titanium Grade 2 Decorative Pipes |
| Titanium Grade 2 Control lines manufacturers | Titanium Grade 2 Pipe exporter in china |
| Titanium Grade 2 Umbilicals suppliers | Titanium Grade 2 Oil Pipe suppliers |
| Titanium Grade 2 Polish Pipe distributor | ASTM B163 Titanium Grade 2 Thick Wall Pipe |
| Titanium Grade 2 Hydraulic Pipe traders | Titanium Grade 2 Triangle Pipe distributor |
| Titanium Grade 2 High pressure Pipe stockist | Titanium Grade 2 High-strength capillary Pipe |
| Titanium Grade 2 Nuclear Fuel Pipe manufacturers | Titanium Grade 2 Bellows Pipes exporter in china |
| Titanium Grade 2 EFW Pipe Suppliers | Titanium Grade 2 precision Pipes stockist |
| distributor of Titanium Grade 2 Instrumentation Pipe | Titanium Grade 2 Transmission Pipes importers |
| Titanium Grade 2 Electropolished Pipe | Titanium Grade 2 Pitot Pipes exporter in china |
| Titanium Grade 2 elliptical and Oval Pipe | Titanium Grade 2 encapsulated coiled Pipe |
| Titanium Grade 2 Rectangular Pipe suppliers | exporter of Titanium Grade 2 high precision Pipes |
| Titanium Grade 2 SCH 40 Pipe exporter in china | Titanium Grade 2 Nuclear Control Rod Pipes |
| Titanium Grade 2 SCH 80 Pipe distributor | Titanium Grade 2 Seamless Pipe stockist |
| Titanium Grade 2 Condenser Pipes stockist | Stockholder of Titanium Grade 2 Gas Pipe Ar 15 |
| Titanium Grade 2 Oil & Gas Pipe distributor | Titanium Grade 2 Bourdon Pipe importers |
| Titanium Grade 2 SCH 40 Pipe distributor | Titanium Grade 2 Seamless Heating Pipe |
| Titanium Grade 2 SCH 80 Pipe manufacturers | Distributor of Titanium Grade 2 Capillary Pipe |
| Titanium Grade 2 seamless coil Pipe wholesaler | Supplier of Titanium Grade 2 Furnace Pipe |
| Titanium Grade 2 seamless straight Pipe | Titanium Grade 2 Gas Pipe manufacturers |
| Titanium Grade 2 cold drawn seamless Pipes | Titanium Grade 2 Decorative Pipe |
| Titanium Grade 2 Aero engine Pipes suppliers | Titanium Grade 2 Mortar Pipe stockholder |
| Titanium Grade 2 Aerospace Engine Pipes stockist | Titanium Grade 2 Radiant Pipe exporter in china |
| Titanium Grade 2 Furnace Pipes manufacturers | Titanium Grade 2 Square Pipe manufacturers |
| Titanium Grade 2 Precision Pipe exporter in china | ASTM B163 Titanium Grade 2 Heat Exchager Pipes |
| Grade 2 High Pressure Pipe | Titanium Grade 2 Pipe |
| Grade 2 Hot finished seamless Pipe (HFS) | Grade 2 Titanium Instrumentation Pipes |
| Grade 2 Cold drawn seamless Pipe (CDS) | Titanium Gr 2 coiled Pipe |
| Grade 2 Drawn over mandrel (DOM) | Titanium Gr 2 straight Pipe heat exchanger |
| supplier of Grade 2 Titanium Finned Pipe | Titanium Gr 2 straight Pipe boiler |
| Grade 2 Pipes for Precision Components | Titanium Grade 2 U Shaped Pipe suppliers |
| High Quality Titanium Grade 2 Seamless Pipe | Titanium Grade 2 exhaust Pipe manufacturers |
| Titanium Grade 2 Square Pipe manufacturers | Titanium Grade 2 Condensers Pipes stockholder |
| Titanium Grade 2 Round Pipe exporter in china | Titanium Grade 2 Protection Pipe |
| Titanium Grade 2 Rectangular Pipe traders | Titanium Grade 2 Super Heater pipe exporter in china |
| ASTM B163 Titanium Grade 2 Round Pipes stockist | distributor of Titanium Grade 2 Pipes for Heat Exchangers |
| Titanium Grade 2 Triangle Pipe exporter in china | Titanium Grade 2 redrawn Pipe suppliers |
