  • Coil grade: Ferrite-SS 409/409L
  • Coil features: Easy to process, corrosion resistant.
  • Coil thickness: 0.4 mm to 12.00 mm
  • Coil width: 1000 mm, 1250 mm, 1500 mm and 2000 mm.
  • Coil surface: 2B, BA, matte, polished, 8k mirror.
    If necessary, stainless steel coils will come with a protective film to protect the metal surface from unnecessary damage.

Global leader in stainless steel Coil fabrication services

Type 409 Stainless Steel (UNS S40900) is a stabilized ferritic stainless steel that has higher oxidation and corrosion resistance than carbon steel. The ease of manufacture, paired with its corrosion resistance and affordability, has considerably increased its use in automotive exhaust and other non-automotive applications. ASTM A240 specifies three (3) subcategories of Type 409 stainless steel: UNS S40910, UNS S40920, and UNS S40930. Each of these designations has slightly different Ti or Nb stabilization requirements. Unless the purchaser specifies otherwise, any of these compositions may be given as UNS S40900. It is manufactured with improved formability properties known as “High Performance” or “Ultra Form” in the industry.

Dah Hsun is an ISO 9001:2008 certified firm that is a major supplier and exporter of ASTM A240 Stainless Steel Coils. Stainless steel coils can be cut to your requirements and include a full set of mill test results. Custom lengths and widths are available up to 2000mm. Exporting is our specialty! We can obtain several hard-to-find grades and/or non-standard sizes to satisfy our customers’ specific needs. We have vast experience processing steel coil goods and can divide all stainless steel coils to the desired sizes. Introducing our extensive line of Dah Hsun Stainless Steel goods – the pinnacle of dependability, durability, and performance. We are glad to provide a wide selection of grades and varieties to fulfill the diverse needs of industrial and architectural applications.

Our stainless steel coil goods, which range from the Austenitic series to the Ferritic series and other special categories, are well-known for their high performance and extensive requirements. The austenitic series includes 304/304L/304J1, 321 and 316/316L/317L/316Ti/310/309, which can fulfill varied thickness requirements and give a variety of surface treatments, including 2B, BA, NO.4, 8K, SB, HL, NO.1, and so on.

Our ferrite line, which includes 430, ultra-pure ferrite 443, and 436L/439/444/441, caters to customers looking for unique qualities and applications. These materials can accommodate thicknesses ranging from 0.4mm to 3.0mm and offer a variety of surface treatment options such as 2B, BA, NO.4, 8K, SB, HL, and so on.

By selecting our stainless steel coils, you are investing in a material that ensures long service life, great reliability, and exceptional performance. Don’t compromise on quality; choose our stainless steel solutions and see the impact they can make in your project. Contact Daxun today for additional information or to place an order for the stainless steel coil specs and quantities that you require.

