x
Envíe su consulta hoy mismo
Presupuesto rápido

Daxun 317 and 317L stainless steel PIPE and TUBE China supplier

As China’s leading Stainless Steel pipe and tube supplier and exporter, Daxun provides stainless steel PIPEs to the world.
  • Grade: AISI 317/317L-S31700-S31703
  • Manufacturing: hot-rolled, cold-drawn, forged, welded
  • Standards: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Type: both seamless and welded pipes
  • Diameter: from small diameter to large diameter pipes
  • Thickness: thin-walled pipes and thick-walled pipes
  • Surface: pickled, polished, bright annealed
  • Length: 3000mm, 6000mm, 9000mm, etc.

Global leader in stainless steel pipe and tube fabrication services

Daxun is an exporter and supplier of 317L Stainless Steel Pipe and UNS S31703 Welded Pipe in various sizes, thicknesses and standards, Check online China SS Grade 1.4438 Stainless Steel Pipe Price

Daxun Alloy is a major maker of stainless steel pipes, and its SS 317/317L seamless pipes are unique. They are renowned for their durability and dimensional correctness. The domestic and worldwide nature of steel raw materials allows for the production of SS 317l pipes in a variety of sizes and thicknesses to meet the individual requirements of business customers. 317L alloy is a low carbon stainless steel with higher chromium, nickel, and molybdenum content than 316L for improved corrosion resistance. This steel is resistant to sulphurous acid, acetic acid, formic acid, citric acid, and tartaric acid, as well as pitting corrosion when exposed to phosphoric acid, chlorides, bromides, and iodides. 317L Stainless Steel Seamless Pipe, 317L Stainless Steel ERW Pipe, 317L Stainless Steel EFW Pipe, and 317L Stainless Steel Welded Pipe and Tube (Conforming to ASTM A213 / A312 / A269 / A358 Standards)

Daxun Alloys has been producing Type 317L Stainless Steel in various sizes and shapes for many years.

We sell 317L alloy that meets or surpasses numerous important international standards, including ASTM, ASME, UNS, DIN, and EN. We also offer SS 317L Tube in a variety of sizes, thicknesses, and specifications based on our customers’ specific needs. Stainless Steel Cold Drawn 317L Tube is a molybdenum-rich austenitic stainless steel, identical to SS 317 but with a greater molybdenum content. SS 317 Tube is available in cut-to-length sizes and can be manufactured or machined to match your specific piping needs. Contact Daxun today.

