Global leader in stainless steel angle fabrication services
304/304L and 316/316L Stainless Steel Angles
As China’s premier supplier of specialty metals, you can trust Daxun for all of your stainless steel angle needs. Our stainless steel angle selection includes 304/304L and 316/316L stainless steel angles. Our extensive product line offers durability and versatility, making it the perfect solution for your structural and fabrication needs.
Our stainless steel angles are available in 304/304L and 316/316L, all from fully certified factories. Our comprehensive product line is both durable and adaptable, ideal for structural and fabrication applications. As a leading stainless steel angle manufacturer, we offer a wide range of specialty angles and L-shaped angles. Daxun offers stainless steel angles in any length, up to 6 meters. The following stainless steel grades are also available: 304/304L and 316/316L. Stainless steel angles are most commonly used for supports or frames, but are also used in food equipment, building supports, structural supports, and medical equipment.
Can be welded and processed using simple procedures, 304/304L stainless steel angles are suitable for many environments, such as general industrial projects, chemical projects. While 316/316L angles are marine grade and have strong corrosion resistance in more demanding conditions.
The surface treatment we use on our stainless steel angles is hot rolling, annealing, and pickling. This surface treatment maximizes corrosion resistance and gives the angles a unique “stainless” appearance.
The two manufacturing methods are laser melting and hot rolling. Hot rolling produces stainless steel angles at a lower price. They usually have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also have a sandblasted, smoother surface. Laser melted stainless steel angles have a smoother surface quality than hot rolled stainless steel angles.
Daxun Alloy manufactures laser melted and hot rolled stainless steel angles in metric and imperial sizes. We can ship them all over the world.
データ
- パラメータ
- エレメント
- 機械的特性
- 物性
- すべて同等
| スタンダード | ASTM、EN、DIN、JIS、ASME、BS、GBなど、, |
| 寸法 | ∠20*20*3mm-∠200*200*24mm |
| 合金 | 201、310、304、304L、316、316L |
| タイプ | 平等、不平等 |
| 長さ | 1.0-12.0m |
| 厚さ | 3mm-25mm |
| カスタムオプション | はい |
| 公差 | ± ¼”, ± 1/16” |
| 表面処理 | ミル、ブラシ、ミラー、ポリッシュ |
| CHEMICAL COMPOSITION: ASTM A240, A666 | ||
| エレメント | Type 316 | Type 316L |
| カーボン | 最大0.08. | 最大0.030. |
| Manganese | 2.00 max. | 2.00 max. |
| Sulfur | 最大0.030. | 最大0.030. |
| Phosphorus | 0.045 max. | 0.045 max. |
| Silicon | 0.75 max. | 0.75 max. |
| Chromium | 16.0 – 18.0 | 16.0 – 18.0 |
| Nickel | 10.00 – 14.00 | 10.00 – 14.00 |
| Molybdenum | 2.00 – 3.00 | 2.00 – 3.00 |
| 窒素 | 最大0.10. | 最大0.10. |
| タイプ | 降伏強さ 0.2% オフセット(KSI) | 引張強さ(KSI) | % Elongation (2″ Gauge length) |
| 316 | 30分. | 75分. | 40分. |
| 316L | 25分. | 70分. | 40分. |
| 密度 (lb./ in^2) @ RT | 0.29 | |
| 引張弾性係数 (psi x 10^6) | 28 | |
| 比熱(BTU/o F/lb.) | 32~212度 | 0.12 |
| 熱伝導率(BTU/hr/ft^2/ft) | 212oF | 9.4 |
| 932oF | 12.4 | |
| 平均熱膨張係数 (in. x 10^-6 per o F) | 32~212oF | 8.9 |
| 32~600oF | 9 | |
| 32~1,000oF | 9.7 | |
| 32~1,200oF | 10.3 | |
| 電気抵抗率(マイクロオーム - cm) | 華氏70度 | 29.4 |
| 融点範囲 | 2500 – 2550 |
| グレード | UNS No | Old British | Euronorm | Swedish SS | Japanese JIS | ||
| BS | En | No | 名称 | ||||
| 316l | S31603 | 316S11 | – | 1.4404 | X2CrNiMo17-12-2 | 2348 | SUS 316L |
Daxunを選択し、顧客を満足させる。.

迅速な対応
We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.Daxun’s stainless steel materials are of reliable quality, and their varieties, specifications and delivery weights strictly comply with the standards.
