  • Grade: AISI 410-Martensite
  • 製造:冷延板、熱延板、鍛造板
  • 規格ASM、ASME、GB、DIN、JIS、ISO、EN、BS
  • 種類:冷間圧延薄板、熱間圧延厚板
  • 表面: 2B、NO.1、NO.4、HL、BA、8K、等。.
  • 長さ: 2438mm3048mm6000mm はカスタマイズすることができます
  • Origin: TISCO, Baosteel, Pohang, Tsingshan, Delong

ステンレス鋼板加工サービスのグローバルリーダー

Martensitic 410 grade stainless steel can be toughened by a “quench and temper” heat treatment, like most non-stainless steels. It contains enough chromium (at least 11.5%) to resist corrosion. It has the highest corrosion resistance when it is polished after tempering and hardening. A general-purpose grade of stainless steel plate called 410 grade is usually hardened, but still machinable, and is used in applications that require moderate heat and corrosion resistance and high strength. The high hardness of martensitic stainless steel is its main feature, but some other characteristics are sacrificed. Poor weldability must be accommodated during manufacturing, and a final heat treatment is usually required. Martensitic stainless steels have lower corrosion resistance than ordinary austenitic stainless steels. They also lose ductility at temperatures below freezing and lose strength at temperatures above freezing due to over-tempering, which limits their useful operating temperature range. 410 alloy stainless steel plate is a widely used 12% chromium martensitic stainless steel plate that can be heat treated to produce a range of mechanical properties. 410 stainless steel plate has high strength and hardness while having good corrosion resistance. 410 Alloy Stainless Steel Plate is ductile and malleable. It is magnetic in all circumstances. Therefore, it is not recommended for use where severe corrosion may occur.

Stainless steel 410 plates are used in many different commercial applications. To meet the needs of their customers, Daxun Alloys producers acquire stainless steel plates in specified sizes and specifications. Because of the special qualities of 410 grade stainless steel, stainless steel plates can be used in steam, mild, and chemical environments. When stainless steel passes numerous, exacting quality tests, these qualities become highly valuable.
As a result, making sure the material is checked prior to delivery is crucial. Daxun Alloys carries out the required testing for any kind of application.

続きを読む

技術データ

Product Parameters:   Stainless Steel Sheet/Plate
幅 10mm~2500mm
厚さ 0.2mm~100mm 厚さ公差 ±0.03mm
スタンダード ASM/ASM240/480、JIS4305、DIN EN 10088-2
表面 2B、BA、8K、NO.1、NO.4、NO.3、ヘアライン、チェック、ゴールド、ブラック、ローズゴールドなど
スペック 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L
 ミル・オリジン TISCO、ZPSS、BAOSTEEL、JISCO、ZSESS、ATI、SMC、HAYNES、VDM、ArcelorMittal、Outokumpuなど。.
認証 ISO、SGS、BV、TUV、CE など
UNS No S41000
EN 1.4006
AISI 410
カーボン(C) 0.08/0.15
ケイ素 (Si) 1
マンガン (Mn) 1
Phosphorus (P) 0.04
硫黄(S) 0.03
クロム(Cr) 11.5/13.5
モリブデン (Mo)
ニッケル(Ni) 0.75
窒素(N)
密度 (lb./ in^2) @ RT 0.28
引張弾性係数 (psi x 10^6) 29
比熱(BTU/o F/lb.) 32~212度 0.11
熱伝導率(BTU/hr/ft^2/ft) 212oF 14.4
932oF 16.6
平均熱膨張係数 (in. x 10^-6 per o F) 32~212oF 5.5
32~1,200oF 6.5
電気抵抗率(マイクロオーム - cm) 華氏70度 22.5

Daxunを選択し、顧客を満足させる。.

今すぐDaxunに連絡する

迅速な配達

We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.

今すぐDaxunに連絡する

410 plate features

耐食性
410 is resistant to dry air, fresh water, mild bases and acids, foods, steam and hot gases.
It must be hardened for maximum heat and corrosion resistance. Best performance when smooth.
Heat Resistance
Good resistance to scaling up to about 650°C, but not generally recommended for use at temperatures between 400 and 580°C as mechanical properties are reduced.
熱処理
Fully anneal 815-900°C, slow furnace cool to 600°C, then air cool.
Process anneal 650-760°C and air cool.
Welding
Easily welded by all standard methods, but requires preheating to 150-260°C and post weld annealing to reduce the likelihood of cracking.

