x
お問い合わせ
クイック見積もり

Daxun is a 409 stainless steel sheet supplier in China

As China’s leading stainless steel plate supplier and exporter, Daxun provides 409 stainless steel plates to the world.
  • Grade: AISI 409
  • 製造:冷延板、熱延板、鍛造板
  • 規格ASM、ASME、GB、DIN、JIS、ISO、EN、BS
  • 種類:冷間圧延薄板、熱間圧延厚板
  • 表面: 2B、NO.1、NO.4、HL、BA、8K、等。.
  • 長さ: 2438mm3048mm6000mm はカスタマイズすることができます
  • Origin: TISCO, Baosteel, Pohang, Tsingshan, Delong

410 Global leader in stainless steel sheet fabrication services

Daxun’s Grade 409 stainless steel plate has good corrosion resistance and is typically one of the least expensive varieties of stainless steel. It has a high tensile strength, is easily welded using arc welding, and is suited for resistance spot and seam welding. It is worth noting that welding type 409 does not reduce its corrosion resistance. It can be utilised in a variety of applications, including vehicle and truck exhaust systems, heat exchangers, agricultural spreaders, fuel filters, gas turbine exhaust mufflers, and others that demand precise shaping, toughness, and better weldability. One of this stainless steel grade’s primary advantages is improved weldability.

Grade 409 is a stabilised ferritic general-purpose stainless steel sheet with 11% chromium. It is especially well-suited for applications that require oxidation or corrosion resistance that carbon steel and some coated steels cannot provide. 409 has strong oxidation resistance and formability, but poor corrosion resistance because to its low chromium concentration. 409 has lower corrosion resistance than grades 304, 430, or 439, but it outperforms mild steels. Roll forming, stretch bending, deep drawing, and press forming are all options for shaping 409. When 409 is annealed, it will not harden when cold treated with mild roll forming processes such as press or stretch bending. Weldability for grade 409 is fair. This stainless material should not be utilised in shock-loaded structures because the grain structure grows in the heat-affected zone, which can have a direct impact on mechanical qualities. 409 is commonly used for tubing and stampings in automotive exhaust system applications. The mechanical qualities of this stainless steel sheet grade provide significant benefits in the automotive and agricultural industries. This offers good protection from exhaust gas and high-temperature ambient corrosion. However, the mechanical properties outweigh the stainless steel’s look. It is not advised for use in decorative purposes.

続きを読む

技術データ

Product Parameters:   Stainless Steel Sheet/Plate
幅 10mm~2500mm
厚さ 0.2mm~100mm 厚さ公差 ±0.03mm
スタンダード ASM/ASM240/480、JIS4305、DIN EN 10088-2
表面 2B、BA、8K、NO.1、NO.4、NO.3、ヘアライン、チェック、ゴールド、ブラック、ローズゴールドなど
スペック 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L
 ミル・オリジン TISCO、ZPSS、BAOSTEEL、JISCO、ZSESS、ATI、SMC、HAYNES、VDM、ArcelorMittal、Outokumpuなど。.
認証 ISO、SGS、BV、TUV、CE など
エレメント % Present (in product form)
カーボン(C) 0.03
ケイ素 (Si) 1
マンガン (Mn) 1
リン (P) 0.04
Sulfur (S) 0.015
クロム(Cr) 10.50 – 12.50
モリブデン (Mo) 6 x (C+N) to 0.65
鉄(Fe) バランス
Product Form
C H
Thickness (mm) Max 8 13.5
Yield Strength Rp0.2 N/mm2 Longitudinal 210
Transverse 220
引張強度 Rm N/mm2 380 – 560
Elongation min. in % A80mm1) <3mm (longitudunal + transverse) 25
A2) ≥3mm (longitudinal + transverse)
密度 熱伝導率 Electrical Modulus of Coefficient of Specific Heat メルティング
lbm/in^3 (BTU/h ft. °F) 抵抗率 Elasticity 熱膨張 (BTU/lb/ Range
(in x 10^-6) (psi x 10^6) (in/in)/ °F) (°F)
°F x 10^-6
12.4 at 932 °F 39.4 at 752°F 6.60 at 32 – 1000°F
49.6 at 1652 °F 6.86 at 32 – 1500°F
at 68°F: 0.280 9.4 at 212°F 28.3 at 68°F 29 5.84 at 32 – 212°F 0.114 at 68°F to 212°F 2500 to 2590
UNS 409 1.4512 409L
ASTM A240 ASTM A240 ASTM A240
ASTM A480 ASTM A480 ASTM A480
ASME SA240 ASME SA240 ASME SA240
AMS 5521 AMS 5521 AMS 5521

Daxunを選択し、顧客を満足させる。.

今すぐDaxunに連絡する

迅速な配達

We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.

今すぐDaxunに連絡する

Advantages/Disadvantages

This stainless steel grade has mechanical qualities that provide significant benefits in the automotive and agricultural industries. This offers enhanced protection from exhaust gas and air corrosion at high temperatures. However, the mechanical characteristics of this stainless steel outweigh its visual look. It is not advised for use in decorative purposes.