大順のメリット
Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel uses the ERP system to achieve full traceability of each angle steel, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.


パッケージング
国際貨物は様々な経路を経て最終目的地に到着するため、梱包は重要な役割を担っています。商品によって、様々な方法で梱包しています。当社では、以下のような様々な方法で商品を梱包しています:
- 箱と木箱
- シュリンクラップ
- 木製パレット
- 木製ボックス
品質、納期、検査
- Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
- During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
当社の納期は、契約に厳密に従います。. - 顧客の第三者機関が工場に検査に行くのをサポートする。
- テスト用の無料サンプルを顧客に提供
- 現場検査またはビデオ工場検査をサポート


ご注文について
Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.
テクニカルサポート
さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.

SS 316-316L Stainless Steel angle Features
大順合金 あなたのブランドを急速に向上させる
- スペック表
| アングル - スチールデータ | |||||||||||||
| 等角と不等角 | |||||||||||||
| ANGLEは、ご要望に応じて他のサイズもご用意できます。 | |||||||||||||
| 説明 | 幅 (W) | 深さ (D) | 厚さ | スタンダード | 重量 | 表面 | |||||||
| (mm) | (mm) | (T) (mm) | 長さ | メートル | 面積 | ||||||||
| (kg/m) | メートル | ||||||||||||
| (m²/m) | |||||||||||||
| アングル 20 X 20 X 3.0mm | 20 | 20 | 3 | 6.0メートル | 0.98 | 0.0897 | |||||||
| アングル 25 X 25 X 3.0mm | 25 | 25 | 3 | 7.5メートル | 1.12 | 0.0953 | |||||||
| アングル 25 x 25 x 5.0mm | 25 | 25 | 5 | 7.5メートル | 1.65 | 0.0953 | |||||||
| アングル 25 X 25 X 6.0mm | 25 | 25 | 6 | 7.5メートル | 2.08 | 0.0953 | |||||||
| アングル 30 X 30 X 2.5mm | 30 | 30 | 2.5 | 6.0メートル | 1.06 | 0.117 | |||||||
| アングル 30 X 30 X 3.0mm | 30 | 30 | 3 | 7.5メートル | 1.35 | 0.115 | |||||||
| アングル 30 X 30 X 5.0mm | 30 | 30 | 5 | 7.5メートル | 2.01 | 0.115 | |||||||
| アングル 30 X 30 X 6.0mm | 30 | 30 | 6 | 7.5メートル | 2.56 | 0.115 | |||||||
| アングル 40 X 40 X 2.5mm | 40 | 40 | 2.5 | 6.0メートル | 1.43 | 0.157 | |||||||
| アングル 40 X 40 X 3.0mm | 40 | 40 | 3 | 7.5メートル | 1.83 | 0.155 | |||||||
| アングル 40 X 40 X 4.0mm | 40 | 40 | 4 | 6.0メートル | 2.2 | 0.155 | |||||||
| アングル 40 X 40 X 5.0mm | 40 | 40 | 5 | 9.0メートル | 2.73 | 0.155 | |||||||
| アングル 40 X 40 X 6.0mm | 40 | 40 | 6 | 9.0メートル | 3.5 | 0.155 | |||||||
| アングル 45 X 45 X 3.0mm | 45 | 45 | 3 | 9.0メートル | 2.06 | 0.175 | |||||||
| アングル 45 X 45 X 5.0mm | 45 | 45 | 5 | 9.0メートル | 3.1 | 0.175 | |||||||
| アングル 45 X 45 X 6.0mm | 45 | 45 | 6 | 9.0メートル | 3.97 | 0.175 | |||||||
| アングル 50 X 50 X 2.5mm | 50 | 50 | 2.5 | 9.0メートル | 1.81 | 0.197 | |||||||
| アングル 50 X 50 X 3.0mm | 50 | 50 | 3 | 7.5メートル | 2.31 | 0.195 | |||||||
| アングル 50 X 50 X 4.0mm | 50 | 50 | 4 | 9.0メートル | 2.79 | 0.195 | |||||||
| アングル 50 X 50 X 5.0mm | 50 | 50 | 5 | 9.0メートル | 3.48 | 0.195 | |||||||
| アングル 50 X 50 X 6.0mm | 50 | 50 | 6 | 9.0メートル | 4.46 | 0.195 | |||||||
| アングル 50 X 50 X 8.0mm | 50 | 50 | 8 | 9.0メートル | 5.68 | 0.195 | |||||||