| Titanium Grade 2 Hexagonal Pipe distributor | Titanium Grade 2 seam-welded Pipe stockist |
| Titanium Grade 2 Hollow Pipes Suppliers | supplier of Titanium Grade 2 cold-drawn coiled Pipe |
| exporter of Titanium Grade 2 thermocouple Pipe | Titanium Grade 2 Chemical Process Pipes stockist |
| Trader of ASTM B338 Titanium Polish Pipe | Titanium Grade 2 Welded coiled Pipe distributor |
| Titanium Grade 2 Cold Drawn Pipe stockist | Titanium Gr 2 heat resistant Pipe |
| Titanium Grade 2 ERW Pipe manufacturers | custom Titanium Grade 2 Pipe |
| exporter of Titanium Grade 2 Colour Coated Pipe | Titanium Grade 2 header Pipe |
| Titanium Grade 2 Welded Pipe stockist | Titanium Grade 2 rectangular Pipe |
| Titanium Grade 2 Secondary & Surplus Pipe | Titanium Grade 2 Cold Rolled Coiled Pipe |
| Titanium Grade 2 Outside Polished Pipe | Titanium Grade 2 Cold Drawn Pipe wholesaler |
| Titanium Grade 2 Brushed Pipe | Titanium Grade 2 Boiler Pipes distributor |
프로젝트의 성공을 위해 Daxun을 선택하세요.

고급 생산: 티타늄 심리스 파이프
- Grade 2 titanium seamless pipes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. The pipes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic flaw detection capabilities. Hot rolled pipe/hot extruded titanium seamless pipe: outer diameter 1.0mm to 325mm, wall thickness 0.3mm to 50mm, length up to 12000mm. Cold rolled titanium seamless pipe: cold processed pipes are supplied after heat treatment, surface etching, water pressure test or ultrasonic flaw detection according to manufacturing specifications. Outer diameter 6mm to 102mm, wall thickness 0.5mm to 20mm, length up to 9000mm.
(위 내용은 특정 상황에 따라 제조업체와 고객이 합의하여 결정합니다.)
Grade 2 Titanium Tube Features
Daxun’s Grade 2 Titanium Tube has medium strength and excellent cold forming properties. It has excellent welding properties and has excellent resistance to oxidation and corrosion.
- High Strength Titanium Alloy
- Excellent Cold Formability
- Excellent Weldability
- Excellent High Oxidation Resistance
- We stock and sell this grade of Grade 2 Titanium Tube, Titanium Welded Tube, Titanium Seamless Tube, Pipe Fittings, Forged Seamless Tube.


고급 생산: 티타늄 용접 튜브
Grade 2 Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), lengths up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.
테스트 보고서
The test reports we provide include: Factory test certificate for Grade 2 Titanium Welded Pipe and Grade 2 Titanium Seamless Pipe, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, NABL approved laboratory report, Destructive Test Report, Non-destructive Testing Report. (DaXun will provide according to customer requirements)


애플리케이션 및 표준
Grade 2 titanium tubes are widely used in the following industries under extreme corrosive conditions:
- Chemical processing parts such as heat exchangers, reaction vessels, evaporators and transmission pipelines, automobile exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
- Specifications: ASTM B861, B862, B338 / ASME SB861, SB862, SB338
- Standards: ASTM, ASME, GB, GJB, API
품질, 배송, 검사
Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 2 Titanium Welded Tube and Grade 2 Titanium Seamless Tube materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.
- 배송 시간은 엄격하게 계약에 따릅니다.
