Daxun is an excellent manufacturer of grade 12 (Ti-0.3Mo-0.8Ni) titanium rods and bars.
- Titanium bar grade: Grade 12-Ti / UNS R53400
- Titanyum çubuk türleri: haddelenmiş çubuklar, çekilmiş çubuklar, dövme titanyum çubuklar
- Titanium bar density: The density of grade 12 titanium is 4.51 g/cm³
- Ana standartlar: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, vb.
- High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.
Ticari olarak saf titanyum çubuk üretim hizmetlerinde dünya lideri
Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 12 titanium alloy rods.
Grade 12 titanium bar (Ti Grade 12 / UNS R53400) is a nickel-molybdenum-enhanced, commercially pure (CP) titanium alloy specifically engineered for superior corrosion resistance in aggressive environments. It consists of titanium (≥99%) with strategic additions of 0.6–0.9% nickel (Ni) and 0.2–0.4% molybdenum (Mo), which significantly enhances its electrochemical properties. This nickel-molybdenum modification substantially improves resistance to reducing acids (e.g., sulfuric, hydrochloric, phosphoric), chloride solutions (including seawater and brines), and crevice corrosion—conditions where standard CP grades like Grade 2 would exhibit accelerated degradation. While maintaining the inherent advantages of titanium—low density (~4.5 g/cm³), high strength-to-weight ratio, excellent weldability, and biocompatibility—Grade 12 offers enhanced performance at elevated temperatures (up to ~315°C/600°F) and in moderately reducing or acidic environments. Its passive oxide layer, reinforced by the nickel-molybdenum combination, provides exceptional protection against chemical attack, making it one of the most cost-effective corrosion-resistant metallic materials available.
Where is Grade 12 titanium bar used?
Grade 12 titanium bar is widely utilized in chemical processing for essential components such as heat exchangers, piping systems, vessel linings, and agitators handling acids, chlorides, or organic compounds. In marine and offshore applications, it serves in seawater desalination plants, condenser tubing, and offshore platform components exposed to high-salinity conditions. The alloy also performs exceptionally well in oil and gas production equipment, pulp and paper processing machinery, and power generation systems due to its durability and corrosion resistance. Despite its moderate premium over standard grades—justified by its alloying elements—Grade 12 delivers outstanding lifecycle value by reducing maintenance requirements, extending service intervals, and minimizing replacement costs in corrosive service. Its reliability in preventing premature failures ensures operational continuity and cost efficiency in applications ranging from chemical processing plants to marine infrastructure, establishing it as an optimal solution for demanding corrosion challenges where budget constraints exist.
Daxun güvenilir titanyum alaşımlı çubuk üretim şirketinizdir. Daxun, ticari olarak saf titanyum serisi CP, titanyum alaşım serisi, titanyum nikel alaşımı vb. dahil olmak üzere tüm titanyum alaşımlarını üretir. Güvenilir performansa sahiptirler ve kritik uygulamalarınız için yüksek performans sağlarlar. Çeşitli endüstrilerde ve uygulamalarda, yüksek mukavemet, yüksek sıcaklık ve aşındırıcı ortamlar için Daxun titanyum alaşımlı çubuklara güvenebilirsiniz. Daxun Metals, onlarca yıldır en zorlu zorlukların üstesinden gelmek için yüksek mühendislik ürünü titanyum alaşımlı çözümler üretmeye kendini adamıştır.