| アングル 55 X 55 X 5.0mm | 55 | 55 | 5 | 9.0メートル | 3.84 | 0.215 | |||||||
| アングル 55 X 55 X 6.0mm | 55 | 55 | 6 | 9.0メートル | 4.93 | 0.215 | |||||||
| アングル 65 X 50 X 5.0mm | 65 | 50 | 5 | 9.0メートル | 4.02 | 0.225 | |||||||
| アングル 65 X 50 X 6.0mm | 65 | 50 | 6 | 9.0メートル | 5.16 | 0.225 | |||||||
| アングル 65 X 50 X 8.0mm | 65 | 65 | 8 | 9.0メートル | 6.59 | 0.225 | |||||||
| アングル 65 X 65 X 4.0mm | 65 | 65 | 4 | 9.0メートル | 3.69 | 0.255 | |||||||
| アングル 65 x 65 x 5.0mm | 65 | 65 | 5 | 9.0メートル | 4.56 | 0.255 | |||||||
| アングル 65 X 65 X 6.0mm | 65 | 65 | 6 | 9.0メートル | 5.87 | 0.255 | |||||||
| アングル 65 X 65 X 8.0mm | 65 | 65 | 8 | 9.0メートル | 7.51 | 0.255 | |||||||
| アングル 65 X 65 X 10.0mm | 65 | 65 | 10 | 9.0メートル | 9.02 | 0.255 | |||||||
| アングル 75 X 50 X 5.0mm | 75 | 50 | 5 | 9.0メートル | 4.4 | 0.244 | |||||||
| アングル 75 X 50 X 6.0mm | 75 | 50 | 6 | 9.0メートル | 5.66 | 0.244 | |||||||
| アングル 75 X 50 X 8.0mm | 75 | 50 | 8 | 9.0メートル | 7.23 | 0.244 | |||||||
| アングル 75 X 75 X 4.0mm | 75 | 75 | 4 | 9.0メートル | 4.29 | 0.295 | |||||||
| アングル 75 X 75 X 5.0mm | 75 | 75 | 5 | 9.0メートル | 5.27 | 0.292 | |||||||
| アングル 75 x 75 x 6.0mm | 75 | 75 | 6 | 9.0メートル | 6.81 | 0.292 | |||||||
| アングル 75 X 75 X 8.0mm | 75 | 75 | 8 | 9.0メートル | 8.73 | 0.292 | |||||||
| アングル 75 X 75 X 10.0mm | 75 | 75 | 10 | 9.0メートル | 10.5 | 0.292 | |||||||
| アングル 90 X 90 X 6.0mm | 90 | 90 | 6.0 | 9.0メートル | 8.22 | 0.352 | |||||||
| アングル 90 X 90 X 8.0mm | 90 | 90 | 8.0 | 9.0メートル | 10.6 | 0.352 | |||||||
| アングル 90 X 90 X 10.0mm | 90 | 90 | 10.0 | 9.0メートル | 12.7 | 0.352 | |||||||
| アングル 100 X 75 X 6.0mm | 100 | 75 | 6.0 | 9.0メートル | 7.98 | 0.342 | |||||||
| アングル 100 X 75 X 8.0mm | 100 | 75 | 8.0 | 9.0メートル | 10.3 | 0.342 | |||||||
| アングル 100 X 75 X 10.0mm | 100 | 75 | 10.0 | 9.0メートル | 12.4 | 0.342 | |||||||
| アングル 100 X 100 X 10.0mm | 100 | 100 | 10.0 | 9.0メートル | 14.2 | 0.392 | |||||||
| アングル 100 X 100 X 12.0mm | 100 | 100 | 12.0 | 9.0メートル | 17.7 | 0.392 | |||||||
| アングル 100 X 100 X 4.0mm | 100 | 100 | 4.0 | 9.0メートル | 5.78 | 0.395 | |||||||
| アングル 100 X 100 X 6.0mm | 100 | 100 | 6.0 | 9.0メートル | 9.16 | 0.392 | |||||||
| アングル 100 X 100 X 8.0mm | 100 | 100 | 8.0 | 9.0メートル | 11.8 | 0.392 | |||||||
| ANGLE125 X 75 X 6.0mm | 125 | 75 | 6.0 | 9.0メートル | 9.16 | 0.392 | |||||||
| アングル 125 X 75 X 8.0mm | 125 | 75 | 8.0 | 9.0メートル | 11.8 | 0.392 | |||||||
| アングル 125 X 75 X 10.0mm | 125 | 75 | 10.0 | 9.0メートル | 14.2 | 0.392 | |||||||
| アングル 125 X 75 X 12.0mm | 125 | 75 | 12.0 | 9.0メートル | 17.7 | 0.392 | |||||||
| アングル 125 X 125 X 8.0mm | 125 | 125 | 8.0 | 9.0メートル | 14.9 | 0.491 | |||||||
