Grade 12 Ti-0.3Mo-0.8Ni Alloy Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:Grade 12 - UNS R53400
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Titanium tube density The density of grade 12 titanium is approximately 4.51 g/cm3
  • Standards:ASTM B338、ASTM B861
  • Softest Ti,High ductility, Very corrosion resistant, good cold formability

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

Grade 12 Titanium Alloy Pipe Manufacturer - Daxun Alloy

Provide High Quality Grade 12 Titanium Pipe to Customers Around The World
Grade 12 titanium pipe is a specialized tubing made from Ti-0.3Mo-0.8Ni titanium alloy, which belongs to a specific grade in the titanium alloy pipe family. This material is created by adding 0.3% molybdenum and 0.8% nickel to pure titanium, significantly enhancing its corrosion resistance, particularly in acidic environments and chloride media. Grade 12 titanium pipe complies with international standards such as ASTM B338 or ASTM B861, featuring a density of approximately 4.51 g/cm³, tensile strength of about 483 MPa, and yield strength of around 345 MPa, while maintaining the lightweight characteristics typical of titanium materials.

Where is Grade 12 titanium pipe used?
Compared to pure titanium, Grade 12 titanium pipe offers superior resistance to crevice corrosion and stress corrosion cracking, making it particularly suitable for chemical processing equipment, heat exchangers, oil and gas industries, and seawater treatment systems. This material provides longer service life and lower maintenance costs while maintaining excellent mechanical properties, making it highly favored in high-end industrial applications and an ideal choice for handling corrosive fluids.
Chemical processing plants utilize it for heat exchangers, reactor vessels, and piping systems handling aggressive acids and chlorides. Marine and offshore installations employ it in seawater cooling systems, desalination equipment, and subsea components, leveraging its exceptional resistance to saltwater corrosion and biofouling. In the oil and gas sector, it serves in downhole tubing, Christmas tree components, and production equipment exposed to sour environments with H₂S and CO₂. Power generation facilities specify Grade 12 titanium for condenser tubes and heat exchangers in cooling systems, while industrial pollution control systems incorporate it in scrubbers and flue gas desulfurization units that handle corrosive gases and acidic condensates.

Key Performance

Strength-Ductility Balance:

  • Tensile Strength: 483 MPa (annealed state) – Matches Grade 2 but with superior corrosion resistance.
  • Yield Strength: 345 MPa (min) – Exceeds Grade 2 (275 MPa), suitable for pressure-containing components.
  • Elongation: 18% (min) – Exceptional ductility for cold forming, flaring, and high fatigue resistance.
  • Density: 4.51 g/cm³ – 60% lighter than steel, ideal for weight-sensitive applications.

Corrosion Resistance:

  • Core Mechanism: Synergistic effect of Molybdenum (0.3%) and Nickel (0.8%) stabilizes the passive oxide layer.
  • Pitting/Crevice Corrosion Resistance:
    • Outstanding performance in seawater, chloride solutions (e.g., NaCl, MgCl₂), and sour gas (H₂S) environments.
    • Resists reducing acids (e.g., H₂SO₄, HCl) where stainless steels fail.
  • Advantages vs. Other Grades:
    • Outperforms Grade 2 in reducing acids and chlorides.
    • Superior to Grade 9 in high-temperature acidic media (e.g., chemical processing).
    • Immune to corrosion in oxidizing media (e.g., HNO₃) and aggressive chemical environments.
  • Optimal Heat Treatment: Annealed at 595°C to maximize corrosion resistance and ductility.
Seguir leyendo

Datos

Elemento Minimum (%) Maximum (%)
Titanium (Ti) Saldo Saldo
Molybdenum (Mo) 0.25 0.40
Nickel (Ni) 0.60 0.90
Hierro (Fe) 0.30
Oxygen (O) 0.25
Carbon © 0.08
Nitrogen (N) 0.03
Hydrogen (H) 0.015
Other Elements 0.40 (total)
Propiedad Value/Range Unit
Densidad 4.48 g/cm³
Punto de fusión 1650 ± 20 °C
Conductividad térmica 7.2 (at 25°C) W/m·K
Specific Heat 560 (at 25°C) J/kg·K
Resistividad eléctrica 1.7 μΩ·m
Susceptibilidad magnética Paramagnetic
Propiedad Minimum Requirement Typical Value Unit Test Method
Resistencia a la tracción 483 520–620 MPa ASTM E8/E8M
Yield Strength (0.2% offset) 345 380–480 MPa ASTM E8/E8M
Elongation 18 22–30 % ASTM E8/E8M
Hardness ≤ 200 (HV) 150–180 (HV) Vickers ASTM E10
Impact Toughness Not specified 40–60 J ASTM E23

Elevated Temperature Performance

Temperature (°C) Resistencia a la tracción (MPa) Límite elástico (MPa) Alargamiento (%)
100 450–500 320–370 20–25
200 400–450 280–330 18–23
300 350–400 240–290 15–20

 

Elija Daxun para que su proyecto despegue.

