Daxun is an excellent manufacturer of CP Grade 3 titanium rods and bars.
- Titanium bar grade: R50550 / CP TI50A
- Tipos de barras de titanio: barras laminadas, barras estiradas, barras de titanio forjado
- Principales normas: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
- High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.
The global leader in commercially titanium alloy rod manufacturing services
Daxun, specializing in the production of alloy titanium rods for extreme environments
As the strongest of the CP grades, Grade 3 offers an outstanding combination of high tensile strength, excellent corrosion resistance, and good formability. This makes it an ideal material for demanding industrial applications where both durability and fabricability are paramount.This titanium grade provides superior strength compared to CP Grade 2, making it perfect for components that must withstand higher mechanical stresses. Its exceptional corrosion resistance ensures longevity in harsh environments, including seawater, chlorides, and oxidizing acids. The material features excellent weldability using standard techniques, allowing for easy fabrication and assembly, while maintaining good formability for bending and machining into complex shapes. Despite its strength, it retains titanium’s characteristic lightweight properties, contributing to overall weight reduction in final assemblies.
Common Applications:
CP Grade 3 titanium bar finds extensive use across critical industries. In chemical processing, it’s trusted for heat exchangers, pressure vessels, and piping systems. The aerospace sector relies on it for airframe and jet engine components, fasteners, and brackets. Marine engineering applications include desalination plant components, propeller shafts, and offshore hardware. Power generation facilities utilize it for condenser and heat exchanger tubing, while the medical industry values it for surgical implants and instruments where high strength is essential.
Key Properties & Advantages:
- Superior Strength: Significantly stronger than CP Grade 2, making it suitable for components that must withstand higher mechanical stresses.
- Exceptional Corrosion Resistance: Highly resistant to corrosion in a wide range of environments, including seawater, chlorides, and oxidizing acids.
- Excellent Weldability: Can be readily welded using standard techniques, ensuring ease of fabrication and assembly.
- Good Formability: Offers better ductility than many titanium alloys, allowing for bending, forming, and machining into complex shapes.
- Lightweight: Retains the characteristic low density of titanium, contributing to overall weight reduction in final assemblies.
| Especificación | Detalles |
|---|---|
| Material | CP Grade 3 Titanium Bar |
| Estándar | ASTM B348, AMS 4921 |
| Dimensiones | EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN |
| Diámetro | 0.125″ – 14″ (3.175mm – 355.6mm), custom |
| Longitud Alcance | Up to 240″ (6096mm), custom |
| Formulario | Round Bar, Square Bar, Hexagonal Bar |
| Acabado superficial | Estirado en frío, rectificado sin centros, pulido o torneado en bruto, negro, acabado NO.4, acabado BA, acabado mate, etc. |
| Condición | Endurecido y templado, recocido |
| Tolerancia | Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm) |
| Formulario | Barras cuadradas de titanio, lingotes de titanio, barras redondas de titanio, barras rectangulares de titanio, barras triangulares de titanio, barras forjadas de titanio, barras hexagonales de titanio, etc. |
Aleación Daxun supply CP Grade 3 titanium bar sourced from premier mills, ensuring every piece meets stringent international standards for quality and consistency. Our material is fully certified and available in a wide range of sizes, with custom cutting services to meet your exact project specifications. Contact our expert team today for a competitive quote and personalized service for your titanium requirements.
Datos
- Parámetro
- Propiedades mecánicas
- Propiedades físicas
| Elemento | Content (%) |
| Titanium (Ti) |
Balance (~99.1%)
|
| Oxygen (O) | 0.10 – 0.27 |
| Hierro (Fe) | ≤ 0.30 |
| Carbon © | ≤ 0.10 |
| Nitrogen (N) | ≤ 0.05 |
| Hydrogen (H) | ≤ 0.015 |
| Propiedad | Valor |
| Resistencia a la tracción |
~450–485 MPa
|
| Yield Strength |
~380–415 MPa
|
| Elongation | ~20–30% |
| Dureza (Brinell) |
~200–240 HB
|
| Propiedad | Valor |
| Densidad | ~4.51 g/cm³ |
| Punto de fusión |
~1660–1670 °C
|
| Módulo de elasticidad |
~103–107 GPa
|
| Conductividad térmica |
~21.9 W/m·K (at 25°C)
|
| Resistividad eléctrica | ~420 nΩ·m |
Elija Daxun para que su proyecto despegue.
Ventajas de la fábrica de Daxun
El concepto de “Gestión de la Excelencia en el Rendimiento” de Daxun promueve el modelo de gestión “PDCA + Lean”. La tarjeta de visita de la empresa dice “Daxun = Calidad fiable”. Daxun utiliza el sistema ERP para lograr la trazabilidad completa de la variedad, especificación y origen de cada barra de titanio, y defiende y fomenta la lucha contra la falsificación en la industria. Daxun confía en la tecnología para el procesamiento y la personalización, y la alta precisión y la alta calidad son los puntos de referencia de la industria; en términos de servicio, promueve la gestión del ciclo de vida del producto, proporciona soluciones profesionales de selección de materiales y procesamiento antes de las ventas, supervisa estrictamente durante las ventas y proporciona garantías de servicio sin preocupaciones después de las ventas.