- 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
- 고객 테스트를 위한 무료 샘플 지원
- 현장 또는 비디오 공장 검사 지원


패키징
상품이 다양한 경로를 거쳐 최종 목적지에 도착하는 국제화물에서 포장은 중요한 역할을 하기 때문에 대순합금은 포장에 각별한 주의를 기울이고 있으며 최고의 품질을 보장합니다. 제품에 따라 다양한 방법으로 상품을 포장합니다. 다음과 같은 다양한 방법으로 제품을 포장합니다:
- 상자 및 상자
- 수축 포장
- 목재 팔레트
- 나무 상자
기술 지원
추가 기술 지원이 필요한 경우 금속 전문가와 지식이 풍부한 직원이 기꺼이 도와드릴 것입니다. 또한 Daxun은 다중 금속 및 플라스틱 재고 업계 최초로 인증된 테스트 실험실을 보유하고 있습니다. 이는 품질에 대한 변함없는 헌신과 풀서비스 공급업체로서의 철학을 보여주는 것이라고 생각합니다.

Grade 2Titanium TUBE Features
Daxun Grade 2 Titanium TUBE Let your brand improve rapidly
- 갤러리
- Titanium pipe/tube
- Surface
- Types of
- 무게
| 아래 나열된 제품 외에 사용 가능한 다른 금속 제품은 여기에 나열되어 있지 않습니다. DAXUN이 제조 및 공급할 수 있는 기타 금속 제품으로는 탄탈륨, 니오븀, 지르코늄, 하프늄, 니켈, 구리 등이 있으며 주로 판재, 바, 튜브 형태입니다. | |
| 제품/처리 표준 | 등급/크기 |
| 티타늄 플레이트, 시트, 코일- ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(두께:( 0.0197”-6”)최대 폭: 12피트, 최대 길이: 50피트) |
| AMS-T-9046 | |
| Titanium and Titanium alloy pipe/tube | |
| 상업적으로 순수한 티타늄(CP) | |
| 코드 지정 | 수율 강도 |
| 최소, KSI 1 / | |
| CP-1 | 70 |
| CP-2 | 55 |
| CP-3 | 40 |
| CP-4 | 25 |
| 알파 티타늄 합금(A) | |
| 코드 지정 | 구성 |
| A-1 | 5A1-2.5Sn |
| A-2 | 5A1-2.5Sn(ELI) 2 / |
| A-3 | 6A1-2Cb-1Ta-0.8Mo |
| A-4 | 8A1-1Mo-1V |
| 알파-베타 티타늄 합금(AB) | |
| 코드 지정 | 구성 |
| AB-1 | 6A1-4V |
| AB-2 | 6A1-4V(ELI) |
| AB-3 | 6A1-6V-2Sn |
| AB-4 | 6A1-2Sn-4Zr-2Mo |
| AB-5 | 3A1-2.5V |
| AB-6 | 8Mn |
| 베타 티타늄 합금(B) | |
| 코드 지정 | 구성 |
| B-1 | 13V-11Cr-3A1 |
| B-2 | 11.5Mo-6Zr-4.5Sn |
| B-3 | 3A1-8V-6Cr-4Mo-4Zr |
| B-4 | 8Mo-8V-2Fe-3A1 |
| 처리 중입니다: | |
| 열간 압연 | 냉간 압연 |
| 사용 가능한 성적: | |
| CP 1등급 | 6Al-2Sn-4Zr-2Mo(6-2-4-2) 등급 |
| CP 2등급 | 6Al-4V ELI 등급(이전 23등급) |
| 7학년 | 6Al-6V-2Sn(6-62) 등급 |
| 19학년 | 8알-1모-1V 등급(8-1-1) |
| 5등급(6Al-4V) | 9등급(3Al-2.5V) |
| 6등급(5Al-2.5Sn) | CP 3등급 |
| 애플리케이션 | |
| 화학 산업 | 해수 담수화 |
| 석유화학 산업 | 항공우주 |
| 기계 가공 분야, 자동차 분야 | 휴대폰 구성 요소 필드. |
| urface Finish | 내부 표면(ID) | 외부 표면(OD) | |||
| 거칠기 평균(RA) | 거칠기 평균(RA) | ||||
| μ 인치 | μm | μ 인치 | μm | ||
| BA | 베이트 어닐링 | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| EP | 일렉트로 폴리쉬 | 15,10,7,5 | 0.38,0.25,0.20;0.13 | 32 | 0.8 |
| MP | 기계식 광택 | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| AP | 절임 & 절임 | 정의되지 않음 | 정의되지 않음 | 40 또는 정의되지 않음 | 1.0 또는 정의되지 않음 |
| Titanium Grade 2 Seamless Pipe | Titanium DIN 3.7035 Seamless Pipe |
| Titanium UNS R50400 Seamless Pipe | |
| Titanium Grade 2 Seamless Pipes | |
| Titanium Alloy Gr.2 Seamless Pipe | |
| ASTM B337 Titanium Grade 2 Seamless Pipe | |
| ASME SB337 Ti Alloy Gr.2 Seamless Pipes | |
| Titanium Grade 2 Welded Pipe | Titanium DIN 3.7035 Welded Pipe |
| Titanium UNS R50400 Welded Pipe | |
