Daxun is an experienced supplier of heat-resistant 310S stainless steel coils

As a leading stainless steel coil supplier and exporter in China, Daxun supplies stainless steel coils to all over the world.
  • Coil grade: S31008-310S
  • Coil features: corrosion resistant, acid and alkali resistant,High temperature resistance
  • Coil thickness: 0.4 mm to 12.00 mm
  • Coil width: 1000 mm, 1250 mm, 1500 mm and 2000 mm.
  • Coil surface: 2B, BA, HL, No.1, Matte, Polished, 8k Mirror
    If necessary, stainless steel coils will come with a protective film to protect the metal surface from unnecessary damage.

Global leader in stainless steel Coil fabrication services

310S Stainless Steel Coil is an austenitic chromium-nickel stainless steel with excellent resistance to oxidation, corrosion, and high temperatures. Type 310S is a high-temperature chromium-nickel austenitic stainless steel with good creep strength and oxidation resistance up to 2000˚F in dry air. Type 310S produces a robust oxide scale at high temperatures and resists spalling, outperforming Type 309 in thermal cycling applications. In mildly carburizing settings, Type 310 resists sulfidation and carburization well. Type 310S is a low-carbon variation of Type 310 that is easier to shape and weld. Type 310S is nonmagnetic when annealed and cold wrought, and it resists corrosion better than Type 304/304L.

310s Stainless Steel Coil, SS 310s Coil, 310s Steel Coil, Hot Rolled 310s Steel Coil, Cold Rolled 310s Steel Coil, 310s HR Coil, 310s CR Coil, ASTM A240 Type 310s Coil, UNS S31000 Coil, UNS S31008 Coil, BIS Approved

Dah Hsun is an ISO 9001:2008 certified firm that is a major supplier and exporter of ASTM A240 Stainless Steel Coils. Stainless steel coils can be cut to your requirements and include a full set of mill test results. Custom lengths and widths are available up to 2000mm. Exporting is our specialty! We can obtain several hard-to-find grades and/or non-standard sizes to satisfy our customers’ specific needs. We have vast experience processing steel coil goods and can divide all stainless steel coils to the desired sizes. Introducing our extensive line of Dah Hsun Stainless Steel goods – the pinnacle of dependability, durability, and performance. We are glad to provide a wide selection of grades and varieties to fulfill the diverse needs of industrial and architectural applications.

Our stainless steel coil goods, which range from the Austenitic series to the Ferritic series and other special categories, are well-known for their high performance and extensive requirements. The austenitic series includes 304/304L/304J1, 321 and 316/316L/317L/316Ti/310/309, which can fulfill varied thickness requirements and give a variety of surface treatments, including 2B, BA, NO.4, 8K, SB, HL, NO.1, and so on.

Our ferrite line, which includes 430, ultra-pure ferrite 443, and 436L/439/444/441, caters to customers looking for unique qualities and applications. These materials can accommodate thicknesses ranging from 0.4mm to 3.0mm and offer a variety of surface treatment options such as 2B, BA, NO.4, 8K, SB, HL, and so on.

By selecting our stainless steel coils, you are investing in a material that ensures long service life, great reliability, and exceptional performance. Don’t compromise on quality; choose our stainless steel solutions and see the impact they can make in your project. Contact Daxun today for additional information or to place an order for the stainless steel coil specs and quantities that you require.

