Daxun is an experienced manufacturer of CP-Grade 1 titanium plates

As China’s leading supplier of titanium and titanium alloy plates, Daxun provides high-performance titanium plates to the world.
  • Titanium plate Grade:CP-1(Kelas 1)- UNS R50250
  • Titanium plate production types: cold rolling, hot rolling, forging.
  • Titanium plate density The density of grade 1 titanium is 4.51 g/cm3
  • Standards: ASTM B265 Gr 1, ASME SB265, ASTM F67 AMS 4919
  • Features: high specific strength, light weight, corrosion resistance
  • Processing: high ductility, easy to form, easy to process

——Daxun produces titanium sheets in China to meet the diverse and demanding needs of customers!

A global leader in commercially pure titanium sheet fabrication services

DAXUN Alloys is a top global supplier of premium Grade 1 titanium plates. Grade 1 titanium offers great ductility and cold formability, perfect for deep drawing. It is also highly resistant to seawater and various solutions, including chlorides, making it a reliable choice for different environments.

Titanium’s low density, high strength-to-weight ratio, and corrosion resistance make it ideal for tough chemical environments. Commercially pure Grade 1 titanium is the softest and most ductile, offering great cold formability and top-notch corrosion resistance. It also welds easily and has good impact strength. Grade 1 titanium is also used in the aerospace industry for manufacturing airframe components due to its excellent properties.

DAXUN specializes in large and small titanium plate projects. We are your trusted partner, dedicated to providing high-quality titanium plates and ongoing technical support for your business. Our focus is on building long-term relationships through reliability and expertise.

Baca Lebih Lanjut

Technical Data Sheet

Alvac Grade ASTM B348 Grade # Chemistry N C HA HB O Fe Pd Other Elements Each Total Other Elements Ti
30 1 Weight %, maximum 0.03 0.10 0.010 0.0125 0.18 0.20 - 0.05 0.30 Bal.

Unalloyed CP titanium (Grades 1, 2, 3, and 4) generally resist crevice corrosion at temperatures below 80°C (175°F) in any pH-treated solution.

Our technical datasheet pdf provides more information about mechanical properties. If you have any concerns or need more details about our product, please contact us.

Physical Properties & Specifications

ASTM Grades I (ATI 30)

ATI 30: 1,630°F ± 25°F (888°C ± 4°C)

ASTM F 67 – Unalloyed Titanium

ISO 5832-2 – Unalloyed Titanium

Perlakuan Panas

Commercially pure titanium can be annealed by heating to 1,000 – 1,300°F (538 – 704°C) for 1/2 to 2 hours and air cooling.

Pilih Daxun untuk membantu proyek Anda berjalan.

Hubungi Daxun sekarang

Pemotongan Khusus

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • Pemotongan jet air
  • Pemotongan laser
  • Plasma cutting
  • Wire cutting
  • Bending
  • Menggorok
  • Menggergaji
Hubungi Daxun sekarang

Grade1 TItanium sheet FINISHES

#1 – Hot rolled, annealed, and descaled for applications that do not require a smooth decorative finish. #2D – Dull finish achieved through cold rolling, annealing, and descaling. Used for deep-drawn pieces and parts requiring lubricants to be kept during the shaping process.

#2B – Smooth finish achieved through cold rolling, annealing, and descaling. A light, cold rolling pass following annealing results in a brighter finish than 2D.

#BA – Cold rolled, brilliant annealed

#CBA: Coarse bright annealed cold rolled matte finish and bright annealed.

Hubungi Daxun sekarang

Produksi Lanjutan

The cold-rolled thickness range for Grade 1 Titanium Plates is 0.3 mm to 6.0 mm, while the hot-rolled range is 4.76 mm to 155 mm. These plates are produced through longitudinal and transverse rolling and are available in hot-rolled or heat-treated conditions. Over 70% of all alloy grades melted are variants of Titanium 6Al-2Sn-4Zr-6Mo, showcasing its significant application in various industries. We also offer cut blanks, allowing complex shapes to be cut from the parent plate as needed.

Hubungi Daxun sekarang

Kualitas, Inspeksi

Daxun performs a variety of quality assurance tests, including flattening, pitting resistance, mechanical, hardness, material identification, and expansion tests. These tests guarantee that the material meets the required standards for its intended application.

During the production process, we measure the diameter, thickness and surface of the product.

  • Mendukung agen pihak ketiga pelanggan untuk pergi ke pabrik untuk pemeriksaan
  • Support free samples for customer testing
  • Mendukung inspeksi pabrik di tempat atau video
Hubungi Daxun sekarang

Dukungan Teknis

Jika Anda memerlukan bantuan teknis tambahan, ahli metalurgi dan staf kami yang berpengetahuan luas akan dengan senang hati membantu. Selain itu, Daxun memiliki laboratorium pengujian bersertifikat-yang pertama dalam industri inventaris multi-logam dan plastik. Ini, menurut pendapat kami, menunjukkan dedikasi kami yang tak tergoyahkan terhadap kualitas dan filosofi kami sebagai pemasok layanan penuh.