Veri
- Parametre
- Malzeme
- Mekanik Özellikler
- Fiziksel Özellikler
| Şartname | Detaylar |
|---|---|
| Malzeme | Titanium rod and bar Grade 12 (UNS R53400) |
| Standart | ASTM B348, ASTM SB348, AMS 4921, AMS 4902 |
| Boyutlar | EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN |
| Çap Aralığı | 0.125″ – 14″ (3.175mm – 355.6mm), custom |
| Uzunluk Aralığı | Up to 240″ (6096mm), custom |
| Bitirmek | Cold (bright) drawn, centerless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centerless Ground & Black |
| Yüzey İşlemi | Soğuk çekilmiş, Puntasız Taşlanmış, Cilalı veya Kaba Tornalanmış, Siyah, NO.4 Kaplama, BA Kaplama, Mat Kaplama, vb. |
| Durum | Sertleştirilmiş ve temperlenmiş, tavlanmış |
| Hoşgörü | Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm) |
| Form | Titanyum kare çubuklar, titanyum külçeler, titanyum yuvarlak çubuklar, dikdörtgen titanyum çubuklar, üçgen titanyum çubuklar, dövme titanyum çubuklar, titanyum altıgen çubuklar vb. |
| Element | Minimum (%) |
Maximum (%)
|
| Titanium (Ti) | Denge | Denge |
| Molibden (Mo) | 0.25 | 0.4 |
| Nikel (Ni) | 0.6 | 0.9 |
| Demir (Fe) | — | 0.3 |
| Oxygen (O) | — | 0.25 |
| Carbon © | — | 0.08 |
| Azot (N) | — | 0.03 |
| Hydrogen (H) | — | 0.015 |
| Diğer Unsurlar | — | 0.40 (total) |
| Mülkiyet | Minimum Requirement | Typical Value | Unit | Test Method |
| Çekme Dayanımı | 483 | 520–620 | MPa |
ASTM E8/E8M
|
| Yield Strength (0.2% offset) | 345 | 380–480 | MPa |
ASTM E8/E8M
|
| Uzama | 18 | 22–30 | % |
ASTM E8/E8M
|
| Sertlik | ≤ 200 (HV) | 150–180 (HV) | Vickers | ASTM E10 |
| Impact Toughness | Not specified | 40–60 | J | ASTM E23 |
Elevated Temperature Performance
|
Temperature (°C)
|
Çekme Dayanımı (MPa) | Yield Strength (MPa) |
Uzama (%)
|
| 100 | 450–500 | 320–370 | 20–25 |
| 200 | 400–450 | 280–330 | 18–23 |
| 300 | 350–400 | 240–290 | 15–20 |
| Mülkiyet | Value/Range | Unit |
| Yoğunluk | 4.48 | g/cm³ |
| Erime Noktası | 1650 ± 20 | °C |
| Termal İletkenlik | 7.2 (at 25°C) | W/m·K |
| Specific Heat | 560 (at 25°C) | J/kg·K |
| Elektriksel Dirençlilik | 1.7 | μΩ·m |
| Manyetik Duyarlılık | Paramagnetic | — |
Projenizin yükselmesine yardımcı olmak için Daxun'u seçin.
DAXUN® Grade 12 Titanium Rod Features
DAXUN® Ti Grade 5, titanyum alaşımlı bir çubuktur (6al-4v):
- İyi sıcak şekillendirilebilirlik ve kaynaklanabilirlik;
- Çekme mukavemeti 1000MPa'ya ulaşabilir;
- Yüksek sıcaklıkta boyutsal çalışma
- Deniz suyuna veya deniz suyuna karşı duyarsız;
- Çeşitli korozif ortamlardan etkilenmez;
- Yüksek mukavemet ve iyi tokluk;
- Çatlak başlangıcına ve çatlak ilerlemesine karşı dirençlidir.
Daxun Fabrika Avantajları
Daxun'un “Performans Mükemmelliği Yönetimi” konsepti “PDCA + Yalın” yönetim modelini teşvik etmektedir. Şirketin kartvizitinde “Daxun = Güvenilir Kalite” yazmaktadır. Daxun, her titanyum çubuğun çeşidinin, özelliklerinin ve kökeninin tam izlenebilirliğini sağlamak için ERP sistemini kullanır ve endüstride sahteciliğin önlenmesini savunur ve teşvik eder. Daxun, işleme ve özelleştirme için teknolojiye güvenir ve yüksek hassasiyet ve yüksek kalite sektörün ölçütleridir; hizmet açısından, ürün yaşam döngüsü yönetimini teşvik eder, satış öncesi profesyonel malzeme seçimi ve işleme çözümleri sağlar, satış sırasında sıkı bir şekilde izler ve satış sonrası endişesiz hizmet garantileri sağlar.