続きを読む

データ

409/409L Stainless Steel Coil Specification ASM A240 / ASME SA240
409/409L Stainless Steel Coil Manufacturing Process Hot Rolled (HR) / Cold Rolled (CR)
409/409L Stainless Steel Coil Grades 201 / 304 / 304L/ 409/409L / 309S / 420 / 316 / 316L / 316Ti / 317L / 321 / 321H / 347 / 347H / 904L etc.
UNS No. –  UNS S409/409L, UNS S31008, UNS S31600, UNS S31603, UNS S31603, UNS S31600, UNS S31703, UNS S32100, UNS S34700, UNS S34709, UNS S8904
EN No.  1.4512,1.4845, 1.4401, 1.4404, 1.4571, 1.4438, 1.4541, 1.4550, 1.4551, 1.4539
409/409L Stainless Steel Coil Thickness 0.6 MM TO 16 MM THICKNESS
409/409L Stainless Steel Coil Width 1250 MM / 1500 MM / 2000 MM / 04 Feet / 05 Feet and Custom Cut Width as Per Requirement
409/409L Stainless Steel Coil Length 2400 MM / 2420 MM / 6000 MM / 08 Feet / 10 Feet / Coil Cut and Custom Cut Length as Per Requirement
409/409L Stainless Steel Coil Surface Finish 2B, 2D, BA, MATT, MATT PVC, No.4, No.5, SB, HR, No.8, Mirror, Hairline, Brush, Textured, Oil base wet Polished, Both sides Polished available.
409/409L Stainless Steel Coil Coating PVC coating Normal / Laser, Film: 100 micrometer, Color: black/white.
409/409L Stainless Steel Coil Other Testing NACE MR0175, Ultrasoung TEST, IGC TEST, Intergranular Corrrosion Test as per ASTM A262 Practice E, Charpy Impact Test, Macro, Grain Size, Hardness, etc.
409/409L Stainless Steel CoilValue Added Services Gas Cutting / CNC Plasma Cutting / Profiling / Rolling / Bending / coil Metal Fabrication / Drill / Punch / Machining / Sand Blasting / Shot Blasting / Heat Treatment
409/409L Stainless Steel Coil Packaging Loose / Carrate / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps
409/409L Stainless Steel Coil Shipment & Transportation By Road – Truck / Train Partial Load, Full Load, By Sea – Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air – Freighter Civil Passenger and Cargo Planes
409/409L Stainless Steel Coil Material Test Certificate Manufacturer Test Certificate As Per EN10204 3.1, 3.2 / Laboratory Test Certificate From NABL Approved Lab. / Under Third Party Inspection Agency Like SGS, TUV, DNV, LLOYDS, ABS, Bureau of Indian Standards BIS Approved ETC
メーカー POSCO, Aperam, Jindal Stainless, DKC Korea, Thyssenkrup, Baosteel, TISCO,Arcelor Mittal, VDM,Nippon Metal, Outokumpu,Qingshan,Delong.
Shipping Port Shanghai/Ningbo port/Tianjin/Qindao
エレメント UNS S40910 UNS S40920 UNS S40930
カーボン 最大0.030. 最大0.030. 0.030 max
Manganese 1.00 max. 1.00 max. 1.00 max.
Sulfur 0.020 max. 0.020 max 0.020 max
Phosphorus 0.040 max. 0.040 max. 0.040 max.
Silicon 1.00 max. 1.00 max. 1.00 max.
Chromium 10.5 – 11.7 10.5 – 11.7 10.5 – 11.7
Nickel 0.50 max. 0.50 max. 0.50 max.
窒素 最大0.030. 最大0.030. 最大0.030.
チタン 6x(C+N) min. – 0.50 max. 8X(C+N)min. / 0.15 – 0.50 0.05 min.
Niobium 0.17 max. 最大0.10.
Ti + Nb [0.08+8x(C+N)] min. – 0.75 max.
タイプ 降伏強さ 0.2% オフセット(KSI) 引張強さ(KSI) % Elongation (2″ Gauge length)
S40910 25分. 55 min 20 min.
S40920 25分. 55 min. 20 min.
S40930 25分. 55 min. 20 min.
密度 (lb./ in^2) @ RT 0.28
引張弾性係数 (psi x 10^6) 29
比熱(BTU/o F/lb.) 32~212度 0.114
熱伝導率(BTU/hr/ft^2/ft) 212oF 14.4
平均熱膨張係数 (in. x 10^-6 per o F) 32~212oF 5.84
32 to 500oF 6.12
32 to 900oF 6.6
32~1,200oF 6.86
電気抵抗率(マイクロオーム - cm) 華氏70度 60
耐酸化性-連続使用(oF) 1450
グレード WERKSTOFF NR. AISI 国連 アフノール BS GOST 日本工業規格
SS 409 1.4512 409 S40900 Z3CT12 409 S 19 SUH 409 –
•  409/409L Stainless Steel HR coil •  Stainless Steel Cladding 409/409L coil
• 409/409L Stainless Steel Chequered coil •  Black SS 409/409L coil 4mm Thick
• 409/409L Stainless Steel Golden Laser Pattern coil •  Bright-pickled Stainless Steel 409/409L coil
• Super thin-Mirror surface BA ss 409/409L coil •  Cold rolled, heat treated 409/409L coil
• Super Austenitic SS 409/409L coil •  3mm Cold Rolled AISI SS 409/409L coil
• ASTM A240 409/409L coil •  Mill Supply SS 409/409L coil
• JMSS cold rolled ss 409/409L coil •  Grade Prime SS 409/409L coil
• Cold Rolled No.1 Finish SS 409/409L coil •  Carpenter Custom 450 Stainless Steel 409/409L coil
• SEW 400 Stainless Steel 409/409L coil •  Cut to Size Stainless Steel 409/409L coil
• Hot Rolled Stainless Steel 409/409L coil •  Non Magnetic Polishing Stainless Steel 409/409L coil
• Sales Promotion SS 409/409L coil •  ASME SA240 409/409L coil
•  Cr Stainless Steel 409/409L coil •  Grade 409/409L Stainless Steel Finish coil
•  SS 409/409L Mill Test Certificate coil •  409/409L Stainless Steel Blank coil
•  ASTM A240 409/409L coil •  409/409L Stainless Steel Perforated coil
•  Cold rolled, bright annealed 409/409L coil •  Embossed ss 409/409L coil
•  Ground Stainless Steel 409/409L coil •  Cheap cold rolled ss 409/409L coil with best price
•  Hot Selling AISI SS 409/409L coil •  Brush finish ss 409/409L coil price list
•  SS 409/409L Rose Golden coil • SS URANUS B6 409/409L coil
• Surface coated Stainless Steel 409/409L coil •  2B SUS SS 409/409L coil
•  Satin finish Stainless Steel 409/409L coil •  Food Grade Stainless Steel 409/409L coil
•  AISI stainless steel 409/409L armor coil •  No. 4 PVC Coated SS 409/409L coil
• Satin finish Stainless Steel 409/409L coil •  SS 409/409L coil Blasted Tin-Gold Rose
•  Mirror Finish SS 409/409L coil •  2mm ASTM SS 409/409L coil
•  SS 409/409L coil Gold Brush Finish •  Stainless Steel Corrugated 409/409L coil
• 409/409L Stainless Steel CR coil •  ASTM B625 409/409L coil
•  409/409L Stainless Steel 2B coil •  Brushed or dull polished Stainless Steel 409/409L coil
•  409/409L Stainless Steel B. Q. Profile coil •  Cold rolled, heat treated, pickled 409/409L coil
•  Best selling 4’x8′ mirror finished ss 409/409L coil •  10K Mirror Finish Surface SS 409/409L coil
•  Decorative hairline inox cold rolled ss 409/409L coil •  Gold Etched SS 409/409L coil
•  Hair Line Finish SS 409/409L coil •  18 Gauge SS 409/409L coil
•  Laser cutting ss 409/409L coil •  Patterned Stainless Steel 409/409L coil
•  Tisco Supplier 3mm Thickness Stainless Steel 409/409L coil •  #4 Finish Stainless Steel 409/409L coil
•  Decorative Stainless Steel 409/409L coil •  Patterned Stainless Steel 409/409L coil
•  Scotch Brite SS 409/409L coil •  Passenger Elevator Cabin SS 409/409L coil
•  Baosteel Stainless Steel 409/409L coil •  Dimensional Stainless Steel Grade 409/409L coil

