x
お問い合わせ
クイック見積もり

Duplex 2507 stainless steel plate, born for extreme environments

As China’s leading stainless steel plate supplier and exporter, Daxun provides 2507 stainless steel plates to the world.
  • Grade: AISI 2507-S32750
  • 特徴:高い強度と信頼性
  • 製造:冷延板、熱延板、鍛造板
  • 規格ASM、ASME、GB、DIN、JIS、ISO、EN、BS
  • 種類:冷間圧延薄板、熱間圧延厚板
  • 表面: 2B、NO.1、NO.4、HL、BA、8K、等。.
  • 長さ: 2438mm3048mm6000mm はカスタマイズすることができます
  • Origin: TISCO, Baosteel, Posco, Tsingshan, Delong, ATI,

2507/S32750 Global leader in stainless steel sheet fabrication services

At Daxun, we are pleased to provide customers with high-quality super duplex 2507 stainless steel plates, which are a 50/50 mixture of austenite and ferrite, stronger than pure austenite or iron alloys. Since its birth in the United States in the 1930s, it has developed to the third generation, and its main feature is that the yield strength can reach 400-550MPa, which is twice that of ordinary stainless steel, so the duplex plate can save materials and reduce equipment manufacturing costs. In terms of corrosion resistance, especially in media environments (such as seawater, high chloride ion content), the resistance to pitting, crevice corrosion, stress corrosion, and corrosion fatigue of duplex stainless steel is better than that of ordinary austenitic stainless steel, and is comparable to high-alloy austenitic stainless steel. Daxun Alloys provides duplex 2507 stainless steel in a variety of forms and sizes, all of which comply with industry and international standards such as ASTM, ASME, EURONORM and AFNOR.

Daxun’s inventory now includes Duplex 2507 stainless steel plate, an excellent super duplex stainless steel containing 25% chromium, 4% molybdenum and 7% nickel. This plate is designed for applications requiring excellent strength and corrosion resistance; such as applications in the chemical processing industry, petrochemical and seawater equipment industries. This grade of plate has excellent resistance to chloride stress corrosion cracking, high thermal conductivity and low thermal expansion coefficient. The high chromium, molybdenum and nickel content provides excellent resistance to pitting, crevice corrosion and general corrosion. Ask Daxun today.

続きを読む

技術データ

ASTM Specification ASM A240 / ASME SA240
スタンダード  ASM A240 / ASME SA240
Length& Sizes Duplex 2507 board 1000 mm x 2000 mm, 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1250mm x 2500mm, 1500mm x 3000mm to 6000mm, 2000mm x 4000mm to 6000mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm, 2m, 2.44m, 3m, 36″ X 120″ or 48″ X 144″, 4′ x 8′, Cut to size available
厚さ 0.1mm~100mm Thk
幅 10-2500mm
Hardness Duplex 2507 board Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.
Temper Annealed
コンディション Polished on both sides
Finish Duplex 2507 board Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Stock in form of Duplex 2507 board Plate, Sheet, Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Clad Plate, Rolling Sheet, Flat Sheet, Rolling Plate, Flat Shim, Blank (Circle), hot rolled, cold rolled, annealed, soft annealed, descaled, sheared, tread plate, Checker Plate
Value Added Service Cladding, Heat Treatment, Annealed, Pickling, Polish, Rolling, Cutting, Bending, Forging, Minor Fabrication Etc.
Dealers & Distributor of ATI, POSCO, JISCO, TISCO,
Test Report Duplex 2507 board Raw Materials Certificate
EN 10204/3.1B
100% Radiography Test Report
High special strength, high melt point
Third Party Inspection Report, etc
Excellent corrosive resistance, good thermal resistance
Customer support after-sales service
Strict Control from Raw Material to Finished
Profiling Duplex 2507 board To provide a full profiling service we use numerous profiling methods including:
Plasma Plate Cutting
Laser Plate Cutting
Oxy-propane Flame Cutting
Specialized in Duplex 2507 board material under 3/16 ” [5.00 mm] in thickness and 24″ [600 mm] and over in width
material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width
cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width
Free Quote, Inquiry answered within 24 hours
We offer a comprehensive services designed to add value to your project: plasma cutting, waterjet cutting, laser cutting, bending and mechanical processing, edge preparation, welding, sawing and shearing.
名称 2507/S32750
国連 S32750
エン・ノー. 1.4410
C(最大) 0.03
ムン 1.2
Si 0.8
Cr 24.0-26.0
ニー 6.0-8.0
モ 3.0-5.0
N 0.24-0.32
銅 0.5
その他 S 最大0.020;P 最大0.035
PREN 40-43
Interval Thermal °C 抵抗率 Thermal Specific Young Shear
Temper expansion conductivity heat modulus modulus
°C ax10M-bK-1 (μ_ cm) (W.m-1.K-1) (J.kg-1.K-1 E G
(GPa) (GPa)
20-100 13 20 80 17 450 200 75
20-100 13 100 92 18 500 190 73
20-200 13.5 200 100 19 530 180 70
20-300 14 300 105 20 560 170 67
グレード 国連 Industry Specifications
2507 Duplex Stainless Steel UNS S32750 ASTM A182 F53, A240, A276, A479, A789, A790, A815, A928, A988
UNS S32760 ASTM A182 F55, A240, A276, A314, A473, A479, A789, A790, A815, A928, A988
SAE J405

