Daxun 316-316L-S31603 stainless steel PIPE and TUBE China supplier
Çin'in önde gelen Paslanmaz Çelik boru ve tüp tedarikçisi ve ihracatçısı olan Daxun, dünyaya paslanmaz çelik BORULAR sağlamaktadır.
- Grade: AISI 316/316L-S31600-S31603
- Manufacturing: hot rolled, cold rolled, forged, welded
- Standartlar: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Types: seamless pipe, welded pipe, forged pipe
- Diameter: from small diameter to large diameter pipe
- Thickness: thin wall pipe and thick wall pipe
- Surface: pickling, polishing, bright annealing
- Uzunluk: 3000mm, 6000mm, 9000mm, vb.
Global leader in stainless steel tuen and pipe fabrication services
ASTM A312 / A358 Stainless Steel 316 Pipe Supplier, 316L/316L Stainless Steel Seamless Pipe, Call Daxun for ASME SA312 316L Stainless Steel Pipe
Daxun Alloys is the leading manufacturer, supplier, and stockist of stainless steel materials. We manufacture many types of pipes and ship them all over the world. These pipes offer excellent ductility and strength. 316 stainless steel pipes are created with high-quality materials and machinery. This grade is classified as commercial grade since it is widely utilised in the industrial sector and has some common residential applications.
316 grade stainless steel is an austenitic stainless steel that gives the alloy good stability and toughness. These 316-grade stainless steel pipes are extremely resistant and durable. It is very resistant to chloride ions. The thickness of these pipes varies from 0.5 mm to 6.35 mm. These pipes are exceedingly heavy in construction. These pipes are mostly utilised in hot applications. These pipelines transmit liquids, gases, fluids, and acids.
316 stainless steel pipes are constructed from a ductile mixture that includes 4% molybdenum. These pipes offer several good qualities, including a variety of functions. These pipes are exceptionally durable, with high yield and tensile strength. Daxun Alloys assures that high-quality materials are used in the production of these exceptional pipes. We also employ a variety of testing procedures to assure the capacity, quality, and robustness of our products. We ship these products all over the world at extremely inexpensive costs. The projected working temperature for these stainless steel pipes is 1010°C-1120°C. These pipes are widely utilised in numerous sectors to transport liquids and other chemicals.
Daxun Alloys offers Type 316 stainless steel pipes in a variety of sizes and shapes, including Type 316 stainless steel welded pipes, Type 316 stainless steel seamless pipes. Like all products supplied and sold by Daxun Alloys, our Type 316 stainless steel meets or exceeds all industry standards.The pipes are all solution annealed.
Stainless Steel Pipe 316/316L is a tube made of the stainless steel alloy 316/316L. The typical molybdenum-containing grade, 316 stainless steel pipe alloy, is the second most popular grade of austenitic stainless steel after 304. The molybdenum in 316 provides stronger overall corrosion resistance than the 304 grade, particularly in chloride conditions. The 316L grade (L=Low Carbon) is similar to the 316 grade, but with an extra-low carbon analysis. This eliminates detrimental precipitation when welding heavier portions in the 800º F to 1500º F range. As a result, 316L is commonly used for heavy-duty welding applications. Typically, there is no price difference between 316 and 316L stainless steel pipes.
Veri
- PARAMETERS
- Bilgi
- İÇİNDEKİLER
- MEKANİK ÖZELLİKLER
- FİZİKSEL ÖZELLİKLER
- EŞDEĞER NOT
- BORU TİPİ
| AISI 316 pipe Material | SA213 TP 316 – ALLOY 316 – UNS S31600 – WNR 1.4401 |
| UNS S31600 Tube Standards | ASTM A213, ASTM A249, ASTM A269, ASME SA213, ASME SA249, ASME SA269, EN 10216-5 TC1 / TC2, PED 97/23/EC, AD 2000, NACE MR0175/ISO 15156 |
| 316 Stainless Steel Seamless Pipes & Tubes Manufacturing Specifications | ASME B36.19 |
| ASTM A213 | |
| ASTM A312 | |
| ASTM A269 | |
| ASTM A632 | |
| ASME SA213 | |
| NFA 49-117 | |
| BS 10216 | |
| Veya müşteri spesifikasyonlarına göre | |
| Dikişsiz Boru Ölçüsü | 3,35 mm dış çap ila 101,6 mm dış çap |