| アングル 125 X 125 X 10.0mm | 125 | 125 | 10.0 | 9.0メートル | 18 | 0.491 | |||||||
| アングル 125 X 125 X 12.0mm | 125 | 125 | 12.0 | 9.0メートル | 22.5 | 0.491 | |||||||
| アングル 125 X 125 X 16.0mm | 125 | 125 | 16.0 | 9.0メートル | 29.1 | 0.491 | |||||||
| アングル 150 X 90 X 8.0mm | 150 | 90 | 8.0 | 9.0メートル | 14.3 | 0.471 | |||||||
| アングル 150 X 90 X 12.0mm | 150 | 90 | 12.0 | 9.0メートル | 21.6 | 0.471 | |||||||
| アングル 150 X 90 X 16.0mm | 150 | 90 | 16.0 | 9.0メートル | 27.9 | 0.471 | |||||||
| アングル 150 X 100 X 10.0mm | 150 | 100 | 10.0 | 9.0メートル | 18 | 0.491 | |||||||
| アングル 150 X 100 X 12.0mm | 150 | 100 | 12.0 | 9.0メートル | 22.5 | 0.491 | |||||||
| アングル 150 X 150 X 10.0mm | 150 | 150 | 10.0 | 9.0メートル | 21.9 | 0.59 | |||||||
| アングル 150 X 150 X 12.0mm | 150 | 150 | 12.0 | 9.0メートル | 27.3 | 0.59 | |||||||
| アングル 150 X 150 X 16.0mm | 150 | 150 | 16.0 | 9.0メートル | 35.4 | 0.59 | |||||||
| アングル 150 X 150 X 19.0mm | 150 | 150 | 19.0 | 9.0メートル | 42.1 | 0.59 | |||||||
| アングル 150 X 90 X 10.0mm | 150 | 90 | 10.0 | 9.0メートル | 17.3 | 0.471 | |||||||
| アングル 200 x 200 x 13.0mm | 200 | 200 | 13.0 | 9.0メートル | 40 | 0.788 | |||||||
| アングル 200 X 200 X 16.0mm | 200 | 200 | 16.0 | 9.0メートル | 48.7 | 0.788 | |||||||
| アングル 200 X 200 X 20.0mm | 200 | 200 | 20.0 | 9.0メートル | 60.1 | 0.788 | |||||||
| アングル 200 X 200 X 26.0mm | 200 | 200 | 26.0 | 9.0メートル | 76.8 | 0.788 | |||||||
SS 316/316L Stainless Steel Angle Surface Type (3)
参照およびダウンロード可能な情報
Daxunは信頼できるステンレス鋼の角度の製造業者である
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel angles have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
最近の注目プロジェクトと製品
関連商品 (8)
中国のステンレス鋼の角度の製造者を導く
Daxun has been engaged in international business for more than ten years. In 2023, the export volume exceeded 100 million US dollars, and the export volume ranked among the top Chinese stainless steel manufacturers. Daxun continuously improves its service skills. To serve the global market, it has established three export service facilities in China, cooperating with engineering companies, steel mills, and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relations with dozens of well-known steel mills around the world. The inventory includes 50,000 tons of conventional stainless steel and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of stable quality, and the varieties, specifications, and delivery weights strictly meet the standards.
316 Stainless Steel Angle
- 316 Stainless Steel Angle is an austenitic chromium nickel angle shape containing molybdenum which provides superior corrosion resistance and increased strength at elevated temperatures when compared to 304 Stainless.