Póngase en contacto con Daxun

Advanced Production:Titanium seamless pipe

  • Titanium seamless tubes are hot rolled or hot extruded, straightened, processed with inner and outer diameters, and surface etched. Tubes can be supplied in heat-treated or non-heat-treated forms. Daxun has 100% ultrasonic testing capabilities. Hot rolled tube/hot extruded titanium seamless tube: outer diameter 1.0 mm to 325 mm, wall thickness 0.3 mm to 50 mm, length up to 12000 mm. Cold rolled titanium seamless tube: cold processed tubes are supplied after heat treatment, surface etching, hydrostatic test or ultrasonic inspection according to the requirements of the manufacturing specification. Outer diameter 6 mm to 102 mm, wall thickness 0.5 mm to 20 mm, length up to 9000 mm.
  • (The above is agreed upon by the manufacturer and the customer based on the specific situation)
Póngase en contacto con Daxun

Grade 12 Titanium Tube Features

Grade 12 Titanium Tube is the softest form of titanium and has the highest ductility. It has good cold forming characteristics and offers excellent corrosion resistance. It also has excellent welding properties and high impact toughness.

  • Softest Titanium
  • Highest Ductility
  • Excellent Corrosion Resistance
  • Good Cold Formability
Póngase en contacto con Daxun

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

Póngase en contacto con Daxun

Informes de las pruebas

The test reports we provide include: Factory test certificate for Grade 12 titanium welded pipe and Grade 12 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

Póngase en contacto con Daxun

Applications and standards

Titanium Grade 12 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
Póngase en contacto con Daxun

Calidad, entrega, inspección

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Grade 12 Titanium Welded Pipe and Grade 12 Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • Nuestro plazo de entrega se ajusta estrictamente a lo estipulado en el contrato.
  • Apoyar a las agencias externas del cliente para que vayan a la fábrica a inspeccionar
  • Muestras gratuitas para las pruebas de los clientes
  • Apoyo a la inspección in situ o por vídeo en fábrica
Póngase en contacto con Daxun

Embalaje

Daxun Alloy garantiza la mejor calidad de embalaje, ya que desempeña un papel importante en el transporte internacional de mercancías, donde las mercancías pasan por varios canales para llegar al destino final, por lo que prestamos especial atención al embalaje. Embalamos nuestras mercancías de muchas maneras dependiendo del producto. Embalamos nuestros productos de muchas maneras, tales como:
- Cajas y cajones
- Retráctil
- Palés de madera
- Cajas de madera

Póngase en contacto con Daxun

Asistencia técnica

Si necesita asistencia técnica adicional, nuestro metalúrgico residente y nuestro personal experto estarán encantados de ayudarle. Además, Daxun cuenta con un laboratorio de pruebas certificado, una primicia en la industria de inventarios multimetal y plástico. Esto, en nuestra opinión, demuestra nuestra inquebrantable dedicación a la calidad y nuestra filosofía como proveedor de servicios completos.

Daxun Grade 12 Titanium TUBE Let your brand improve rapidly

Grade 12 titanium tube form (4)

  • Titanium seamless tubes are made by piercing and drawing solid titanium bars, and the hollow part of the tube is made by piercing or hot extrusion. Titanium seamless tubes are ideal for very large diameter to wall thickness ratios and have very good external dimensional tolerances.

  • Titanium welded pipe is a tubular product made of strip titanium that is roll formed and fusion welded along the longitudinal seam. The welding process used by Daxun Alloy does not use any filler metal during the welding process.

  • Titanium square tubes are drawn from round tubes or round tube billets and can be formed into right angles or rounded corners. They can also be cold extruded, which is efficient and low cost. The only disadvantage is that the tolerance will gradually increase.

  • Tubular products are welded and then re-drawn to final size. Welding and drawing is ideal for producing thick walled, large diameter tubes that cannot be welded directly to size but still offer cost savings over seamless tubes. All Daxun welded and drawn tubes are bright annealed.

Proyectos y productos recientes

Grade 12 Titanium pipe and tube
Grade 12 Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium pipe and tube
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
¿Qué grado de titanio es el mejor?