| Titanium Grade 2 Welded Pipes | |
| Titanium Alloy Gr.2 Welded Pipe | |
| ASTM B337 Titanium Grade 2 Welded Pipes | |
| ASME SB337 Ti Alloy Gr.2 Welded Pipes | |
| Titanium Grade 2 Round Pipe | Titanium DIN 3.7035 Round Pipe |
| Titanium UNS R50400 Round Pipes | |
| Titanium Grade 2 Round Pipes | |
| Titanium Alloy Gr.2 Round Pipe | |
| Titanium Grade 2 Round Pipe | |
| Ti Alloy Gr.2 Round Pipes | |
| Titanium Gr.2 Seamless Tubes | Titanium DIN 3.7035 Seamless Tubes |
| Titanium UNS R50400 Seamless Tubes | |
| Titanium Grade 2 Seamless Tubing | |
| Titanium Alloy Gr.2 Seamless Tubes | |
| ASTM B338 Titanium Gr.2 Seamless Tubing | |
| ASME SB338 Ti Alloy Grade 2 Seamless Tubes | |
| Titanium Grade 2 Welded Tubes | Titanium DIN 3.7035 Welded Tubes |
| Titanium UNS R50400 Welded Tubes | |
| Titanium Grade 2 Welded Tubing | |
| Titanium Alloy Gr.2 Welded Tubes | |
| ASTM B338 Titanium Grade 2 Welded Tubing | |
| ASME SB338 Ti Alloy Gr.2 Welded Tubes | |
| Titanium Grade 2 Round Tubes | Titanium DIN 3.7035 Round Tubes |
| Titanium UNS R50400 Round Tubes | |
| Titanium Grade 2 Round Tubing | |
| Titanium Alloy Gr.2 Round Tubes | |
| Titanium Grade 2 Round Tubing | |
| Ti Alloy Gr.2 Round Tubes | |
| Titanium Grade 2 Pipe | Titanium DIN 3.7035 Pipe |
| Titanium UNS R50400 Pipes | |
| Titanium Grade 2 Pipe | |
| Titanium Alloy Gr.2 Pipes | |
| Titanium Grade 2 Pipes | |
| Ti Alloy Gr.2 Pipe | |
| Titanium Grade 2 Tube | Titanium DIN 3.7035 Tubes |
| Titanium UNS R50400 Tube | |
| Titanium Grade 2 Tubing | |
| Titanium Alloy Gr.2 Tubes | |
| Titanium Grade 2 Tubes | |
| Ti Alloy Gr.2 Tubes |
| NPS | 외경 | 벽 두께 | 무게 | 무게 | |||
| in | mm | in | mm | Sched | kg/Mtr | 파운드/피트 | |
| 1/2″ | 0.84 | 21 | 0.109 | 2.769 | 40 STD | 1.268 | 0.851 |
| 0.147 | 3.734 | 80 STD | 1.621 | 1.088 | |||
| 3/4″ | 1.05 | 27 | 0.113 | 2.87 | 40 STD | 1.684 | 1.131 |
| 0.154 | 3.912 | 80 STD | 2.195 | 1.474 | |||
| 1″ | 1.315 | 33 | 0.133 | 3.378 | 40 STD | 2.501 | 1.679 |
| 0.179 | 4.547 | 80 STD | 3.325 | 2.172 | |||
| 1 1/4″ | 1.66 | 42 | 0.14 | 3.556 | 40 STD | 3.385 | 2.273 |
| 0.191 | 4.851 | 80 STD | 4.464 | 2.997 | |||
| 1 1/2″ | 1.9 | 48 | 0.145 | 3.683 | 40 STD | 4.048 | 2.718 |
| 0.2 | 5.08 | 80 STD | 5.409 | 3.361 | |||
| 2″ | 2.375 | 60 | 0.154 | 3.912 | 40 STD | 5.441 | 3.653 |
| 0.218 | 5.537 | 80 STD | 7.48 | 5.022 | |||
| 2 1/2″ | 2.875 | 73 | 0.203 | 5.516 | 40 STD | 8.629 | 5.793 |
| 0.276 | 7.01 | 80 STD | 11.411 | 7.661 | |||
| 3″ | 3.5 | 89 | 0.216 | 5.486 | 40 STD | 11.284 | 7.576 |
| 0.3 | 7.62 | 80 STD | 15.272 | 10.253 | |||