CP Grade 3 Titanium Rod Production Method
Daxun produce barras de titanio de alta calidad y alto rendimiento, y también puede fabricar según el acuerdo del cliente:
- Los lingotes de titanio deben someterse a tratamiento térmico y mecanizado, pruebas de ultrasonidos por inmersión, pruebas de propiedades mecánicas, inspección estructural macroscópica y microscópica y otros procesos. Proceso de producción: barras de titanio laminado en caliente - alta eficiencia, rendimiento estable, barras de titanio forjado - tamaño flexible, forja multi-fuego, mejorar el rendimiento integral de barras de titanio, barras de titanio estirado en frío - barras de titanio de alta precisión por lo general de pequeño tamaño; las barras de titanio anteriores se entregan con superficie brillante.
Calidad, entrega, inspección
Daxun performs several quality assurance tests, these tests include mechanical tests like area tensile, chemical analysis, material positive identification – PMI test, micro and macro testing, intergranular corrosion (IGC) test, ultrasonic flaw detection test, pitting and resistance test, hardness test, material positive identification, expansion test etc. All these tests ensure that the CP Grade 3 Titanium Rod and CP Grade 3 Titanium Round Bar material is suitable for the required application. During the production process, we measure the diameter, thickness and surface of the product.
- Nuestro plazo de entrega se ajusta estrictamente a lo estipulado en el contrato.
- Apoyar a las agencias externas del cliente para que vayan a la fábrica a inspeccionar
- Muestras gratuitas para las pruebas de los clientes
- Apoyo a la inspección in situ o por vídeo en fábrica
Embalaje
Daxun Alloy garantiza la mejor calidad de embalaje, ya que desempeña un papel importante en el transporte internacional de mercancías, donde las mercancías pasan por varios canales para llegar al destino final, por lo que prestamos especial atención al embalaje. Embalamos nuestras mercancías de muchas maneras dependiendo del producto. Embalamos nuestros productos de muchas maneras, tales como:
- Cajas y cajones
- Retráctil
- Palés de madera
- Cajas de madera
Asistencia técnica
Si necesita asistencia técnica adicional, nuestro metalúrgico residente y nuestro personal experto estarán encantados de ayudarle. Además, Daxun cuenta con un laboratorio de pruebas certificado, una primicia en la industria de inventarios multimetal y plástico. Esto, en nuestra opinión, demuestra nuestra inquebrantable dedicación a la calidad y nuestra filosofía como proveedor de servicios completos.
Daxun CP Grade 3 Titanium Rods help your brand improve quickly
- Tolerances for CP Grade 3 Titanium Round Bars
|
TAMAÑO NOMINAL
|
h5
|
h6
|
h7
|
h8
|
h9
|
H10
|
H11
|
h12
|
|
DIÁMETRO mm
|
||||||||
| ~ a 3 | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| de 3 a 6 años | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| de 6 a 10 años | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| de 10 a 18 años | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| de 18 a 30 años | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| más de 30 a 50 | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| más de 50 a 80 | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| más de 80 a 120 | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| más de 120 a 180 | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| más de 180 a 250 | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
Types of CP Grade 3 Titanium Rods (3)
Varilla de titanio
Proyectos y productos recientes
Productos relacionados (8)
CP Grade 3 is the strongest of the commercially pure titanium grades, offering approximately 20-30% higher tensile strength than Grade 2. You should choose Grade 3 when your application demands higher mechanical strength and pressure resistance. However, CP Grade 2 is slightly more formable, weldable, and typically more cost-effective. The simple rule is: Choose Grade 3 for strength, and Grade 2 for better formability and value.
Machining CP Grade 3 requires following standard practices for titanium. It demands slower cutting speeds, higher feed rates, and ample coolant compared to steel. Using sharp carbide tools and maintaining a constant cut to avoid work hardening is key. While it machines slower than steel, it can be precisely fabricated into complex shapes with the right equipment and techniques.
Its corrosion resistance is exceptional, particularly in oxidizing environments like seawater, salt spray, and chloride solutions. It forms a stable, passive oxide film that protects it from most forms of corrosion, including pitting and crevice corrosion, making it a premier choice for the chemical processing and marine industries.
Absolutely. All our CP Grade 3 titanium bars comply with international standards such as ASTM B348 y AMS 4921. Every shipment is accompanied by a full Material Test Report (MTR) / mill certification, verifying its chemical composition and mechanical properties for your complete peace of mind.
Rellene el formulario de la página “Contacto” o llame a nuestro responsable de ventas al “+86 13382898899”, nos pondremos en contacto con usted lo antes posible. Nuestro WhatsApp está en línea, y el correo electrónico ([email protected]) se comprobará en un plazo de 6 horas. Cada consulta o mensaje será respondido con prontitud. Además, compartimos información de mercado con nuestros clientes cada semana
Podemos proporcionarle muestras de barras de titanio para que compruebe la calidad. La muestra es gratis y usted sólo paga el flete.
Hemos exportado a más de 42 países, como Canadá, Chile, Kuwait, Alemania, Corea del Sur, Arabia Saudí, Singapur, etc.
Los pedidos de prueba pueden entregarse en una semana. Los pedidos normales tardan unas dos semanas.