Grade 12 Titanium Rod Production Method
Daxun, yüksek performanslı yüksek kaliteli titanyum çubuklar üretir ve ayrıca müşterinin anlaşmasına göre üretim yapabilir:
- Titanyum külçelerin ısıl işlem ve işleme, daldırma ultrasonik test, mekanik özellik testi, makroskopik ve mikroskopik yapısal inceleme ve diğer işlemlerden geçmesi gerekir. Üretim süreci: sıcak haddelenmiş titanyum çubuklar - yüksek verimlilik, istikrarlı performans, dövme titanyum çubuklar - esnek boyut, çoklu ateş dövme, titanyum çubukların kapsamlı performansını artırır, soğuk çekilmiş titanyum çubuklar - genellikle küçük boyutlu yüksek hassasiyetli titanyum çubuklar; Yukarıdaki titanyum çubukların tümü parlak yüzeyli olarak teslim edilir.
Test Raporları
Sağladığımız test raporları şunları içerir: Sınıf 2 Titanyum Çubuk ve Sınıf 2 Titanyum Yuvarlak Çubuk Fabrika Test Sertifikası, EN 10204 3.1, Kimyasal Rapor, Mekanik Rapor, PMI Test Raporu, Görsel Muayene Raporu, Üçüncü Taraf Muayene Raporu, NABL Onaylı Laboratuvar Raporu, Tahribatlı Test Raporu, Tahribatsız Muayene Raporu. (Daxun müşteri ihtiyaçlarına göre sağlayacaktır)
Grade 12 Rods Applications and Standards
Grade 12 Titanium Rods are widely used in the following industries under extreme corrosive conditions:
- Havacılık ve uzay, gemi yapımı, petrol ve gaz endüstrisi, deniz mühendisliği, kimyasal tesisler, endüstriyel makineler, enerji endüstrisi, kağıt ve kağıt hamuru endüstrisi, gıda işleme endüstrisi, rafineriler, askeri endüstri, ilaç ve gıda işleme ekipmanları vb.
- Teknik Özellikler: AMS 4928, AMS 4967, AMS 4965, AMS 6931, ASTM B 348
- Standartlar: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
Kalite, teslimat, denetim
Daxun çeşitli kalite güvence testleri gerçekleştirir, bu testler alan çekme, kimyasal analiz, malzeme pozitif tanımlama - PMI testi, mikro ve makro testler, taneler arası korozyon (IGC) testi, ultrasonik hata tespit testi, çukurlaşma ve direnç testi, sertlik testi, malzeme pozitif tanımlama, genleşme testi vb. gibi mekanik testleri içerir. Tüm bu testler, Grade 2 Titanyum Çubuk ve Grade 2 Titanyum Yuvarlak Çubuk malzemesinin gerekli uygulama için uygun olmasını sağlar. Üretim sürecinde ürünün çapını, kalınlığını ve yüzeyini ölçüyoruz.
- Teslimat süremiz kesinlikle sözleşmeye uygundur.
