Daxun is a 17-4 stainless steel sheet supplier in China
As China’s leading stainless steel plate supplier and exporter, Daxun provides 17-4 stainless steel plates to the world.
- Grade: AISI 17-4PH-630-Precipitation Hardening Steel
- Manufaktur: pelat canai dingin, pelat canai panas, pelat tempa
- Standar: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Jenis: pelat tipis canai dingin, pelat tebal canai panas
- Permukaan: 2B, NO.1, NO.4, HL, BA, 8K, dll.
- Panjang: 2438mm3048mm6000mm dapat disesuaikan
- Asal: TISCO, Baosteel, Pohang, Tsingshan, Delong
17-4PH Global leader in stainless steel sheet fabrication services
Type 17-4 PH stainless steel plate is the most widely used of all precipitation hardening stainless steels. Its valuable combination of properties gives designers the opportunity to improve the reliability of their products while simplifying the manufacturing process and reducing costs. Type 17-4 PH is a martensitic precipitation hardening stainless steel that offers exceptional high strength, good corrosion resistance, and good mechanical properties at temperatures up to 600°F (316°C). Its unique combination of properties makes this alloy an effective solution to many design and production problems. Contact Daxun today
17-4PH stainless steel, otherwise known as SAE Type 630, is frequently used with operations demanding high tensile strength and a middling level of corrosion resistance. 17-4 PH is the most-used grade of martensitic precipitation hardenable alloys and is regarded as the most broadly formed precipitation hardening grade. Its intense tensile strength keeps its ductility and hardness at high temperatures while still demonstrating exceptional corrosion resistance in all conditions.Contact Daxun now to obtain the latest technical documents and information.
Data Teknis
- Parameter
- Komposisi Kimia
- Sifat mekanik
- Sifat Fisik
- Standar
| Product Parameters: 17-4PH Stainless Steel Sheet/Plate | |||
| Lebar | 10mm ~ 2500mm | ||
| Ketebalan | 0.2mm ~ 100mm | Toleransi ketebalan | +/- 0,03mm |
| Standar | ASTM/ASME 240/480, JIS 4305, DIN EN 10088-2 | ||
| Permukaan | 2B, BA, 8K, NO.1, NO.4, NO.3, garis rambut, kotak-kotak, emas, hitam, emas mawar, dll | ||
| spesifikasi | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
| Asal Pabrik | TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, dan lain-lain. | ||
| Sertifikasi | ISO, SGS, BV, TUV, CE, dll | ||
| Karbon | 0.07% (Max) |
| Silikon | 1.00% (Max) |
| Mangan | 1.00% (Max) |
| Phosphorous | 0.040% (Max) |
| Belerang | 0.030% (Max) |
| Kromium | 15%-17.5% |
| Molybdenum | 0.50% (Max) |
| Nikel | 3%-5% |
| Copper | 3%-5% |
| Material Type | Kondisi | Ultimate Tensile Strength (PSI) | 0.2% Yield Strength (PSI) | Elongation (% In 2in.) | Reduction Of Area (%) | Hardness Brinell | Hardness Rockwell |
| 17-4 PH | H900 | 190,000 | 170,000 | 10 | 40 | 388 | C40 |
| H1025 | 155,000 | 145,000 | 12 | 45 | 331 | C35 | |
| H1075 | 145,000 | 125,000 | 13 | 45 | 311 | C32 | |
| H1150 | 135,000 | 105,000 | 16 | 50 | 277 | C28 | |
| H1150-M | 115,000 | 75,000 | 18 | 55 | 255 | C24 | |
| H1150-D | 125,000 | 105,000 | 16 | 50 | 255 min – 311 max | C24 – 33 |
| Heat Treated Condition | H900 |
| Density, lbs/in3 | 0.282 |
| Electrical Resistivity, microhm-cm | 77 |
| Specific Heat, BTU/lb/°F (32-212°F) | 0.1 |
| Thermal Conductivity, BTU/hr/ft2/in/°F | |
| 300°F | 124 |
| 500°F | 135 |
| 860°F | 156 |
| 900°F | 157 |
| Mean Coefficient of Thermal Expansion, in/in/°F | |
| -100 to 70°F | 5.8 x 10^-6 |
| 70 – 200°F | 6.0 x 10^-6 |
| 70 – 400°F | 6.0 x 10^-6 |
| 70 – 600°F | 6.3 x 10^-6 |
| 70 – 800°F | 6.5 x 10^-6 |
| 70 – 900°F | — |
| Modulus of Elasticity, ksi | 28.5 x 10^3 |
| Modulus of Rigidity, ksi | 11.2 x 10^3 |
| Poisson’s Ratio (all conditions) | 0.272 |
| Kelas | UNS | Industry Specifications |
| 17-4 Duplex Stainless Steel | UNS 17-4PH | UNS: S17400 • AMS: 5604 • ASTM: A693 • ASME: SA693 • W. Nr./EN: 1.4548 |
| UNS 630 | UNS: S17400 • AMS: 5604 • ASTM: A693 • ASME: SA693 • W. Nr./EN: 1.4548 |
Pilih Daxun dan buat pelanggan Anda puas.