| 4″ | 4.5 | 114 | 0.237 | 6.02 | 16.073 | 10.79 | |
| 0.337 | 8.56 | 22.318 | 14.983 | ||||
| 6″ | 6.625 | 168 | 0.188 | 4.775 | 19.252 | 12.924 | |
| 0.203 | 5.516 | 20.739 | 13.923 | ||||
| 0.219 | 5.563 | 22.318 | 14.983 | ||||
| 0.25 | 6.35 | 25.354 | 17.021 | ||||
| 0.28 | 7.112 | 40 STD | 58.263 | 18.974 | |||
| 0.312 | 7.925 | 31.334 | 21.036 | ||||
| 0.375 | 9.525 | 37.285 | 25.031 | ||||
| 0.432 | 10.973 | 80 XHY | 42.561 | 28.573 | |||
| 0.5 | 12.7 | 48.719 | 32.708 | ||||
| 8″ | 8.625 | 219 | 0.188 | 4.775 | 25.233 | 16.94 | |
| 0.203 | 5.156 | 27.198 | 18.259 | ||||
| 0.219 | 5.563 | 29.286 | 19.661 | ||||
| 0.25 | 6.35 | 20 | 33.308 | 22.361 | |||
| 0.277 | 7.036 | 30 | 36.786 | 24.696 | |||
| 0.322 | 8.179 | 40 | 42.352 | 28.554 | |||
| 0.375 | 9.525 | 49.216 | 33.041 | ||||
| 0.406 | 10.312 | 60 | 53.085 | 35.638 | |||
| 0.5 | 12.7 | 80 XHY | 64.627 | 43.388 | |||
| 10″ | 10.75 | 273 | 0.188 | 4.775 | 31.588 | 21.207 | |
| 0.219 | 5.563 | 36.689 | 24.631 | ||||
| 0.25 | 6.35 | 20 | 41.759 | 28.035 | |||
| 0.307 | 7.798 | 30 | 51.002 | 34.24 | |||
| 0.344 | 8.738 | 56.946 | 38.231 | ||||
| 0.365 | 9.271 | 40 STD | 63.301 | 40.483 | |||
| 0.438 | 11.125 | 71.852 | 48.238 | ||||
| 0.5 | 12.7 | 60 XHY | 81.53 | 54.735 | |||
| 0.594 | 15.088 | 80 | 95.969 | 64.429 | |||
| 12″ | 12.75 | 324 | 0.188 | 4.775 | 37.57 | 25.222 | |
| 0.219 | 5.563 | 43.657 | 29.309 | ||||
| 0.25 | 6.35 | 49.713 | 33.375 | ||||
| 0.281 | 7.137 | 55.739 | 37.42 | ||||
| 0.312 | 7.925 | 61.735 | 41.445 | ||||
| 0.375 | 9.525 | 73.824 | 49.562 | ||||
| 0.406 | 10.312 | 79.727 | 53.525 | ||||
| 0.5 | 12.7 | 97.438 | 65.415 | ||||
| 0.562 | 14.275 | 108.966 | 73.154 | ||||
| 14″ | 14 | 356 | 0.188 | 4.775 | 41.308 | 27.732 | |
| 0.219 | 5.563 | 48.012 | 32.233 | ||||
| 0.25 | 6.35 | 20 | 54.685 | 36.713 | |||
| 0.281 | 7.137 | 61.327 | 41.172 | ||||
| 0.312 | 7.925 | 67.939 | 45.611 | ||||
| 0.375 | 9.525 | STD | 81.281 | 54.568 | |||
| 0.438 | 11.125 | 40 | 94.498 | 63.441 | |||
| 0.5 | 12.7 | XHY | 107.381 | 72.09 | |||
| 0.625 | 15.875 | 132.983 | 89.278 | ||||
| 16” | 16 | 406 | 0.188 | 4.775 | 47.29 | 21.748 | |
| 0.219 | 5.563 | 54.98 | 36.91 | ||||
| 0.25 | 6.35 | 10 | 62.639 | 42.053 | |||
| 0.281 | 7.137 | 70.268 | 47.174 | ||||
| 0.312 | 7.925 | 20 | 77.866 | 52.275 | |||
| 0.344 | 8.738 | 85.677 | 57.519 | ||||
| 0.375 | 9.525 | 30 | 93.213 | 62.578 | |||
| STD | |||||||
| 0.438 | 11.125 | 108.433 | 72.797 | ||||
| 0.5 | 12.7 | 40 | 123.289 | 82.77 | |||
| XHY | |||||||
| 18″ | 18 | 457 | 0.219 | 5.563 | 61.948 | 41.588 | |
| 0.25 | 6.35 | 70.593 | 47.393 | ||||