Seguir leyendo

Datos

AISI 317 pipe Material SA213 TP 317 – ALLOY 317 – UNS S31700 – WNR 1.4438
UNS S31700 Tube Standards ASTM A213, ASTM A249, ASTM A269, ASME SA213, ASME SA249, ASME SA269, EN 10216-5 TC1 / TC2, PED 97/23/EC, AD 2000, NACE MR0175/ISO 15156
317 Stainless Steel Seamless Pipes & Tubes Manufacturing Specifications ASME B36.19
ASTM A213
ASTM A312
ASTM A269
ASTM A632
ASME SA213
NFA 49-117
BS 10216
Or as per customer specifications
Seamless Tube Size 3.35 mm OD To 101.6 mm OD
Welded Tube Size 6.35 mm OD To 152 mm OD
Stainless Steel 317 Seamless Tube Swg & Bwg 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg.
SS 317 ERW Pipe Wall thickness 0.020″ –0.220″, (special wall thicknesses available)
ASTM A312 TP317 Pipe Length Single Random, Double Random, Standard & Cut length
SS DIN 1.4438 / 1.4436 Rectangular Welded Pipes Finish Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF
AMS 5573 Tube Form Straight, Coiled, Seamless, Round Pipes/ Tubes, Square Pipes/ Tubes, Rectangular Pipe/ Tubes, Coiled Tubes, “U” Shape, Pan Cake Coils, Hydraulic Tubes, Straight or ‘U’ bent Tubes, Hollow, LSAW Tubes Etc.
UNS S31700 Square Pipes Type Seamless, ERW, EFW, Welded, Fabricated
SS 317 Pipe Schedule SCH5, SCH10, SCH10S, SCH20, SCH30, SCH40, SCH40S, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
317 Stainless Steel Tube Electropolished (EP) Electropolished for Ultra High Purity Systems
ASTM A312 TP317 Pipe Non-Electropolished (BA) Bright Annealed or (AP) Annealed & Pickled for High-Purity, (CFOS) Cleaned for Oxygen Grade Service or Corrosive Systems
Stainless Steel 317 Seamless Tube & Pipe I.D. Surface Finish Options 5, 7 & 10 µin. Ra
317 Rectangular tubing JIS 8A to 250A
SS 317 Tube Tolerances In accordance with: ASTM: A269 & A632, JIS: G 3459
317 stainless steel tubing End Plain End, Beveled End, Treaded, Ends are suitable for orbital welding
AMS 5573 Tube Marking All 317 Stainless Steel tubes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.)
317 stainless steel tubing Application Oil Tube, Gas Tube, Fluid Tube, Boiler and Heatexchanger
SS 317 welded round tubes Value Added Service Draw & Expansion as per required Size & Length, Polish (Electro & Commercial) Annealed & Pickled Bending, Machining Etc.
AMS 5584 Seamless/ welded tube Specialize in Stainless Steel 317 Capillary Tube & Other Odd Size
Stainless Steel 317 Heat Exchanger & Condenser Tubes
Stainless Steel 317 Hydraulic tubing with OD up to 50.8 mm (2.0 in.) are delivered in bright annealed condition
Stainless Steel 317 hydraulic tube with OD larger than 50.8 mm are supplied in the annealed and pickled condition, Or in polished condition
SS 317 welded square tubes Marking & Traceability Each Stainless Steel 317 Tubing is traceable to its producing mill and heat by an identification number etched within 24″ (610mm) of one end.
317 stainless steel tubing Test Certificate Manufacturer Test Certificate according to EN 10204 3.1 B
Laboratory Test Certificate from Govt. Approved Lab.
Under Third Party Inspection
317 stainless steel tubing Testing & Inspection Visual inspection • Surface roughness measurement • Helium-leak testing • Scanning Electron Microscopy (SEM) • Auger Electron Microscopy (AES) • Election Spectroscopy for Chemical Analysis (ESCA or XPS) • Particle testing • Moisture testing