- Because of the 4% molybdenum concentration, the 316 material is resistant to chloride ion stress corrosion. Stainless Steel 304 Unequal Angle Sizes vary depending on the application needs. Angles are used to hold components together using a grip. There are also angles with bolt holes for screws and bolts. The 316 Stainless Steel Unequal Angle is suitable for more corrosive applications than the 304 angles. The Stainless Steel Unequal Angle is just as frequent as the Equal Angle. They are utilized in a variety of applications, including brackets, trim, and reinforcements. Please contact us for more information about the angles and their costs.
特性
- Cold Working: Good
- Corrosion Resistance: Excellent
- Heat Resistance: Good
- Heat Treatment: Poor
- Hot Working: Fair
- Machinability: Good
- Weldability: Very Good
なぜあなたはDaxunからステンレス鋼の角度を購入する必要がありますか?
Daxun’s objective is to supply you with the highest quality and most durable stainless steel angles and steel. We provide hundreds of stainless steel angles in various leg lengths, thicknesses, and material grades. Our 316/316L and 304/304L stainless steel angles are made at our well-equipped production facility using high-quality raw materials and cutting-edge technology, overseen by qualified workers. Some other significant benefits of partnering with us include:
- 当社からスチール製品をご購入いただくと、メーカーから直接製品を入手することができます。.
- 当社の従業員は、お客様がすぐにプロジェクトを開始できるように、最低価格と最短の出荷時間を提供することに専念しています!
- 私たちは、品質チェック、梱包、出荷に熟練した有能な従業員を擁している。.
- 私たちは複数の品質チェックレベルに従い、最高水準の製品であることを保証しています。.
- 万が一問題が発生した場合は、24時間365日体制で有資格の専任サポートチームが対応します。.
中国からの製造者はサイズにステンレス鋼の角度を作る
- Daxunは、中国のステンレス鋼製品の大手サプライヤーです。高品質の製品とカスタマイズされたサービスで、我々はすべてのステンレス鋼角度のニーズを満たすことができます。オンラインまたは電話で注文し、最速15日でお届けします。.
304および316グレードステンレス鋼アングル
- This versatile right angle steel has a wide range of applications and is available in grades 304 /30L and 316 /316L. Grade 304 is the most versatile and commonly used grade of stainless steel angle steel and is suitable for most general applications. It is easy to weld and has good formability and corrosion resistance. Sometimes called 18/8 stainless steel because its composition includes 18% chromium and 8% nickel, grade 304 is well suited to most applications.
- Grade 316 is more suitable for harsh environments, such as exposure to salt water and areas with high industrialization. Due to the higher nickel content and the addition of molybdenum to the metal, it has higher corrosion resistance than grade 304, especially to chlorides and chlorinated solutions. It also has good weldability, but is more difficult to process than grade 304.
ステンレス・スチール・アングルの製造には、基本的に2つの工程がある:
- laser melting and hot rolling. Hot rolled stainless steel angles are less expensive. They typically have rounded or tapered edges. On the other hand, laser melted stainless steel angles have consistent sharp and square corners. They also include sandblasting and a smoother finish. The surface of laser melted stainless steel angles is smoother than that of hot rolled stainless steel angles.
サイズとサイズを選ぶ
- We offer a wide variety of stainless steel angles, so whatever your needs, we have you covered. Grade 304 stainless steel angles come in a variety of sizes with thicknesses from 3mm-16mm and lengths of 1m, 3m, or 6m.
- 当社のグレード316アングルは、厚さ3mm~16mm、長さ1m、3m、6mです。アングルは様々なサイズがあります。.
ご希望のステンレス鋼アングルサプライヤーにご相談ください。
- It couldn’t be easier to buy the stainless steel angles you need, as well as all of our other products, through our website. Alternatively, you can call our sales team in China at +8613382898899 to place your order and they will be happy to process your order. If you have any questions, you can even send an email to [email protected] and our team will get back to you as soon as possible.
お問い合わせ “ページのフォームにご記入いただくか、”+86 13382898899 “までお電話ください。WhatsAppはオンライン、Eメール([email protected])は6時間以内に確認いたします。すべてのお問い合わせやメッセージは、迅速に対応させていただきます。また、毎週お客様と市場情報を共有しています。
サンプルは無料で提供できるが、運賃は顧客負担となり、協力後に返金される。.
カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.
Our MOQ is 1 ton for 316L Stainless Steel Angle.
We have a complete organization from raw material purchasing to processing and shipment arranging. In the whole chain, the documentary people ad QC will look for and check it by precise requirements.The third party inspection is welcomed.
トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.