Pengiriman cepat
We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.
17-4PH stainless steel plate advantages:
• Excellent corrosion resistance
• Provides toughness to both the base metal and the weld.
• Ideal for applications that require ease of fabrication, then increased strength/hardness for increased reliability
• The physical properties of 17-4 PH stainless steel plate are dependent on any tempering process performed on the material. If your application requires specific physical properties, please contact a DAHSUN sales representative to ensure this material meets your needs.

Stainless Steel 17-4PH Applications
• Aerospace applications
• Chemical processing equipment
• Oil and petroleum refining equipment
• Food processing equipment
• General metalworking
• Base plates
• Nuclear components
• Food grade stainless steel for processing equipment
• General metalworking applications that call for precipitation-hardening
stainless steel
Kualitas, pengiriman, inspeksi
- Daxun juga melakukan beberapa tes jaminan kualitas. Pengujian ini meliputi uji perataan, uji lubang dan ketahanan, uji mekanis, uji kekerasan, identifikasi positif material, uji ekspansi, dll. Semua pengujian ini memastikan bahwa bahan tersebut cocok untuk aplikasi yang dibutuhkan.
- Selama proses produksi, kami mengukur diameter, ketebalan, dan permukaan produk. Waktu pengiriman standar kami adalah 7-15 hari, kecuali untuk beberapa produk ukuran khusus, waktu pengiriman kami akan bertambah menjadi 20 hari.
Waktu pengiriman kami benar-benar sesuai dengan kontrak. - Mendukung agen pihak ketiga pelanggan untuk pergi ke pabrik untuk pemeriksaan
- Mendukung sampel gratis kepada pelanggan untuk pengujian
- Mendukung inspeksi pabrik di tempat atau video
Dukungan Teknis
Jika Anda memerlukan bantuan teknis tambahan, ahli metalurgi dan staf kami yang berpengetahuan luas akan dengan senang hati membantu. Selain itu, Daxun memiliki laboratorium pengujian bersertifikat-yang pertama dalam industri inventaris multi-logam dan plastik. Ini, menurut pendapat kami, menunjukkan dedikasi kami yang tak tergoyahkan terhadap kualitas dan filosofi kami sebagai pemasok layanan penuh.
Informasi Pemesanan
The purchase order shall include quantity, PSL grade, type or category, API5L reference, diameter, finish, length and any applicable attachments or additional requirements relating to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish or end finish. Bars are solution bright annealed.