今すぐDaxunに連絡する

Stainless Steel 409 Applications

  • 409 stainless steel plate for agricultural machinery
  • 409 stainless steel plate for automotive panels
  • 409 stainless steel plate for stamping products
  • 409 stainless steel plate for cookware
  • 409 stainless steel plate for home appliances
  • 409 stainless steel plate for kitchens
  • 409 stainless steel plate for food service equipment
  • 409 stainless steel plate for sinks
  • 409 stainless steel plate for railway vehicles
  • 409 stainless steel plate for exhaust
今すぐDaxunに連絡する

品質、納期、検査

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    当社の納期は、契約に厳密に従います。.
  • 顧客の第三者機関が工場に検査に行くのをサポートする。
  • テスト用の無料サンプルを顧客に提供
  • 現場検査またはビデオ工場検査をサポート
今すぐDaxunに連絡する

テクニカルサポート

さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.

409 plate stainless steel Features

高強度
耐食性
耐熱性
低温耐性
環境保護
溶接性能

Daxun ブランドを急速に向上させる

2Bシートの公差
サイズ 寛容度ランク
グループ1 グループ2 グループ3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
No.1熱延板の公差
サイズ 寛容度ランク
グループ1 グループ2 グループ3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
デリバリー・ステートの選択 表面状態
冷間圧延 2B
2D
文学士
ヘアライン
第3位
第4位
6K
8K
注:
1.上記と異なる配送方法をご希望の場合は、弊社までご確認ください。.
2.お問い合わせやご注文の際、ここに記載されていないご要望がございましたら、何なりとお申し付けください。.
配信状態
デリバリー・ステートの選択 表面状態
熱間圧延 第1位
第3位
第4位
6K
8K
ピクルス
注:
1.上記と異なる配送方法をご希望の場合は、弊社までご確認ください。.
2.お問い合わせやご注文の際、ここに記載されていないご要望がございましたら、何なりとお申し付けください。.
グレード タイプ 厚さ 表面
オーステナイト系 304/304H/304L/304J1 0.25-150mm 2B/BA/4番/8K/SB/HL/1番
321 0.4-80mm 2B/BA/4番/8K/SB/HL/1番
316/316L/317L/316Ti 0.3-80mm 2B/BA/4番/8K/SB/HL/1番
フェライト 430 0.4-3.0mm 2b/ba/no.4/8k/sb/hl
超高純度フェライト 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
グレード タイプ 厚さ オリジナル
耐熱鋼 309S 0.5-40mm 中国
310S 0.5-40mm 中国
二相鋼 2101 1.5-50mm 中国
2304 3.0-50mm 中国
2205 0.5-60mm 中国
2507 1.0-60mm スイス/日本/中国
スーパーオーステナイト鋼 N08904 0.6-50mm スイス/日本/中国
S31254 0.5-50mm スイス/日本/中国
N08926 0.5-50mm スイス/日本/中国
N08367 0.5-50mm スイス/日本/中国
ニッケル基合金 N08031 1.0-50mm アメリカ / 日本 / ドイツ
N08810/N08800 0.8-50mm アメリカ / 日本 / 中国
N08028 1.0-20mm アメリカ / ドイツ / 日本
N08020 1.0-20mm アメリカ / ドイツ / 日本
N08825 0.8-40mm アメリカ / ドイツ / スイス / 日本 / 中国
N10276 0.5-50mm アメリカ / ドイツ / 日本
N06022 1.0-50mm アメリカ / ドイツ / 日本
N06625 0.8-20mm アメリカ / ドイツ / 中国
N04400 1.0-20mm アメリカ / ドイツ / 日本
N06600 1.0-50mm アメリカ / ドイツ / 日本 / 中国
N02201 0.5-20mm アメリカ / 日本
チタン TA1/Gr1 0.5-50mm 日本 / 中国
TA2/Gr2 0.5-50mm 日本 / 中国
溶接材料 ERNiCrMo-13 1.2、2.4mm ドイツ
ERNiCrMo-3 2.4mm ドイツ
ERNiCrMo-4 2.4mm 米国

The surface and shape of 409 stainless steel plate (7)

Daxunは信頼できるステンレス鋼板メーカーです。

Daxunは専門メーカーとして、生産するすべての製品が高品質であることを保証します。そのため、すべてのステンレス鋼板はISO9001、SGS、CE、OQCなどの国際品質規格の認証を取得しています。また、ステンレス鋼板の欠陥が少ないことを保証するために、厳格な品質管理を行っています。Daxunでは、すべての製品は、耐久性、高品質、高性能であることをご安心ください。.

最近の注目プロジェクトと製品

409 plate stainless steel
astm a240 409 stainless steel plate
409 flat stainless steel plate
409 stainless steel sheet suppliers
409 2b stainless steel sheet
409ステンレス鋼板
サンプルをいただけますか?

私達は質を点検するためにあなたのためのステンレス鋼板のサンプルを提供してもいいです。サンプルは無料で、お客様は運賃を支払うだけです。.

すでに輸出した国は?

カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.

MOQはいくらですか?

私達の MOQ はステンレス鋼シートのための 1 トンです。.

納期はどのくらいですか?

トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.

お問い合わせ
クイック見積もり