x
Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat

Daxun is an excellent manufacturer of grade 7 (Ti-0.15Pd) titanium rods and bars.

  • Titanium bar grade: Grade 7-Ti / UNS R52400
  • Titanium bar types: rolled bars, drawn bars, forged titanium bars
  • Titanium bar density: The density of grade 7 titanium is 4.51 g/cm³
  • Main standards: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
  • High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.

The global leader in commercially pure titanium rod manufacturing services

Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 7 titanium alloy rods.

Grade 7 titanium bar (Ti Grade 7 / UNS R52400) is a palladium-enhanced, commercially pure (CP) titanium alloy specifically engineered for supreme corrosion resistance in aggressive environments. It consists of titanium (≥99%) with a critical addition of 0.12–0.25% palladium (Pd), which fundamentally alters its electrochemical behavior. This palladium modification dramatically improves resistance to reducing acids (e.g., sulfuric, hydrochloric, phosphoric), chloride solutions (including seawater and brines), and crevice/pitting corrosion—scenarios where standard CP grades like Grade 2 would rapidly degrade. While retaining the inherent advantages of titanium—low density (~4.5 g/cm³), high strength-to-weight ratio, excellent weldability, and biocompatibility—Grade 7 exhibits superior performance at elevated temperatures (up to ~400°C/750°F) and in highly oxidizing or acidic conditions. Its passive oxide layer, stabilized by palladium, provides unparalleled protection against chemical attack, making it one of the most corrosion-resistant metallic materials available.

Where is Grade 7 titanium bar used?

Grade 7 titanium bar is extensively used in chemical processing for critical components like valve stems, pump shafts, fasteners, and instrumentation components handling acids, chlorides, or organic solvents. In marine and offshore engineering, it serves in seawater desalination equipment, heat exchanger components, and subsea fastening systems exposed to high-salinity environments. The alloy also excels in pollution control systems (e.g., scrubber components), pharmaceutical manufacturing equipment, and medical implants (e.g., surgical instruments and orthopedic devices) due to its inertness and longevity. Despite its higher initial cost—driven by palladium content—Grade 7 delivers exceptional lifecycle value by minimizing downtime, maintenance, and replacement costs in corrosive service. Its reliability in preventing catastrophic failures ensures safety and efficiency in applications ranging from nuclear waste containment to aerospace fluid systems, justifying its selection as a premium solution for the most demanding corrosion challenges.

Daxun is your trusted titanium alloy rod production company. Daxun produces all grades of titanium alloys, including commercially pure titanium series CP, titanium alloy series, titanium nickel alloy, etc. They have reliable performance and provide high performance for your critical applications. In various industries and applications, you can rely on Daxun titanium alloy rods for high strength, high temperature and corrosive environments. For decades, Daxun Metals has been committed to producing highly engineered titanium alloy solutions to meet the most severe challenges.

Baca Lebih Lanjut

Data

Spesifikasi Details
Bahan Titanium rod and bar Grade 7 (UNS R52400)
Standar ASTM B348, ASTM SB348, AMS 4921, AMS 4902
Dimensions EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN
Diameter Range 0.125″ – 14″ (3.175mm – 355.6mm), custom
Length Range Up to 240″ (6096mm), custom
Finish Cold (bright) drawn, centerless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centerless Ground & Black
Permukaan akhir Cold drawn, Centerless Ground, Polished, Or Rough Turned, Black, NO.4 Finish, BA Finish, Matt Finish, etc.
Kondisi Hardened & tempered, annealed
Toleransi Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm)
Form Titanium square bars, titanium ingots, titanium round bars, rectangular titanium bars, triangular titanium bars, forged titanium bars, titanium hexagonal bars, etc.
Elemen Symbol Composition Range (wt.%)
Titanium Ti Balance (>99%)
Palladium Pd 0.12–0.25%
Besi Fe ≤0.30%
Oksigen O ≤0.25%
Karbon C ≤0.08%
Nitrogen N ≤0.03%
Hidrogen H ≤0.015%
Elemen Lainnya Each ≤0.40% (single element)

 