317/317L Pipe and Tubing
Sizes Standard Tolerances
Productos OD Wall Lengths and/or coils Grades OD Wall Lengths
Welded Austenitic Steel Boiler, Super Heater, Heat-Exchangers & Condenser Tubes 3/16″ (4.76 mm) to 4″ (101.6 mm) 0.020″ (0.51 mm) to 0.220″ (5.59 mm) Random or cut lengths up to 90′ (27.4 m) Coils to 1-1/2″ OD 317/317L Under 1″ (25.4 mm) ±0.004″ (0.10 mm) ±10% Randoms up to +2″ (50.8 mm) Cuts +1/8″ (3 mm) -0″ Coils to 80,000′ (24,384 m)
Specifications: ASTM-A249, ASME-SA249, ASTM-A688, ASME-SA688 Metric sizes available 1″ (25.4 mm) to 1-1/2″ (38.1 mm) ±0.006″ (0.15 mm)
>1-1/2″ (38.1 mm) to 2″ (50.8 mm) ±0.008″ (0.20 mm)
>2″ (50.8 mm) to 2-1/2″ (63.5 mm) ±0.010″ (0.25 mm)
>2-1/2″ (63.5 mm) to 3″ (76.2 mm) ±0.012″ (0.30 mm)
3″ (76.2 mm) to 4″ (101.6 mm) ±0.015″ (0.38 mm)
Pressure & Corrosion Tubing 1/16″ (1.59 mm) to 4″ (101.6 mm) 0.010″ (0.25 mm) to 0.220″ (5.59 mm) Random or cut lengths up to 90′ (27.4 m) 317/317L <1-1/2″ (38.1 mm) ±0.005″ (0.13 mm) 1-1/2″ (38.1 mm) to 3″ (76.2 mm) ±0.010″ (0.25 mm) ±10% Randoms up to +2″ (50.8 mm)
Meets or exceeds requirements for welded Metric sizes available Coils to 1-1/2″ OD 3-1/2″ (88.9 mm) to 4″ (101.6 mm) ±0.015″ (0.38 mm) Cuts +1/8″ (3 mm) -0″
Specifications: ASTM-A269, ASTM-A1016, and ASTM-A632 Coils to 80,000′ (24,384 m)
Instrumentation Tubing 1/16″ (1.59 mm) to 1/2″ (12.7 mm) 0.010″ (0.25 mm) to 0.065″ (1.65 mm) Random or cut lengths up to 40′ (12.2 m) 317/317L ±0.005″ (0.13 mm) ±10% Randoms up to +2″ (50.8 mm)
Specifications: ASTM-A269 and ASTM-A632 Metric sizes available Cuts +1/8″ (3 mm) -0″
Composition of 317/317L tubing and pipe
Grado 317 317L
UNS Designation S31700 S31703
Carbon (C) Max. 0.08 0.035*
Manganese (Mn) Max. 2 2
Phosphorous (P) Max. 0.04 0.04
Sulphur (S) Max. 0.03 0.03
Silicon (Si) Max. 1 1
Cromo (Cr) 18.0–20.0 18.0–20.0
Nickel (Ni) 11.0–14.0 11.0–15.0
Molybdenum (Mo) 3.0–4.0 3.0–4.0
Nitrogen (N)
Hierro (Fe) Bal. Bal.
Other Elements
*Maximum carbon content of 0.04% acceptable for drawn tubes
Physical Properties of 317/317L Alloys in the Annealed Condition at -20°F to +100°F
Resistencia a la tracción Yield Strength
Alloy UNS Designation Spec. psi MPa ksi psi MPa ksi Elongation in 2 inches (min.) % Grain Size Req. Max. Hardness Modulus of Elasticity (x106 psi) Mean Coefficient of Thermal Expansion (IN./IN./°F x 10-6) Thermal Conductivity (BTU-in/ft2-h-°F)
317 S31700 A249, A312 75,000 515 75 30,000 205 30 35 90 Rb 28 9.2 116
317L S31703 A249, A312 70,000 485 70 25,000 170 25 35 90 Rb 28 9.2 116
Grado Density (kg/m3) Elastic Modulus (GPa) Mean Coefficient of Thermal Expansion (m/m/0C) Thermal Conductivity (W/m.K) Specific Heat 0-1000C (J/kg.K) Electrical Resistivity (n.m)
0-1000C 0-3150C 0-5380C at 1000C at 5000C
317L 8000 193 17.2 17.8 18.4 16.2 21.5 500 720
317 8000 193 17.2 17.8 18.4 16.2 21.5 500 720
Grado UNS No Old British Euronorm Swedish SS Japanese JIS
BS En No Nombre
317L S31703 1.4438
317 S31700 1.4449
Din W.-Nr. 1.4438 Aisi 317L Corrugated Tube Stainless Steel 317L Round Tube