- Müşterinin üçüncü taraf acentelerinin denetim için fabrikaya gitmesine destek olun
- Müşteri testleri için ücretsiz numune desteği
- Yerinde veya video fabrika denetimini destekleyin
Paketleme
Daxun Alloy, malların nihai varış noktasına ulaşmak için çeşitli kanallardan geçtiği uluslararası taşımacılıkta önemli bir rol oynadığı için en iyi ambalaj kalitesini sağlar, bu nedenle ambalajlamaya özel önem veririz. Ürünlerimizi ürüne bağlı olarak birçok şekilde paketliyoruz. Ürünlerimizi aşağıdaki gibi birçok şekilde paketliyoruz:
- Kutular ve kasalar
- Shrink ambalaj
- Ahşap paletler
- Ahşap kutular
Teknik Destek
Herhangi bir ek teknik yardıma ihtiyacınız olursa, yerleşik metalürji uzmanımız ve bilgili personelimiz size yardımcı olmaktan memnuniyet duyacaktır. Ayrıca Daxun, çoklu metal ve plastik envanter endüstrisinde bir ilk olan sertifikalı bir test laboratuvarına sahiptir. Bu, bize göre, kaliteye olan sarsılmaz bağlılığımızı ve tam hizmet tedarikçisi olarak felsefemizi göstermektedir.
Daxun Grade 12 Titanium Rods help your brand improve quickly
- Tolerances for Grade 12 Titanium Round Bars (BS EN ISO 286-2)
| NOMİNAL BOYUT | h5 | h6 | h7 | h8 | h9 | H10 | H11 | h12 |
|---|---|---|---|---|---|---|---|---|
| ÇAP mm | ||||||||
| ~ 3'e kadar | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| 3 ila 6 yaş üstü | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| 6'dan 10'a kadar | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| 10 ila 18 yaş üstü | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| 18 ila 30 yaş üstü | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| 30'dan 50'ye kadar | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| 50'den 80'e kadar | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| 80'den 120'ye kadar | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| 120'den 180'e kadar | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| 180'den 250'ye kadar | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
Types of Grade 12 Titanium Rods (3)
Titanyum çubuk
Güncel sıcak vaka projeleri ve ürünleri
İlgili Ürünler (8)
Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 12 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.
ÖZELLİKLER
ASTM B348 – Titanium and Titanium Alloy Bars and Billets
ASTM SB348 – Specification for Titanium and Titanium Alloy Bars and Billets
AMS 4921 – Titanium Alloy Bars, Wire, and Forgings
AMS 4924 – Titanium Alloy Bars and Billets, Grade 12
ISI TEDAVİSİ
When enhanced corrosion resistance and mechanical properties are required, annealing can be performed at 1,200-1,400°F (649-760°C).
DAXUN Grade 12 alloy can be heat treated in a variety of ways:
- Anneal: 1,200-1,400°F (649-760°C), 1 to 2 hours, air cool
- Stress Relief Anneal: 900-1,100°F (482-593°C), 1 to 4 hours, air cool
SERTLİK
Typical hardness in the annealed condition is Rockwell B 70-80, providing excellent machinability while maintaining superior corrosion resistance.
Forgeability / Formability
Grade 12 titanium alloy bar is forged at 1,650-1,750°F (899-954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 30% reduction is recommended for optimum properties.
Grade 12 alloy bar exhibits good formability in the annealed condition. For severe forming operations such as bending or stretching, these can be performed at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000-1,200°F (538-649°C).
İşlenebilirlik
Grade 12 titanium alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids. The nickel-molybdenum content does not significantly affect machinability compared to other CP titanium grades.
Kaynaklanabilirlik
Grade 12 titanium rod is readily weldable in the annealed condition. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. The nickel-molybdenum addition enhances weld integrity in corrosive environments.
Özel Hususlar
Grade 12 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics. The nickel-molybdenum content provides additional protection against corrosion in contaminated conditions.
Size Range
Grade 12 Titanium Bar Dimensions
Ø 0.7 – 30 mm (drawn, ground)
Ø 16 - 400 mm (sıcak haddelenmiş, soyulmuş)
Tolerances: h11–h5 (ISO 286-2)
İstek üzerine daha sıkı veya farklı toleranslar mevcuttur
Çapa bağlı olarak 9.000 mm'ye kadar uzunluklar
Daha büyük çaplar için, diğer çubuk uzunlukları ve toleransları talep üzerine kabul edilebilir
Availability Grade 7 Titanium Rods
Processing options include:
- Çizim, düzleştirme
- Çizim, düzeltme, parlatma
- Çizim, taşlama, parlatma
- Çekme, doğrultma, taşlama, parlatma
- Çekme, tavlama, doğrultma
- Çekme, tavlama, parlatma
- Çekme, tavlama, taşlama, parlatma
- Çekme, tavlama, doğrultma, taşlama, parlatma
İhtiyaçlarınıza göre çubuklar üretiyoruz.
