  • Titanium bar grade: Grade 23-Ti6Al 4V ELI- USN R56401
  • Titanium bar types: rolled bars, drawn bars, forged titanium bars
  • Titanium bar density The density of grade 23 titanium is 4.43 g/cm3
  • Main standards: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
  • High strength, high temperature resistance, corrosion resistance, light
  • weight, excellent comprehensive performance.

————Daxunは中国でチタン棒を生産し、多様なニーズに応えている。 ——顧客の厳しいニーズ!

純チタン棒製造サービスのグローバルリーダー

Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 23 titanium alloy rods.

Grade 23 titanium bar, also known as Ti-6Al-4V ELI, is a high-performance alloy known for its excellent strength-to-weight ratio, corrosion resistance, and biocompatibility. It is widely used in aerospace, medical, and high-tech industries due to its ability to withstand extreme conditions while remaining lightweight. Compared to other titanium grades, Grade 23 offers enhanced ductility and fracture toughness, making it ideal for critical applications such as aircraft components, surgical implants, and advanced engineering parts.

大順 is your trusted titanium alloy rod production company. Daxun produces all grades of titanium alloys, including commercially pure titanium series CP, titanium alloy series, titanium nickel alloy, etc. They have reliable performance and provide high performance for your critical applications. In various industries and applications, you can rely on Daxun titanium alloy rods for high strength, high temperature and corrosive environments. For decades, Daxun Metals has been committed to producing highly engineered titanium alloy solutions to meet the most severe challenges.

続きを読む

データ

仕様 詳細
素材 Titanium rod and bar Grade 23 (UNS R56400)
スタンダード ASMB348、ASMSB348、AMS4921、AMS4902
寸法 EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN
直径範囲 0.125″ – 14″ (3.175mm – 355.6mm), custom
長さの範囲 Up to 240″ (6096mm), custom
表面処理 Cold (bright) drawn, centerless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centerless Ground & Black
表面仕上げ 冷間引抜、センタレス研磨、ポリッシュ、ラフ切削、黒色、NO.4仕上げ、BA仕上げ、マット仕上げ等。.
コンディション 焼入れ、焼戻し、アニール
寛容 Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm)
様式 チタン角棒、チタンインゴット、チタン丸棒、チタン角棒、チタン三角棒、鍛造チタン棒、チタン六角棒など。.
物理的性質 密度: 0.163 lb/in³ (4.51 g/cm³), 融点: 3,020°F (1,660°C), 伸び: 20-30%, 弾性率: 16.5 x 10⁶ psi (114 GPa)
化学組成 チタン(最小):99.2%、酸素(最大):0.25%、炭素(最大):0.08%、鉄(最大):0.30%、窒素(最大):0.03%、水素(最大):0.015%

 

エレメント Minimum (%) Maximum (%)
チタン (Ti) 99.2 –
Aluminum (Al) 5.5 6.75
Vanadium (V) 3.5 4.5
Oxygen (O) – 0.25
Carbon © – 0.08
鉄(Fe) – 0.30
窒素(N) – 0.03
Hydrogen (H) – 0.015
プロパティ 価値
引張強度 130,000–170,000 psi (900–1,170 MPa)
降伏点(0.2%変形) 115,000–150,000 psi (800–1,035 MPa)
伸び 20–30%
硬度(ブリネル) 300–360 HB
弾性係数 16.5 × 10⁶ psi (114 GPa)
プロパティ 価値
密度 0.163 lb/in³ (4.51 g/cm³)
融点 3,020°F (1,660°C)
熱伝導率 13.4 W/m·K (at 25°C)
熱膨張係数 8.6 µm/m·°C (20–100°C)
電気抵抗率 4.1 × 10⁻⁷ Ω·m

Daxunを選んで、あなたのプロジェクトを成功に導きましょう。.

今すぐDaxunに連絡する

DAXUN® Grade 23 Titanium Rod Features

DAXUN® Ti Grade 5 is a titanium alloy bar (6al-4v) featuring:

  • Good hot formability and weldability;
  • Tensile strength can reach 1000MPa;
  • Dimensional work at high temperature
  • Insensitive to seawater or seawater;
  • Not affected by various corrosive media;
  • High strength and good toughness;
  • Resist crack initiation and crack propagation.
今すぐDaxunに連絡する

Daxun Factory Advantages

Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

今すぐDaxunに連絡する

Grade 23 Titanium Rod Production Method

Daxun produces high-quality titanium bars with high performance, and can also manufacture according to customer’s agreement:

  • Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
今すぐDaxunに連絡する

Grade 23 Rods Applications and Standards

Grade 23 Titanium Rods are widely used in the following industries under extreme corrosive conditions:

  • Aerospace, shipbuilding, oil and gas industry, marine engineering, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, military industry, pharmaceutical and food processing equipment, etc.
  • Specifications: AMS 4928,AMS 4967,AMS 4965 ,AMS 6931 ,ASTM B 348
  • Standards: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
今すぐDaxunに連絡する

品質、納期、検査

Daxun performs several quality assurance tests, these tests include mechanical tests like area tensile, chemical analysis, material positive identification – PMI test, micro and macro testing, intergranular corrosion (IGC) test, ultrasonic flaw detection test, pitting and resistance test, hardness test, material positive identification, expansion test etc. All these tests ensure that the Grade 2 Titanium Rod and Grade 2 Titanium Round Bar material is suitable for the required application. During the production process, we measure the diameter, thickness and surface of the product.