UNS S31703 Seamless Pipe Stainless Steel 317L Seamless Round Pipe
S31703 Stainless Steel U Shaped Tube 317L Stainless Steel Square Tube Mirror Finish
Din 1.4438 Material Seamless Pipe WERKSTOFF NR. 1.4438 Coaxial Tube
317L Stainless Steel Rectangular Pipe 317L Stainless Steel Hypodermic Pipe for Medical Needle
317L Stainless Steel Oval Pipe SS 317L Needle Tube
Din 1.4438 Stainless Steel Welded Pipe ASTM A358 TP317L Coil Pipe Heat Exchanger
SAE J405 Uns S31703 Thin Wall Pipe 317L Stainless Steel Metric Pipe
ASTM A312 TP317L Coiled Pipe Stainless Steel Inox 317L Capillary Pipe
ASTM A312 gr TP 317L Aerospace tubes ASTM A632 TP317L Electric Fusion Welding Pipe
Jis 317L Stainless Steel Coil Pipe Stainless Steel 317L Seamless Pipe
Schedule 10 Type 317L Stainless Steel Pipe Schedule 40 Type 317L Stainless Steel Pipe
Stainless Steel 317L Grade Pipe Type 317L Stainless Steel Polished Pipe
ASTM A312 TP317L Elliptical Tubes ASTM A213 SS TP 317L Stainless Steel Rectangular Tube
Material 1.4438 Aisi 317L Slotted Handrail Tube SA312 TP317L Thin Wall Tube
Austenitic Stainless Steel 317L Pipe DIN 1.4438 SS 317L Pipe
Alloy 317L Pipe Stainless Steel 317L Seamless Pipe
Stainless Steel 317L EFW Pipe Stainless Steel 317L Round Pipe
TP317L SS Welded Pipe SS 317L Santiary Tube
ASTM A312 TP317L Pipe SA312 TP317L square tubes
AISI 317l Stainless Steel Pipe SS 317L Needle Tube
ASTM A269 TP317L Round Tube ASTM A249 TP317L 317L hydraulic tube
Alloy 317L Pipe NACE MR0175
SA213 TP 317L Thick Wall Tube En 1.4438 / Aisi 317L Hydraulic Pipe
Stainless Steel 317L Ornamental Pipe Stainless Steel 317L Fin Tube / Finned Tube
1.4438 Instrument Pipe 317L Stainless Steel Square Pipe
Ultra-High Purity Electropolished Stainless Steel 317L Tube Thin Wall S31703 Stainless Steel Pipe
317L Stainless Steel ERW Pipe Corrugated 317L Stainless Steel Tube (CSST) for Gas
SA 312 TP317L Seamless Pipe Polished 317L Stainless Steel Pipe
317L Stainless Steel Threaded Pipe SAE 317L Stainless Steel Rectangular Tube
JIS SUS317L Seamless Tubes Din 1.4438 Stainless Steel Tube
SA312 TP317L Welded Tubes AISI 317L Seamless Tube
317L Stainless Steel Seamless Square Pipe Large Diameter 317L Stainless Steel Tube
SS 317L Erw Pipe 317L Stainless Steel Instrumentation Pipe
High-pressure 317L Stainless Steel Water Pipe Stainless Steel 317L Hexagonal Pipe
ASTM A358 TP317L Polished Pipe 317L Stainless Steel Ornamental Tube
ASTM A312 TP317L erw 317L Stainless Steel Spiral Pipe
ASME SA213 TP317L Perforated Tube Din 1.4438 Material Tube
SA 688 TP317L Finned Tube SA312 TP317L Dom Tube
Din 1.4438 AISI 317L Perforated Exhaust Tube Stainless Steel 317L Hypodermic Pipe
ASTM A213 TP317L Condenser Tube Stainless Steel 317L Welded Pipe & Tube
ASTM A269 TP317L straight tube 317L Stainless Steel Welded Tube
ASTM A249 TP317L Mirror Tube Jis 317L Stainless Steel Pipe
317L Stainless Steel Seamless Pipe SS UNS S31703 Welded Pipe
ASTM A312 TP 317L SS Seamless Pipe 317L SS Electropolished Pipe
DIN 1.4438 SS 317L Pipe Stainless Steel 317L Pipe
Stainless Steel 317L Seamless Pipe WERKSTOFF NR.1.4449 SS 317L Pipe
SS 317L Hexagonal Pipe 317L SS Hollow Pipe
SS 317L Bush Hex Pipe SS 317L Welded Pipe
SS TP317L Seamless Pipe TP317L SS Welded Pipe