| Kaynaklı Boru Ölçüsü | 6,35 mm OD ila 152 mm OD |
| Stainless Steel 316 Seamless Tube Swg & Bwg | 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg. |
| SS 316 ERW Pipe Wall thickness | 0.020″ -0.220″, (özel duvar kalınlıkları mevcuttur) |
| ASTM A312 TP316 Pipe Length | Tek Rastgele, Çift Rastgele, Standart ve Kesim uzunluğu |
| SS DIN 1.4401 / 1.4436 Rectangular Welded Pipes Finish | Cilalı, AP (Tavlı ve Salamura), BA (Parlak ve Tavlı), MF |
| AMS 5573 Tüp Formu | Düz, Kangal, Dikişsiz, Yuvarlak Borular / Borular, Kare Borular / Borular, Dikdörtgen Borular / Borular, Kangal Borular, “U” Şekli, Pan Kek Ruloları, Hidrolik Borular, Düz veya ‘U’ bükülmüş Borular, İçi Boş, LSAW Borular vb. |
| UNS S31600 Square Pipes Type | Dikişsiz, ERW, EFW, Kaynaklı, Fabrikasyon |
| SS 316 Pipe Schedule | SCH5, SCH10, SCH10S, SCH20, SCH30, SCH40, SCH40S, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| 316 Stainless Steel Tube Electropolished | (EP) Ultra Yüksek Saflık Sistemleri için Elektro Parlatılmış |
| ASTM A312 TP316 Pipe Non-Electropolished | (BA) Parlak Tavlanmış veya (AP) Yüksek Saflık için Tavlanmış ve Asitlenmiş, (CFOS) Oksijen Sınıfı Hizmet veya Korozif Sistemler için Temizlenmiş |
| Stainless Steel 316 Seamless Tube & Pipe I.D. Surface Finish Options | 5, 7 ve 10 µin. Ra |
| 316 Rectangular tubing JIS | 8A ila 250A |
| SS 316 Tube Tolerances | Uygun olarak: ASTM: A269 & A632, JIS: G 3459 |
| 316 stainless steel tubing End | Düz Uç, Eğimli Uç, Dişli, Uçlar orbital kaynak için uygundur |
| AMS 5573 Tüp İşaretleme | All 316 Stainless Steel tubes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.) |
| 316 stainless steel tubing Application | Yağ Borusu, Gaz Borusu, Akışkan Borusu, Kazan ve Eşanjör |
| SS 316 welded round tubes Value Added Service | İstenilen Boyut ve Uzunluğa göre Çekme ve Genişletme, Cila (Elektro ve Ticari) Tavlanmış ve Turşu Bükme, İşleme vb. |
| AMS 5584 Dikişsiz / kaynaklı boru Uzmanlaşmak | Stainless Steel 316 Capillary Tube & Other Odd Size |
| Stainless Steel 316 Heat Exchanger & Condenser Tubes | |
| Stainless Steel 316 Hydraulic tubing with OD up to 50.8 mm (2.0 in.) are delivered in bright annealed condition | |
| Stainless Steel 316 hydraulic tube with OD larger than 50.8 mm are supplied in the annealed and pickled condition, Or in polished condition | |
| SS 316 welded square tubes Marking & Traceability | Each Stainless Steel 316 Tubing is traceable to its producing mill and heat by an identification number etched within 24″ (610mm) of one end. |
| 316 stainless steel tubing Test Certificate | EN 10204 3.1 B'ye göre Üretici Test Sertifikası |
| Devlet Onaylı Laboratuvardan Laboratuvar Test Sertifikası. | |
| Üçüncü Taraf Denetimi Altında | |
| 316 stainless steel tubing Testing & Inspection | Görsel inceleme - Yüzey pürüzlülüğü ölçümü - Helyum sızıntı testi - Taramalı Elektron Mikroskopisi (SEM) - Auger Elektron Mikroskopisi (AES) - Kimyasal Analiz için Seçim Spektroskopisi (ESCA veya XPS) - Parçacık testi - Nem testi |
| We can also cut, thread, and groove Stainless Steel 316 Tubes to meet your specifications | |
| Boyutlar | Standart Toleranslar | ||||||
| Ürünler | OD | Duvar | Uzunluklar ve/veya bobinler | Notlar | OD | Duvar | Uzunluklar |
| Kaynaklı Östenitik Çelik Kazan, Süper Isıtıcı, Isı Eşanjörleri ve Kondenser Boruları | 3/16″ (4,76 mm) ila 4″ (101,6 mm) | 0,020″ (0,51 mm) ila 0,220″ (5,59 mm) | 90′ (27,4 m) uzunluğa kadar rastgele veya kesilmiş uzunluklar | 316/316L | 1″ (25,4 mm) altında ±0,004″ (0,10 mm) | ±10% | 2″'ye (50,8 mm) kadar randımanlar |
| Teknik Özellikler: ASTM-A249, ASME-SA249, ASTM-A688, ASME-SA688 | Metrik boyutlar mevcuttur | 1-1/2" dış çapa kadar bobinler | 1″ (25,4 mm) ila 1-1/2″ (38,1 mm) ±0,006″ (0,15 mm) | +1/8″ (3 mm) -0″ keser | |||
| >1-1/2″ (38,1 mm) ila 2″ (50,8 mm) ±0,008″ (0,20 mm) | |||||||
| >2″ (50,8 mm) ila 2-1/2″ (63,5 mm) ±0,010″ (0,25 mm) | 80.000′ (24.384 m)'ye kadar bobinler | ||||||
| >2-1/2″ (63,5 mm) ila 3″ (76,2 mm) ±0,012″ (0,30 mm) | |||||||
| 3″ (76,2 mm) ila 4″ (101,6 mm) ±0,015″ (0,38 mm) | |||||||