Hubungi Daxun sekarang

Fast Delivery

We ensure timely delivery of Grade 1 titanium plates, supported by our strong production capacity, seamless information flow, and efficient logistics. Daxun’s order data is instantly integrated with our logistics system, enabling smooth coordination. Our processing center is strategically located near highways, rivers, and ports, allowing for quick scheduling, storage, and transportation. With efficient loading, we guarantee that your goods arrive on time.

We provide different way to ship our product, including FOB, CFR, CIF, DDP and DAP.

Waktu pengiriman kami benar-benar sesuai dengan kontrak.

Hubungi Daxun sekarang

Pengemasan

Daxun pays special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- Kotak dan peti
• Shrinkwrap
- Palet kayu
- Kotak kayu

Grade 1 Titanium Plate Features

Kekuatan tinggi
Ketahanan korosi
Tahan panas
Tahan suhu rendah
Perlindungan lingkungan
Ringan

Daxun Grade 1 Titanium sheet Let your brand improve rapidly

Selain produk yang tercantum di bawah ini, produk logam lain yang tersedia tidak tercantum di sini. Produk logam lain yang dapat diproduksi dan dipasok DAXUN termasuk Tantalum, Niobium, Zirkonium, Hafnium, Nikel, Tembaga, dll., Yang sebagian besar dalam bentuk Plat, Batang dan Tabung.
Standar Produk/Pemrosesan Kelas / Ukuran
Plat Titanium, Lembaran, Kumparan- ASME SB265, AMS 4911, AMS 4919, AMS 4914, ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7, GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3 (Ketebalan: (0,0197 ”-6”) Lebar Maksimum: 12 kaki, Panjang Maksimum: 50 kaki)
AMS-T-9046
Lembaran paduan Titanium dan Titanium, pelat
Titanium murni komersial (CP)
Penunjukan kode Kekuatan luluh
minimum, ksi 1 /
CP-1 70
CP-2 55
CP-3 40
CP-4 25
Paduan titanium alfa (A)
Penunjukan kode Komposisi
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn (ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
Paduan titanium alfa-beta (AB)
Penunjukan kode Komposisi
AB-1 6A1-4V
AB-2 6A1-4V (ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
Paduan titanium beta (B)
Penunjukan kode Komposisi
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
Pemrosesan:
Penggulungan Panas Penggulungan Dingin
Nilai yang Tersedia:
CP Kelas 1 Kelas 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP Kelas 2 Kelas 6Al-4V ELI (Sebelumnya Kelas 23)
Kelas 7 Kelas 6Al-6V-2Sn (6-62)
Kelas 19 Kelas 8Al-1Mo-1V (8-1-1)
Kelas 5 (6Al-4V) Kelas 9 (3Al-2.5V)
Kelas 6 (5Al-2.5Sn) CP Kelas 3
Aplikasi
Industri Kimia Desalinasi Air Laut
Industri Petrokimia Dirgantara
Bidang Permesinan, Bidang Otomotif Bidang Komponen Telepon Seluler.

Daxun is a professional manufacturer committed to high-quality products. We ensure all our titanium plates meet international standards. This includes certifications from ISO9001, SGS, CE, and OQC. Our strict quality control process minimizes defects.

Proyek dan produk hot case terbaru

Grade 1 Titanium Plate and sheet
Listrik nuklir
Grade 1 Titanium Plate and sheet
Dirgantara
Plat dan lembaran Titanium
Bahan kimia
Plat dan lembaran Titanium
Bejana Tekan
Plat dan lembaran Titanium
Industri energi baru
Plat dan lembaran Titanium
Teknik Kelautan
Plat dan lembaran Titanium
Desalinasi
Plat dan lembaran Titanium
Industri Tenaga Listrik
Plat dan lembaran Titanium
Energi Fotovoltaik
Titanium plate and sheet Grade 1 

We specialize in pure titanium plates. Our products serve both the industrial and aerospace sectors. We excel in meeting customer needs. Our clients trust our capabilities. We consistently deliver the products they require.

DAXUN has always worked with overseas clients. We have strong ties to global titanium industry leaders. Our technology ensures high-quality materials. We meet specific project needs.

We have established supply chains and maintain research laboratories. Alpha-beta alloys, such as Ti 6Al-4V, are heat-treatable and extensively used in various industries, including aerospace and marine applications. We operate through subsidiaries to ensure top-quality production. We adapt to any specific product request. Every order receives our full attention. Quality is our priority from start to finish.

DAXUN values customer service highly. It’s a key part of our business. We provide clear information to customers. Our pricing is comprehensive. We interact closely with our customers and answer their technical questions. Our support goes beyond the product itself.

When you buy from us, you get more. You receive raw materials, of course. But you also get excellent service.