Mükemmel yüzey ve düzlük, mükemmel yuvarlaklık ve en sıkı çap toleransları (ISO 286-2'ye göre h5'e kadar). Düzleştirilmiş, taşlanmış, parlatılmış olarak mevcuttur.
Testere
- Şerit testereler (Ø510 mm'ye kadar)
- Bench band saws (up to 6,000 x 3,000 x 400 mm)
- Hassas kesim için yüksek performanslı testere makineleri
Titanium Bar End Machining
- Tek veya çift taraflı
- Pah 90° (45°)
- Nokta 60° (30°)
- Düz uç
- Merkezlenmiş
Delivery Form
- ASTM American Society for Testing and Materials Standards
- AMS American Aerospace Materials Standards
- NACE American Association of Corrosion Engineers International Standards
- ASME American Society of Mechanical Engineers Standards
- GB Chinese National Standards
- GJB Chinese National Military Standards
- ISO International Standards
- DIN German Standards
- EN European Standards
- API American Petroleum Institute Standards
Detection Method
Tahribatsız muayene > 100% testi
Testing methods:
- Eddy current testing / eddy current crack testing
- Kusursuz yüzey (seviye 4)
- Düz dipli delik çapı 0,7 mm ve 0,4 mm
- Blind area can be cut off according to fixed length > Test to the end of the bar
- Tam çap ultrasonik test
Titanyum Çubuk Malzeme Hizmetlerimiz
As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.
We will be happy to provide you with a consultation and explain everything you need to know about obtaining Grade 7 titanium bar material, including which standards require greater attention for the components to be manufactured.
Uzun vadeli bir tedarik taahhüdünüz varsa, Daxun ile bir çerçeve anlaşması yapabilirsiniz. Belirli bir süre için fiyatları ve miktarları garanti ediyoruz.
Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 12 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.
Sipariş Bilgileri
Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.
İhtiyacınız olan titanyum alaşımı sınıfı, üzerinde çalıştığınız projeye bağlıdır, çünkü her sınıfın farklı faydaları vardır.
Titanyum alaşımının tüm sınıfları son derece güçlü ve korozyona dayanıklıdır, bu da en zorlu koşullarda bile iyi çalışmaya devam edecekleri anlamına gelir.
Titanyum alaşımının daha yüksek dereceleri (5-12) belirli faydalar için tasarlanmış alaşımlardır. Örneğin, 12. sınıf titanyum alaşımı mükemmel ısı direncine sahiptir, bu da onu kabuk ve borulu ısı eşanjörleri, hidrolik borular ve kimya endüstrisi ekipmanları için mükemmel bir seçim haline getirir.
1-4. Sınıflar saf titanyum alaşımlarıdır ve boru sistemleri ve borular için kaynaklanabilir, sünek bir malzemeye ihtiyacınız varsa mükemmel bir seçimdir. Denizcilik ve endüstriyel endüstrilerde kullanılan daha düşük kaliteler bulacaksınız.
Bir projeye başlıyorsanız ve hangi titanyum alaşımının sizin için en iyisi olduğundan emin değilseniz, bugün bizimle iletişime geçin; size yardımcı olmaktan mutluluk duyarız.
DAXUN'da, 1. sınıftan 12. sınıfa kadar çok çeşitli titanyum alaşım kaliteleri sunuyoruz.
1-4. sınıflar saf titanyumdur, daha yüksek sınıflar ise alaşımlardır.