  • 当社の納期は、契約に厳密に従います。.
  • 顧客の第三者機関が工場に検査に行くのをサポートする。
  • 顧客テストのための無料サンプルをサポート
  • 現場検査またはビデオ工場検査をサポート
今すぐDaxunに連絡する

パッケージング

国際貨物は様々な経路を経て最終目的地に到着するため、梱包は重要な役割を担っています。商品によって、様々な方法で梱包しています。当社では、以下のような様々な方法で商品を梱包しています:
- 箱と木箱
- シュリンクラップ
- 木製パレット
- 木製ボックス

今すぐDaxunに連絡する

テクニカルサポート

さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.

Daxun Grade 23 Titanium Rods help your brand improve quickly

NOMINAL SIZE h5 h6 h7 h8 h9 H10 H11 h12
DIAMETER mm
~ to 3 +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
over 3 to 6 +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
over 6 to 10 +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
over 10 to 18 +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
over 18 to 30 +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
over 30 to 50 +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
over 50 to 80 +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
over 80 to 120 +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
over 120 to 180 +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
over 180 to 250 +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

チタン棒

最近の注目プロジェクトと製品

Ti6AL-4V ELI Titanium Alloy Bar, Titanium Bar Grade 23/UNS R56401

Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 23 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.


仕様

AMS 4928 – Bars, Forgings, and Forging Stock (Annealed)
AMS 4965 – Bars, Forgings (Solution treated and aged)
AMS 4967 – Bars, Forgings (Annealed, Heat Treatable)


HEAT TREATMENT

When high hardness, tensile strength, and fatigue strength are required, annealing can be performed at 1,700-1,900°F (927 – 1,038°C).
DAXUN 6-4™ Grade 23 alloy can be heat treated in a variety of ways:

  1. Anneal: 1,275 – 1,400°F (691 – 760°C), ½ to 2 hours, air or furnace cool
  2. Stress Relief Anneal: 1,000 – 1,200°F (538 – 649°C), 1 to 8 hours, air or furnace cool
  3. Solution Heat Treat: 1,675 – 1,750°F (913 – 954°C), 1 hour, water quench
  4. Aging: 975 – 1,025°F (524 – 552°C), 4 to 8 hours – air cool

In the solution treated and aged condition, rapid quenching of small sections yields optimum properties. Larger section sizes and/or delayed quenching may result in less than optimum properties.


HARDNESS

Typical hardness in the annealed condition is Rockwell C 30-34, and about Rockwell C 35-39 in the solution and aged condition.


Forgeability / Formability

Ti-6Al-4V ELI (Grade 23) alloy bar is forged at 1,750°F (954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 35% reduction is recommended for optimum properties.

Grade 23 alloy bar is difficult to form at room temperature, even in the annealed condition. Therefore, severe forming operations such as bending or stretching can be performed on annealed material at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000 – 1,200°F (538 – 649°C).


加工性

Ti-6Al-4V ELI (Grade 23) alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids.


溶接性

Grade 23 titanium rod is readily weldable in the annealed condition or in the solution and partially aged condition, with aging being accomplished during post weld heat treatment. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. Spot, seam, and flash welding may be performed without the aid of a protective atmosphere.


Special Considerations

Grade 23 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics.


サイズ範囲

Grade 23 Titanium Bar Dimensions
Ø 0.7 – 30 mm (drawn, ground)
Ø 16 – 400 mm (hot rolled, peeled)
Tolerances: h11–h5 (ISO 286-2)
Tighter or different tolerances available on request
Lengths up to 9,000 mm long, depending on diameter
For larger diameters, other bar lengths and tolerances can be agreed upon request


Availability Grade 23 Titanium Rods

Processing options include:

  • Drawing, straightening
  • Drawing, straightening, polishing
  • Drawing, grinding, polishing
  • Drawing, straightening, grinding, polishing
  • Drawing, annealing, straightening
  • Drawing, annealing, polishing
  • Drawing, annealing, grinding, polishing
  • Drawing, annealing, straightening, grinding, polishing

We produce bars according to your requirements.
Excellent surface and straightness, perfect roundness and tightest diameter tolerances (according to ISO 286-2 up to h5). Available in straightened, ground, polished conditions.