続きを読む

データ

310S Stainless Steel Coil Specification ASM A240 / ASME SA240
310S Stainless Steel Coil Manufacturing Process Hot Rolled (HR) / Cold Rolled (CR)
310S Stainless Steel Coil Grades 201 / 304 / 304L/ 310S / 309S / 310S / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L etc.
UNS No. –  UNS S310S, UNS S31008, UNS S31600, UNS S31603, UNS S31603, UNS S31600, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904
EN No. – 1.4301, 1.4307, 1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539
310S Stainless Steel Coil Thickness 0.6 MM TO 80 MM THICKNESS
310S Stainless Steel Coil Width 1250 MM / 1500 MM / 2000 MM / 04 Feet / 05 Feet and Custom Cut Width as Per Requirement
310S Stainless Steel Coil Length 2400 MM / 2420 MM / 6000 MM / 08 Feet / 10 Feet / Coil Cut and Custom Cut Length as Per Requirement
310S Stainless Steel Coil Surface Finish 2B, 2D, BA, MATT, MATT PVC, No.4, No.5, SB, HR, No.8, Mirror, Hairline, Brush, Textured, Oil base wet Polished, Both sides Polished available.
310S Stainless Steel Coil Coating PVC coating Normal / Laser, Film: 100 micrometer, Color: black/white.
310S Stainless Steel Coil Other Testing NACE MR0175, Ultrasoung TEST, IGC TEST, Intergranular Corrrosion Test as per ASTM A262 Practice E, Charpy Impact Test, Macro, Grain Size, Hardness, etc.
310S Stainless Steel CoilValue Added Services Gas Cutting / CNC Plasma Cutting / Profiling / Rolling / Bending / coil Metal Fabrication / Drill / Punch / Machining / Sand Blasting / Shot Blasting / Heat Treatment
310S Stainless Steel Coil Packaging Loose / Carrate / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps
310S Stainless Steel Coil Shipment & Transportation By Road – Truck / Train Partial Load, Full Load, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes
310S Stainless Steel Coil Material Test Certificate Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of Indian Standards BIS Approved ETC
メーカー POSCO, Aperam, Jindal Stainless, DKC Korea, Thyssenkrup, Baosteel, TISCO,Arcelor Mittal, VDM,Nippon Metal, Outokumpu,Qingshan,Delong.
Shipping Port Shanghai/Ningbo port/Tianjin/Qindao
エレメント Type 310 Type 310S
カーボン 最大0.25. 最大0.08.
Manganese 2.00 max. 2.00 max.
Sulfur 最大0.030. 最大0.030.
Phosphorus 0.045 max. 0.045 max.
Silicon 1.50 max. 1.50 max.
Chromium 24.0 – 26.0 24.0 – 26.0
Nickel 19.0 – 22.0 19.0 – 22.0
タイプ 降伏強さ 0.2% オフセット(KSI) 引張強さ(KSI) % Elongation (2″ Gauge length)
310 30分. 75分. 40分.
310S 30分. 75分. 40分.
密度 (lb./ in^2) @ RT 0.29
引張弾性係数 (psi x 10^6) 29
比熱(BTU/o F/lb.) 32~212度 0.12
熱伝導率(BTU/hr/ft^2/ft) 212oF 8
932oF 10.8
平均熱膨張係数 (in. x 10^-6 per o F) 68 to 212oF 8.8
68 to 932oF 9.5
68 to 1832oF 10.5
電気抵抗率(マイクロオーム - cm) 華氏70度 30.7
耐酸化性-連続使用(oF) 2000
スタンダード WERKSTOFF NR. 国連  日本工業規格 BS GOST アフノール  EN
