Daxun is a 201 stainless steel sheet supplier from China
As China’s leading stainless steel plate supplier and exporter, Daxun provides 201 stainless steel plates to the world.
- Grade: AISI 201/S20100
- Manufacture: cold rolled plate, hot rolled plate, forged plate
- Estándar: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- Type: cold rolled thin plate and hot rolled thick plate
- Surface: 2B, NO.1, NO.4, HL, BA, 8K etc
- Longitud: 2438mm3048mm6000mm se puede personalizar
- Origin: TISCO, Baosteel, Posco, Tsingshan, Delong
Líder mundial en servicios de fabricación de chapa de acero inoxidable
Daxun stocks 201 stainless steel plates (hot rolled and cold rolled). Because a portion of the nickel used in 300 series stainless steels (such as Type 304) is replaced with manganese, the 201 grade alloy is generally a high performance, lower cost, more stable austenitic stainless steel. In addition, the chemical composition of the 201 stainless steel provides better annealed mechanical properties than Type 304, which may provide further advantages in terms of weight reduction. Because the tensile strength of Type 201 is approximately 10% higher than that of Type 304, thinner gauges can be used, using less material overall. However, Type 201 stainless steel has lower chromium and nickel contents, so it is not as corrosion resistant as Type 304. 201 grade stainless steel is frequently used in domestic and commercial food service applications, construction applications, appliances, and other uses.
Corrosion Resistance: 201 stainless steel plate has excellent corrosion resistance suitable for both indoor and outdoor applications. Its excellent corrosion resistance. Stainless steel sheet has excellent resistance to atmospheric conditions, moisture and specific chemicals, thus guaranteeing long-lasting performance and durability. By providing excellent resistance to atmospheric conditions, moisture and specific chemicals, it guarantees long-lasting performance and durability.
High Strength: 201 stainless steel plate is able to withstand heavy weight and pressure due to its high tensile strength. Steel sheet is able to withstand large mass and pressure due to its high tensile strength. Parts and structural components that require extreme durability.
Steel sheet is a beautiful material that can add a touch of elegance to any project due to its smooth, polished surface. It is suitable for architectural elements, kitchen utensils and decorative applications due to its easy-to-clean and shiny surface. It is perfect for architectural elements, kitchen utensils and decorative applications due to its easy-to-clean and shiny surface.
It is a cost-effective solution compared to other grades of stainless steel without sacrificing quality. It is favored by budget-constrained projects due to its reliable performance and reasonable price. It is the choice of budget-constrained projects due to its reliable performance and reasonable price.
At Daxun, we offer high quality 201 Stainless Steel Plate at very competitive prices. We understand the importance of maintaining the superior quality of metal sheet products while keeping them affordable. Contact us today to secure the most competitive prices for SS 201 Stainless Steel Plate and experience the superior quality of our products. Contact us today to secure the most competitive prices for 201 Stainless Steel Plate and experience the superior quality of our products.
Datos técnicos
- Parámetro
- Ingredients and properties
- PHYSICAL PROPERTIES:
- Propiedades mecánicas
| Product Parameters: 201/201LN Stainless Steel Sheet/Plate | |||
| Anchura | 10mm~2500mm | ||
| Espesor | 0,2 mm~100 mm | Tolerancia de espesor | +/-0,03 mm |
| Estándar | ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2 | ||
| Superficie | 2B,BA,8K,NO.1,NO.4,NO.3,rayita,a cuadros,oro,negro,oro rosa,etc. | ||
| especificación | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
| Origen del molino | TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc. | ||
| Certificación | ISO, SGS, BV, TUV, CE, etc. | ||
| Estándar | Werkstoff Nr. | UNS | JIS | BS | GOST | AFNOR | EN | CN |
| SS 201 | 1.4372 | S20100 | SUS 201 | 904S13 | STS 317J5 | Z2 NCDU 25-20 | X1NiCrMoCu25-20-5 | 1Cr17Mn6Ni5N |
| Grado | C | Mn | Si | P | S | Cr | Ni | N |
| 201 | 0.25% | 5.5%-7.5% | 1% | 0.60% | 0.30% | 16%-18% | 3.5%-5.5% | 0.25% |
| Density (lb./ in^2) @ RT | 0.283 | |
| Modulus of Elasticity in Tension (psi x 10^6) | 28.6 | |
| Specific Heat (BTU/o F/lb.) | 32 to 212 oF | 0.12 |
| Thermal Conductivity (BTU/hr/ft^2/ft) | 212oF | 9.4 |
| Mean Coefficient of Thermal Expansion (in. x 10^-6 per o F) | 32 to 212oF | 8.7 |
| 32 to 600oF | 9.7 | |
| 32 to 1,000oF | 10.2 | |
| Electrical Resistivity (micro ohms – cm) | at 70oF | 69 |
| Melting Point Range (oF) | 2550/2650 | |
| Oxidation Resistance – Continuous Service(oF) | 1550 | |
| Oxidation Resistance – Intermittent Service(oF) | 1500 |
| Resistencia a la tracción | 99,400 PSI = 520MPa |
| Yield Strength | 42,400 PSI = 275MPa |
| Elongation | 55 – 60% |
| Elastic Modulus | 29,000,000 psi = 203000MPa |
| Hardness Requirement | 183 n/was (MPa) |
| Densidad | .280 LBS /cubic inch(density 7.93g/cm3) |
Elija Daxun y haga que sus clientes queden satisfechos.

