x
Sorgunuzu Bugün Gönderin
Hızlı Alıntı

Grade 12 Ti-0.3Mo-0.8Ni Alloy Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:12. Sınıf - UNS R53400
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of grade 12 titanium is approximately 4.51 g/cm3
  • Standards:ASTM B338、ASTM B861
  • Softest Ti,High ductility, Very corrosion resistant, good cold formability

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

Grade 12 Titanium Alloy Pipe Manufacturer - Daxun Alloy

Provide High Quality Grade 12 Titanium Pipe to Customers Around The World
Grade 12 titanium pipe is a specialized tubing made from Ti-0.3Mo-0.8Ni titanium alloy, which belongs to a specific grade in the titanium alloy pipe family. This material is created by adding 0.3% molybdenum and 0.8% nickel to pure titanium, significantly enhancing its corrosion resistance, particularly in acidic environments and chloride media. Grade 12 titanium pipe complies with international standards such as ASTM B338 or ASTM B861, featuring a density of approximately 4.51 g/cm³, tensile strength of about 483 MPa, and yield strength of around 345 MPa, while maintaining the lightweight characteristics typical of titanium materials.

Where is Grade 12 titanium pipe used?
Compared to pure titanium, Grade 12 titanium pipe offers superior resistance to crevice corrosion and stress corrosion cracking, making it particularly suitable for chemical processing equipment, heat exchangers, oil and gas industries, and seawater treatment systems. This material provides longer service life and lower maintenance costs while maintaining excellent mechanical properties, making it highly favored in high-end industrial applications and an ideal choice for handling corrosive fluids.
Chemical processing plants utilize it for heat exchangers, reactor vessels, and piping systems handling aggressive acids and chlorides. Marine and offshore installations employ it in seawater cooling systems, desalination equipment, and subsea components, leveraging its exceptional resistance to saltwater corrosion and biofouling. In the oil and gas sector, it serves in downhole tubing, Christmas tree components, and production equipment exposed to sour environments with H₂S and CO₂. Power generation facilities specify Grade 12 titanium for condenser tubes and heat exchangers in cooling systems, while industrial pollution control systems incorporate it in scrubbers and flue gas desulfurization units that handle corrosive gases and acidic condensates.

Key Performance

Strength-Ductility Balance:

  • Tensile Strength: 483 MPa (annealed state) – Matches Grade 2 but with superior corrosion resistance.
  • Yield Strength: 345 MPa (min) – Exceeds Grade 2 (275 MPa), suitable for pressure-containing components.
  • Elongation: 18% (min) – Exceptional ductility for cold forming, flaring, and high fatigue resistance.
  • Density: 4.51 g/cm³ – 60% lighter than steel, ideal for weight-sensitive applications.

Corrosion Resistance:

  • Core Mechanism: Synergistic effect of Molybdenum (0.3%) and Nickel (0.8%) stabilizes the passive oxide layer.
  • Pitting/Crevice Corrosion Resistance:
    • Outstanding performance in seawater, chloride solutions (e.g., NaCl, MgCl₂), and sour gas (H₂S) environments.
    • Resists reducing acids (e.g., H₂SO₄, HCl) where stainless steels fail.
  • Advantages vs. Other Grades:
    • Outperforms Grade 2 in reducing acids and chlorides.
    • Superior to Grade 9 in high-temperature acidic media (e.g., chemical processing).
    • Immune to corrosion in oxidizing media (e.g., HNO₃) and aggressive chemical environments.
  • Optimal Heat Treatment: Annealed at 595°C to maximize corrosion resistance and ductility.
Daha fazla bilgi edinin

Veri

Element Minimum (%) Maximum (%)
Titanium (Ti) Denge Denge
Molibden (Mo) 0.25 0.40
Nikel (Ni) 0.60 0.90
Demir (Fe) 0.30
Oxygen (O) 0.25
Carbon © 0.08
Azot (N) 0.03
Hydrogen (H) 0.015
Diğer Unsurlar 0.40 (total)
Mülkiyet Value/Range Unit
Yoğunluk 4.48 g/cm³
Erime Noktası 1650 ± 20 °C
Termal İletkenlik 7.2 (at 25°C) W/m·K
Specific Heat 560 (at 25°C) J/kg·K
Elektriksel Dirençlilik 1.7 μΩ·m
Manyetik Duyarlılık Paramagnetic
Mülkiyet Minimum Requirement Typical Value Unit Test Method
Çekme Dayanımı 483 520–620 MPa ASTM E8/E8M
Yield Strength (0.2% offset) 345 380–480 MPa ASTM E8/E8M
Uzama 18 22–30 % ASTM E8/E8M
Sertlik ≤ 200 (HV) 150–180 (HV) Vickers ASTM E10
Impact Toughness Not specified 40–60 J ASTM E23

Elevated Temperature Performance

Temperature (°C) Çekme Dayanımı (MPa) Yield Strength (MPa) Uzama (%)
100 450–500 320–370 20–25
200 400–450 280–330 18–23
300 350–400 240–290 15–20

 

Projenizin yükselmesine yardımcı olmak için Daxun'u seçin.

