x
Envíe su consulta hoy mismo
Presupuesto rápido

Daxun is an experienced carbon steel plate manufacturer

As a leading carbon steel plate supplier and exporter in China, Daxun supplies carbon steel plates to the world.
  • Fabricación: chapa laminada en frío, chapa laminada en caliente, chapa forjada
  • Standards: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Thickness: 0.8mm-60mm
  • Width: 1000mm-1200mm-1500mm-2000mm-2500mm etc.
  • Length: 2438mm-3048mm-6000mm-8000mm etc.
  • Origin: Baosteel, Shagang, Angang, Shandong Steel, Shougang etc.

A global leader in carbon steel plate fabrication services

Carbon steel plates are among the most widely used materials across a wide range of industries. Composed primarily of iron and carbon, these alloys are produced by rolling carbon steel ingots or continuously cast slabs to meet customers’ specific requirements for size or chemical composition.

Available in the “as rolled” or heat treated state, these plates are supplied in standard sizes or custom cut sizes to specific design profiles. High-grade carbon steel plates are integral components in numerous applications, including steel frame buildings, storage tanks, welded structures, freight containers, chimneys, bridges, heat exchangers, pipelines, cranes and a wide range of industrial machinery parts.

Daxun offers a comprehensive range of carbon steel plates and sheets, available in a variety of lengths, widths, thicknesses and diameters to suit varying project specifications. Our inventory includes products that meet ASTM standards, ensuring precise dimensions and weights (in kilograms) to meet stringent industry requirements.

The weight and thickness of a carbon steel plate are key factors in determining its suitability for a particular application, affecting aspects such as structural integrity and load-bearing capacity. By offering a wide range of options, Daxun ensures that customers are able to select the right material to achieve optimal performance in their respective projects.

Datos

AISI AISI 1020, 1045, 4130, 4140
ASTM/ASME (Structural Grades) A36, A572, A588 (CorTen), A656 , A709-36, (36W, 36WT, 36WF), A709-50, A709-HPS70W, A514 (grades B, S, F, H, Q), 100XF, A871
ASTM/ASME (Pressure Vessel Grades) A285-C, A387, A455, A516(N), A517, A612(N)
CSA G40.21 (Structural Grades) 38W-38WT/260W-260WT, 44W-44WT/300W-300WT, 50W-50WT/350W-350WT, 50A-50AT/350A-350AT, 60W-60WT/400W-400WT
ABRASIVE RESISTANT GRADES AR200, AR235, AR400F, AR450F, AR500
SHIPBUILDING AND OFFSHORE GRADES ABS, Lloyds, DNV, A131, API 2H Grade 50
EURONORM EN10025 (Available by special request) S235, S275, S355, S420, S460, S500, S690
MILITARY GRADES MIL-A-12560, MIL-A-46100, MIL-DTL-46177C
Espesor 3/16″ to 8″
Master Width 72″ to 154″

 

China America Japan Germany England France ISO
GB ASTM JIS DIN, DINEN BS, BSEN NF, NFEN ISO 630
Q195 Cr.B SS330; SPHC; SPHD S185 040;A10;S185 S185
Q215A Cr.C; Cr.58 SS330; SPHC
Q235A Cr.D SS440; SM400A E235B
Q235B Cr.D SS440; SM400A S235JR; S235JRG1; S235JRG2 S235JR; S235JRG1; S235JRG2 S235JR; S235JRG1; S235JRG2 E235B
Q255A SS440; SM400A
Q275 SS490 E275A

Elija Daxun y haga que sus clientes queden satisfechos.

Póngase en contacto con Daxun

Stock Carbon Steel Plate Types

Low carbon steel plate
Medium carbon steel plate
High carbon steel plate
Structural steel plate
Wear-resistant steel plate
Pressure vessel plate
Armor and ship plate

Póngase en contacto con Daxun

Advanced machining

As one of the largest processors and distributors of carbon plate products in China, we offer a large supply of high-quality, competitively priced products through our network of metal service centers. We leverage our industry expertise, extensive experience and investment in innovative technologies to provide an unparalleled supply of carbon steel plate.

Póngase en contacto con Daxun

Advantages of Buying Carbon Steel Plates in China

High quality and innovation:
Cost effectiveness:
Diverse product range and customization:
Government support and policy stability:
Combined with these factors, China becomes a strong sourcing source for carbon steel plates, offering a balance of quality, price and reliability.

Póngase en contacto con Daxun

Please contact DAXUN experts when deciding on steel grade

Here are the international grades for carbon steel plates: ASTM Standards: A36, A283 (Grade A, B, C, D), A572 (Grade 42, 50, 55, 60, 65), A516 (Grade 55, 60, 65, 70), A1011 (CS Type A, B, C), A1008 (CS Type A, B, C); EN Standards: S235JR, S275JR, S355JR, S355J2, S460NL; JIS Standards: SS330, SS400, SS490, SPHC, SPHD, SPHE; GB/T Standards: Q195, Q235, Q275, Q345; Other International Grades: DIN 17100 (St37-2, St52-3), ISO 630 (Fe360A, Fe430B).