Alaşım kaliteleri, yüksek mukavemet/ağırlık oranları nedeniyle popülerdir.
Bulduğumuz en yaygın kullanılan titanyum alaşım sınıfı 5. sınıftır. Titanyum oranı hala yüksek olsa da, bu sınıf en güvenilir olanlardan biridir çünkü 600 ° F'ye kadar sıcaklıklara dayanabilir ve aşırı koşullara dayanabilir.
Daha yüksek kaliteler, aşınma ve korozyon dirençleri nedeniyle havacılık ve denizcilik endüstrileri gibi endüstriler tarafından tercih edilmektedir.
Buna karşılık, daha düşük kaliteler daha düşük mukavemetleri nedeniyle öncelikle kaynak için kullanılır.
To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.
Titanyum sınıfı maliyeti biraz artırsa da, toplam maliyet öncelikle ihtiyacınız olan titanyum şekli ve formu tarafından belirlenir.
DAXUN'da, plakalar, tüpler, bobinler ve çubuklar dahil olmak üzere çok çeşitli titanyum ürünleri sunuyoruz. İhtiyacınız olan her bir ürünün uzunluğu, genişliği ve miktarı, ödeme sırasında ödeyeceğiniz tutarı etkileyecektir.
Ne yazık ki, projeniz ve titanyumun ne için kullanılacağı hakkında çok fazla bilgi sahibi olmadan çevrimiçi bir fiyat bulmak zordur.
Neyse ki, uzman ekibimiz titanyum ihtiyaçlarınız konusunda size yardımcı olmak ve tavsiyelerde bulunmak için her zaman burada. [email protected] adresine bir e-posta göndererek, size bazı tavsiyeler ve doğru bir fiyat teklifi ile geri dönebileceğiz.
İhtiyaçlarınızı daha iyi anlamak için ihtiyacınız olan titanyum sınıfı, şekli ve miktarı hakkında mümkün olduğunca fazla bilgi eklediğinizden emin olun.
DAXUN'daki ekip deneyimli, bilgili ve arkadaş canlısıdır. Sektördeki yılların tecrübesiyle, kullanımları, faydaları ve kaliteleri de dahil olmak üzere titanyum hakkında her şeyi biliyorlar.
Titanyum, kullanım alanları ve sektörlerdeki uygulamaları hakkında düzenli güncellemeler için blogumuza göz atmayı unutmayın. Uzmanlarımız, sorularınız olduğunda her zaman başvurabileceğiniz, takip etmesi kolay kılavuzlar yazdı.
Hala sorun yaşıyorsanız, bizimle iletişime geçmekten çekinmeyin; size yardımcı olmaktan memnuniyet duyarız.
[email protected] adresine bir e-posta göndererek hızlı bir yanıt alabilirsiniz. Uygun bir çözüm önerebilmemiz için sorunuza mümkün olduğunca fazla ayrıntı eklediğinizden emin olun.
Lütfen “Bize Ulaşın” sayfasındaki formu doldurun veya “+86 13382898899” adresinden satış müdürümüzü arayın, en kısa sürede sizinle iletişime geçeceğiz. WhatsApp'ımız çevrimiçidir ve e-posta ([email protected]) 6 saat içinde kontrol edilecektir. Her soruya veya mesaja derhal yanıt verilecektir. Ayrıca, her hafta müşterilerimizle pazar bilgilerini paylaşıyoruz
Kaliteyi kontrol etmeniz için titanyum çubuk örnekleri sağlayabiliriz. Örnek ücretsizdir ve sadece navlunu ödersiniz.
Kanada, Şili, Kuveyt, Almanya, Güney Kore, Suudi Arabistan, Singapur gibi 42'den fazla ülkeye ihracat yaptık.
Our MOQ is 300 Kg for titanium rod.
Deneme siparişleri bir hafta içinde teslim edilebilir. Normal siparişler için bu süre yaklaşık iki haftadır.