Daxun ile şimdi iletişime geçin

Advanced Production:Titanium seamless pipe

  • Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.
  • (The above is agreed upon by the manufacturer and the customer based on the specific situation)
Daxun ile şimdi iletişime geçin

Grade 12 Titanium Tube Features

Grade 12 Titanium Tube is the softest form of titanium and has the highest ductility. It has good cold forming characteristics and offers excellent corrosion resistance. It also has excellent welding properties and high impact toughness.

  • Softest Titanium
  • Highest Ductility
  • Excellent Corrosion Resistance
  • Good Cold Formability
Daxun ile şimdi iletişime geçin

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

Daxun ile şimdi iletişime geçin

Test Raporları

The test reports we provide include: Factory test certificate for Grade 12 titanium welded pipe and Grade 12 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

Daxun ile şimdi iletişime geçin

Applications and standards

Titanium Grade 12 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
Daxun ile şimdi iletişime geçin

Kalite, teslimat, denetim

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 12 Titanium Welded Pipe and Grade 12 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • Teslimat süremiz kesinlikle sözleşmeye uygundur.
  • Müşterinin üçüncü taraf acentelerinin denetim için fabrikaya gitmesine destek olun
  • Müşteri testleri için ücretsiz numune desteği
  • Yerinde veya video fabrika denetimini destekleyin
Daxun ile şimdi iletişime geçin

Paketleme

Daxun Alloy, malların nihai varış noktasına ulaşmak için çeşitli kanallardan geçtiği uluslararası taşımacılıkta önemli bir rol oynadığı için en iyi ambalaj kalitesini sağlar, bu nedenle ambalajlamaya özel önem veririz. Ürünlerimizi ürüne bağlı olarak birçok şekilde paketliyoruz. Ürünlerimizi aşağıdaki gibi birçok şekilde paketliyoruz:
- Kutular ve kasalar
- Shrink ambalaj
- Ahşap paletler
- Ahşap kutular

Daxun ile şimdi iletişime geçin

Teknik Destek

Herhangi bir ek teknik yardıma ihtiyacınız olursa, yerleşik metalürji uzmanımız ve bilgili personelimiz size yardımcı olmaktan memnuniyet duyacaktır. Ayrıca Daxun, çoklu metal ve plastik envanter endüstrisinde bir ilk olan sertifikalı bir test laboratuvarına sahiptir. Bu, bize göre, kaliteye olan sarsılmaz bağlılığımızı ve tam hizmet tedarikçisi olarak felsefemizi göstermektedir.

Daxun Grade 12 Titanium TUBE Let your brand improve rapidly

Grade 12 titanium tube form (4)

  • Titanium seamless tubes are made by piercing and drawing solid titanium bars, and the hollow part of the tube is made by piercing or hot extrusion. Titanium seamless tubes are ideal for very large diameter to wall thickness ratios and have very good external dimensional tolerances.

  • Titanium welded pipe is a tubular product made of strip titanium that is roll formed and fusion welded along the longitudinal seam. The welding process used by Daxun Alloy does not use any filler metal during the welding process.

  • Titanium square tubes are drawn from round tubes or round tube billets and can be formed into right angles or rounded corners. They can also be cold extruded, which is efficient and low cost. The only disadvantage is that the tolerance will gradually increase.

  • Tubular products are welded and then re-drawn to final size. Welding and drawing is ideal for producing thick walled, large diameter tubes that cannot be welded directly to size but still offer cost savings over seamless tubes. All Daxun welded and drawn tubes are bright annealed.

Güncel sıcak vaka projeleri ve ürünleri

Grade 12 Titanium pipe and tube
Grade 12 Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
Hangi titanyum sınıfı en iyisidir?

İhtiyacınız olan titanyum alaşımı sınıfı, üzerinde çalıştığınız projeye bağlıdır, çünkü her sınıfın farklı faydaları vardır.

Titanyum alaşımının tüm sınıfları son derece güçlü ve korozyona dayanıklıdır, bu da en zorlu koşullarda bile iyi çalışmaya devam edecekleri anlamına gelir.

Titanyum alaşımının daha yüksek dereceleri (5-12) belirli faydalar için tasarlanmış alaşımlardır. Örneğin, 12. sınıf titanyum alaşımı mükemmel ısı direncine sahiptir, bu da onu kabuk ve borulu ısı eşanjörleri, hidrolik borular ve kimya endüstrisi ekipmanları için mükemmel bir seçim haline getirir.