Properti Value (Imperial) Value (Metric)
Kekuatan Tarik 50,000–65,000 psi 345–450 MPa
Kekuatan Hasil 30,000–45,000 psi 207–310 MPa
Perpanjangan 20–30% 20–30%
Kekerasan (Brinell) 120–160 HB 120–160 HB
Modulus Elastisitas 14.9–16.0 × 10⁶ psi 103–110 GPa
Properti Value (Imperial) Value (Metric)
Kepadatan 0.163 lb/in³ 4.51 g/cm³
Titik Leleh 3,000–3,050°F 1,650–1,680°C
Konduktivitas Termal 9.5 Btu/(hr·ft·°F) 16.4 W/(m·K)
Coefficient of Thermal Expansion 4.8 × 10⁻⁶/°F 8.6 × 10⁻⁶/K
Tahanan Listrik 1.78 × 10⁻⁶ Ω·cm 1.78 μΩ·m

 

Pilih Daxun untuk membantu proyek Anda berjalan.

Hubungi Daxun sekarang

DAXUN® Grade 7 Titanium Rod Features

DAXUN® Ti Grade 5 is a titanium alloy bar (6al-4v) featuring:

  • Good hot formability and weldability;
  • Tensile strength can reach 1000MPa;
  • Dimensional work at high temperature
  • Insensitive to seawater or seawater;
  • Not affected by various corrosive media;
  • High strength and good toughness;
  • Resist crack initiation and crack propagation.
Hubungi Daxun sekarang

Daxun Factory Advantages

Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

Hubungi Daxun sekarang

Grade 7 Titanium Rod Production Method

Daxun produces high-quality titanium bars with high performance, and can also manufacture according to customer’s agreement:

  • Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
Hubungi Daxun sekarang

Test Reports

The test reports we provide include: Grade 2 Titanium Rod and Grade 2 Titanium Round Bar Factory Test Certificate, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, NABL Approved Laboratory Report, Destructive Test Report, Non-destructive Testing Report. (Daxun will provide according to customer requirements)

Hubungi Daxun sekarang

Grade 7 Rods Applications and Standards

Grade 7 Titanium Rods are widely used in the following industries under extreme corrosive conditions:

  • Aerospace, shipbuilding, oil and gas industry, marine engineering, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, military industry, pharmaceutical and food processing equipment, etc.
  • Specifications: AMS 4928,AMS 4967,AMS 4965 ,AMS 6931 ,ASTM B 348
  • Standards: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
Hubungi Daxun sekarang

Kualitas, pengiriman, inspeksi

Daxun performs several quality assurance tests, these tests include mechanical tests like area tensile, chemical analysis, material positive identification – PMI test, micro and macro testing, intergranular corrosion (IGC) test, ultrasonic flaw detection test, pitting and resistance test, hardness test, material positive identification, expansion test etc. All these tests ensure that the Grade 2 Titanium Rod and Grade 2 Titanium Round Bar material is suitable for the required application. During the production process, we measure the diameter, thickness and surface of the product.

  • Waktu pengiriman kami benar-benar sesuai dengan kontrak.
  • Mendukung agen pihak ketiga pelanggan untuk pergi ke pabrik untuk pemeriksaan
  • Support free samples for customer testing
  • Mendukung inspeksi pabrik di tempat atau video
Hubungi Daxun sekarang

Pengemasan

Daxun Alloy memastikan kualitas kemasan terbaik karena memainkan peran penting dalam pengiriman internasional di mana barang melewati berbagai saluran untuk mencapai tujuan akhir, jadi kami memberikan perhatian khusus pada pengemasan. Kami mengemas barang-barang kami dengan berbagai cara tergantung pada produknya. Kami mengemas produk kami dengan berbagai cara seperti:
- Kotak dan peti
- Kecilkan bungkus
- Palet kayu
- Kotak kayu

Hubungi Daxun sekarang

Dukungan Teknis

Jika Anda memerlukan bantuan teknis tambahan, ahli metalurgi dan staf kami yang berpengetahuan luas akan dengan senang hati membantu. Selain itu, Daxun memiliki laboratorium pengujian bersertifikat-yang pertama dalam industri inventaris multi-logam dan plastik. Ini, menurut pendapat kami, menunjukkan dedikasi kami yang tak tergoyahkan terhadap kualitas dan filosofi kami sebagai pemasok layanan penuh.

