스테인리스 스틸 막대 및 바

  • Round stainless steel bar, round steel
  • Rectangular stainless steel square bar
  • Special shaped stainless steel bar

Daxun Stainless steel rod and bar

Hot rolled rod

Stainless steel rod and bar is heated and rolled through multiple passes in a rolling mill. It has complete specifications and its performance meets standards and requirements.

Cold drawn bright Stainless steel rods

Cold-drawn Stainless steel rods are Stainless steel rods drawn under cold working conditions. They have a smooth surface and can also be polished and ground.

Forged Stainless steel rod and bar

Forged Stainless steel rods are forged multiple times to improve the mechanical properties and higher strength of the Stainless steel rods.

Daxun Stainless steel rod and bar

제품 매개변수: 스테인리스 스틸 로드
사양 ASTM A276, ASME SA276 / ASTM A479 ASME SA479
치수 EN, DIN, JIS, ASTM, BS, ASME, AISI
Stainless Round Bars 4mm ~ 500mm 범위의 외경
Stainless Bright Bars 4mm~100mm 범위의 외경
Stainless Hex Bars 18mm - 57mm(11/16인치 ~ 2-3/4인치)
완료 블랙, 밝은 광택, 러프 턴, NO.4 마감, 무광 마감, BA 마감
길이 1~6미터, 맞춤형 절단 길이
양식 원형, 정사각형, 육각(A/F), 직사각형, 빌렛, 잉곳, 단조 등.

Our network of service centers stock stainless steel bar products for fast, ready supply of bar in common sizes and alloys.We also produce custom-sized stainless steel rods and can arrange inventory schedules for quick turnaround in a timely manner if quantities are below factory minimums.Daxun Alloys stocks stainless steel round bars with diameters ranging from 1/16″ to 26″. Round bars are available in nearly every grade of stainless steel, including 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205, and Alloy 20. Heat treated stainless steel round bars are offered in 17-4PH, H900 temper (on request), H1025, H1150, Double H1150, and H1150M. Other heat-treated tempers can be manufactured upon request. We stock the following 400 series stainless steels: 410, 430, and 416. We also carry 303, 304, and 316/L precision and bearing quality stainless steel round bars. The majority of our inventory consists of our unique machined bar grades: stainless steel round bars that are melted to consistent standards to increase machinability and lower total cost per component. Our stainless steel bar processing machinery allows Daxun Alloys to produce to our customers’ exact specifications.

Daxun has a complete stainless steel round bar production technology cycle: from raw material processing to finished product production with a high degree of mechanical processing.

자세히 보기

Materials and characteristics of various stainless steel rods

Each stainless steel rod material has its different usage scenarios.

이 제품에 대한 자세한 정보를 보려면 이미지를 클릭하세요.

이 제품에 대한 자세한 정보를 보려면 이미지를 클릭하세요.

이 제품에 대한 자세한 정보를 보려면 이미지를 클릭하세요.

이 제품에 대한 자세한 정보를 보려면 이미지를 클릭하세요.

이 제품에 대한 자세한 정보를 보려면 이미지를 클릭하세요.

이 제품에 대한 자세한 정보를 보려면 이미지를 클릭하세요.

이 제품에 대한 자세한 정보를 보려면 이미지를 클릭하세요.

stainless steel rods and bar 19
309s stainless steel rod and bar

이 제품에 대한 자세한 정보를 보려면 이미지를 클릭하세요.

20 Products Found.

Stainless Steel Rod Small Diameter

Bright surface, precise dimensions

Bright surface, precise dimensions

Bright surface, precise dimensions

Bright surface, precise dimensions

12개의 제품이 발견되었습니다.

Stainless steel rod production process

With our reliable stainless steel rods, their performance can be customized to suit your application.

Main features of titanium rod

작업성

Stainless steel rod materials are excellent options for various applications, like fabrications. They are simple to work with and ideal for massive industrial and intricate usage.

귀중한 금속

The smarter option material SS rod have far lesser drawbacks than other alloys. They provide excellent value, cost-effectiveness, and durability. SS is an easy-to-clean metal material.

저렴한 비용

Since SS rods have a lower melting point, they don’t need special tools. They are also durable and lasting materials, making industries save on working and maintenance costs.

내식성

The chemical compositions on stainless steel rods protect them from rust. Their corrosion resistance feature increases with necessarily polished finishes, perfect for kitchen appliances.

Daxun’s Stainless steel rods manufacturing capabilities

Forming capabilities include state-of-the-art radial forging machines, heat treatment furnaces, melting furnaces and rolling mills for manufacturing titanium rods, as well as a unique hydroforming process for manufacturing parts.