| 0.281 | 7.137 | 79.208 | 53.176 | ||||
| 0.312 | 7.925 | 20 | 87.792 | 58.939 | |||
| 0.375 | 9.525 | STD | 105.144 | 70.588 | |||
| 0.438 | 11.125 | 30 | 122.369 | 82.152 | |||
| 0.5 | 12.7 | XHY | 139.198 | 93.45 | |||
| 0.562 | 14.275 | 40 | 155.904 | 104.666 | |||
| 0.625 | 15.875 | 172.754 | 115.978 | ||||
| 20″ | 20 | 508 | 0.25 | 6.35 | 78.547 | 52.733 | |
| 0.282 | 7.163 | 88.458 | 59.386 | ||||
| 0.312 | 7.925 | 97.719 | 65.604 | ||||
| 0.375 | 9.525 | 20 STD | 117.075 | 78.598 | |||
| 0.438 | 11.125 | 136.305 | 91.508 | ||||
| 0.5 | 12.7 | 30 XHY | 155.106 | 104.13 | |||
| 0.594 | 15.088 | 40 | 183.378 | 123.11 | |||
| 0.625 | 15.875 | 192.64 | 129.328 | ||||
| 0.688 | 17.475 | 211.368 | 141.901 | ||||
| 24″ | 24 | 610 | 0.25 | 6.35 | 94.456 | 63.413 | |
| 0.281 | 7.137 | 106.029 | 71.183 | ||||
| 0.312 | 7.925 | 117.573 | 18.932 | ||||
| 0.375 | 9.525 | 20 STD | 140.938 | 64.618 | |||
| 0.438 | 11.125 | 164.176 | 110.219 | ||||
| 0.5 | 12.7 | XHY | 186.923 | 125.49 | |||
| 0.625 | 15.875 | 232.41 | 156.028 | ||||
| 0.688 | 17.475 | 40 | 255.148 | 171.293 | |||
| 0.75 | 19.05 | 277.401 | 186.233 | ||||
| 30″ | 30 | 762 | 0.25 | 6.35 | 118.318 | 79.433 | |
| 0.281 | 7.137 | 132.851 | 89.189 | ||||
| 0.312 | 7.925 | 10 | 147.353 | 98.925 | |||
| 0.375 | 9.525 | STD | 176.731 | 118.648 | |||
| 0.438 | 11.125 | 205.983 | 138.286 | ||||
| 0.5 | 12.7 | 20 XHY | 234.647 | 157.53 | |||
| 0.625 | 15.875 | 30 | 292.066 | 196.078 | |||
| 0.688 | 17.475 | 320.817 | 215.38 | ||||
| 0.75 | 19.05 | 348.988 | 234.293 | ||||
| 36″ | 36 | 914 | 0.25 | 6.35 | 142.18 | 95.453 | |
| 0.281 | 7.137 | 159.672 | 107.196 | ||||
| 0.312 | 7.925 | 10 | 177.133 | 118.918 | |||
| 0.375 | 9.525 | STD | 215.525 | 142.678 | |||
| 0.438 | 11.125 | 247.79 | 166.353 | ||||
| 0.5 | 12.7 | 20 XHY | 282.372 | 198.57 | |||
| 0.625 | 15.875 | 351.723 | 236.128 | ||||
| 0.688 | 17.475 | 386.487 | 259.467 | ||||
| 0.75 | 19.05 | 420.576 | 282.353 | ||||
| 42″ | 42 | 1067 | 0.312 | 7.925 | 206.914 | 138.911 | |
| 0.375 | 9.525 | STD | 248.319 | 166.708 | |||
| 0.5 | 12.7 | XHY | 33.097 | 221.61 | |||
| 0.75 | 19.05 | 492.163 | 330.413 | ||||
| 48″ | 48 | 1219 | 0.375 | 9.525 | STD | 284.112 | 190.738 |
| 0.438 | 11.125 | 331.404 | 222.487 | ||||
| 0.5 | 12.7 | XHY | 377.822 | 253.65 | |||
| 0.75 | 19.05 | 563.75 | 378.473 | ||||
| 0.875 | 22.225 | 655.969 | 440.383 | ||||
Grade 2 titanium tube form (4)
참조 및 다운로드 가능한 정보
Daxun is a trustworthy stainless steel pipe/tube manufacturer
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel pipe/tubes have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