| Basınç ve Korozyon Boruları | 1/16″ (1,59 mm) ila 4″ (101,6 mm) | 0,010″ (0,25 mm) ila 0,220″ (5,59 mm) | 90′ (27,4 m) uzunluğa kadar rastgele veya kesilmiş uzunluklar | 316/316L | <1-1/2″ (38,1 mm) ±0,005″ (0,13 mm) 1-1/2″ (38,1 mm) ila 3″ (76,2 mm) ±0,010″ (0,25 mm) | ±10% | 2″'ye (50,8 mm) kadar randımanlar |
| Kaynaklı ürünler için gereksinimleri karşılar veya aşar | Metrik boyutlar mevcuttur | 1-1/2" dış çapa kadar bobinler | 3-1/2″ (88,9 mm) ila 4″ (101,6 mm) ±0,015″ (0,38 mm) | +1/8″ (3 mm) -0″ keser | |||
| Teknik Özellikler: ASTM-A269, ASTM-A1016 ve ASTM-A632 | 80.000′ (24.384 m)'ye kadar bobinler | ||||||
| Beverage Tubing | 1/4″(6.35 mm) 5/16″ (7.94 mm) 3/8″ (9.53 mm) 1/2″ (12.7 mm) | 0.020″ (0.51 mm) to 0.028″ (0.71 mm) | 40′ (12,2 m) uzunluğa kadar rastgele veya kesilmiş uzunluklar | 316L | ±0,005″ (0,13 mm) | ±10% | 2″'ye (50,8 mm) kadar randımanlar |
| Metrik boyutlar mevcuttur | +1/8″ (3 mm) -0″ keser | ||||||
| Coils to 15,000′ (4,572 m) | |||||||
| Enstrümantasyon Boruları | 1/16″ (1,59 mm) ila 1/2″ (12,7 mm) | 0,010″ (0,25 mm) ila 0,065″ (1,65 mm) | 40′ (12,2 m) uzunluğa kadar rastgele veya kesilmiş uzunluklar | 316/316L | ±0,005″ (0,13 mm) | ±10% | 2″'ye (50,8 mm) kadar randımanlar |
| Teknik Özellikler: ASTM-A269 ve ASTM-A632 | Metrik boyutlar mevcuttur | +1/8″ (3 mm) -0″ keser | |||||
| Food/Dairy Tubing, Pharmaceutical/ BioPharmaceutical Tubing, High Purity Tubing, Ultra High Purity Tubing | 1/2″ (12.7 mm) to 8″ (203.2 mm) | 0.049″ (1.24 mm) to 0.109″ (2.77 mm) | 20′ (6.1 m) stock lengths. | 316/316L | 1/2″ (12.7 mm) ± 0.005″ (0.13 mm) | ±10% | +1/8″ (3 mm) -0″ |
| Other lengths available upon request. | 3/4″ (19.1 mm) ± 0.005″ (0.13 mm) | ||||||
| 1″ (25.4 mm) ± 0.005″ (0.13 mm) | ±10% | +1/8″ (3 mm) -0″ | |||||
| 1-1/2″ (38.1 mm) ± 0.008″ (0.20 mm) | |||||||
| 2″ (50.8 mm) ± 0.008″ (0.20 mm) | ±10% | +1/8″ (3 mm) -0″ | |||||
| 2-1/2″ (63.5 mm) ± 0.010″ (0.25 mm) | |||||||
| 3″ (76.2 mm) ± 0.010″ (0.25 mm) | ±10% | +1/8″ (3 mm) -0″ | |||||
| 4″ (101.6 mm) ± 0.015″ (0.38 mm) | |||||||
| 6″ (152.4 mm) ± 0.030″ (0.76 mm) | ±10% | +1/8″ (3 mm) -0″ | |||||
| 8″ (203.2 mm) +0.061″ (1.55 mm), -0.031″ (0.79 mm) | |||||||
| ±10% | +1/8″ (3 mm) -0″ | ||||||
| ±10% | +1/8″ (3 mm) -0″ | ||||||
| ±10% | +1/8″ (3 mm) -0″ | ||||||
| ±10% | +1″ (25.4 mm) -0″ | ||||||
| ±10% | +1″ (25.4 mm) -0″ | ||||||
| The Chemical Composition of grade 316L Stainless Steel is outlined in the following table | ||||||||||
| Sınıf | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 316 | Min | - | - | - | 0 | - | 16 | 2 | 10 | - |
| Max | 0.08 | 2 | 0.75 | 0.045 | 0.03 | 18 | 3 | 14 | 0.1 | |
| 316L | Min | - | - | - | - | - | 16 | 2 | 10 | - |
| Max | 0.03 | 2 | 0.75 | 0.045 | 0.03 | 18 | 3 | 14 | 0.1 | |
| 316H | Min | 0.04 | 0.04 | 0 | - | - | 16 | 2 | 10 | - |
| max | 0.1 | 0.1 | 0.75 | 0.045 | 0.03 | 18 | 3 | 14 | - | |
| The Mechanical Properties of grade 316L Stainless Steel are displayed in the following table. | |||||
| Sınıf | Tensile Str | Yield Str | Elong | Sertlik | |
| (MPa) min | 0.2% Proof | (% in 50mm) min | |||
| (MPa) min | Rockwell B (HR B) max | Brinell (HB) max | |||
| 316 | 515 | 205 | 40 | 95 | 217 |
| 316L | 485 | 170 | 40 | 95 | 217 |
| 316H | 515 | 205 | 40 | 95 | 217 |
| Sınıf | Yoğunluk (kg/m3) | Elastik Modül (GPa) | Ortalama Termal Genleşme Katsayısı (m/m/0C) | Termal İletkenlik (W/m.K) | Özgül Isı 0-1000C (J/kg.K) | Elektriksel Özdirenç (n.m) | |||
| 0-1000C | 0-3150C | 0-5380C | 1000C'de | 5000C'de | |||||
| SA213 Stainless Steel 316 Welded Pipe | 7750 | 200 | 15.9 | 16.2 | 17 | 14.2 | 18.7 | 500 | 720 |
| Sınıf | ÇİN | UNS No | Eski İngiliz | Euronorm | İsveç SS | Japon JIS | ||
| BS | En | Hayır | İsim | |||||
| 316 | 06Cr17Ni12Mo2 | S31600 | 304S11 | 58E | 1.4401 | X5CrNiMo17-12-2 | 2347 | SUS 316 |
| ASTM A213 TP316 Condenser Tube | AMS 5573 1/4hd Seamless Aero engine Pipe |
| ASTM A269 TP316 straight tube | AMS 5584 Welded furnace tube |
| ASTM A249 TP316 Mirror Tube | AMS 5573 1/8hd Welded Pipe, High-Pressure Hydraulic |
| JIS SUS316 Seamless Pipe | 316 SS Round Tube |
| SA312 TP316 Welded Pipe | AMS 5584 Seamless Tube |
| ASTM A312 TP316 Coiled Pipe | Stainless Steel Inox 316 Capillary Pipe |