SS 310  1.4841 S31000 SUS 310  310S24 20Ch25N20S2 – X15CrNi25-20
SS 310S 1.4845 S31008 SUS 310S 310S16 20Ch23N18 – X8CrNi25-21
•  310s Stainless Steel HR coil •  Stainless Steel Cladding 310s coil
• 310s Stainless Steel Chequered coil •  Black SS 310s coil 4mm Thick
• 310s Stainless Steel Golden Laser Pattern coil •  Bright-pickled Stainless Steel 310s coil
• Super thin-Mirror surface BA ss 310s coil •  Cold rolled, heat treated 310s coil
• Super Austenitic SS 310s coil •  3mm Cold Rolled AISI SS 310s coil
• ASTM A240 310s coil •  Mill Supply SS 310s coil
• JMSS cold rolled ss 310s coil •  Grade Prime SS 310s coil
• Cold Rolled No.1 Finish SS 310s coil •  Carpenter Custom 450 Stainless Steel 310s coil
• SEW 400 Stainless Steel 310s coil •  Cut to Size Stainless Steel 310s coil
• Hot Rolled Stainless Steel 310s coil •  Non Magnetic Polishing Stainless Steel 310s coil
• Sales Promotion SS 310s coil •  ASME SA240 310s coil
•  Cr Stainless Steel 310s coil •  Grade 310S Stainless Steel Finish coil
•  SS 310s Mill Test Certificate coil •  310s Stainless Steel Blank coil
•  ASTM A240 310s coil •  310s Stainless Steel Perforated coil
•  Cold rolled, bright annealed 310s coil •  Embossed ss 310s coil
•  Ground Stainless Steel 310s coil •  Cheap cold rolled ss 310s coil with best price
•  Hot Selling AISI SS 310s coil •  Brush finish ss 310s coil price list
•  SS 310s Rose Golden coil • SS URANUS B6 310s coil
• Surface coated Stainless Steel 310s coil •  2B SUS SS 310s coil
•  Satin finish Stainless Steel 310s coil •  Food Grade Stainless Steel 310s coil
•  AISI stainless steel 310s armor coil •  No. 4 PVC Coated SS 310s coil
• Satin finish Stainless Steel 310s coil •  SS 310s coil Blasted Tin-Gold Rose
•  Mirror Finish SS 310s coil •  2mm ASTM SS 310s coil
•  SS 310s coil Gold Brush Finish •  Stainless Steel Corrugated 310s coil
• 310s Stainless Steel CR coil •  ASTM B625 310s coil
•  310s Stainless Steel 2B coil •  Brushed or dull polished Stainless Steel 310s coil
•  310s Stainless Steel B. Q. Profile coil •  Cold rolled, heat treated, pickled 310s coil
•  Best selling 4’x8′ mirror finished ss 310s coil •  10K Mirror Finish Surface SS 310s coil
•  Decorative hairline inox cold rolled ss 310s coil •  Gold Etched SS 310s coil
•  Hair Line Finish SS 310s coil •  18 Gauge SS 310s coil
•  Laser cutting ss 310s coil •  Patterned Stainless Steel 310s coil
•  Tisco Supplier 3mm Thickness Stainless Steel 310s coil •  #4 Finish Stainless Steel 310s coil
•  Decorative Stainless Steel 310s coil •  Patterned Stainless Steel 310s coil
•  Scotch Brite SS 310s coil •  Passenger Elevator Cabin SS 310s coil
•  Baosteel Stainless Steel 310s coil •  Dimensional Stainless Steel Grade 310S coil