Daxunを選択し、顧客を満足させる。.

今すぐDaxunに連絡する

迅速な配達

We provide timely and fast delivery of 2507 stainless steel plate products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

今すぐDaxunに連絡する

2507 stainless steel plate advantages:

  1. 2507 stainless steel plate has high resistance to pitting corrosion, with a PREN value of up to 43, and has excellent corrosion resistance. Duplex 2507 steel plate also exhibits excellent resistance to other forms of corrosion, including stress corrosion cracking (SCC), crevice corrosion, and general corrosion. These combined corrosion resistance properties make duplex 2507 a versatile and reliable choice for a wide range of applications in harsh environments.
  2. 2507 has a yield strength that is twice that of 300 series stainless steel. This strength advantage allows the use of thinner steel sections under the same load conditions and reduces the material cost of the equipment.
  3. It has a yield strength and tensile strength that is twice that of ordinary stainless steel. This significantly improves wear resistance.
今すぐDaxunに連絡する

Stainless Steel 2507 Applications

  • 海水淡水化。.
  • Oil and gas industry equipment, including offshore platforms, pipelines, and well casings.
  • Chemical processing equipment, especially for handling corrosive chemicals.
  • Pulp and paper industry, particularly bleaching process equipment.
  • Petrochemical industry applications, including PVC strippers.
  • 海水淡水化プラント。.
  • Power industry equipment, such as flue gas desulfurization (FGD) systems.
  • Marine components, including ship propellers and shafts.
  • Pollution control equipment such as scrubbers.
  • Fittings are crucial components for connecting and controlling the flow of fluids in pipelines and systems. This includes elbows, tees, stub-ends, returns, caps, crosses, reducers, and pipe nipples, among others.
今すぐDaxunに連絡する

品質、納期、検査

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    当社の納期は、契約に厳密に従います。.
  • 顧客の第三者機関が工場に検査に行くのをサポートする。
  • テスト用の無料サンプルを顧客に提供
  • 現場検査またはビデオ工場検査をサポート
今すぐDaxunに連絡する

テクニカルサポート

さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.

今すぐDaxunに連絡する

高度な機械加工

Daxun Stainless Steel uses the ERP system to achieve full traceability of the type, specification, and origin of each stainless steel plate, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and its high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