製材

  • Band saws (up to Ø510 mm)
  • Bench band saws (up to 6,000 x 3,000 x 400 mm)
  • High-performance sawing machines for precise sawing

Titanium Bar End Machining

  • Single or double sided
  • Chamfer 90° (45°)
  • Point 60° (30°)
  • Flat end
  • Centered

Delivery Form

  • ASTM American Society for Testing and Materials Standards
  • AMS American Aerospace Materials Standards
  • NACE American Association of Corrosion Engineers International Standards
  • ASME American Society of Mechanical Engineers Standards
  • GB Chinese National Standards
  • GJB Chinese National Military Standards
  • ISO International Standards
  • DIN German Standards
  • EN European Standards
  • API American Petroleum Institute Standards

Detection Method

Non-destructive testing > 100% testing
Testing methods:

  • Eddy current testing / eddy current crack testing
  • Defect-free surface (level 4)
  • Flat bottom hole diameter 0.7 mm and 0.4 mm
  • Blind area can be cut off according to fixed length > Test to the end of the bar
  • Full diameter ultrasonic testing

Our Titanium Bar Material Services

As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.

We will be happy to provide you with a consultation and explain everything you need to know about obtaining Grade 23 titanium bar material, including which standards require greater attention for the components to be manufactured.

If you have a long-term supply commitment, you can establish a framework agreement with 大順. We guarantee prices and quantities for a specified period.

Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 23 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.


ご注文について

Purchase orders should include quantity, grade, type or category, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact 大順 now, we will reply to your email as soon as possible.

どのグレードのチタンが最適ですか?

必要なチタン合金のグレードは、取り組んでいるプロジェクトによって異なります。各グレードには異なる利点があるためです。

すべてのグレードのチタン合金は極めて強靭で耐食性に優れており、過酷な環境下でも良好な性能を維持し続けます。

チタン合金の高グレード品(5~12)は、特定の利点を目的として設計された合金である。例えば、グレード12チタン合金は優れた耐熱性を有し、シェルアンドチューブ式熱交換器、油圧配管、化学工業用機器に最適な選択肢となる。

グレード1~4は純チタン合金であり、配管システムやチューブ用に溶接可能で延性のある材料が必要な場合に最適な選択肢です。低グレード品は船舶産業や工業分野で使用されています。

プロジェクトを開始するにあたり、どのグレードのチタン合金が最適かお悩みでしたら、ぜひ当社までご連絡ください。喜んでご支援いたします。

高品位チタンと低品位チタンはどのように異なるのですか?

大迅では、グレード1からグレード12まで幅広いチタン合金グレードを提供しています。

グレード1~4は純チタンであり、それより上のグレードは合金である。

合金グレードは、高い強度重量比で人気がある。

最も一般的に使用されるチタン合金グレードはグレード5です。チタン含有量は依然として高いものの、このグレードは600°F(約315℃)までの高温に耐え、過酷な条件にも耐えられるため、最も信頼性の高いグレードの一つです。

航空宇宙産業や海洋産業などの業界では、耐摩耗性と耐食性に優れていることから、より高品位のグレードが好まれている。

逆に、低品位の鋼材は強度が低いため、主に溶接用として使用される。

各種チタン合金のグレードの違いについて詳しく知りたい方は、本日+86 13382898899までお電話ください。専門家が直接ご説明いたします。

チタンのグレードはコストに影響しますか?

チタンのグレードはコストをわずかに増加させますが、総コストは主に必要なチタンの形状と形態によって決定されます。

At DAXUN, we offer a wide range of titanium products, including plates, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

残念ながら、プロジェクトの詳細やチタニウムの使用目的がわからないと、オンラインで価格をお見積もりするのは難しいです。

幸いなことに、当社の専門家チームが常に皆様のチタンに関するご要望にお応えし、アドバイスを提供いたします。daxunalloy@gmail.com までメールをお送りいただければ、アドバイスと正確な見積もりをご案内いたします。

ご要望のチタニウムのグレード、形状、数量について、可能な限り詳細な情報をご提供ください。これにより、お客様のニーズをより正確に把握できます。

チタンのグレードについて、どこで詳しく学べますか?

DAXUNのチームは経験豊富で知識が深く、親しみやすいです。業界での長年の経験から、チタンの用途、利点、グレードに至るまで、あらゆることを熟知しています。

チタニウムの最新情報、用途、および産業分野における応用事例については、当社のブログをぜひご覧ください。専門家による分かりやすいガイドを掲載しており、疑問が生じた際にはいつでもご参照いただけます。

もし問題が解決しない場合は、お気軽にお問い合わせください。喜んでお手伝いいたします。

daxunalloy@gmail.com 宛にメールをお送りいただければ、迅速なご返答を差し上げます。お問い合わせの際は、可能な限り詳細な情報をご記載ください。そうすることで、適切な解決策をご提案できます。

早急に見積もりを取る、あるいはマーケット情報を理解するには?

お問い合わせ “ページのフォームにご記入いただくか、”+86 13382898899 “までお電話ください。WhatsAppはオンライン、Eメール(Daxunalloy@gmail.com)は6時間以内に確認いたします。すべてのお問い合わせやメッセージに迅速に対応させていただきます。また、毎週お客様と市場情報を共有しています。

サンプルをいただけますか?

We can provide titanium rod samples for you to check the quality. Sample is free and you just pay the freight.

すでに輸出した国は?

カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.

MOQはいくらですか?

Our MOQ is 300 Kg for titanium rod.