관련 제품 (8)
Grade 2 Titanium Tube (UNS R50400 / Werkstoff WS 3.7034)
This is the most often used titanium tube for industrial applications, providing a superb balance of moderate strength and reasonable ductility. It offers excellent corrosion resistance in both highly oxidising and slightly reducing conditions (including chlorides). It provides good corrosion protection in the chemical and offshore industries, as well as aircraft manufacture, where strength and ease of forming are required. It’s also utilised in heat exchangers, hypochlorite systems, fire water systems, ballast water systems, industrial and aerospace components, CPI equipment, and pipes.
Fabrication
Stock Availability
Weight Reduction
Crystal Structure
Grade 2 Titanium Seamless Pipe Manufacturing Process
Grade 2 Titanium Welded Pipe Manufacturing Process
Power Industry Reference List
| 회사 | Project |
|---|---|
| Alstom Power | Calpine Fox Energy |
| Alstom Power | Skikda |
| The Atlantic Group | Savannah Electric Power Kraft #2 |
| Constellation Power | Wagner Station Unit #2 |
| Ecolaire/Yuba Heat Transfer | Connectiv Energy |
| Ellet Industries | — |
| Graham Corp | — |
| Hantech | — |
| High Performance Tube | — |
| Joseph Oat | BP Chemical |
| Larsen & Toubro | TATA Power — UMPP Mundra |
| Salem Tube | — |
| The Atlantic Group | Savannah Electric Power Kraft #2 |
| Tico Titanium | — |
| Titan Metal Fab | BP Chemical |
| Titanium Fabricators | — |
| Tubes Inc. | — |
| Uniti Titanium | — |
| Waterco | — |
| Waterpik Technologies | — |
Our services
- We customise your grade 2 titanium tubes to your specifications, certify them with various certifying organisations (e.g., TÜV Rheinland or DNV), and begin upgrading titanium semi-finished products for the corresponding applications.
- We will be delighted to advise and explain what you need to know when obtaining titanium tubes, as well as which criteria you should pay particular attention to while producing the components.
- If you have long-term delivery responsibilities, you can enter into a framework agreement with Daxun. We guarantee prices and quantities within specified dates.
- Benefit from our extensive knowledge in the worldwide procurement industry. Since 2003, we have served small, medium-sized, and large businesses at home and abroad.
- Have you got any questions? Our service centre would be delighted to answer any queries you have about finished titanium tubes and unusual materials. We look forward to hearing from you.
필요한 티타늄 합금의 등급은 각 등급마다 다른 이점이 있으므로 작업 중인 프로젝트에 따라 다릅니다.