Elija Daxun y haga que sus clientes queden satisfechos.

Póngase en contacto con Daxun

Quick response-317 Stainless Steel pipe

  • Provide seamless and welded pipes
  • Good formability and weldability
  • Increased resistance to chemical attack from acids
  • Lower carbon content leads to resistance to sensitization when welded
  • Excellent corrosion resistance in harsh environments.
  • Higher creep strength, rupture stress and tensile strength.
  • Pitting and crevice corrosion resistance
Póngase en contacto con Daxun

Daxun Advantages

  • Variety: From small to large diameter stainless steel pipe, we offer a wide range of sizes and grades, including 304L, 316L, 317L and more.
  • Flexibility: Whether you need seamless or welded steel pipe, our stainless steel pipe lengths are designed to meet your specific project requirements.
    Quality
  • Standards: Our stainless steel pipes meet stringent standards such as ISO9001, ABS, NSF/ANSI Standard 61, and NACE MR0175 to ensure reliability and performance.
  • Custom Orders: Looking for special size stainless steel pipes? We offer a variety of stainless steel pipe custom options at competitive prices and convenient online ordering.
Póngase en contacto con Daxun

317 Stainless Steel pipe packaging

  1. Woven bag bale cargo (hexagonal)
  2. Special crates for U-bend pipes, (steel/wood) divided
  3. Each bale is wrapped in plastic to protect against wind and rain.
  4. SS 317 seamless pipes are protected by plastic covers.
  5. Plastic strips are used to secure the bale.
  6. Export-specific fumigation-free wooden crate packaging.
  7. Laminated packing slip attached to the bale or crate.
  8. Customized packaging as per customer needs.
Póngase en contacto con Daxun

317 Stainless Steel pipe Ordering Information

317 stainless steel pipe The purchase order shall include quantity, PSL grade, type or class, API5L reference, outside diameter, wall thickness, length and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Pipe is solution bright annealed.

Póngase en contacto con Daxun

Calidad, entrega, inspección

  • Daxun también lleva a cabo varias pruebas de garantía de calidad. Estas pruebas incluyen la prueba de aplanamiento, la prueba de picaduras y resistencia, la prueba mecánica, la prueba de dureza, la identificación positiva del material, la prueba de expansión, etc. Todas estas pruebas garantizan que el material es adecuado para la aplicación requerida.
  • Durante el proceso de producción, medimos el diámetro, el grosor y la superficie del producto. Nuestro plazo de entrega estándar es de 7-15 días, excepto para algunos productos de tamaño especial, nuestro plazo de entrega aumentará a 20 días.
    Nuestro plazo de entrega se ajusta estrictamente a lo estipulado en el contrato.
  • Apoyar a las agencias externas del cliente para que vayan a la fábrica a inspeccionar
  • Ofrecer muestras gratuitas a los clientes para que las prueben
  • Apoyo a la inspección in situ o por vídeo en fábrica
Póngase en contacto con Daxun

Asistencia técnica

Si necesita asistencia técnica adicional, nuestro metalúrgico residente y nuestro personal experto estarán encantados de ayudarle. Además, Daxun cuenta con un laboratorio de pruebas certificado, una primicia en la industria de inventarios multimetal y plástico. Esto, en nuestra opinión, demuestra nuestra inquebrantable dedicación a la calidad y nuestra filosofía como proveedor de servicios completos.