Daxun Grade 7 Titanium Rods help your brand improve quickly

NOMINAL SIZE h5 h6 h7 h8 h9 H10 H11 h12
DIAMETER mm
~ to 3 +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
over 3 to 6 +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
over 6 to 10 +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
over 10 to 18 +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
over 18 to 30 +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
over 30 to 50 +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
over 50 to 80 +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
over 80 to 120 +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
over 120 to 180 +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
over 180 to 250 +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

Proyek dan produk hot case terbaru

Grade 7 Titanium rod and bar
Batang dan batang titanium
Batang dan batang titanium
Batang dan batang titanium
Batang dan batang titanium
Batang dan batang titanium
Titanium Alloy Bar, Titanium Bar Grade 7/UNS 52400

Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 7 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.


SPECIFICATIONS

ASTM B348 – Titanium and Titanium Alloy Bars and Billets
ASTM SB348 – Specification for Titanium and Titanium Alloy Bars and Billets
AMS 4921 – Titanium Alloy Bars, Wire, and Forgings
AMS 4902 – Titanium Alloy Bars and Billets


HEAT TREATMENT

When enhanced corrosion resistance and mechanical properties are required, annealing can be performed at 1,200-1,400°F (649-760°C).
DAXUN Grade 7 alloy can be heat treated in a variety of ways:

  1. Anneal: 1,200-1,400°F (649-760°C), 1 to 2 hours, air cool
  2. Stress Relief Anneal: 900-1,100°F (482-593°C), 1 to 4 hours, air cool

HARDNESS

Typical hardness in the annealed condition is Rockwell B 70-80, providing excellent machinability while maintaining superior corrosion resistance.


Forgeability / Formability

Grade 7 titanium alloy bar is forged at 1,650-1,750°F (899-954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 30% reduction is recommended for optimum properties.

Grade 7 alloy bar exhibits good formability in the annealed condition. For severe forming operations such as bending or stretching, these can be performed at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000-1,200°F (538-649°C).


Kemampuan mesin

Grade 7 titanium alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids. The palladium content does not significantly affect machinability compared to other CP titanium grades.


Kemampuan las

Grade 7 titanium rod is readily weldable in the annealed condition. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. The palladium addition enhances weld integrity in corrosive environments.


Special Considerations

Grade 7 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics. The palladium content provides additional protection against corrosion in contaminated conditions.


Size Range

Grade 7 Titanium Bar Dimensions
Ø 0.7 – 30 mm (drawn, ground)
Ø 16 – 400 mm (hot rolled, peeled)
Tolerances: h11–h5 (ISO 286-2)
Tighter or different tolerances available on request
Lengths up to 9,000 mm long, depending on diameter
For larger diameters, other bar lengths and tolerances can be agreed upon request


Availability Grade 7 Titanium Rods

Processing options include:

  • Drawing, straightening
  • Drawing, straightening, polishing
  • Drawing, grinding, polishing
  • Drawing, straightening, grinding, polishing
  • Drawing, annealing, straightening
  • Drawing, annealing, polishing
  • Drawing, annealing, grinding, polishing
  • Drawing, annealing, straightening, grinding, polishing

We produce bars according to your requirements.
Excellent surface and straightness, perfect roundness and tightest diameter tolerances (according to ISO 286-2 up to h5). Available in straightened, ground, polished conditions.