모든 등급의 티타늄 합금은 매우 강하고 부식에 강하기 때문에 가장 혹독한 환경에서도 잘 작동합니다.
더 높은 등급의 티타늄 합금(5-12)은 특정 이점을 위해 설계된 합금입니다. 예를 들어, 12등급 티타늄 합금은 내열성이 뛰어나 쉘 및 튜브 열교환기, 유압 배관 및 화학 산업 장비에 적합합니다.
1~4등급은 순수 티타늄 합금으로, 배관 시스템과 튜빙에 용접 가능한 연성 소재가 필요한 경우 완벽한 선택입니다. 그보다 낮은 등급은 해양 및 산업 산업에서 사용됩니다.
프로젝트를 시작하면서 어떤 등급의 티타늄 합금이 가장 적합한지 잘 모르겠다면 지금 바로 문의하시면 기꺼이 도와드리겠습니다.
DAXUN에서는 1등급부터 12등급까지 다양한 티타늄 합금 등급을 제공합니다.
1~4등급은 순수 티타늄이고 그 이상 등급은 합금입니다.
합금 등급은 무게 대비 강도가 높기 때문에 인기가 높습니다.
가장 일반적으로 사용되는 티타늄 합금 등급은 5등급입니다. 티타늄 함량이 여전히 높지만 이 등급은 최대 600°F의 온도와 극한의 조건을 견딜 수 있기 때문에 가장 신뢰할 수 있는 등급 중 하나입니다.
항공우주 및 해양 산업과 같은 산업에서는 내마모성과 내식성 때문에 등급이 높을수록 선호합니다.
반대로 낮은 등급은 강도가 낮기 때문에 주로 용접에 사용됩니다.
다양한 등급의 티타늄 합금의 차이점에 대해 자세히 알아보려면 지금 바로 +86 13382898899으로 전화하여 전문가와 직접 상담하세요.
티타늄의 등급에 따라 비용이 약간 증가하지만, 총 비용은 주로 필요한 티타늄의 모양과 형태에 따라 결정됩니다.
At DAXUN, we offer a wide range of titanium products, including pipe/tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.
안타깝게도 프로젝트와 티타늄의 용도에 대해 잘 알지 못하면 온라인에서 가격을 책정하기 어렵습니다.
다행히도 저희 전문가 팀이 언제나 티타늄 관련 문의에 대해 도움을 드리고 조언해 드립니다. [email protected] 으로 이메일을 보내주시면 몇 가지 조언과 정확한 견적을 알려드리겠습니다.
필요한 티타늄의 등급, 모양 및 수량에 대해 가능한 한 많은 정보를 포함하여 요구 사항을 더 잘 파악할 수 있도록 하세요.
DAXUN의 팀은 경험이 풍부하고 지식이 풍부하며 친절합니다. 업계에서 다년간의 경험을 바탕으로 티타늄의 용도, 장점, 등급 등 티타늄에 대한 모든 것을 잘 알고 있습니다.
티타늄, 티타늄의 용도 및 산업 전반에 걸친 티타늄의 활용에 대한 정기적인 업데이트를 확인하려면 블로그를 확인하세요. 궁금한 점이 있을 때 언제든지 참고할 수 있도록 전문가들이 쉽게 따라할 수 있는 가이드를 작성했습니다.
여전히 문제가 있는 경우 언제든지 문의해 주세요. 기꺼이 도와드리겠습니다.
[email protected] 으로 이메일을 보내주시면 빠른 답변을 받으실 수 있습니다. 적합한 솔루션을 추천할 수 있도록 질문에 가능한 한 자세한 내용을 포함해 주세요.
“문의하기” 페이지의 양식을 작성하거나 영업 관리자(+86 13382898899)에게 전화하시면 최대한 빨리 연락드리겠습니다. WhatsApp은 온라인 상태이며 이메일([email protected])은 6시간 이내에 확인합니다. 모든 문의나 메시지는 신속하게 답변해 드립니다. 또한 매주 고객과 시장 정보를 공유합니다.
We can provide stainless steel pipe/tube samples for you to check the quality. Sample is free and you just pay the freight.
캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.
Our MOQ is 1 ton for stainless steel pipe/tube.
체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.