Grade 7 (Ti-0.15Pd) Titanium Alloy Plate Manufacturer - Daxun Alloy

As a leading supplier of titanium in China, Daxun provides high-performance titanium plates to the world.

  • Plate Grade:7학년 UNS R52400
  • Plate Production type:cold rolling, hot rolling, forging.
  • Standard:ASTM B 265,ASME SB265,AMS491 etc
  • Features:High strength, Lightweight, High-temperature resistance
  • Surface:bright, polished, pickled, sandblasted, etc.
  • Size:0.3mm ≤ 1000mm ≤ 2500mm or as your request

————Daxun produces titanium sheets in China to meet the diverse and ——고객의 까다로운 요구 사항!

Providing High-quality Grade 7 Titanium Plate to Serve Customers Worldwide

Grade 7 titanium plate (Ti Grade 7 / UNS R52400) is a palladium-enhanced, commercially pure (CP) titanium alloy specifically engineered for supreme corrosion resistance in aggressive environments. It consists of titanium (≥99%) with a critical addition of 0.12–0.25% palladium (Pd), which fundamentally alters its electrochemical behavior. This palladium modification dramatically improves resistance to reducing acids (e.g., sulfuric, hydrochloric, phosphoric), chloride solutions (including seawater and brines), and crevice/pitting corrosion—scenarios where standard CP grades like Grade 2 would rapidly degrade. While retaining the inherent advantages of titanium—low density (~4.5 g/cm³), high strength-to-weight ratio, excellent weldability, and biocompatibility—Grade 7 exhibits superior performance at elevated temperatures (up to ~400°C/750°F) and in highly oxidizing or acidic conditions. Its passive oxide layer, stabilized by palladium, provides unparalleled protection against chemical attack, making it one of the most corrosion-resistant metallic materials available.

Where is Grade 7 titanium plate used?

Grade 7 titanium plate is extensively used in chemical processing for critical components like reactor vessels, heat exchangers, piping systems, and agitators handling acids, chlorides, or organic solvents. In marine and offshore engineering, it serves in seawater desalination plants, heat rejection systems, and subsea equipment exposed to high-salinity environments. The alloy also excels in pollution control systems (e.g., flue-gas desulfurization scrubbers), pharmaceutical manufacturing, and medical implants (e.g., orthopedic devices) due to its inertness and longevity. Despite its higher initial cost—driven by palladium content—Grade 7 delivers exceptional lifecycle value by minimizing downtime, maintenance, and replacement costs in corrosive service. Its reliability in preventing catastrophic failures ensures safety and efficiency in applications ranging from nuclear waste containment to aerospace fluid systems, justifying its selection as a premium solution for the most demanding corrosion challenges.

데이터

요소 기호 구성 범위(% 무게)
티타늄 Ti 밸런스(>99%)
팔라듐 Pd 0.12-0.25%
Iron Fe ≤0.30%
산소 O ≤0.25%
탄소 C ≤0.08%
질소 N ≤0.03%
수소 H ≤0.015%
기타 요소 ≤0.40%(단일 요소)

주요 특징

  • 무게 대비 강도 비율: 순수 티타늄(1~4등급)과 비슷하지만 Ti-6Al-4V(5등급) 또는 Ti-3Al-2.5V(9등급)보다 낮습니다. 기계적 강도보다 내식성에 최적화되어 있습니다.
  • 내식성: 환원성 산(예: HCl, H₂SO₄), 염화물 및 틈새 부식 환경에서 탁월한 성능을 발휘합니다. 팔라듐(Pd) 안정화로 인해 모든 상업용 순도 등급(1~4등급) 및 5/9등급보다 강한 화학 매질에서 뛰어난 성능을 발휘합니다.
  • 생체 적합성: 완전 무독성이며 MRI와 호환됩니다. 수술 기구 및 화학 처리 장비에 적합하지만 영구 임플란트에는 사용되지 않습니다(23등급 선호).
  • 형성성: 순수 티타늄의 우수한 냉간 성형성, 용접성 및 가공성을 유지합니다. 5/9 등급보다 훨씬 쉽게 제작할 수 있어 특수 공구 없이 복잡한 형상을 구현할 수 있습니다.
속성 가치(임페리얼) 값(메트릭)
밀도 0.163 lb/in³ 4.51g/cm³
녹는점 3,000-3,050°F 1,650-1,680°C
열 전도성 9.5 Btu/(hr-ft-°F) 16.4W/(m-K)
열팽창 계수 4.8 × 10-⁶/°F 8.6 × 10-⁶/K
전기 저항 1.78 × 10-⁶ Ω-cm 1.78 μΩ-m

 

속성 가치(임페리얼) 값(메트릭)
인장 강도 50,000-65,000 psi 345-450 MPa
수율 강도 30,000-45,000 psi 207-310 MPa
신장 20-30% 20-30%
경도(브리넬) 120-160 HB 120-160 HB
탄성 계수 14.9-16.0 × 10⁶ psi 103-110 GPa

 

프로젝트의 성공을 위해 Daxun을 선택하세요.

Common applications

Grade 7 titanium plates and sheets are primarily utilized in applications requiring exceptional corrosion resistance, particularly in aggressive chemical environments, combined with moderate strength and excellent weldability.