Daxunを選択し、顧客を満足させる。.

今すぐDaxunに連絡する

迅速な対応

We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.Daxun’s stainless steel materials are of reliable quality, and their varieties, specifications and delivery weights strictly comply with the standards.

今すぐDaxunに連絡する

大順のメリット

Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel achieves full traceability of each steel coil from the ERP system, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strict monitoring during sales, and provides worry-free service guarantees after sales.

今すぐDaxunに連絡する

Stainless steel coil packaging

国際貨物は様々な経路を経て最終目的地に到着するため、梱包は重要な役割を担っています。商品によって、様々な方法で梱包しています。当社では、以下のような様々な方法で商品を梱包しています:
- 箱と木箱
- シュリンクラップ
- 木製パレット
- 木製ボックス

今すぐDaxunに連絡する

品質、納期、検査

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    当社の納期は、契約に厳密に従います。.
  • 顧客の第三者機関が工場に検査に行くのをサポートする。
  • テスト用の無料サンプルを顧客に提供
  • 現場検査またはビデオ工場検査をサポート
今すぐDaxunに連絡する

ご注文について

Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.

今すぐDaxunに連絡する

テクニカルサポート

さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.

SS 310S Stainless Steel Coil Features

高強度
耐食性
耐熱性
低温耐性
環境保護
溶接性能

大順合金 あなたのブランドを急速に向上させる

グレード タイプ 厚さ 表面
オーステナイト系 304/304H/304L/304J1 0.25-150mm 2B/BA/4番/8K/SB/HL/1番
321 0.4-80mm 2B/BA/4番/8K/SB/HL/1番
316/316L/317L/316Ti 0.3-80mm 2B/BA/4番/8K/SB/HL/1番
フェライト 430 0.4-3.0mm 2b/ba/no.4/8k/sb/hl
超高純度フェライト 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
スーパーオーステナイト鋼 N08904 0.6-50mm スイス/日本/中国
S31254 0.5-50mm スイス/日本/中国
N08926 0.5-50mm スイス/日本/中国
N08367 0.5-50mm スイス/日本/中国
ニッケル基合金 N08031 1.0-50mm アメリカ / 日本 / ドイツ
N08810/N08800 0.8-50mm アメリカ / 日本 / 中国
N08028 1.0-20mm アメリカ / ドイツ / 日本
N08020 1.0-20mm アメリカ / ドイツ / 日本
N08825 0.8-40mm アメリカ / ドイツ / スイス / 日本 / 中国
N10276 0.5-50mm アメリカ / ドイツ / 日本
N06022 1.0-50mm アメリカ / ドイツ / 日本
N06625 0.8-20mm アメリカ / ドイツ / 中国
N04400 1.0-20mm アメリカ / ドイツ / 日本
N06600 1.0-50mm アメリカ / ドイツ / 日本 / 中国
N02201 0.5-20mm アメリカ / 日本
チタン TA1/Gr1 0.5-50mm 日本 / 中国
TA2/Gr2 0.5-50mm 日本 / 中国
溶接材料 ERNiCrMo-13 1.2、2.4mm ドイツ
ERNiCrMo-3 2.4mm ドイツ
ERNiCrMo-4 2.4mm 米国
Subsidiary Main Equipments Qty Annual Capacity
Daxun Stainless steel co.(JiangSu) Slitting Machine 1 Decorative Sheet:60,000 tons
Cutting Machine 1
No.4 And Hairline Sheet To Sheet Polishing Machine 1
No.4/Hairline Coil To Coil Polishing Machines 1
8K/Super Mirror Sheet To Sheet Polishing Machines 2
8K/Super Mirror Coil To Coil Polishing Machines 3
PVD Color Coating Machines 4
Liquid Chemical Coating Machines 2
Anti Finger Printing Machines 2
Auto Pick and Place machines 16
coil Washing Machine 1
Daxun Stainless steel co.(Shanghai) Cold Rolling Machine 3 2B Coils:100,000 tons
Annealing & Pickling Line 2 Decorative Sheet;30,000 tons
Slitting Machine 1
Cut to Length Machine 1
No.4/HL Polishing Machine(Sheet to Sheet) 3
8K Polishing Machine(Sheet to Sheet) 13
PVD Titanium Coating Machine 4
Liquid Chemical Coating Machines 1
Daxun Stainless steel co.(Shandong) Cold Rolling Machine 3 2B & BA Coil:220,000 tons
Annealing & Pickling Line(2B & BA) 2 Decorative Sheet:60,000 tons
Tension Levering & Skin Pass 1
Slitting Machine 1
Cut to Length Machine 1
No.4/HL Polishing Machine(Sheet to Sheet) 1
8K Polishing Machine(Sheet to Sheet) 11
Automatic Copper Coating Machine 1
Digital Printing Machine 1
PVD Titanium Coating Machine 3
Liquid Chemical Coating Machines 1
Anti-finger Machine 1
Daxun Stainless steel co.(Sichuan) Slitting Machine 1 2B & BA Coil:180,000 tons
Cutting Machine 1 Decorative Sheet:50,000 tons
No.4 And Hairline Sheet To Sheet Polishing Machine 1
No.4/Hairline Coil To Coil Polishing Machines 1
8K/Super Mirror Sheet To Sheet Polishing Machines 1
8K/Super Mirror Coil To Coil Polishing Machines 1
PVD Color Coating Machines 1
Liquid Chemical Coating Machines 1
Anti Finger Printing Machines 1