Carbon steel plate characteristics

Alta resistencia
Resistencia a la corrosión
Resistencia al calor
Resistencia a bajas temperaturas
Protección del medio ambiente
Rendimiento de soldadura

Let your brand improve rapidly

Cold rolled sheet tolerances

Talla Rango de tolerancia
Grupo 1 Grupo 2 Grupo 3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
Hot rolled plate tolerance
Talla Rango de tolerancia
Grupo 1 Grupo 2 Grupo 3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
Grado Tipo Espesor Superficie
Austenítico 304/304H/304L/304J1 0,25-150 mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0,4-80 mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0,3-80 mm 2B/BA/NO.4/8K/SB/HL/NO.1
Ferrita 430 0,4-3,0 mm 2B/BA/NO.4/8K/SB/HL
Ferrita ultrapura 443 0,4-2,0 mm 2B
436L/439/444/441 0,5-3,0 mm 2B、2D
409L 0,4-2,5 mm 2B、2D
Grado Tipo Espesor Original
Acero resistente al calor 309S 0,5-40 mm CHN
310S 0,5-40 mm CHN
Acero dúplex 2101 1,5-50 mm CHN
2304 3,0-50 mm CHN
2205 0,5-60 mm CHN
2507 1,0-60 mm SWE / JPN / CHN
Acero súper austenítico N08904 0,6-50 mm SWE / JPN / CHN
S31254 0,5-50 mm SWE / JPN / CHN
N08926 0,5-50 mm SWE / JPN / CHN
N08367 0,5-50 mm SWE / JPN / CHN
Aleación a base de níquel N08031 1,0-50 mm US / JPN / GER
N08810/N08800 0,8-50 mm US / JPN / CHN
N08028 1,0-20 mm US / GER / JPN
N08020 1,0-20 mm US / GER / JPN
N08825 0,8-40 mm US / GER / SWE / JPN / CHN
N10276 0,5-50 mm US / GER / JPN
N06022 1,0-50 mm US / GER / JPN
N06625 0,8-20 mm US / GER / CHN
N04400 1,0-20 mm US / GER / JPN
N06600 1,0-50 mm US / GER / JPN / CHN
N02201 0,5-20 mm US / JPN
Titanio TA1/Gr1 0,5-50 mm JPN / CHN
TA2/Gr2 0,5-50 mm JPN / CHN
Material de soldadura ERNiCrMo-13 1.2、2.4mm GER
ERNiCrMo-3 2,4 mm GER
ERNiCrMo-4 2,4 mm US

Información disponible para consulta y descarga

Aleación Daxun
Daxun provides all the carbon steel plate data required by customers

Daxun is a trustworthy steel plate manufacturer

As a carbon steel plate manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all carbon steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the carbon steel plates have less defects.

Q1: What is carbon steel?

A1: Carbon steel is a type of steel where the primary alloying element is carbon. It is commonly used in construction, automotive, and manufacturing industries due to its strength, durability, and versatility.

Q2: What are the different types of carbon steel plates?

A2: Carbon steel plates are generally classified into three types based on carbon content: low carbon steel (0.05% – 0.25% carbon), medium carbon steel (0.25% – 0.60% carbon), and high carbon steel (0.60% – 1.00% carbon).

Q3: What are the common grades of carbon steel plates?

A3: Common grades include ASTM A36, ASTM A572, ASTM A516, S235JR, S275JR, S355JR, and JIS SS400, among others.

Q4: What are the uses of carbon steel plates?

A4: Carbon steel plates are used in construction, shipbuilding, automotive manufacturing, machinery, pressure vessels, and structural components due to their strength and versatility.

Q5: What is the difference between low carbon and high carbon steel plates?

A5: Low carbon steel has higher ductility and is easier to weld and form, while high carbon steel has greater hardness and strength but is less ductile and more prone to cracking during welding.

Q6: Can carbon steel plates be welded?

A6: Yes, carbon steel plates can be welded, though the specific welding process and techniques may vary depending on the carbon content and plate thickness.

Q7: How do you prevent carbon steel plates from rusting?

A7: To prevent rusting, carbon steel plates should be properly coated with paint, oil, or other protective coatings. In some cases, galvanizing or applying corrosion-resistant alloys can also help protect the steel.

Q8: What are the advantages of using carbon steel plates?

A8: The main advantages include high strength, durability, low cost, and ease of fabrication. Carbon steel plates are also widely available and can be heat-treated to meet various requirements.

Q9: What are the disadvantages of carbon steel plates?

A9: The main disadvantages include susceptibility to corrosion, especially in harsh environments, and lower resistance to wear compared to other materials like stainless steel.

Q10: How do you select the right grade of carbon steel plate?

A10: Selection depends on factors such as the intended application, required strength, welding capability, environmental conditions, and cost considerations. It is important to choose the grade that meets both mechanical and chemical property requirements for the specific use case.

If you need more details or have other questions, please contact Daxun’s sales team and experts, we will serve you quickly!

Envíe su consulta hoy mismo
Presupuesto rápido