| ASTM A312 gr TP 316 Aerospace Pipe | AMS 5573 Electric Fusion Welding Pipe |
| Stainless Steel 316 Grade Pipe | Type 316 Stainless Steel Polished Pipe |
| ASTM A312 TP316 Elliptical and Oval Pipe | AMS 5584 Rectangular Tube |
| Din 1.4401 / 1.4436 Stainless Steel Welded Pipe | ASTM A358 TP316 Coil Pipe Heat Exchanger |
| SAE J405 Uns S31600 Thin Wall Pipe | 316 Stainless Steel Metric Pipe |
| 316 Stainless Steel Seamless Square Pipe | Large Diameter 316 Stainless Steel Tube |
| SS 316 ERW Pipe | 316 Stainless Steel Instrumentation Pipe |
| High-pressure 316 Stainless Steel Water Pipe | Stainless Steel 316 Hexagonal Pipe |
| Din W.-Nr. 1.4401 / 1.4436 Aisi 316 Corrugated Tube | Stainless Steel 316 Round Tube |
| UNS S31600 Seamless Pipe | Stainless Steel 316 Seamless Round Pipe |
| ASTM A358 TP316 Polished Pipe | 316 Stainless Steel Ornamental Tube |
| 316 Stainless Steel Exhaust Pipe | 316 Stainless Steel Spiral Pipe |
| ASME SA213 TP316 Perforated Tube | WERKSTOFF NR. 1.4401 / 1.4436 Flexible Tube |
| SA 688 TP316 Finned Tube | SA312 TP316 Dom Tube |
| Din 1.4401 / 1.4436 AISI 316 Perforated Exhaust Tube | Stainless Steel 316 Hypodermic Pipe |
| Material 1.4401 / 1.4436 Aisi 316 Slotted Handrail Tube | SA312 TP316 Thin Wall Tube |
| En 1.4401 / 1.4436 / Aisi 316 Thick Wall Tube | 316 Stainless Steel Hydraulic Pipe |
| Stainless Steel 316 Ornamental Pipe | Stainless Steel 316 Fin Tube / Finned Tube |
| S31600 Stainless Steel U Shaped Tube | 316 Stainless Steel Square Tube Mirror Finish |
| Din 1.4401 / 1.4436 Material Seamless Pipe | WERKSTOFF NR. 1.4401 / 1.4436 Coaxial Tube |
| 316 Stainless Steel Rectangular Pipe | 316 Stainless Steel Hypodermic Pipe for Medical Needle |
| 1.4401 / 1.4436 Instrument Pipe | 316 Stainless Steel Square Pipe |
| Ultra-High Purity Electropolished Stainless Steel 316 Tube | Thin Wall Stainless Steel 316 Tube |
| 316 Stainless Steel ERW Pipe | Corrugated 316 Stainless Steel Tube (CSST) for Gas |
| Jis 316 Stainless Steel Coil Pipe | Stainless Steel 316 Seamless Pipe |
| Schedule 10 Type 316 Stainless Steel Pipe | Schedule 40 Type 316 Stainless Steel Pipe |
| AMS 5573 1/8hd Seamless Pipe | Polished 316 Stainless Steel Pipe |
| 316 Stainless Steel Threaded Pipe | SAE 30316 Stainless Steel Rectangular Tube |
| Stainless steel 316 pipe | SS 316 Pipe |
| 316 SS SCHEDULE 10 PIPE | SS 316 SEAMLESS PIPE. |
| 316 SS Tube Stockist | 316 Stainless steel Exhaust Pipe |
| SS 316 Tube | 316 STAINLESS STEEL Pipe |
| STAINLESS STEEL 316 WELDED Pipe | SS 316 erw pipe |
| 316 stainless steel exhaust pipe | Schedule 5 316 stainless steel pipe |
| Schedule 20 316 stainless steel pipe | 316 Stainless steel seamless Pipe |
| Type 316 Stainless steel Pipe | Stainless Steel 316 Cold Drawn Pipe |
| SS UNS S31600 Seamless Pipe | 316 Stainless steel seamless tube |
| 316 Stainless Steel Seamless Pipe & Pipe | ASTM A312 SS 316 Round Pipe |
| Stainless Steel 316 Seamless Tube | TP 316 SS Polished Pipe |
| SS 316 ERW Pipe | ASTM A269 316 Pipe |
| ASTM A312 TP316 Pipe | TP 316 SS ERW Pipe |
| SS DIN 1.4401 / 1.4436 Rectangular Welded Pipe | 316 Stainless Steel EFW Pipe |
| AMS 5573 Tube | SS 316 Seamless Pipe |
| UNS S31600 Square Pipe | 316 stainless steel rectangular tube |
| 316 Stainless Steel Tube | SS 316 Cold Rolled Coiled Pipe |
| ASTM A312 TP316 Pipe | Stainless Steel 316 Oval Tube |
| Stainless Steel 316 Seamless Tube & Pipe | 316 Stainless Steel Seamless Pipe |
| 316 Rectangular Pipe | Stainless Steel 316 EFW Pipe |
| SS 316 Tube | 316 Paslanmaz Çelik Boru |
| AMS 5573 Tube | Stainless Steel 316 Polished Tube |
| SS 316 welded round Pipe | Stainless Steel 316 precision Pipe |
| AMS 5584 Seamless/ welded tube | Stainless Steel 316 Welded Tube |
| SS 316 welded square Pipe | Stainless Steel 316 instrumentation Pipe |
| ASTM A312 TP316 Stainless Steel Pipe & Tube | Stainless Steel 316 Seamless Round Pipe |
| Stainless Steel 316 Pipe & Tube | SS 316 Needle Tube |
| Stainless Steel 316 Welded Pipe & Tube | SS 316 Round Tube |
| UNS S31600 Square Pipe | 316 Stainless Steel Oval Pipe |
| ASTM A249 TP 316 SS Seamless Pipe | 316 Paslanmaz Çelik Boru |
Daxun'u seçin ve müşterilerinizi memnun edin.