参照およびダウンロード可能な情報

Daxun is a trustworthy stainless steel coil manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel coils have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

最近の注目プロジェクトと製品

310Sステンレス鋼コイル
stainless steel seamless coil
ステンレス・コイル
SS 310S stainless steel coil
Stainless Steel Polished coil
SS 310S steel coil
ステンレス・コイル
BA stainless steel coil
SS310S stainless coil
ステンレス・コイル
Stainless steel precision coil
Stainless steel coil 310S
詳細紹介

Leading stainless steel coil Suppliers in China

Daxun has been engaged in international business for more than ten years. In 2023, its export revenue exceeded US$100 million, and its export volume ranked among the top Chinese stainless steel manufacturers. Daxun continues to improve its service skills. In order to serve the global market, we have established three export service facilities in China and cooperated with engineering enterprises, steel mills and international trading companies. Daxun provides stainless steel chain services and has established long-term cooperative relationships with dozens of well-known steel mills around the world. Its inventory includes 50,000 tons of conventional stainless steel coils and 20,000 tons of duplex steel, nickel-based alloys, heat-resistant steel and other metals. Daxun’s stainless steel materials are of consistent quality. Types, specifications and delivery weights strictly comply with standards.


310/310S stainless steel features:

  • 310/310S stainless steel is noted for its strong high-temperature qualities, as it maintains an austenitic structure at normal temperature and cannot be toughened through heat treatment. Cold working can increase its tensile and yield strength, but it needs be paired with subsequent annealing to maintain its qualities. The 310 version is intended to work well in high-temperature situations, whilst the 310S is tailored for low-temperature applications while still offering strong heat resistance. It is crucial to note that cold working may diminish the alloy’s creep resistance at high temperatures, which is an important factor in applications requiring high temperature endurance.

310/310S stainless steel uses.

310/310S stainless steel is well-known for its superior high temperature and oxidation resistance, and it is widely utilized in many industries. Its adaptability is proved in a variety of applications, including:

  • Components include conveyor belts, drums, burners, refractory supports, and pipe supports.
  • Application in the realm of chemical processing:
  • Applications in food processing:
  • Used to make stamping dies, fixtures, cutting tools, measurement devices, paper cutters, and ancillary equipment.
  • Employment opportunities include oil and gas, electronics, pharmaceuticals, textiles, machinery, construction, nuclear energy, aerospace, and defense, among others.

310S Stainless Steel Label

  • AISI 310S, UNS S31008, Acero 310S, Inox 310S, SUS 310S, 1.4845, and 310S grade

GENERAL PROPERTIES

  • Alloy 310 is an austenitic stainless steel that has outstanding high-temperature characteristics while also being ductile and weldable. It is commonly used for high-temperature applications because of its high chromium and nickel content, which provides robust corrosion resistance, great oxidation resistance, and exceptional strength at temperatures of up to 2100°F. Because of its high chromium and nickel concentration, it outperforms 304 or 309 stainless in most applications.

APPLICATIONS

  • Higher alloyed stainless steels often offer good strength at high temperatures, as well as exceptional resistance to creep deformation and environmental damage. As a result, Alloy 310 is widely employed in industries like heat treatment and chemical processing. Examples include:
  • Furnace Parts
  • Oil Burner Parts
  • Heat Exchangers
  • Welding Filler Wire and Electrodes
  • Annealing Covers
  • Combustion Tubes
  • Fire Box coils

RESISTANCE

Stainless Steel Alloy 310 Stainless Steel Tubes and Pipes offer excellent resistance to corrosion and heat, even in the most demanding environments.

CORROSION RESISTANCE

  • Provides excellent corrosion resistance
  • High chromium content allows for good aqueous corrosion resistance
  • Excellent resistance at normal temperatures and also has good resistance to oxidizing and carburizing atmospheres

HEAT RESISTANCE

  • Good resistance to oxidation in intermittent service in air at temperatures up to 1040°C and 1150°C in continuous service.
  • Good resistance to thermal fatigue and cyclic heating.
  • Widely used where sulphur dioxide gas is encountered at elevated temperatures.
  • Continuous use in 425-860°C range not recommended due to carbide precipitation, if subsequent aqueous corrosion resistance is needed
  • Generally used at temperatures starting from about 800 or 900°C – above the temperatures at which 304H and 321 are effective.