Daxunを選択し、顧客を満足させる。.

今すぐDaxunに連絡する

迅速な対応

We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.Daxun’s stainless steel materials are of reliable quality, and their varieties, specifications and delivery weights strictly comply with the standards.

今すぐDaxunに連絡する

Stainless steel coil packaging

Quality is belief, and integrity is a business card. Daxun pioneered the concept of “performance excellence management” and implemented the “PDCA+Lean” management model. The company’s business card says “Daxun = assured quality”. Daxun Stainless Steel achieves full traceability of each steel coil from the ERP system, including variety, specification, and origin, and advocates and encourages industry anti-counterfeiting. Daxun Stainless Steel relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strict monitoring during sales, and provides worry-free service guarantees after sales.

今すぐDaxunに連絡する

Steel tube packaging

国際貨物は様々な経路を経て最終目的地に到着するため、梱包は重要な役割を担っています。商品によって、様々な方法で梱包しています。当社では、以下のような様々な方法で商品を梱包しています:
- 箱と木箱
- シュリンクラップ
- 木製パレット
- 木製ボックス

今すぐDaxunに連絡する

品質、納期、検査

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    当社の納期は、契約に厳密に従います。.
  • 顧客の第三者機関が工場に検査に行くのをサポートする。
  • テスト用の無料サンプルを顧客に提供
  • 現場検査またはビデオ工場検査をサポート
今すぐDaxunに連絡する

ご注文について

Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.

今すぐDaxunに連絡する

テクニカルサポート

さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.