  1. Applications include chemical processing equipment such as heat exchangers, reactor vessels, and piping systems that handle chlorides, acids, and other corrosive substances.
  2. Industrial applications include marine components, offshore oil and gas equipment, and desalination plants where exposure to saltwater and harsh chemicals is common.
  3. Pharmaceutical and food processing equipment that demands high purity standards and resistance to corrosive cleaning agents.
  4. Laboratory equipment and analytical instruments that require superior chemical resistance for accurate testing and processing.
  5. Pollution control systems, including scrubbers and ductwork in power plants and industrial facilities that handle corrosive exhaust gases.

빠른 배송

Daxun provides customers with timely and fast delivery of grade 7 titanium plate products. Behind the speed is the system support from professional production capacity, and information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected.

맞춤 커팅

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • 워터젯 절단
  • 레이저 커팅
  • Plasma cutting
  • Wire cutting
  • Bending
  • Slitting
  • 톱질

패키징

We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- 상자 및 상자
• Shrinkwrap
- 목재 팔레트
- 나무 상자

기술 지원

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Daxun Grade 7 Titanium sheet Let your brand improve rapidly

아래 나열된 제품 외에 사용 가능한 다른 금속 제품은 여기에 나열되어 있지 않습니다. DAXUN이 제조 및 공급할 수 있는 기타 금속 제품으로는 탄탈륨, 니오븀, 지르코늄, 하프늄, 니켈, 구리 등이 있으며 주로 판재, 바, 튜브 형태입니다.
제품/처리 표준 등급/크기
티타늄 플레이트, 시트, 코일- ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(두께:( 0.0197”-6”)최대 폭: 12피트, 최대 길이: 50피트)
AMS-T-9046
티타늄 및 티타늄 합금 시트, 플레이트
상업적으로 순수한 티타늄(CP)
코드 지정 수율 강도
최소, KSI 1 /
CP-1 Gr1 70
CP-2 Gr2 55
CP-3 Gr3 40
CP-4 Gr4 25
알파 티타늄 합금(A)
코드 지정 구성
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
알파-베타 티타늄 합금(AB)
코드 지정 구성
AB-1 Gr5 6A1-4V
AB-2 Gr5 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
베타 티타늄 합금(B)
코드 지정 구성
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
처리 중입니다:
열간 압연 냉간 압연
사용 가능한 성적:
CP 1등급 6Al-2Sn-4Zr-2Mo(6-2-4-2) 등급
CP 2등급 6Al-4V ELI 등급(이전 23등급)
7학년 6Al-6V-2Sn(6-62) 등급
19학년 8알-1모-1V 등급(8-1-1)
5등급(6Al-4V) 9등급(3Al-2.5V)
6등급(5Al-2.5Sn) CP 3등급
애플리케이션
화학 산업 해수 담수화
석유화학 산업 항공우주
기계 가공 분야, 자동차 분야 휴대폰 구성 요소 필드.

최근 인기 있는 사례 프로젝트 및 제품

Grade 7 Titanium Plate and sheet
Grade 7 Titanium Plate and sheet
티타늄 플레이트 및 시트
티타늄 플레이트 및 시트
티타늄 플레이트 및 시트
티타늄 플레이트 및 시트
What is Grade 7 titanium plate and what makes it unique?

Grade 7 titanium plate is a commercially pure titanium alloy with the addition of 0.12-0.25% palladium, which significantly enhances its corrosion resistance. This combination maintains the excellent formability and weldability of pure titanium while providing superior resistance to reducing acids and other highly corrosive environments.

What are the mechanical properties of Grade 7 titanium plates?

Grade 7 titanium plates offer good strength with a minimum yield strength of 275 MPa and minimum tensile strength of 485 MPa. They maintain excellent ductility with approximately 20% elongation, allowing for good formability during fabrication processes.

Can Grade 7 titanium plates be welded easily?

Yes, Grade 7 titanium plates can be welded using standard titanium welding procedures including TIG, MIG, and plasma arc welding. However, proper shielding with inert gas is essential to prevent contamination during welding. The palladium addition does not significantly affect weldability compared to other commercially pure titanium grades.

What surface finishes are available for Grade 7 titanium plates?

We offer Grade 7 titanium plates in various surface finishes including hot-rolled, pickled, sandblasted, and polished finishes. Custom surface treatments can also be provided based on specific application requirements.

How do you ensure the quality of your Grade 7 titanium plates?

Our Grade 7 titanium plates undergo strict quality control including chemical composition analysis, mechanical property testing, and ultrasonic inspection. We provide full material traceability and certification with each order, ensuring compliance with applicable standards such as ASTM B265 and AMS 4902.

What lead times can customers expect when ordering Grade 7 titanium plates?

Standard lead times for Grade 7 titanium plates typically range from 2-4 weeks depending on size, thickness, and quantity requirements. We also maintain a stock of commonly used dimensions for immediate delivery and can accommodate urgent requests when possible.

견적을 받거나 시장 정보를 최대한 빨리 파악하려면 어떻게 해야 하나요?

“문의하기” 페이지의 양식을 작성하거나 영업 관리자(+86 13382898899)에게 전화하시면 최대한 빨리 연락드리겠습니다. WhatsApp은 온라인 상태이며 이메일([email protected])은 6시간 이내에 확인합니다. 모든 문의나 메시지는 신속하게 답변해 드립니다. 또한 매주 고객과 시장 정보를 공유합니다.

샘플을 받을 수 있나요?

We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.

이미 수출한 국가는 어디인가요?

캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.

오늘 문의 보내기
빠른 견적