El grado de aleación de titanio que necesita depende del proyecto en el que esté trabajando, ya que cada grado tiene ventajas diferentes.

Todos los grados de aleación de titanio son extremadamente fuertes y resistentes a la corrosión, lo que significa que seguirán funcionando bien en las condiciones más duras.

Los grados superiores de aleación de titanio (5-12) son aleaciones diseñadas para prestaciones específicas. Por ejemplo, la aleación de titanio de grado 12 tiene una excelente resistencia al calor, por lo que es una opción perfecta para intercambiadores de calor de carcasa y tubos, tuberías hidráulicas y equipos de la industria química.

Los grados 1-4 son aleaciones de titanio puro y son la elección perfecta si necesita un material soldable y dúctil para sistemas de tuberías y conductos. Los grados inferiores se utilizan en la industria naval e industrial.

Si está iniciando un proyecto y no está seguro de qué grado de aleación de titanio es el más adecuado para usted, póngase en contacto con nosotros hoy mismo; estaremos encantados de ayudarle.

¿En qué se diferencian los grados superiores de titanio de los inferiores?

En DAXUN, ofrecemos una amplia gama de grados de aleación de titanio, desde el grado 1 hasta el grado 12.

Los grados 1-4 son titanio puro, mientras que los grados superiores son aleaciones.

Los grados de aleación son populares por su elevada relación resistencia-peso.

El grado de aleación de titanio más utilizado que encontramos es el grado 5. Aunque sigue teniendo un alto contenido en titanio, este grado es uno de los más fiables porque puede soportar temperaturas de hasta 600 °F y soportar condiciones extremas.

Las calidades superiores son las preferidas por industrias como la aeroespacial y la naval por su resistencia al desgaste y a la corrosión.

Por el contrario, las calidades inferiores se utilizan principalmente para soldar debido a su menor resistencia.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

¿Influye el grado de titanio en el coste?

Aunque el grado de titanio aumenta ligeramente el coste, el coste total viene determinado principalmente por la forma del titanio que necesite.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

Por desgracia, es difícil dar un precio en línea sin saber mucho sobre su proyecto y para qué se utilizará el titanio.

Afortunadamente, nuestro equipo de expertos está siempre a su disposición para ayudarle y asesorarle en sus necesidades de titanio. Enviando un correo electrónico a [email protected], podremos responderle con algunos consejos y un presupuesto preciso.

Asegúrese de incluir toda la información posible sobre el grado, la forma y la cantidad de titanio que necesita para conocer mejor sus necesidades.

¿Dónde puedo obtener más información sobre las calidades del titanio?

El equipo de DAXUN es experimentado, experto y amable. Con años de experiencia en el sector, lo saben todo sobre el titanio, incluidos sus usos, ventajas y calidades.

Si desea información actualizada sobre el titanio, sus usos y aplicaciones en distintos sectores, no deje de consultar nuestro blog. Nuestros expertos han escrito guías fáciles de seguir a las que siempre podrá recurrir cuando tenga preguntas.

Si sigues teniendo problemas, no dudes en ponerte en contacto con nosotros; estaremos encantados de ayudarte.

Si envía un correo electrónico a [email protected], recibirá una respuesta rápida. Asegúrate de incluir en tu pregunta todos los detalles posibles para que podamos recomendarte una solución adecuada.

¿Cómo obtener un presupuesto O conocer la información del mercado lo antes posible?

Rellene el formulario de la página “Contacto” o llame a nuestro responsable de ventas al “+86 13382898899”, nos pondremos en contacto con usted lo antes posible. Nuestro WhatsApp está en línea, y el correo electrónico ([email protected]) se comprobará en un plazo de 6 horas. Cada consulta o mensaje será respondido con prontitud. Además, compartimos información de mercado con nuestros clientes cada semana

¿Puedo obtener algunas muestras?

Podemos proporcionarle muestras de chapa de acero inoxidable para que compruebe la calidad. La muestra es gratuita y usted sólo paga el flete.

¿A qué países ha exportado ya?

Hemos exportado a más de 42 países, como Canadá, Chile, Kuwait, Alemania, Corea del Sur, Arabia Saudí, Singapur, etc.

¿Cuál es su MOQ?

Nuestro MOQ es de 1 tonelada de chapa de acero inoxidable.

¿Cuál es el plazo de entrega?

Los pedidos de prueba pueden entregarse en una semana. Los pedidos normales tardan unas dos semanas.

Envíe su consulta hoy mismo
Presupuesto rápido