Quick response-316 Stainless Steel pipe
– Excellent weldability
– Good machinability
– Good corrosion resistance
– Excellent resistance to pitting corrosion
– Austenitic structure gives it excellent toughness even at low temperatures
– Considered resistant to drinking water
– Excellent resistance to chlorides
– Resistant to aggressive chemicals
– Better resistance to cracking and pitting corrosion
Daxun Avantajları
- Variety: From small to large diameter stainless steel pipe, we offer a wide range of sizes and grades, including 304L, 316L, and more.
- Esneklik: İster dikişsiz ister kaynaklı çelik boruya ihtiyacınız olsun, paslanmaz çelik boru uzunluklarımız özel proje gereksinimlerinizi karşılamak üzere tasarlanmıştır.
Kalite - Standartlar: Paslanmaz çelik borularımız, güvenilirlik ve performans sağlamak için ISO9001, ABS, NSF/ANSI Standard 61 ve NACE MR0175 gibi katı standartları karşılar.
- Özel Siparişler: Özel boyutta paslanmaz çelik borular mı arıyorsunuz? Rekabetçi fiyatlarla ve uygun çevrimiçi siparişle çeşitli paslanmaz çelik boru özel seçenekleri sunuyoruz.


316 Stainless Steel pipe packaging
- Dokuma torba balya kargo (altıgen)
- U-bükümlü borular için özel kasalar, (çelik/ahşap) bölünmüş
- Her balya, rüzgar ve yağmura karşı korumak için plastikle sarılır.
- SS 316L seamless pipes are protected by plastic covers.
- Balyayı sabitlemek için plastik şeritler kullanılır.
- İhracata özel fümigasyonsuz ahşap sandık ambalajı.
- Balya veya kasaya iliştirilmiş lamine ambalaj fişi.
- Müşteri ihtiyaçlarına göre özelleştirilmiş ambalaj.
316 Stainless Steel pipe Ordering Information
The purchase order shall include quantity, PSL grade, type or class, API5L reference, outside diameter, wall thickness, length and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Pipe is solution bright annealed.


Kalite, teslimat, denetim
- Daxun ayrıca çeşitli kalite güvence testleri de gerçekleştirmektedir. Bu testler arasında düzleştirme testi, çukurlaşma ve direnç testi, mekanik test, sertlik testi, malzeme pozitif tanımlama, genleşme testi vb. bulunmaktadır. Tüm bu testler, malzemenin gerekli uygulama için uygun olmasını sağlar.
- Üretim sürecinde ürünün çapını, kalınlığını ve yüzeyini ölçüyoruz. Standart teslimat süremiz 7-15 gündür, bazı özel ebatlı ürünler haricinde teslimat süremiz 20 güne çıkacaktır.
Teslimat süremiz kesinlikle sözleşmeye uygundur. - Müşterinin üçüncü taraf acentelerinin denetim için fabrikaya gitmesine destek olun
- Test için müşterilere ücretsiz numune desteği
- Yerinde veya video fabrika denetimini destekleyin
Teknik Destek
Herhangi bir ek teknik yardıma ihtiyacınız olursa, yerleşik metalürji uzmanımız ve bilgili personelimiz size yardımcı olmaktan memnuniyet duyacaktır. Ayrıca Daxun, çoklu metal ve plastik envanter endüstrisinde bir ilk olan sertifikalı bir test laboratuvarına sahiptir. Bu, bize göre, kaliteye olan sarsılmaz bağlılığımızı ve tam hizmet tedarikçisi olarak felsefemizi göstermektedir.