SS 409/409L Stainless Steel Coil Features

高強度
耐食性
耐熱性
低温耐性
環境保護
溶接性能

大順合金 あなたのブランドを急速に向上させる

グレード タイプ 厚さ 表面
オーステナイト系 304/304H/304L/304J1 0.25-150mm 2B/BA/4番/8K/SB/HL/1番
321 0.4-80mm 2B/BA/4番/8K/SB/HL/1番
316/316L/317L/316Ti 0.3-80mm 2B/BA/4番/8K/SB/HL/1番
フェライト 430 0.4-3.0mm 2b/ba/no.4/8k/sb/hl
超高純度フェライト 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
スーパーオーステナイト鋼 N08904 0.6-50mm スイス/日本/中国
S31254 0.5-50mm スイス/日本/中国
N08926 0.5-50mm スイス/日本/中国
N08367 0.5-50mm スイス/日本/中国
ニッケル基合金 N08031 1.0-50mm アメリカ / 日本 / ドイツ
N08810/N08800 0.8-50mm アメリカ / 日本 / 中国
N08028 1.0-20mm アメリカ / ドイツ / 日本
N08020 1.0-20mm アメリカ / ドイツ / 日本
N08825 0.8-40mm アメリカ / ドイツ / スイス / 日本 / 中国
N10276 0.5-50mm アメリカ / ドイツ / 日本
N06022 1.0-50mm アメリカ / ドイツ / 日本
N06625 0.8-20mm アメリカ / ドイツ / 中国
N04400 1.0-20mm アメリカ / ドイツ / 日本
N06600 1.0-50mm アメリカ / ドイツ / 日本 / 中国
N02201 0.5-20mm アメリカ / 日本
チタン TA1/Gr1 0.5-50mm 日本 / 中国
TA2/Gr2 0.5-50mm 日本 / 中国
溶接材料 ERNiCrMo-13 1.2、2.4mm ドイツ
ERNiCrMo-3 2.4mm ドイツ
ERNiCrMo-4 2.4mm 米国
Subsidiary Main Equipments Qty Annual Capacity
Daxun Stainless steel co.(JiangSu) Slitting Machine 1 Decorative Sheet:60,000 tons
Cutting Machine 1
No.4 And Hairline Sheet To Sheet Polishing Machine 1
No.4/Hairline Coil To Coil Polishing Machines 1
8K/Super Mirror Sheet To Sheet Polishing Machines 2
8K/Super Mirror Coil To Coil Polishing Machines 3
PVD Color Coating Machines 4
Liquid Chemical Coating Machines 2
Anti Finger Printing Machines 2
Auto Pick and Place machines 16
coil Washing Machine 1
Daxun Stainless steel co.(Shanghai) Cold Rolling Machine 3 2B Coils:100,000 tons
Annealing & Pickling Line 2 Decorative Sheet;30,000 tons
Slitting Machine 1
Cut to Length Machine 1
No.4/HL Polishing Machine(Sheet to Sheet) 3
8K Polishing Machine(Sheet to Sheet) 13
PVD Titanium Coating Machine 4
Liquid Chemical Coating Machines 1
Daxun Stainless steel co.(Shandong) Cold Rolling Machine 3 2B & BA Coil:220,000 tons
Annealing & Pickling Line(2B & BA) 2 Decorative Sheet:60,000 tons
Tension Levering & Skin Pass 1
Slitting Machine 1
Cut to Length Machine 1
No.4/HL Polishing Machine(Sheet to Sheet) 1
8K Polishing Machine(Sheet to Sheet) 11
Automatic Copper Coating Machine 1
Digital Printing Machine 1
PVD Titanium Coating Machine 3
Liquid Chemical Coating Machines 1
Anti-finger Machine 1
Daxun Stainless steel co.(Sichuan) Slitting Machine 1 2B & BA Coil:180,000 tons
Cutting Machine 1 Decorative Sheet:50,000 tons
No.4 And Hairline Sheet To Sheet Polishing Machine 1
No.4/Hairline Coil To Coil Polishing Machines 1
8K/Super Mirror Sheet To Sheet Polishing Machines 1
8K/Super Mirror Coil To Coil Polishing Machines 1
PVD Color Coating Machines 1
Liquid Chemical Coating Machines 1
Anti Finger Printing Machines 1

参照およびダウンロード可能な情報

Daxun is a trustworthy stainless steel coil manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steels are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel coils have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

最近の注目プロジェクトと製品

409/409L stainless steel coil
stainless steel seamless coil
SS 409/409L stainless steel coil
Stainless Steel Polished coil
SS 409/409L steel coil
ステンレス・コイル
BA stainless steel coil
SS 409/409L stainless coil
ステンレス・コイル
Stainless steel precision coil
Stainless steel coil 409/409L
早急に見積もりを取る、あるいはマーケット情報を理解するには?

お問い合わせ “ページのフォームにご記入いただくか、”+86 13382898899 “までお電話ください。WhatsAppはオンライン、Eメール(Daxunalloy@gmail.com)は6時間以内に確認いたします。すべてのお問い合わせやメッセージは、迅速に対応させていただきます。また、毎週お客様と市場情報を共有しています。

サンプルをいただけますか?

サンプルは無料で提供できるが、運賃は顧客負担となり、協力後に返金される。.

すでに輸出した国は?

カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.

MOQはいくらですか?

Our MOQ is 1 ton for stainless steel coil.

品質管理はどのように?

We have a complete organization from raw material purchasing to processing and shipment arranging. In the whole chain, the documentary people ad QC will look for and check it by precise requirements.The third party inspection is welcomed.

納期はどのくらいですか?

トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.

お問い合わせ
クイック見積もり