Grade 23 Ti 6Al-4V ELI Titanium Alloy Pipe Manufacturer
中国におけるチタン及びチタン合金管の主要サプライヤーとして、大勋は高性能チタン管を世界へ提供しています。
- Titanium tube Grade:Grade 23 – UNS R56401
- Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
- Titanium tube density The density of grade 23 titanium is 4.43 g/cm3
- Standards:ASTM B338/ASME SB338、ASTM B337/ASME SB337、ASTM B861/ASME SB861、ASTM B862/ASME SB862、AMS4911、AMS4928
大迅は中国でチタン管を生産し、多様で——顧客の厳しいニーズに応えます!
Provide High Quality Grade 23 Titanium Pipe to Customers Around The World
Grade 23 titanium tubing, also known as Ti-6Al-4V ELI, is a high-strength, lightweight alloy composed of titanium with 6% aluminum and 4% vanadium in an extra-low interstitial (ELI) form.It is an improved alloy based on the classic Ti-6Al-4V (grade 5) by further reducing the content of interstitial elements such as oxygen, iron, and nitrogen (such as oxygen content ≤ 0.13%).Its extra-low interstitial (ELI) composition significantly enhances fracture toughness and fatigue resistance compared to standard titanium alloys, allowing it to perform reliably under cyclic loading conditions. The alloy maintains its impressive strength-to-weight ratio even at cryogenic temperatures, unlike many metals that become brittle in extreme cold. Additionally, Grade 23 exhibits superior corrosion resistance in both acidic and chloride environments, outperforming many stainless steels and other titanium grades in aggressive chemical settings.
Where is Grade 23 titanium pipe used?
Grade 23 titanium tubing has unique applications in cutting-edge medical devices, particularly orthopedic implants such as spinal fusion cages and joint replacement components, which require lifelong biocompatibility and fatigue resistance. It is particularly well-suited for dental implant systems, where osseointegration (a direct structural connection between bone and implant) is crucial to the long-term success of the system. In aerospace, it is the material of choice for hydraulic and fuel lines in commercial and military aircraft, which must balance weight reduction with extreme pressure requirements. The material’s properties also make it an ideal choice for high-performance bicycle frames used by professional cyclists, where its vibration-absorbing properties and fatigue resistance provide a competitive advantage.
キーノート
ELI (Extra Low Interstitial):グレード23は、標準的なグレード5(Ti-6Al-4V)に比べ、酸素、窒素、水素、炭素の制限が厳しく、延性と生体適合性を高めている。.
主な合金元素:アルミニウム(Al)とバナジウム(V)は強度と相安定性に寄与する。.
不純物管理:鉄、炭素、窒素、水素が少なく、優れた耐食性と疲労性能を確保。.
主なパフォーマンス
高強度+高靭性:引張強度は895-930MPa(アニール状態)、伸びは≥10%に達することができ、通常のグレード5よりも優れており、動的負荷がかかるシーンに適している。.
優れた耐食性:耐酸性(塩酸、硫酸など)、耐アルカリ性、耐海水性、医療用インプラントや化学装置で優れた性能を発揮。.
生体適合性:非磁性、無毒性、人体組織との優れた適合性を持ち、整形外科用インプラントに好ましい材料である。.
加工性:鍛造、圧延、機械加工によって形成することができ、溶接性能は通常のチタン合金よりも優れている。.
データ
- パラメータ
- 機械的特性
- 物理的性質
| エレメント | ティ | アル | V | O | フェ | C | N | H | その他の要素 |
| 組成範囲(wt.%) | >89% | 5.50 - 6.75% | 3.50 - 4.50% | ≤ 0.13% | ≤ 0.25% | ≤ 0.08% | ≤ 0.05% | ≤ 0.0125% | ≤ 0.4% |
| プロパティ | 価値 |
|---|---|
| Ultimate Tensile Strength | 860-950 MPa |
| 降伏強度 | 825-860 MPa |
| 伸び | 10-15% |
| Fatigue Strength | ~500 MPa (at 10⁷ cycles) |
| Fracture Toughness | 70-90 MPa√m |
| 硬度 | 320-350 HV |
| 弾性係数 | 90-110 GPa |
| プロパティ | 価値 |
|---|---|
| 密度 | 4.43 g/cm³ |
| 融点 | 1660-1680°C |
| 熱伝導率 | 7.2 W/m·K |
| 熱膨張係数 | 8.6 × 10⁻⁶ /°C |
| 電気抵抗率 | 1.78 μΩ·m |
| 比熱容量 | 560 J/kg·K |
Daxunを選んで、あなたのプロジェクトを成功に導きましょう。.