2507 plate stainless steel Features

高強度
耐食性
耐熱性
低温耐性
環境保護
溶接性能

Daxun ブランドを急速に向上させる

2Bシートの公差
サイズ 寛容度ランク
グループ1 グループ2 グループ3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
No.1熱延板の公差
サイズ 寛容度ランク
グループ1 グループ2 グループ3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
デリバリー・ステートの選択 表面状態
冷間圧延 2B
2D
文学士
ヘアライン
第3位
第4位
6K
8K
注:
1.上記と異なる配送方法をご希望の場合は、弊社までご確認ください。.
2.お問い合わせやご注文の際、ここに記載されていないご要望がございましたら、何なりとお申し付けください。.
配信状態
デリバリー・ステートの選択 表面状態
熱間圧延 第1位
第3位
第4位
6K
8K
ピクルス
注:
1.上記と異なる配送方法をご希望の場合は、弊社までご確認ください。.
2.お問い合わせやご注文の際、ここに記載されていないご要望がございましたら、何なりとお申し付けください。.
グレード タイプ 厚さ 表面
オーステナイト系 304/304H/304L/304J1 0.25-150mm 2B/BA/4番/8K/SB/HL/1番
321 0.4-80mm 2B/BA/4番/8K/SB/HL/1番
316/316L/317L/316Ti 0.3-80mm 2B/BA/4番/8K/SB/HL/1番
フェライト 430 0.4-3.0mm 2b/ba/no.4/8k/sb/hl
超高純度フェライト 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
グレード タイプ 厚さ オリジナル
耐熱鋼 309S 0.5-40mm 中国
310S 0.5-40mm 中国
二相鋼 2101 1.5-50mm 中国
2304 3.0-50mm 中国
2205 0.5-60mm 中国
2507 1.0-60mm スイス/日本/中国
スーパーオーステナイト鋼 N08904 0.6-50mm スイス/日本/中国
S31254 0.5-50mm スイス/日本/中国
N08926 0.5-50mm スイス/日本/中国
N08367 0.5-50mm スイス/日本/中国
ニッケル基合金 N08031 1.0-50mm アメリカ / 日本 / ドイツ
N08810/N08800 0.8-50mm アメリカ / 日本 / 中国
N08028 1.0-20mm アメリカ / ドイツ / 日本
N08020 1.0-20mm アメリカ / ドイツ / 日本
N08825 0.8-40mm アメリカ / ドイツ / スイス / 日本 / 中国
N10276 0.5-50mm アメリカ / ドイツ / 日本
N06022 1.0-50mm アメリカ / ドイツ / 日本
N06625 0.8-20mm アメリカ / ドイツ / 中国
N04400 1.0-20mm アメリカ / ドイツ / 日本
N06600 1.0-50mm アメリカ / ドイツ / 日本 / 中国
N02201 0.5-20mm アメリカ / 日本
チタン TA1/Gr1 0.5-50mm 日本 / 中国
TA2/Gr2 0.5-50mm 日本 / 中国
溶接材料 ERNiCrMo-13 1.2、2.4mm ドイツ
ERNiCrMo-3 2.4mm ドイツ
ERNiCrMo-4 2.4mm 米国

The surface and shape of 2507 stainless steel plate (7)

Daxunは信頼できるステンレス鋼板メーカーです。

Daxunは専門メーカーとして、生産するすべての製品が高品質であることを保証します。そのため、すべてのステンレス鋼板はISO9001、SGS、CE、OQCなどの国際品質規格の認証を取得しています。また、ステンレス鋼板の欠陥が少ないことを保証するために、厳格な品質管理を行っています。Daxunでは、すべての製品は、耐久性、高品質、高性能であることをご安心ください。.

最近の注目プロジェクトと製品

2507 plate stainless steel
astm a240 2507 stainless steel plate
2507 flat stainless steel plate
2507 stainless steel sheet suppliers
2507 2b stainless steel sheet
2507 2b stainless steel sheet
Can Duplex 2507 Stainless Steel Be Welded?

Yes. Duplex 2507 stainless steel has good weldability and can be joined to itself and other materials using a variety of welding methods, including SMAW (shielded metal arc welding), PAW (plasma arc welding), GTAW (gas tungsten arc welding), FCW (flux cored wire) and SAW (submerged arc welding). When welding 2507, it is best to use 2507/P100 filler metal.

Does Duplex 2507 Stainless Steel Rust?

Yes. Although duplex 2507 stainless steel is very corrosion resistant, it can still rust in extreme situations. It is, nevertheless, less likely to rust than other varieties of stainless steel. The high quantities of chromium and molybdenum in 2507 make it extremely resistant to uniform corrosion caused by organic acids like formic and acetic acid. The exceptional corrosion resistance of 2507 steel makes it suited for use in corrosive conditions such as seawater, acids, and chemicals, where it retains its integrity and does not rust or corrode quickly.

Is Duplex 2507 Stainless Steel Magnetic?

Yes, the presence of ferritic grains within its composition renders 2507 duplex stainless steel a magnetic material.

Is Duplex 2507 Stainless Steel Expensive?

Yes, duplex 2507 is an expensive metal. This is primarily due to its high alloying content, but it comes with the added benefit of exceptional corrosion resistance in extreme environments.

サンプルをいただけますか?

私達は質を点検するためにあなたのためのステンレス鋼板のサンプルを提供してもいいです。サンプルは無料で、お客様は運賃を支払うだけです。.

すでに輸出した国は?

カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.

MOQはいくらですか?

私達の MOQ はステンレス鋼シートのための 1 トンです。.

納期はどのくらいですか?

トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.

お問い合わせ