 FABRICATION

  • Commonly used in the heat treatment and process industries due to high temperature and corrosive environments
  • Often fabricated into complex structures
  • Roller-forms, stamps and draws readily
  • Because 310 work hardens, severe forming operations should be followed by an anneal

WELDABILITY

  • Austenitic stainless steel is generally considered to be weldable
  • Generally considered to have weldability equivalent to 304 and 304L
  • Special consideration is needed to compensate for a higher coefficient of thermal expansion to avoid warping and distortion

What are the commonly used surfaces of stainless steel coils?

The surface finish of 201 stainless steel coil might vary depending on the cold rolling processing methods used and the surface treatment used after rolling. Surface treatments for stainless steel coils include NO.1, 2B, 4, HL, 6, 8, BA, TR hard, heavy rolling bright 2H, polished bright, and other surface treatments:

  • NO.1: The surface obtained after hot rolling, heat treatment and pickling of stainless steel strip. It is used to remove the black oxide scale formed by pickling or similar processes during hot rolling and heat treatment. It ranks first in surface treatment. The No. 1 surface is silvery white and matte. It is generally used in heat-resistant and corrosion-resistant industries that do not require high surface gloss, such as the alcohol industry, chemical industry, large containers, etc.
  • 2B: Unlike the 2D surface, the 2B surface is smoothed by a light roller, and the surface is brighter. The surface roughness Ra value measured by the equipment ranges from 0.1 to 0.5μm, which is a typical value for most processing types. This stainless steel strip surface has the strongest adaptability and is suitable for industries such as chemical, papermaking, petroleum, medical, and a wide range of fields such as building curtain walls.
  • TR hard surface: TR stainless steel is also called hard steel. Its characteristic steel grades include 304 and 301, which are used for items that require high strength and hardness, such as railway vehicles, conveyor belts, springs and washers. The idea is to use the work hardening characteristics of austenitic stainless steel to improve the strength and hardness of steel coils through cold working methods such as rolling. In order to replace the gentle flatness of the 2B base surface, the hard material is gently rolled by a few percent to tens of percent, and no annealing is performed after rolling. Therefore, the TR hard surface of the hard material is the rolled surface after the cold rolling process.
  • Re-rolled bright 2H: After the rolling operation, the stainless steel strip will be bright annealed. A continuous annealing line can be used to quickly cool the strip. The stainless steel strip travels along the line at a speed of 60-80m/min. After this process, the surface finish will be 2H re-rolled bright.
  • No. 4: The No. 4 surface has a good polishing effect and is brighter than No. 3. It can also be obtained by polishing the cold-rolled stainless steel coil with a 2D or 2B surface, and then polishing the processed surface with a sanding belt with a particle size of 150-180#. The tool measures the surface roughness (Ra) between 0.2 and 1.5μm. The No. 4 surface is widely used in restaurants and cooking equipment, medical equipment, architectural decoration, containers and other applications.
  • HL: The HL surface is often called a hairline finish. The Japanese JIS standard specifies a continuous hairline abrasive surface obtained by polishing with a 150-240# abrasive belt. The restrictions under the Chinese GB3280 standard are unclear. HL surface finish is commonly used for architectural decoration, such as elevators, escalators, and exterior walls.
  • No. 6: The No. 6 surface is further polished on the basis of No. 4 with a Tampico brush or a W63 grit abrasive material specified in the GB2477 standard. The surface has good metallic luster, softness, weak reflection, and no imaging. Due to its good performance, it is very suitable for curtain walls, tassel decoration, and cooking supplies.
  • BA: BA is a surface that is brightly heat treated after cold rolling. Bright heat treatment is annealing in a protective atmosphere to ensure that the surface is not oxidized and retain the gloss of the cold-rolled surface, and then it is polished with a high-precision smooth roller to improve the surface brightness. The instrument evaluates the surface roughness to be 0.05-0.1μm, indicating that the surface is close to a mirror surface. BA surfaces can be used in a variety of applications, including food utensils, household appliances, medical equipment, automotive parts, and decorations.
  • No. 8: Mirror surface, maximum reflectivity, no abrasive particles. The stainless steel deep processing industry also refers to 8K board. BA material is often used as raw material for mirror processing. It only needs to be polished. The surface is beautiful after mirror processing and is often used in building entrances and interior decoration.