1-4. Sınıflar saf titanyum alaşımlarıdır ve boru sistemleri ve borular için kaynaklanabilir, sünek bir malzemeye ihtiyacınız varsa mükemmel bir seçimdir. Denizcilik ve endüstriyel endüstrilerde kullanılan daha düşük kaliteler bulacaksınız.

Bir projeye başlıyorsanız ve hangi titanyum alaşımının sizin için en iyisi olduğundan emin değilseniz, bugün bizimle iletişime geçin; size yardımcı olmaktan mutluluk duyarız.

Daha yüksek titanyum sınıfları daha düşük sınıflardan nasıl farklıdır?

DAXUN'da, 1. sınıftan 12. sınıfa kadar çok çeşitli titanyum alaşım kaliteleri sunuyoruz.

1-4. sınıflar saf titanyumdur, daha yüksek sınıflar ise alaşımlardır.

Alaşım kaliteleri, yüksek mukavemet/ağırlık oranları nedeniyle popülerdir.

Bulduğumuz en yaygın kullanılan titanyum alaşım sınıfı 5. sınıftır. Titanyum oranı hala yüksek olsa da, bu sınıf en güvenilir olanlardan biridir çünkü 600 ° F'ye kadar sıcaklıklara dayanabilir ve aşırı koşullara dayanabilir.

Daha yüksek kaliteler, aşınma ve korozyon dirençleri nedeniyle havacılık ve denizcilik endüstrileri gibi endüstriler tarafından tercih edilmektedir.

Buna karşılık, daha düşük kaliteler daha düşük mukavemetleri nedeniyle öncelikle kaynak için kullanılır.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

Titanyum sınıfı maliyeti etkiler mi?

Titanyum sınıfı maliyeti biraz artırsa da, toplam maliyet öncelikle ihtiyacınız olan titanyum şekli ve formu tarafından belirlenir.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

Ne yazık ki, projeniz ve titanyumun ne için kullanılacağı hakkında çok fazla bilgi sahibi olmadan çevrimiçi bir fiyat bulmak zordur.

Neyse ki, uzman ekibimiz titanyum ihtiyaçlarınız konusunda size yardımcı olmak ve tavsiyelerde bulunmak için her zaman burada. [email protected] adresine bir e-posta göndererek, size bazı tavsiyeler ve doğru bir fiyat teklifi ile geri dönebileceğiz.

İhtiyaçlarınızı daha iyi anlamak için ihtiyacınız olan titanyum sınıfı, şekli ve miktarı hakkında mümkün olduğunca fazla bilgi eklediğinizden emin olun.

Titanyum kaliteleri hakkında daha fazla bilgiyi nereden edinebilirim?

DAXUN'daki ekip deneyimli, bilgili ve arkadaş canlısıdır. Sektördeki yılların tecrübesiyle, kullanımları, faydaları ve kaliteleri de dahil olmak üzere titanyum hakkında her şeyi biliyorlar.

Titanyum, kullanım alanları ve sektörlerdeki uygulamaları hakkında düzenli güncellemeler için blogumuza göz atmayı unutmayın. Uzmanlarımız, sorularınız olduğunda her zaman başvurabileceğiniz, takip etmesi kolay kılavuzlar yazdı.

Hala sorun yaşıyorsanız, bizimle iletişime geçmekten çekinmeyin; size yardımcı olmaktan memnuniyet duyarız.

[email protected] adresine bir e-posta göndererek hızlı bir yanıt alabilirsiniz. Uygun bir çözüm önerebilmemiz için sorunuza mümkün olduğunca fazla ayrıntı eklediğinizden emin olun.

Fiyat teklifi nasıl alınır veya piyasa bilgileri en kısa sürede nasıl anlaşılır?

Lütfen “Bize Ulaşın” sayfasındaki formu doldurun veya “+86 13382898899” adresinden satış müdürümüzü arayın, en kısa sürede sizinle iletişime geçeceğiz. WhatsApp'ımız çevrimiçidir ve e-posta ([email protected]) 6 saat içinde kontrol edilecektir. Her soruya veya mesaja derhal yanıt verilecektir. Ayrıca, her hafta müşterilerimizle pazar bilgilerini paylaşıyoruz

Biraz örnek alabilir miyim?

Kaliteyi kontrol etmeniz için paslanmaz çelik sac örnekleri sağlayabiliriz. Numune ücretsizdir ve siz sadece navlunu ödersiniz.

Şimdiye kadar hangi ülkelere ihracat yaptınız?

Kanada, Şili, Kuveyt, Almanya, Güney Kore, Suudi Arabistan, Singapur gibi 42'den fazla ülkeye ihracat yaptık.

MOQ'unuz nedir?

Paslanmaz çelik sac için MOQ'umuz 1 tondur.

Teslimat süreniz ne kadar?

Deneme siparişleri bir hafta içinde teslim edilebilir. Normal siparişler için bu süre yaklaşık iki haftadır.

Sorgunuzu Bugün Gönderin
Hızlı Alıntı