アドバンスド・プロダクション
We offer a comprehensive selection of Grade 23 titanium tubing solutions, including both welded and seamless options to meet diverse industrial requirements. Our inventory features precision-engineered tubes manufactured to the highest quality standards, ensuring optimal performance in demanding applications. Whether you need welded tubes for cost-effective solutions or seamless tubes for superior pressure capabilities, our Grade 23 titanium products deliver exceptional strength-to-weight ratios, outstanding corrosion resistance, and biocompatibility for aerospace, medical, marine, and chemical processing industries.
試験報告書
We provide comprehensive documentation and certification reports for all our Grade 23 titanium tubing, ensuring complete transparency and compliance with industry standards. Our documentation package includes material test reports (MTRs), chemical analysis certificates, mechanical property verification, and non-destructive testing results. Each batch of our Grade 23 titanium tubes comes with full traceability records, detailing the manufacturing process, heat treatment information, and quality assurance protocols.


品質、納期、検査
Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 23 Titanium Welded Pipe and Grade 23 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.
- 当社の納期は、契約に厳密に従います。.
- 顧客の第三者機関が工場に検査に行くのをサポートする。
- 顧客テストのための無料サンプルをサポート
- 現場検査またはビデオ工場検査をサポート
テクニカルサポート
さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.

Daxun Grade 23 Titanium TUBE Let your brand improve rapidly
- ギャラリー
Grade 23 titanium tube form (4)
関連商品 (5)
Grade 23 titanium pipe (Ti-6Al-4V ELI) is an extra low interstitial version of the popular Grade 5 titanium alloy. It contains reduced levels of oxygen, iron, and other interstitial elements, which results in improved fracture toughness, better fatigue resistance, and enhanced biocompatibility while maintaining high strength-to-weight ratio.
Grade 23 titanium tubes offer excellent biocompatibility, reducing the risk of adverse reactions when implanted in the human body. They have a modulus of elasticity closer to bone than many other metals, which helps reduce stress shielding. Additionally, their superior fatigue resistance ensures long-term performance in load-bearing medical applications.
Grade 23 titanium tubes exhibit outstanding corrosion resistance in most environments, including seawater, chlorides, and acidic conditions. The protective oxide layer that forms on the surface provides exceptional resistance to pitting and crevice corrosion, making them suitable for marine and chemical processing applications.
We offer Grade 23 titanium tubes in a comprehensive range of sizes, with outer diameters from 6mm to 120mm and wall thicknesses from 0.5mm to 10mm. We can also provide custom dimensions and special tolerances to meet specific project requirements.
Yes, we can supply Grade 23 titanium tubes with various surface treatments including anodizing, passivation, polishing, and coating options. These treatments can enhance specific properties such as wear resistance, friction characteristics, or aesthetic appearance depending on your application needs.
All our Grade 23 titanium tubes undergo rigorous quality control including ultrasonic testing, eddy current inspection, and dimensional verification. We provide full material traceability and complete documentation including chemical analysis, mechanical properties, and non-destructive testing reports with every order.
チタンのグレードはコストをわずかに増加させますが、総コストは主に必要なチタンの形状と形態によって決定されます。
大迅では、チューブ、パイプ、コイル、棒材など、幅広いチタン製品を取り扱っております。お客様がご指定される各製品の長さ、幅、数量により、お支払い金額が変動いたします。
残念ながら、プロジェクトの詳細やチタニウムの使用目的がわからないと、オンラインで価格をお見積もりするのは難しいです。
幸いなことに、当社の専門家チームが常に皆様のチタンに関するご要望にお応えし、アドバイスを提供いたします。daxunalloy@gmail.com までメールをお送りいただければ、アドバイスと正確な見積もりをご案内いたします。
ご要望のチタニウムのグレード、形状、数量について、可能な限り詳細な情報をご提供ください。これにより、お客様のニーズをより正確に把握できます。
お問い合わせ “ページのフォームにご記入いただくか、”+86 13382898899 “までお電話ください。WhatsAppはオンライン、Eメール(Daxunalloy@gmail.com)は6時間以内に確認いたします。すべてのお問い合わせやメッセージに迅速に対応させていただきます。また、毎週お客様と市場情報を共有しています。
We can provide titanium tube samples for you to check the quality. Sample is free and you just pay the freight.
トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.