317 and 317L Stainless Steel pipe and tube Features

Alta resistencia
Resistencia a la corrosión
Resistencia al calor
Resistencia a bajas temperaturas
Protección del medio ambiente
Rendimiento de soldadura

Daxun Alloy Let your brand improve rapidly

NPS Outside Diameter Wall Thickness Weight Weight
in mm in mm Sched kg/Mtr Lb/ft
1/2″ 0.84 21 0.109 2.769 40 STD 1.268 0.851
0.147 3.734 80 STD 1.621 1.088
3/4″ 1.05 27 0.113 2.87 40 STD 1.684 1.131
0.154 3.912 80 STD 2.195 1.474
1″ 1.315 33 0.133 3.378 40 STD 2.501 1.679
0.179 4.547 80 STD 3.325 2.172
1 1/4″ 1.66 42 0.14 3.556 40 STD 3.385 2.273
0.191 4.851 80 STD 4.464 2.997
1 1/2″ 1.9 48 0.145 3.683 40 STD 4.048 2.718
0.2 5.08 80 STD 5.409 3.361
2″ 2.375 60 0.154 3.912 40 STD 5.441 3.653
0.218 5.537 80 STD 7.48 5.022
2 1/2″ 2.875 73 0.203 5.516 40 STD 8.629 5.793
0.276 7.01 80 STD 11.411 7.661
3″ 3.5 89 0.216 5.486 40 STD 11.284 7.576
0.3 7.62 80 STD 15.272 10.253
4″ 4.5 114 0.237 6.02 16.073 10.79
0.337 8.56 22.318 14.983
6″ 6.625 168 0.188 4.775 19.252 12.924
0.203 5.516 20.739 13.923
0.219 5.563 22.318 14.983
0.25 6.35 25.354 17.021
0.28 7.112 40 STD 58.263 18.974
0.312 7.925 31.334 21.036
0.375 9.525 37.285 25.031
0.432 10.973 80 XHY 42.561 28.573
0.5 12.7 48.719 32.708
8″ 8.625 219 0.188 4.775 25.233 16.94
0.203 5.156 27.198 18.259
0.219 5.563 29.286 19.661
0.25 6.35 20 33.308 22.361
0.277 7.036 30 36.786 24.696
0.322 8.179 40 42.352 28.554
0.375 9.525 49.216 33.041
0.406 10.312 60 53.085 35.638
0.5 12.7 80 XHY 64.627 43.388
10″ 10.75 273 0.188 4.775 31.588 21.207
0.219 5.563 36.689 24.631
0.25 6.35 20 41.759 28.035
0.307 7.798 30 51.002 34.24
0.344 8.738 56.946 38.231
0.365 9.271 40 STD 63.301 40.483
0.438 11.125 71.852 48.238
0.5 12.7 60 XHY 81.53 54.735
0.594 15.088 80 95.969 64.429
12″ 12.75 324 0.188 4.775 37.57 25.222
0.219 5.563 43.657 29.309
0.25 6.35 49.713 33.375
0.281 7.137 55.739 37.42
0.312 7.925 61.735 41.445
0.375 9.525 73.824 49.562
0.406 10.312 79.727 53.525
0.5 12.7 97.438 65.415
0.562 14.275 108.966 73.154
14″ 14 356 0.188 4.775 41.308 27.732
0.219 5.563 48.012 32.233
0.25 6.35 20 54.685 36.713
0.281 7.137 61.327 41.172
0.312 7.925 67.939 45.611
0.375 9.525 STD 81.281 54.568
0.438 11.125 40 94.498 63.441
0.5 12.7 XHY 107.381 72.09
0.625 15.875 132.983 89.278
16” 16 406 0.188 4.775 47.29 21.748
0.219 5.563 54.98 36.91
0.25 6.35 10 62.639 42.053
0.281 7.137 70.268 47.174
0.312 7.925 20 77.866 52.275
0.344 8.738 85.677 57.519
0.375 9.525 30 93.213 62.578
STD
0.438 11.125 108.433 72.797
0.5 12.7 40 123.289 82.77
XHY
18″ 18 457 0.219 5.563 61.948 41.588
0.25 6.35 70.593 47.393
0.281 7.137 79.208 53.176
0.312 7.925 20 87.792 58.939
0.375 9.525 STD 105.144 70.588
0.438 11.125 30 122.369 82.152
0.5 12.7 XHY 139.198 93.45
0.562 14.275 40 155.904 104.666
0.625 15.875 172.754 115.978
20″ 20 508 0.25 6.35 78.547 52.733
0.282 7.163 88.458 59.386
0.312 7.925 97.719 65.604
0.375 9.525 20 STD 117.075 78.598
0.438 11.125 136.305 91.508
0.5 12.7 30 XHY 155.106 104.13
0.594 15.088 40 183.378 123.11
0.625 15.875 192.64 129.328
0.688 17.475 211.368 141.901
24″ 24 610 0.25 6.35 94.456 63.413
0.281 7.137 106.029 71.183
0.312 7.925 117.573 18.932
0.375 9.525 20 STD 140.938 64.618
0.438 11.125 164.176 110.219
0.5 12.7 XHY 186.923 125.49
0.625 15.875 232.41 156.028
0.688 17.475 40 255.148 171.293
0.75 19.05 277.401 186.233
30″ 30 762 0.25 6.35 118.318 79.433