17-4PH plate stainless steel Features
Daxun Biarkan merek Anda meningkat dengan cepat
- Galeri
- Toleransi
- Status pengiriman
- Seri produk lainnya
| Toleransi untuk Lembar 2B | |||
| Ukuran | Peringkat Toleransi | ||
| Kelompok 1 | Kelompok 2 | Kelompok 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Toleransi untuk Pelat Canai Panas No.1 | |||
| Ukuran | Peringkat Toleransi | ||
| Kelompok 1 | Kelompok 2 | Kelompok 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Pilihan Status Pengiriman | Kondisi Permukaan |
| Digulung Dingin | 2B |
| 2D | |
| BA | |
| Garis rambut | |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Catatan: | |
| 1. Jika Anda memerlukan status pengiriman yang berbeda dari yang tercantum di atas, mohon konfirmasi dengan kami. | |
| 2. Jika ada pertanyaan atau pesanan, mohon beritahukan kepada kami persyaratan tambahan yang tidak disebutkan di sini. | |
| Status Pengiriman | |
| Pilihan Status Pengiriman | Kondisi Permukaan |
| Canai Panas | No.1 |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Acar | |
| Catatan: | |
| 1. Jika Anda memerlukan status pengiriman yang berbeda dari yang tercantum di atas, mohon konfirmasi dengan kami. | |
| 2. Jika ada pertanyaan atau pesanan, mohon beritahukan kepada kami persyaratan tambahan yang tidak disebutkan di sini. | |
| Kelas | Jenis | Ketebalan | Permukaan |
| Austenitik | 304/304H/304L/304J1 | 0,25-150mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0,3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferit | 430 | 0.4-3.0mm | 2B/BA/NO.4/8K/SB/HL |
| Ferit Ultra Murni | 443 | 0.4-2.0mm | 2B |
| 436L/439/444/441 | 0.5-3.0mm | 2B 、 2D | |
| 409L | 0,4-2,5 mm | 2B 、 2D | |
| Kelas | Jenis | Ketebalan | Asli |
| Baja tahan panas | 309S | 0,5-40mm | CHN |
| 310S | 0,5-40mm | CHN | |
| Baja Dupleks | 2101 | 1,5-50mm | CHN |
| 2304 | 3.0-50mm | CHN | |
| 2205 | 0,5-60mm | CHN | |
| 2507 | 1.0-60mm | SWE / JPN / CHN | |
| Baja Austenitik Super | N08904 | 0,6-50mm | SWE / JPN / CHN |
| S31254 | 0,5-50mm | SWE / JPN / CHN | |
| N08926 | 0,5-50mm | SWE / JPN / CHN | |
| N08367 | 0,5-50mm | SWE / JPN / CHN | |
| Paduan Dasar Nikel | N08031 | 1.0-50mm | AS / JPN / GER |
| N08810 / N08800 | 0,8-50mm | AS / JPN / CHN | |
| N08028 | 1.0-20mm | AS / JERMAN / JPN | |
| N08020 | 1.0-20mm | AS / JERMAN / JPN | |
| N08825 | 0,8-40mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0,5-50mm | AS / JERMAN / JPN | |
| N06022 | 1.0-50mm | AS / JERMAN / JPN | |
| N06625 | 0,8-20mm | AS / GER / CHN | |
| N04400 | 1.0-20mm | AS / JERMAN / JPN | |
| N06600 | 1.0-50mm | US / GER / JPN / CHN | |
| N02201 | 0,5-20mm | AS / JPN | |
| Titanium | TA1/Gr1 | 0,5-50mm | JPN / CHN |
| TA2/Gr2 | 0,5-50mm | JPN / CHN | |
| Bahan Pengelasan | ERNiCrMo-13 | 1.2 、 2.4mm | GER |
| ERNiCrMo-3 | 2.4mm | GER | |
| ERNiCrMo-4 | 2.4mm | AS |
The surface and shape of 17-4PH stainless steel plate (7)
Informasi yang tersedia untuk referensi dan diunduh
Daxun adalah produsen pelat baja tahan karat yang dapat dipercaya
Sebagai produsen profesional, Daxun memastikan bahwa semua produk yang kami hasilkan berkualitas tinggi. Oleh karena itu, kami memastikan bahwa semua pelat baja tahan karat disertifikasi oleh ISO9001, SGS, CE, OQC, dan lebih banyak standar kualitas internasional, serta memiliki kontrol kualitas yang ketat untuk memastikan bahwa pelat baja tahan karat memiliki lebih sedikit cacat. Di Daxun, yakinlah bahwa semua produk tahan lama, berkualitas tinggi, dan berkinerja tinggi.
Proyek dan produk hot case terbaru
Produk Terkait (13)
Pemasok Lembaran Baja Tahan Karat Terkemuka di Cina
Daxun can provide upon request: Alloy 17-4 (H900, UNS S17400) plates.
CORROSION RESISTANCE:
- Withstands corrosive attacks better than any of the standard hardenable stainless steels.
- Comparable to Alloy 304 in most media.
- Corrosion resistant in some chemical, petroleum, dairy, and food process industries.
- Subject to crevice or pitting attack if exposed to stagnant sea water for any length of time.
WELDABILITY:
- Successfully welded by most common fusion and resistance methods.
- Should not be joined by oxyacetylene welding.
- Generally no pre-heating required.
- Inter-pass temperature must be limited to 248°F.
- Better toughness is obtained in the weld after a complete heat treatment.
ELEVATED TEMPERATURE USE:
- Excellent resistance to oxidation to approximately 1100°F.
- Long-term exposure to elevated temperature can result in reduced toughness in the precipitation hardened conditions.
PROCESSING – HOT FORMING:
- To forge, heat uniformly to 2150 / 2200°F and hold for half hour per inch.