What is the standard sea packaging  stainless steel coil?

  • Standard export sea packaging:
    Waterproof Paper Winding+PVC Film+Strap Banding+Wooden Pallet or Wooden Case;
  • Customized packaging as your request (Logo or other contents accepted to be printed on the packaging);
  • Other special packaging will be designed as customer’s request;
    Eye to wall and eye to sky are both available;
  • By International Express: DHL/UPS/FEDEX/EMS and our own express line;
  • By air, sea or land;
  • Shipping Port: Shanghai, Ningbo, Qingdao, Tianjin or as your request.

Why choose Daxun’s stainless steel coils?

Reliable Stainless Steel Coils and Sheets Inventory Guarantee

  • Have you ever been in a situation where you required a significant quantity of stainless steel coils right away, only to discover that the supplier was running low on stock? This condition may impair your workflow and plans.
  • Our Advantages: With us, this situation will be a thing of the past. Our inventory is always ample, guaranteeing that even the largest orders are fulfilled quickly and in accordance with your business schedule.

Custom Stainless Steel Material Processing

  • You may have experienced a circumstance in which bespoke processing is required, but locating the correct supplier to match your exact requirements might be difficult.
  • Our Advantages: We have great processing capabilities to satisfy any of your specific needs. Whether it is size, stainless steel surface treatment, or other unique requirements, we offer expert one-stop service.

Competitive Stainless Steel Prices

  • When looking for a stainless steel coil provider, price is typically a major factor. You may have to make a compromise with your chosen supplier due to excessive costs.
  • Our Advantages: We keep pricing low by implementing excellent cost control and improved sourcing methods. This implies that by choosing us, you will not only receive high-quality products but also outstanding value for money.

Various Specifications of Stainless Steel Coils in Stock

  • Finding stainless steel coils with exact specifications might be a challenge. It is critical to select a supplier who understands and serves these specific needs.
  • Our Advantages: Our portfolio demonstrates versatility, with a wide choice of materials, thicknesses, and widths. We take pleasure in our ability to satisfy your project’s exact specifications.

Precision Stainless Steel Shearing Service.

  • Precision shearing is required for the usage of stainless steel coils, but not all vendors offer this precise service.
  • Our Advantages: Our shearing service is both professional and efficient, delivering precise cuts that fit your exact demands.

Contact your stainless steel coil suppliers

  • You can easily order stainless steel coils in any size and quantity online.
    Alternatively, our friendly sales team will be happy to take your order. Simply call +86 13382898899 or email Daxunhejin@gmail and we will get back to you as soon as possible.
早急に見積もりを取る、あるいはマーケット情報を理解するには?

お問い合わせ “ページのフォームにご記入いただくか、”+86 13382898899 “までお電話ください。WhatsAppはオンライン、Eメール(Daxunalloy@gmail.com)は6時間以内に確認いたします。すべてのお問い合わせやメッセージは、迅速に対応させていただきます。また、毎週お客様と市場情報を共有しています。

サンプルをいただけますか?

サンプルは無料で提供できるが、運賃は顧客負担となり、協力後に返金される。.

すでに輸出した国は?

カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.

MOQはいくらですか?

Our MOQ is 1 ton for stainless steel coil.

品質管理はどのように?

We have a complete organization from raw material purchasing to processing and shipment arranging. In the whole chain, the documentary people ad QC will look for and check it by precise requirements.The third party inspection is welcomed.