316/316L Stainless Steel pipe and tube Features
Daxun Alloy Markanızın hızla gelişmesine izin verin
- Galeri
- 316/316L STEEL PIPE DATA pipe
- BASINÇ DERECESI
- BOYUT
- Yüzey kaplaması
| NPS | Dış Çap | Duvar Kalınlığı | Ağırlık | Ağırlık | |||
| içinde | mm | içinde | mm | Sched | kg/Mtr | Lb/ft | |
| 1/2″ | 0.84 | 21 | 0.109 | 2.769 | 40 STD | 1.268 | 0.851 |
| 0.147 | 3.734 | 80 STD | 1.621 | 1.088 | |||
| 3/4″ | 1.05 | 27 | 0.113 | 2.87 | 40 STD | 1.684 | 1.131 |
| 0.154 | 3.912 | 80 STD | 2.195 | 1.474 | |||
| 1″ | 1.315 | 33 | 0.133 | 3.378 | 40 STD | 2.501 | 1.679 |
| 0.179 | 4.547 | 80 STD | 3.325 | 2.172 | |||
| 1 1/4″ | 1.66 | 42 | 0.14 | 3.556 | 40 STD | 3.385 | 2.273 |
| 0.191 | 4.851 | 80 STD | 4.464 | 2.997 | |||
| 1 1/2″ | 1.9 | 48 | 0.145 | 3.683 | 40 STD | 4.048 | 2.718 |
| 0.2 | 5.08 | 80 STD | 5.409 | 3.361 | |||
| 2″ | 2.375 | 60 | 0.154 | 3.912 | 40 STD | 5.441 | 3.653 |
| 0.218 | 5.537 | 80 STD | 7.48 | 5.022 | |||
| 2 1/2″ | 2.875 | 73 | 0.203 | 5.516 | 40 STD | 8.629 | 5.793 |
| 0.276 | 7.01 | 80 STD | 11.411 | 7.661 | |||
| 3″ | 3.5 | 89 | 0.216 | 5.486 | 40 STD | 11.284 | 7.576 |
| 0.3 | 7.62 | 80 STD | 15.272 | 10.253 | |||
| 4″ | 4.5 | 114 | 0.237 | 6.02 | 16.073 | 10.79 | |
| 0.337 | 8.56 | 22.318 | 14.983 | ||||
| 6″ | 6.625 | 168 | 0.188 | 4.775 | 19.252 | 12.924 | |
| 0.203 | 5.516 | 20.739 | 13.923 | ||||
| 0.219 | 5.563 | 22.318 | 14.983 | ||||
| 0.25 | 6.35 | 25.354 | 17.021 | ||||
| 0.28 | 7.112 | 40 STD | 58.263 | 18.974 | |||
| 0.312 | 7.925 | 31.334 | 21.036 | ||||
| 0.375 | 9.525 | 37.285 | 25.031 | ||||
| 0.432 | 10.973 | 80 XHY | 42.561 | 28.573 | |||
| 0.5 | 12.7 | 48.719 | 32.708 | ||||
| 8″ | 8.625 | 219 | 0.188 | 4.775 | 25.233 | 16.94 | |
| 0.203 | 5.156 | 27.198 | 18.259 | ||||
| 0.219 | 5.563 | 29.286 | 19.661 | ||||
| 0.25 | 6.35 | 20 | 33.308 | 22.361 | |||
| 0.277 | 7.036 | 30 | 36.786 | 24.696 | |||
| 0.322 | 8.179 | 40 | 42.352 | 28.554 | |||
| 0.375 | 9.525 | 49.216 | 33.041 | ||||
| 0.406 | 10.312 | 60 | 53.085 | 35.638 | |||
| 0.5 | 12.7 | 80 XHY | 64.627 | 43.388 | |||
| 10″ | 10.75 | 273 | 0.188 | 4.775 | 31.588 | 21.207 | |
| 0.219 | 5.563 | 36.689 | 24.631 | ||||
| 0.25 | 6.35 | 20 | 41.759 | 28.035 | |||
| 0.307 | 7.798 | 30 | 51.002 | 34.24 | |||
| 0.344 | 8.738 | 56.946 | 38.231 | ||||
| 0.365 | 9.271 | 40 STD | 63.301 | 40.483 | |||
| 0.438 | 11.125 | 71.852 | 48.238 | ||||
| 0.5 | 12.7 | 60 XHY | 81.53 | 54.735 | |||
| 0.594 | 15.088 | 80 | 95.969 | 64.429 | |||
| 12″ | 12.75 | 324 | 0.188 | 4.775 | 37.57 | 25.222 | |
| 0.219 | 5.563 | 43.657 | 29.309 | ||||
| 0.25 | 6.35 | 49.713 | 33.375 | ||||
| 0.281 | 7.137 | 55.739 | 37.42 | ||||
| 0.312 | 7.925 | 61.735 | 41.445 | ||||
| 0.375 | 9.525 | 73.824 | 49.562 | ||||
| 0.406 | 10.312 | 79.727 | 53.525 | ||||
| 0.5 | 12.7 | 97.438 | 65.415 | ||||
| 0.562 | 14.275 | 108.966 | 73.154 | ||||
| 14″ | 14 | 356 | 0.188 | 4.775 | 41.308 | 27.732 | |
| 0.219 | 5.563 | 48.012 | 32.233 | ||||
| 0.25 | 6.35 | 20 | 54.685 | 36.713 | |||
| 0.281 | 7.137 | 61.327 | 41.172 | ||||
| 0.312 | 7.925 | 67.939 | 45.611 | ||||
| 0.375 | 9.525 | STD | 81.281 | 54.568 | |||
| 0.438 | 11.125 | 40 | 94.498 | 63.441 | |||
| 0.5 | 12.7 | XHY | 107.381 | 72.09 | |||
| 0.625 | 15.875 | 132.983 | 89.278 | ||||
| 16” | 16 | 406 | 0.188 | 4.775 | 47.29 | 21.748 | |
| 0.219 | 5.563 | 54.98 | 36.91 | ||||
| 0.25 | 6.35 | 10 | 62.639 | 42.053 | |||
| 0.281 | 7.137 | 70.268 | 47.174 | ||||
| 0.312 | 7.925 | 20 | 77.866 | 52.275 | |||
| 0.344 | 8.738 | 85.677 | 57.519 | ||||