0.281 7.137 132.851 89.189
0.312 7.925 10 147.353 98.925
0.375 9.525 STD 176.731 118.648
0.438 11.125 205.983 138.286
0.5 12.7 20 XHY 234.647 157.53
0.625 15.875 30 292.066 196.078
0.688 17.475 320.817 215.38
0.75 19.05 348.988 234.293
36″ 36 914 0.25 6.35 142.18 95.453
0.281 7.137 159.672 107.196
0.312 7.925 10 177.133 118.918
0.375 9.525 STD 215.525 142.678
0.438 11.125 247.79 166.353
0.5 12.7 20 XHY 282.372 198.57
0.625 15.875 351.723 236.128
0.688 17.475 386.487 259.467
0.75 19.05 420.576 282.353
42″ 42 1067 0.312 7.925 206.914 138.911
0.375 9.525 STD 248.319 166.708
0.5 12.7 XHY 33.097 221.61
0.75 19.05 492.163 330.413
48″ 48 1219 0.375 9.525 STD 284.112 190.738
0.438 11.125 331.404 222.487
0.5 12.7 XHY 377.822 253.65
0.75 19.05 563.75 378.473
0.875 22.225 655.969 440.383
PRESSURE RATING (PSIG)
SIZES SCHEDULE (SCH) OUTSIDE WALL TEMPERATURE (OF)
(INCHES) DIA. THICK. 100 200 300 400 500 600 650 700 750
(IN) (IN) ALLOWABLE STRESS (PSI)
16700 16700 16700 15500 14400 13500 13200 12900 12600
1″ 40 1.315 0.133 2205 2205 2205 2047 1902 1783 1743 1703 1664
80 1.315 0.179 3061 3061 3061 2841 2640 2475 2420 2365 2310
160 1.315 0.25 4493 4493 4493 4170 3874 3632 3552 3471 3390
1 1/2″ 40 1.9 0.145 1629 1629 1629 1512 1404 1317 1287 1258 1229
80 1.9 0.2 2303 2303 2303 2138 1986 1862 1821 1779 1738
160 1.9 0.281 3362 3362 3362 3120 2899 2717 2657 2597 2536
2″ 40 2.375 0.154 1371 1371 1371 1272 1182 1108 1083 1059 1034
80 2.375 0.218 1985 1985 1985 1843 1712 1605 1569 1534 1498
160 2.375 0.344 3283 3283 3283 3047 2831 2654 2595 2536 2477
3″ 40 3.5 0.216 1301 1301 1301 1208 1122 1052 1028 1005 982
80 3.5 0.3 1844 1844 1844 1712 1590 1491 1458 1425 1391
160 3.5 0.438 2787 2787 2787 2587 2403 2253 2203 2153 2103
4″ 40 4.5 0.237 1102 1102 1102 1023 950 891 871 851 831
80 4.5 0.337 1596 1596 1596 1482 1377 1291 1262 1233 1204
160 4.5 0.531 2611 2611 2611 2424 2552 2111 2064 2017 1970
5″ 40 5.563 0.258 965 965 965 896 832 780 763 746 728
80 5.563 0.375 1428 1428 1428 1325 1231 1154 1129 1103 1077
160 5.563 0.625 2474 2474 2474 2296 2133 2000 1955 1911 1866
6″ 40 6.625 0.28 877 877 877 814 756 709 693 677 661
80 6.625 0.432 1379 1379 1379 1280 1189 1115 1090 1065 1040
160 6.625 0.719 2382 2382 2382 2211 2054 1925 1883 1840 1797
8″ 40 8.625 0.322 771 771 771 716 665 623 610 596 582
80 8.625 0.5 1218 1218 1218 1131 1050 985 963 941 919
160 8.625 0.906 2298 2298 2298 2133 1982 1858 1817 1775 1734
10″ 40 10.75 0.365 699 699 699 649 603 565 553 540 528
80 10.75 0.594 1159 1159 1159 1075 999 937 916 895 874
160 10.75 1.125 2289 2289 2289 2124 1974 1850 1809 1768 1727
Types Out diameter Sizes Length
NB Sizes (in stock) .0035” ~ 20” 1/8″, 1/4″, 3/8″, 1/2″, 5/8″, 3/4″, 1″, 1.25″, 1.5″, 2″, 2.5″, 3″, 4″, 5″, 6″etc Cut to length
Stainless Steel 317/317L Seamless Tube (Custom Sizes) 6.35 mm OD To 508 mm OD As per requirement Cut to length
Stainless Steel 317/317L Welded Tube (ERW Tube) (in Stock + Custom Sizes) 6.35 mm OD To 1219 mm OD As per requirement Cut to length
Acabado superficial Internal Surface(ID) Exterbal Surface(OD)
Roughness Average(RA) Roughness Average(RA)
μ inch μm μ inch μm
AP Annealed & Pickled Not defined Not defined 40 or Not defined 1.0 or Not defined
BA Beight Annealed 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
MP Mechanical Polish 40,32,25,20 1.0,0.8,0.6,0.5 32 0.8
EP Electro Polish 15,10,7,5 0.38,0.25,0.20;0.13 32 0.8