Daxun’s heat treatment furnace

Stainless steel rod heat treatment uses advanced heat treatment furnace equipment to ensure the stability and high performance of the material.

Daxun’s smelting ability

Daxun Stainless Steel uses the world’s most advanced vacuum induction furnace, vacuum consumable furnace, and electroslag furnace to reduce impurities during the smelting process and improve the performance of the finished stainless steel rods.

Powerful Stainless steel rod solutions

inventory
services-

Daxun is one of the few vertically integrated companies and is the world’s leading manufacturer of stainless steel rods and rolled products.

기술 정보

재료 테스트 인증

당사의 모든 스테인리스 스틸 소재는 ISO9001:2008, ISO14001:2014, AAA 인증, CQGC 인증 등 다양한 산업 표준의 인증을 받았습니다. 또한 ISO9001:2015 품질 경영 시스템 인증도 보유하고 있습니다.

우수한 애프터 서비스

당사의 지원과 서비스는 거래 시작부터 제한되지 않습니다. 주문을 받은 후에도 TuoLian은 계속해서 우수한 애프터 서비스를 제공할 것입니다. 주문에 대한 지원과 보증을 계속 제공할 것입니다.

All our stainless steel round bars and rods are packed as per international standards to prevent any possible damage or loss. By default, we bundle finished pipes together in bulk using thick woven plastic bags. However, for some specialty pipes that are susceptible to dirt, scratches, pressure, or rough handling, we use wooden crates for protection.

By default, we will quote based on sea transportation, such as FOB, CFR, CIF and the like for most enquiries or orders. Quotation based on air transportation is also optional upon your request for urgent demands.

Application cases of stainless steel rods in different industries.

항공우주

It can be used in stainless steel structural parts such as aircraft landing gear, aerospace equipment, rockets, artificial satellites, missiles, spacecraft shells, blades, etc.

석유화학

Serving the chemical industry/can be used in: electrolyzers, blowers, reaction towers, heat exchangers, pressure shafts, distillation towers, valves, pumps, etc. When you choose Daxun as your stainless steel rod supplier, you know we truly understand the oil and gas industry. Contact Daxun today.

Military armor

Due to its superior performance, stainless steel materials are often used to manufacture car bodies, armor, turrets, etc. At the same time, stainless steel is gradually being explored at home and abroad to manufacture road wheels, balance shafts, and gear boxes. Stainless steel rods will become the most popular material for the construction of armored vehicles.

배송 필드

Stainless steel rods are used to manufacture ship pumps, valves, drive shafts, propellers, whip antennas, acoustic devices, fire-fighting equipment and other components.

해양 엔지니어링

Deep-sea exploration equipment Deep-sea exploration is one of the important directions in the field of marine engineering. Stainless steel rods have become an ideal material for various deep-sea exploration equipment due to their corrosion resistance and high strength. Drill pipes, deep-sea buoys, detectors, sonar equipment, etc. can all use stainless steel rods to ensure long-term reliable operation in harsh marine environments.

제약, 생물학

Serving the pharmaceutical and biopharmaceutical industries has been a welcome challenge for Daxun. From raw material selection to delivery, we have developed high purity and ultra-high purity services to meet and exceed industry standards. When only the best stainless steel rods can meet the demand, more and more pharmaceutical and biopharmaceutical companies trust Daxun.

전력 분야

Daxun serves the power generation industry and is able to combine technical expertise and experience to produce the best stainless steel rods available today. When you choose the best, you get the best. Follow what countless other companies have done – trust Daxun. High-demand industries need big news.

about-feature3
Let us be your trustworthy Stainless steel Rod supplier

Our stainless steel products are fully certified and traceable. We supply the highest quality stainless steel to leading industries including aerospace, industrial, medical, marine and military.

기술 정보

지름(mm) Durface 길이(mm) 댓글
φ3.0-12.0 bright 3000 AAA
φ14.0-25.0 bright 6000 AAA
φ25.0-50.0 bright 6000 AAA
>80 ~ ≤120 Bright/primary color 6000 AAA
>120 ~ ≤140 Bright/primary color 6000 AAA
>140 ~ ≤180 Bright/primary color 6000 AAA
>180 ~ ≤200 Bright/primary color 6000 AAA
>200 ~ ≤220 Bright/primary color 6000 AAA
>220 ~ ≤240 Bright/primary color 6000 AAA
>240 ~ ≤250 Bright/primary color 6000 AAA
>250 ~ ≤300+

 

Bright/primary color

 

6000

 

AAA

 

사이즈에 대해 더 자세히 알고 싶으시면 Daxun에 문의하세요.