| 0.375 | 9.525 | 30 | 93.213 | 62.578 | |||
| STD | |||||||
| 0.438 | 11.125 | 108.433 | 72.797 | ||||
| 0.5 | 12.7 | 40 | 123.289 | 82.77 | |||
| XHY | |||||||
| 18″ | 18 | 457 | 0.219 | 5.563 | 61.948 | 41.588 | |
| 0.25 | 6.35 | 70.593 | 47.393 | ||||
| 0.281 | 7.137 | 79.208 | 53.176 | ||||
| 0.312 | 7.925 | 20 | 87.792 | 58.939 | |||
| 0.375 | 9.525 | STD | 105.144 | 70.588 | |||
| 0.438 | 11.125 | 30 | 122.369 | 82.152 | |||
| 0.5 | 12.7 | XHY | 139.198 | 93.45 | |||
| 0.562 | 14.275 | 40 | 155.904 | 104.666 | |||
| 0.625 | 15.875 | 172.754 | 115.978 | ||||
| 20″ | 20 | 508 | 0.25 | 6.35 | 78.547 | 52.733 | |
| 0.282 | 7.163 | 88.458 | 59.386 | ||||
| 0.312 | 7.925 | 97.719 | 65.604 | ||||
| 0.375 | 9.525 | 20 STD | 117.075 | 78.598 | |||
| 0.438 | 11.125 | 136.305 | 91.508 | ||||
| 0.5 | 12.7 | 30 XHY | 155.106 | 104.13 | |||
| 0.594 | 15.088 | 40 | 183.378 | 123.11 | |||
| 0.625 | 15.875 | 192.64 | 129.328 | ||||
| 0.688 | 17.475 | 211.368 | 141.901 | ||||
| 24″ | 24 | 610 | 0.25 | 6.35 | 94.456 | 63.413 | |
| 0.281 | 7.137 | 106.029 | 71.183 | ||||
| 0.312 | 7.925 | 117.573 | 18.932 | ||||
| 0.375 | 9.525 | 20 STD | 140.938 | 64.618 | |||
| 0.438 | 11.125 | 164.176 | 110.219 | ||||
| 0.5 | 12.7 | XHY | 186.923 | 125.49 | |||
| 0.625 | 15.875 | 232.41 | 156.028 | ||||
| 0.688 | 17.475 | 40 | 255.148 | 171.293 | |||
| 0.75 | 19.05 | 277.401 | 186.233 | ||||
| 30″ | 30 | 762 | 0.25 | 6.35 | 118.318 | 79.433 | |
| 0.281 | 7.137 | 132.851 | 89.189 | ||||
| 0.312 | 7.925 | 10 | 147.353 | 98.925 | |||
| 0.375 | 9.525 | STD | 176.731 | 118.648 | |||
| 0.438 | 11.125 | 205.983 | 138.286 | ||||
| 0.5 | 12.7 | 20 XHY | 234.647 | 157.53 | |||
| 0.625 | 15.875 | 30 | 292.066 | 196.078 | |||
| 0.688 | 17.475 | 320.817 | 215.38 | ||||
| 0.75 | 19.05 | 348.988 | 234.293 | ||||
| 36″ | 36 | 914 | 0.25 | 6.35 | 142.18 | 95.453 | |
| 0.281 | 7.137 | 159.672 | 107.196 | ||||
| 0.312 | 7.925 | 10 | 177.133 | 118.918 | |||
| 0.375 | 9.525 | STD | 215.525 | 142.678 | |||
| 0.438 | 11.125 | 247.79 | 166.353 | ||||
| 0.5 | 12.7 | 20 XHY | 282.372 | 198.57 | |||
| 0.625 | 15.875 | 351.723 | 236.128 | ||||
| 0.688 | 17.475 | 386.487 | 259.467 | ||||
| 0.75 | 19.05 | 420.576 | 282.353 | ||||
| 42″ | 42 | 1067 | 0.312 | 7.925 | 206.914 | 138.911 | |
| 0.375 | 9.525 | STD | 248.319 | 166.708 | |||
| 0.5 | 12.7 | XHY | 33.097 | 221.61 | |||
| 0.75 | 19.05 | 492.163 | 330.413 | ||||
| 48″ | 48 | 1219 | 0.375 | 9.525 | STD | 284.112 | 190.738 |
| 0.438 | 11.125 | 331.404 | 222.487 | ||||
| 0.5 | 12.7 | XHY | 377.822 | 253.65 | |||
| 0.75 | 19.05 | 563.75 | 378.473 | ||||
| 0.875 | 22.225 | 655.969 | 440.383 | ||||
| BASINÇ DEĞERI (PSIG) | ||||||||||||
| BEDENLER | SCHEDULE (SCH) | DIŞ | DUVAR | SICAKLIK (OF) | ||||||||
| (İNÇ) | DIA. | KALIN. | 100 | 200 | 300 | 400 | 500 | 600 | 650 | 700 | 750 | |
| (IN) | (IN) | IZIN VERILEN GERILME (PSI) | ||||||||||
| 16700 | 16700 | 16700 | 15500 | 14400 | 13500 | 13200 | 12900 | 12600 | ||||
| 1″ | 40 | 1.315 | 0.133 | 2205 | 2205 | 2205 | 2047 | 1902 | 1783 | 1743 | 1703 | 1664 |
| 80 | 1.315 | 0.179 | 3061 | 3061 | 3061 | 2841 | 2640 | 2475 | 2420 | 2365 | 2310 | |
| 160 | 1.315 | 0.25 | 4493 | 4493 | 4493 | 4170 | 3874 | 3632 | 3552 | 3471 | 3390 | |
| 1 1/2″ | 40 | 1.9 | 0.145 | 1629 | 1629 | 1629 | 1512 | 1404 | 1317 | 1287 | 1258 | 1229 |
| 80 | 1.9 | 0.2 | 2303 | 2303 | 2303 | 2138 | 1986 | 1862 | 1821 | 1779 | 1738 | |
| 160 | 1.9 | 0.281 | 3362 | 3362 | 3362 | 3120 | 2899 | 2717 | 2657 | 2597 | 2536 | |