今すぐDaxunに連絡する

Stainless Steel 410 Applications

 

  • Automobile exhaust pipes, engine parts;
  • Medical devices;
  • Knives and kitchen utensils;
  • Petrochemical applications;
  • Stainless steel cutlery, kitchen utensils;
  • Manufacturing flat springs;
  • Hand tools;
  • Bolts, nuts, springs and fasteners;
今すぐDaxunに連絡する

品質、納期、検査

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    当社の納期は、契約に厳密に従います。.
  • 顧客の第三者機関が工場に検査に行くのをサポートする。
  • テスト用の無料サンプルを顧客に提供
  • 現場検査またはビデオ工場検査をサポート
今すぐDaxunに連絡する

SS 410 Plate Surface Treatment

1D:粒子形状が不連続で表面はマット。.
2D:シルバーがかった白。.
2B:シルバーグレーで、2D表面よりも光沢と平坦性に優れる。.
バ:鏡面に近く、光沢と反射性に優れる。.
No.3:光沢が良く、表面が粗い。.
No.4:表面に細かい線があり、光沢がある。.
HL:シルバーグレーに金色の髪。.
8K:鏡面。.

今すぐDaxunに連絡する

加工

さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.

410 plate stainless steel Features

高強度
耐食性
耐熱性
低温耐性
環境保護
溶接性能

Daxun ブランドを急速に向上させる

2Bシートの公差
サイズ 寛容度ランク
グループ1 グループ2 グループ3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
No.1熱延板の公差
サイズ 寛容度ランク
グループ1 グループ2 グループ3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
デリバリー・ステートの選択 表面状態
冷間圧延 2B
2D
文学士
ヘアライン
第3位
第4位
6K
8K
注:
1.上記と異なる配送方法をご希望の場合は、弊社までご確認ください。.
2.お問い合わせやご注文の際、ここに記載されていないご要望がございましたら、何なりとお申し付けください。.
配信状態
デリバリー・ステートの選択 表面状態
熱間圧延 第1位
第3位
第4位
6K
8K
ピクルス
注:
1.上記と異なる配送方法をご希望の場合は、弊社までご確認ください。.
2.お問い合わせやご注文の際、ここに記載されていないご要望がございましたら、何なりとお申し付けください。.
グレード タイプ 厚さ 表面
オーステナイト系 304/304H/304L/304J1 0.25-150mm 2B/BA/4番/8K/SB/HL/1番
321 0.4-80mm 2B/BA/4番/8K/SB/HL/1番
316/316L/317L/316Ti 0.3-80mm 2B/BA/4番/8K/SB/HL/1番
フェライト 430 0.4-3.0mm 2b/ba/no.4/8k/sb/hl
超高純度フェライト 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
グレード タイプ 厚さ オリジナル
耐熱鋼 309S 0.5-40mm 中国
310S 0.5-40mm 中国
二相鋼 2101 1.5-50mm 中国
2304 3.0-50mm 中国
2205 0.5-60mm 中国
2507 1.0-60mm スイス/日本/中国
スーパーオーステナイト鋼 N08904 0.6-50mm スイス/日本/中国
S31254 0.5-50mm スイス/日本/中国
N08926 0.5-50mm スイス/日本/中国
N08367 0.5-50mm スイス/日本/中国
ニッケル基合金 N08031 1.0-50mm アメリカ / 日本 / ドイツ
N08810/N08800 0.8-50mm アメリカ / 日本 / 中国
N08028 1.0-20mm アメリカ / ドイツ / 日本
N08020 1.0-20mm アメリカ / ドイツ / 日本
N08825 0.8-40mm アメリカ / ドイツ / スイス / 日本 / 中国
N10276 0.5-50mm アメリカ / ドイツ / 日本
N06022 1.0-50mm アメリカ / ドイツ / 日本
N06625 0.8-20mm アメリカ / ドイツ / 中国
N04400 1.0-20mm アメリカ / ドイツ / 日本
N06600 1.0-50mm アメリカ / ドイツ / 日本 / 中国
N02201 0.5-20mm アメリカ / 日本
チタン TA1/Gr1 0.5-50mm 日本 / 中国
TA2/Gr2 0.5-50mm 日本 / 中国
溶接材料 ERNiCrMo-13 1.2、2.4mm ドイツ
ERNiCrMo-3 2.4mm ドイツ
ERNiCrMo-4 2.4mm 米国

The surface and shape of 410 stainless steel plate (7)

Daxunは信頼できるステンレス鋼板メーカーです。

Daxunは専門メーカーとして、生産するすべての製品が高品質であることを保証します。そのため、すべてのステンレス鋼板はISO9001、SGS、CE、OQCなどの国際品質規格の認証を取得しています。また、ステンレス鋼板の欠陥が少ないことを保証するために、厳格な品質管理を行っています。Daxunでは、すべての製品は、耐久性、高品質、高性能であることをご安心ください。.

最近の注目プロジェクトと製品

410 plate stainless steel
astm a240 410 stainless steel plate
410 flat stainless steel plate
410 stainless steel sheet suppliers
410 2b stainless steel sheet
サンプルをいただけますか?

私達は質を点検するためにあなたのためのステンレス鋼板のサンプルを提供してもいいです。サンプルは無料で、お客様は運賃を支払うだけです。.

すでに輸出した国は?

カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.

MOQはいくらですか?

私達の MOQ はステンレス鋼シートのための 1 トンです。.

納期はどのくらいですか?

トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.

お問い合わせ
クイック見積もり