Tolerance for Hot Rolled Round Bars
크기 허용 오차 순위
그룹 1 그룹 2 그룹 3
>7 ~ ≤20 ±0.25 ±0.35 ±0.40
>20 ~ ≤30 ±0.30 ±0.40 ±0.50
>30 ~ ≤50 ±0.40 ±0.50 ±0.60
>50 ~ ≤80 ±0.60 ±0.70 ±0.80
>80 ~ ≤110 ±0.90 ±1.00 ±1.10
>110 ~ ≤150 ±1.20 ±1.30 ±1.40
Tolerance for Hot Forging Round Bars
크기 허용 오차 순위
그룹 1 그룹 2
>50 ~ ≤60 0.5 1
>60 ~ ≤80 1 1.5
>80 ~ ≤100 1.5 2
>100 ~ ≤120 1 1.5
>120 ~ ≤140 1.5 2
>140 ~ ≤160 1 2
>160 ~ ≤180 2 3
>180 ~ ≤200 3 4
>200 ~ ≤220 2 3
>220 ~ ≤240 3 4
>240 ~ ≤250 4 5
>250 ~ ≤300 5 6
Tolerance for Cold Drawn Round Bars
크기 허용 오차 순위
H8 H9 H10 H11 H12 H13
3 0 ~ -0.014 0 ~ -0.025 0 ~ -0.040 0 ~ -0.060 0 ~ -0.100 0 ~ -0.140
>3 ~ ≤6 0 ~ -0.018 0 ~ -0.030 0 ~ -0.048 0 ~ -0.075 0 ~ -0.120 0 ~ -0.180
>6 ~ ≤10 0 ~ -0.022 0 ~ -0.036 0 ~ -0.058 0 ~ -0.090 0 ~ -0.150 0 ~ -0.220
>10 ~ ≤18 0 ~ -0.027 0 ~ -0.043 0 ~ -0.070 0 ~ -0.110 0 ~ -0.180 0 ~ -0.270
>18 ~ ≤30 0 ~ -0.033 0 ~ -0.052 0 ~ -0.084 0 ~ -0.130 0 ~ -0.210 0 ~ -0.330
>30 ~ ≤50 0 ~ -0.039 0 ~ -0.062 0 ~ -0.100 0 ~ -0.160 0 ~ -0.250 0 ~ -0.390
>50 ~ ≤80 0 ~ -0.046 0 ~ -0.074 0 ~ -0.120 0 ~ -0.190 0 ~ -0.300 0 ~ -0.460
배송 상태 선택 표면 상태
Forged 블랙
광택
열간 압연 블랙
광택
밝음
피클
콜드 드로잉 광택
밝음
참고:
1. 위에 나열된 것과 다른 배송 상태가 필요한 경우 당사에 문의해 주시기 바랍니다.
2. 문의 또는 주문 시 여기에 표시되지 않은 추가 요구 사항이 있으면 친절하게 알려주시기 바랍니다.

  • “Thank you Daxun for the extremely durable, world-class quality Stainless Steel rods. I also appreciate the professional customization service. I am happy to work with you for my Stainless Steel rod needs. Looking forward to working with you next time!”

    중동에 위치한 고객의 사용 후기
  • “Daxun has always been a trustworthy company when it comes to Stainless Steel rods. All the Stainless Steel rods I have purchased are of very high quality. I ordered Stainless Steel rods at a very low price at Daxun. The staff was also happy to answer my questions .” Asked questions and was impressed with my needs! “

    유럽과 미국에 위치한 고객의 사용 후기
  • “We are very impressed with the quality and superiority of  Daxun Stainless Steel rods. They are available in a variety of sizes and are perfect for our needs. Additionally, we are very grateful for their affordable prices and service.”

    러시아에 위치한 고객의 사용 후기

Daxun 합금

Regarding Stainless Steel rods, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.

재고가 있나요?

예, 완벽한 사양과 재고를 보유하고 있으며 고객의 요구 사항을 신속하게 충족할 수 있습니다.

사용자 지정할 수 있나요?

예, 사용자 지정이 가능합니다. 당사에 문의하여 맞춤형 사양과 수량을 보내주시면 됩니다.

상품을 어떻게 배송하나요?

당사의 운송 방법에는 일반적으로 해상 운송, 육상 운송 및 해상 운송이 포함됩니다. 빠르고 안전하게 도착합니다.

가격은 어떻게 되나요?

생산량이 많기 때문에 원가가 훨씬 낮아져 가격도 저렴합니다.

품질은 어떤가요?

당사는 제품 품질을 매우 중요하게 생각하며 다양한 품질 시스템 테스트를 통과했습니다.

오늘 문의 보내기
빠른 견적