- Preferred temperature range for hot forming is at 650-900°F, while the steel is still austenitic.
- To ensure the best condition for the hardening operations, the forgings must be re-heat treated at 1875-1925°F.
- Cool forgings to below 90°F to ensure grain refinement.
PROCESSING – COLD FORMING:
- Alloy 17-4 is limited to mild operations since in the annealed (solution treated) condition the material is hard.
- For severe cold working the material should be heat treated to condition H1150. This will help prevent possible cracking.
- Bend radius in excess of 7T is often required.
- To improve stress corrosion resistance after cold forming, re-aging at the precipitation-hardening temperature is recommended.
MACHINABILITY:
- Can be machined in both solution-treated and precipitation-hardening conditions.
Sifat Mekanis
- Type 17-4PH stainless steel has excellent mechanical properties. For applications requiring high strength and hardness as well as corrosion resistance, Type 17-4PH stainless is an outstanding choice, and it is more cost effective than many high nickel non-ferrous alloys.
17-4PH Grade Stainless Steel Sheets in a Variety of Finishes
Lembaran baja tahan karat kami (kadang-kadang disebut lembaran baja) tersedia dalam berbagai hasil akhir yang indah: hasil akhir yang disikat, hasil akhir yang halus 2B, atau hasil akhir cermin 8K.
Sisi akhir dari setiap lembaran baja tahan karat yang kami suplai dilapisi dengan film. Film ini mudah terkelupas setelah fabrikasi atau pemasangan dan melindungi permukaan material dari keausan dan bekas. Sisi belakang belum selesai.
17-4ph Grade Stainless Steel Sheet is the most commonly used variety. It is easily weldable, formable, and has good corrosion resistance.
Kami dapat membantu menyediakan lembaran baja tahan karat dalam berbagai ukuran yang dibutuhkan.
Untuk memenuhi kebutuhan spesifik Anda, lembaran baja tahan karat kami tersedia dalam tiga sentuhan akhir dan berbagai ukuran. Kami dapat dengan mudah menyediakan ukuran khusus apa pun yang Anda butuhkan dengan layanan pemotongan gratis tanpa batas.
Kami dapat memenuhi kebutuhan ukuran apa pun antara 0,3 dan 30 mm dalam ketebalan dan antara 50 x 50 mm dan 2500 x 1250 mm. Selain itu, kami menyediakan pemotongan gratis tanpa batas untuk setiap pesanan, menggunakan mesin pemotong yang canggih untuk memenuhi kebutuhan Anda secara tepat.
Pesan Lembaran Baja Tahan Karat melalui Telepon atau Online.
Tidak pernah ada cara yang lebih mudah untuk mendapatkan lembaran baja tahan karat. Cukup lihat instruksi sederhana dan terperinci di situs web kami. Atau, staf penjualan kami akan dengan senang hati menerima pesanan Anda atau menjawab pertanyaan apa pun saat Anda menelepon +86 13382898899 atau email [email protected].
Waktu pengiriman kami hanya satu hingga dua hari.
Catatan Keselamatan Penting:
Tepi lembaran logam yang kami jual tidak dipoles, digiling atau difinishing, sehingga bisa jadi tajam, sama seperti tepi lembaran baja tahan karat lainnya. Kami mengingatkan pengguna untuk menggunakan, memasang, dan menangani perangkat ini dengan hati-hati.
17-4 stainless steel may not be the only choice for the job. At Daxun Alloys, we offer a wide variety of materials suitable for your job.
Like all alloy steels, when 17-4 stainless steel is hardened, it becomes magnetic.
The alloy is considered to be highly resistant to rust, particularly in comparison to other types of stainless steel. However, 17-4 stainless steel can still rust in certain conditions if it is exposed to harsh environments for long periods of time and not properly maintained.
Prices will vary depending on your project, so the best way to get accurate pricing is to contact Daxun for a custom quote.
Kami dapat menyediakan sampel lembaran baja tahan karat untuk Anda periksa kualitasnya. Sampel gratis dan Anda hanya membayar ongkos kirim.
Kami telah mengekspor ke lebih dari 42 negara, seperti Kanada, Chili, Kuwait, Jerman, Korea Selatan, Arab Saudi, Singapura, dll.
MOQ kami adalah 1 ton untuk lembaran baja tahan karat.
Pesanan percobaan dapat dikirim dalam waktu satu minggu. Untuk pesanan reguler, kira-kira membutuhkan waktu dua minggu.