| 2″ | 40 | 2.375 | 0.154 | 1371 | 1371 | 1371 | 1272 | 1182 | 1108 | 1083 | 1059 | 1034 |
| 80 | 2.375 | 0.218 | 1985 | 1985 | 1985 | 1843 | 1712 | 1605 | 1569 | 1534 | 1498 | |
| 160 | 2.375 | 0.344 | 3283 | 3283 | 3283 | 3047 | 2831 | 2654 | 2595 | 2536 | 2477 | |
| 3″ | 40 | 3.5 | 0.216 | 1301 | 1301 | 1301 | 1208 | 1122 | 1052 | 1028 | 1005 | 982 |
| 80 | 3.5 | 0.3 | 1844 | 1844 | 1844 | 1712 | 1590 | 1491 | 1458 | 1425 | 1391 | |
| 160 | 3.5 | 0.438 | 2787 | 2787 | 2787 | 2587 | 2403 | 2253 | 2203 | 2153 | 2103 | |
| 4″ | 40 | 4.5 | 0.237 | 1102 | 1102 | 1102 | 1023 | 950 | 891 | 871 | 851 | 831 |
| 80 | 4.5 | 0.337 | 1596 | 1596 | 1596 | 1482 | 1377 | 1291 | 1262 | 1233 | 1204 | |
| 160 | 4.5 | 0.531 | 2611 | 2611 | 2611 | 2424 | 2552 | 2111 | 2064 | 2017 | 1970 | |
| 5″ | 40 | 5.563 | 0.258 | 965 | 965 | 965 | 896 | 832 | 780 | 763 | 746 | 728 |
| 80 | 5.563 | 0.375 | 1428 | 1428 | 1428 | 1325 | 1231 | 1154 | 1129 | 1103 | 1077 | |
| 160 | 5.563 | 0.625 | 2474 | 2474 | 2474 | 2296 | 2133 | 2000 | 1955 | 1911 | 1866 | |
| 6″ | 40 | 6.625 | 0.28 | 877 | 877 | 877 | 814 | 756 | 709 | 693 | 677 | 661 |
| 80 | 6.625 | 0.432 | 1379 | 1379 | 1379 | 1280 | 1189 | 1115 | 1090 | 1065 | 1040 | |
| 160 | 6.625 | 0.719 | 2382 | 2382 | 2382 | 2211 | 2054 | 1925 | 1883 | 1840 | 1797 | |
| 8″ | 40 | 8.625 | 0.322 | 771 | 771 | 771 | 716 | 665 | 623 | 610 | 596 | 582 |
| 80 | 8.625 | 0.5 | 1218 | 1218 | 1218 | 1131 | 1050 | 985 | 963 | 941 | 919 | |
| 160 | 8.625 | 0.906 | 2298 | 2298 | 2298 | 2133 | 1982 | 1858 | 1817 | 1775 | 1734 | |
| 10″ | 40 | 10.75 | 0.365 | 699 | 699 | 699 | 649 | 603 | 565 | 553 | 540 | 528 |
| 80 | 10.75 | 0.594 | 1159 | 1159 | 1159 | 1075 | 999 | 937 | 916 | 895 | 874 | |
| 160 | 10.75 | 1.125 | 2289 | 2289 | 2289 | 2124 | 1974 | 1850 | 1809 | 1768 | 1727 | |
| Türleri | Dış çap | Boyutlar | Uzunluk |
| NB Boyutları (stokta) | .0035” ~ 20” | 1/8″, 1/4″, 3/8″, 1/2″, 5/8″, 3/4″, 1″, 1.25″, 1.5″, 2″, 2.5″, 3″, 4″, 5″, 6″vb | Boyuna kes |
| Stainless Steel 316/316L Seamless Tube (Custom Sizes) | 6,35 mm dış çap ila 508 mm dış çap | İhtiyaca göre | Boyuna kes |
| Stainless Steel 316/316L Welded Tube (ERW Tube) (in Stock + Custom Sizes) | 6,35 mm dış çap ila 1219 mm dış çap | İhtiyaca göre | Boyuna kes |
| Yüzey İşlemi | İç Yüzey (ID) | Dış Yüzey (OD) | |||
| Pürüzlülük Ortalaması (RA) | Pürüzlülük Ortalaması (RA) | ||||
| μ inç | μm | μ inç | μm | ||
| AP | Tavlanmış & Salamura | Tanımlanmamış | Tanımlanmamış | 40 veya Tanımlanmamış | 1.0 veya Tanımlanmamış |
| BA | Beight Tavlı | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| MP | Mekanik Cila | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| EP | Elektro Cila | 15,10,7,5 | 0.38,0.25,0.20;0.13 | 32 | 0.8 |
The surface and shape of 316/316L stainless steel TUBE (6)
Referans ve indirme için mevcut bilgiler
Daxun güvenilir bir paslanmaz çelik boru ve tüp üreticisidir
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel pipes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the 316 stainless steel tubes have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
Güncel sıcak vaka projeleri ve ürünleri
İlgili Ürünler (10)
We can provide 316 Stainless Steel pipe samples for you to check the quality. Sample is free and you just pay the freight.
Kanada, Şili, Kuveyt, Almanya, Güney Kore, Suudi Arabistan, Singapur gibi 42'den fazla ülkeye ihracat yaptık.
Our MOQ is 1 ton for 316 Stainless Steel pipe.
Deneme siparişleri bir hafta içinde teslim edilebilir. Normal siparişler için bu süre yaklaşık iki haftadır.