Menggergaji

  • Band saws (up to Ø510 mm)
  • Bench band saws (up to 6,000 x 3,000 x 400 mm)
  • High-performance sawing machines for precise sawing

Titanium Bar End Machining

  • Single or double sided
  • Chamfer 90° (45°)
  • Point 60° (30°)
  • Flat end
  • Centered

Delivery Form

  • ASTM American Society for Testing and Materials Standards
  • AMS American Aerospace Materials Standards
  • NACE American Association of Corrosion Engineers International Standards
  • ASME American Society of Mechanical Engineers Standards
  • GB Chinese National Standards
  • GJB Chinese National Military Standards
  • ISO International Standards
  • DIN German Standards
  • EN European Standards
  • API American Petroleum Institute Standards

Detection Method

Non-destructive testing > 100% testing
Testing methods:

  • Eddy current testing / eddy current crack testing
  • Defect-free surface (level 4)
  • Flat bottom hole diameter 0.7 mm and 0.4 mm
  • Blind area can be cut off according to fixed length > Test to the end of the bar
  • Full diameter ultrasonic testing

Our Titanium Bar Material Services

As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.

We will be happy to provide you with a consultation and explain everything you need to know about obtaining Grade 7 titanium bar material, including which standards require greater attention for the components to be manufactured.

If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.

Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 7 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.


Informasi Pemesanan

Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.

Which grade of titanium is the best?

The grade of titanium alloy you need depends on the project you are working on, as each grade has different benefits.

All grades of titanium alloy are extremely strong and corrosion resistant, which means they will continue to work well in the harshest conditions.

The higher grades of titanium alloy (5-12) are alloys designed for specific benefits. For example, grade 12 titanium alloy has excellent heat resistance, making it a perfect choice for shell and tube heat exchangers, hydraulic piping, and chemical industry equipment.

Grades 1-4 are pure titanium alloys, and they are a perfect choice if you need a weldable, ductile material for piping systems and tubing. You will find lower grades used in the marine and industrial industries.

If you are starting a project and are unsure which grade of titanium alloy is best for you, contact us today; we are more than happy to help you.

How are higher grades of titanium different to the lower grades?

At DAXUN, we offer a wide range of titanium alloy grades from grade 1 to grade 12.

Grades 1-4 are pure titanium, while higher grades are alloys.

Alloy grades are popular for their high strength-to-weight ratio.

The most commonly used titanium alloy grade we find is grade 5. While still high in titanium, this grade is one of the most reliable because it can withstand temperatures up to 600°F and withstand extreme conditions.

Higher grades are favored by industries such as aerospace and marine industries for their wear and corrosion resistance.

Conversely, lower grades are primarily used for welding due to their lower strength.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

Does the grade of titanium affect the cost?

While the grade of titanium does increase the cost slightly, the total cost is primarily determined by the shape and form of titanium you require.

At DAXUN, we offer a wide range of titanium products, including plates, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

Unfortunately, it is difficult to come up with a price online without knowing much about your project and what the titanium will be used for.

Fortunately, our team of experts are always here to help and advise you on your titanium needs. By sending an email to [email protected], we will be able to get back to you with some advice and an accurate quote.

Make sure to include as much information as possible about the grade, shape and quantity of titanium you require to get a better understanding of your needs.

Where can I learn more about grades of titanium?

The team at DAXUN is experienced, knowledgeable, and friendly. With years of experience in the industry, they know all about titanium, including its uses, benefits, and grades.

For regular updates on titanium, its uses, and its applications across industries, be sure to check out our blog. Our experts have written easy-to-follow guides that you can always refer to when you have questions.

If you’re still having trouble, feel free to contact us; we’ll be happy to help.

By sending an email to [email protected], you’ll receive a quick response. Make sure to include as much detail as possible in your question so we can recommend a suitable solution.

Bagaimana cara mendapatkan penawaran atau memahami informasi pasar secepatnya?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email ([email protected]) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week

Bisakah saya mendapatkan beberapa sampel?

We can provide titanium rod samples for you to check the quality. Sample is free and you just pay the freight.

Negara mana saja yang sudah Anda ekspor?

Kami telah mengekspor ke lebih dari 42 negara, seperti Kanada, Chili, Kuwait, Jerman, Korea Selatan, Arab Saudi, Singapura, dll.

Apa MOQ Anda?

Our MOQ is 300 Kg for titanium rod.

Berapa lama waktu pengiriman Anda?

Pesanan percobaan dapat dikirim dalam waktu satu minggu. Untuk pesanan reguler, kira-kira membutuhkan waktu dua minggu.

Kirim Pertanyaan Anda Hari Ini
Kutipan Cepat