The surface and shape of 317/317L stainless steel PIPE (6)

Información disponible para consulta y descarga

Daxun is a trustworthy stainless steel pipe and tube manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel tube are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 317 Stainless Steel pipe and tube have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

Proyectos y productos recientes

317/317L stainless steel pipe
stainless steel seamless pipe
large diameter stainless steel pipe
317/317L stainless steel pipe
Stainless Steel Polished Tube
317/317L seamless pipe
Stainless steel tube
BA stainless steel pipe
Stainless steel tube / pipe
317/317L stainless pipe
Stainless steel welded pipe
Stainless steel precision tube
¿Puedo obtener algunas muestras?

We can provide 317 Stainless Steel pipe and tube samples for you to check the quality. Sample is free and you just pay the freight.

¿A qué países ha exportado ya?

Hemos exportado a más de 42 países, como Canadá, Chile, Kuwait, Alemania, Corea del Sur, Arabia Saudí, Singapur, etc.

¿Cuál es su MOQ?

Our MOQ is 1 ton for stainless steel 317 Stainless Steel pipe and tube.

¿Cuál es el plazo de entrega?

Los pedidos de prueba pueden entregarse en una semana. Los pedidos normales tardan unas dos semanas.

Envíe su consulta hoy mismo
Presupuesto rápido