Titanium Plate and sheet Grade 1 Data sheet

ASTM B265 | ASME SB265 | ASTM F67 | ISO 5832-2 | 3.7025 | UNS R50250

Grade 1 pure titanium sheet is highly ductile. It has excellent cold formability, making it ideal for deep drawing. Grade 1 titanium resists corrosion well. It stands up to general corrosion. It also withstands seawater corrosion. The material resists oxidizing media. It handles neutral solutions too. Even mildly reducing media, like chlorides.

Titanium has a low density. It’s about half as dense as nickel-based alloys. Titanium offers a high strength-to-weight ratio. Its corrosion resistance is remarkable.

These properties make titanium versatile. It performs well in harsh chemical conditions. Many industries choose it for demanding applications.

Grade 1 Titanium Plate Features and Corrosion Resistance

High ductility;
Good cold formability and impact strength;
Medium strength;
High corrosion resistance and notched impact strength;
Excellent biocompatibility;
Very easy to weld and not magnetic.

Which grade of titanium is the best?

The grade of titanium alloy you need depends on the project you are working on, as each grade has different benefits.

All grades of titanium alloy are extremely strong and corrosion-resistant, which means they will continue to work well even in the harshest conditions.

The higher grades of titanium alloy (5-12) are alloys designed for specific benefits. It also knows as beta alloyes for different usage like metal support in human body. For example, grade 12 titanium alloy has excellent heat resistance, making it a perfect choice for shell and tube heat exchangers, hydraulic piping, and chemical industry equipment.

Grades 1-4 are pure titanium grades, and they are a perfect choice if you need a weldable, ductile material for piping systems and tubing.

When considerding titanium grades, the common physcial properties are heat treatment, fracture toughness, thermal conductivity, mechanical properties, tensile strength and yield strength. Also, we need to understand application to help you to archive your goal.

If you are starting a project and are unsure which grade is best for you, contact us now; we are more than happy to help you.

How are higher grades of titanium different from the lower grades?

Titanium Gerades as known as commercially pure titanium and titanium alloys grade level.

At DAXUN, we offer a wide range of titanium alloy grades from grade 1 to grade 18.

Grades 1-4 are pure titanium, while higher grades are alloys. Alloy grades are popular for their high strength-to-weight ratio.

The most commonly used titanium alloy grades is grade 5 (ti 6al 4v). From grade 5, it combines with different metals together, like aluminum and iron. These excellent combination extends the excellent weldability and high temperature creep strength.

Higher grades are favored by industries such as aerospace and marine industries for their wear and corrosion resistance.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

Does the grade of titanium affect the cost?

While the grade of titanium does increase the cost slightly, the total cost is primarily determined by the shape and form of titanium you require.

At DAXUN, we offer all sorts of titanium products, including plates, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

It is difficult to offer a price online without knowing much about your project and what the metal will be used for.

But don’t worry. Our team is always here to help with your titanium needs. By sending an email to us, we will be able to get back to you with some advice and an accurate quote. Make sure to include as much information as possible about your needs.

Where can I learn more about the grades of titanium?

The team at DAXUN is experienced, knowledgeable, and friendly. With years of experience in the industry, they know all about titanium, including its uses, benefits, and grades.

For regular updates on titanium, its uses, and its applications across industries, be sure to check out our blog. Our experts have written easy-to-follow posts that you can always refer to.

By sending an email to [email protected], you’ll receive a quick response.

Bagaimana cara mendapatkan penawaran atau memahami informasi pasar secepatnya?

Silakan isi formulir di halaman “Hubungi Kami”, atau hubungi manajer penjualan kami di “+86 13382898899”, kami akan menghubungi Anda sesegera mungkin. WhatsApp kami sedang online, dan email ([email protected]) akan diperiksa dalam waktu 6 jam. Setiap pertanyaan atau pesan akan ditanggapi dengan segera. Selain itu, kami membagikan informasi pasar kepada pelanggan kami setiap minggu.

Bisakah saya mendapatkan beberapa sampel?

We can provide Titanium sheet samples for you to check the quality. The sample is free and you just pay the freight. Contact us for more details and we are happy to make you a special offer.

Apa MOQ Anda?

MOQ is 1 ton for the Titanium sheet.

Overview of Titanium Alloys

Titanium alloys are a blend of titanium and other chemical elements, designed to offer exceptional tensile strength and toughness, even under extreme temperatures. These alloys are lightweight, exhibit extraordinary corrosion resistance, and can endure high temperatures, making them indispensable in various industries. From aerospace and aircraft to medical devices and jewelry, titanium alloys are integral to many high-stress applications.

Commercially pure titanium, known for its acceptable mechanical properties, is often used in orthopedic and dental implants. The most common titanium alloy, Ti 6Al 4V, includes small amounts of aluminum and vanadium (6% and 4% by weight, respectively). This combination allows for precipitation strengthening, enhancing the alloy’s mechanical properties. Whether in the form of alpha alloys, beta alloys, or alpha-beta alloys, titanium alloys continue to be a cornerstone in industries requiring materials that offer both strength and corrosion resistance.

Kutipan Cepat