Entrega rápida
Daxun provides customers with timely and fast delivery of 201 stainless steel plate products. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to ports and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Advanced machining
Daxun’s typical service of “more, faster, better and cheaper” for 201 stainless steel plate materials starts with Daxun’s stainless steel varieties, specifications and spot inventory. It has strategic resource support from many large steel mills at home and abroad to ensure a stable supply chain and meet customers’ personalized needs for specific materials. It can be called the “Wal-Mart” of the stainless steel industry. With more than 20 years of experience, it has established the brand image of “Look for Daxun for stainless steel plates” in the Chinese market.


Quick response
- 201 stainless steel plate has high reliability
- Chemical composition of pure steel
- Easy to weld and excellent welding effect
- Optimal shape and excellent precision
- Long service life
- Relatively low cost
- Fácil de procesar
201 stainless steel plate packaging
Daxun Alloy ensures the best quality of 201 stainless steel plate packaging, because packaging plays an important role in international freight, and the goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways according to the products. We pack our products in many ways, such as:
- Cajas y cajones
• Kraft paper + wooden pallets
- Retráctil
• Fumigation-free wooden pallets
• Fumigation-free wooden boxes


SS 201 Plate Surface Treatment
1D: La superficie es mate con forma de partícula discontinua.
2D: Blanco con un tono plateado.
2B: Gris plateado con mejor brillo y planitud que la superficie 2D.
Ba: Superficie cercana al espejo con excelente brillo y reflectividad.
No.3: Buen brillo y superficie rugosa.
No.4: La superficie tiene líneas finas y buen brillo.
HL: Gris plateado con pelo dorado.
8K: Superficie de espejo.
201 Stainless Steel Sheet Processing:
- Etching processing
- Welding processing
- Bending processing
- Embossing processing
- Sandblasting processing
- Polishing processing
- Punching processing
- Stamping processing
- Cutting processing

201 plate stainless steel Features
Daxun Deje que su marca mejore rápidamente
- Galería
- Otras series de productos
- Tolerancia
- Estado de entrega
| Grado | Tipo | Espesor | Superficie |
| Austenítico | 304/304H/304L/304J1 | 0,25-150 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0,4-80 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0,3-80 mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| Ferrita | 430 | 0,4-3,0 mm | 2B/BA/NO.4/8K/SB/HL |
| Ferrita ultrapura | 443 | 0,4-2,0 mm | 2B |
| 436L/439/444/441 | 0,5-3,0 mm | 2B、2D | |
| 409L | 0,4-2,5 mm | 2B、2D | |
| Grado | Tipo | Espesor | Original |
| Acero resistente al calor | 309S | 0,5-40 mm | CHN |
| 310S | 0,5-40 mm | CHN | |
| Acero dúplex | 2101 | 1,5-50 mm | CHN |
| 2304 | 3,0-50 mm | CHN | |
| 2205 | 0,5-60 mm | CHN | |
| 2507 | 1,0-60 mm | SWE / JPN / CHN | |
| Acero súper austenítico | N08904 | 0,6-50 mm | SWE / JPN / CHN |
| S31254 | 0,5-50 mm | SWE / JPN / CHN | |
| N08926 | 0,5-50 mm | SWE / JPN / CHN | |
| N08367 | 0,5-50 mm | SWE / JPN / CHN | |
| Aleación a base de níquel | N08031 | 1,0-50 mm | US / JPN / GER |
| N08810/N08800 | 0,8-50 mm | US / JPN / CHN | |
| N08028 | 1,0-20 mm | US / GER / JPN | |
| N08020 | 1,0-20 mm | US / GER / JPN | |
| N08825 | 0,8-40 mm | US / GER / SWE / JPN / CHN | |
| N10276 | 0,5-50 mm | US / GER / JPN | |
| N06022 | 1,0-50 mm | US / GER / JPN | |
| N06625 | 0,8-20 mm | US / GER / CHN | |
| N04400 | 1,0-20 mm | US / GER / JPN | |
| N06600 | 1,0-50 mm | US / GER / JPN / CHN | |
| N02201 | 0,5-20 mm | US / JPN | |
| Titanio | TA1/Gr1 | 0,5-50 mm | JPN / CHN |
| TA2/Gr2 | 0,5-50 mm | JPN / CHN | |
| Material de soldadura | ERNiCrMo-13 | 1.2、2.4mm | GER |
| ERNiCrMo-3 | 2,4 mm | GER | |
| ERNiCrMo-4 | 2,4 mm | US |
| Tolerancia para chapa 2B | |||
| Talla | Rango de tolerancia | ||
| Grupo 1 | Grupo 2 | Grupo 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| Tolerancia de la chapa laminada en caliente n.º 1 | |||
| Talla | Rango de tolerancia | ||
| Grupo 1 | Grupo 2 | Grupo 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| Elección del Estado de entrega | Estado de la superficie |
| Laminado en frío | 2B |
| 2D | |
| BA | |
| Línea del cabello | |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| Nota: | |
| 1. Si necesita un estado de entrega diferente al indicado anteriormente, confírmelo con nosotros. | |
| 2. En caso de cualquier consulta o pedido, por favor, háganos saber cualquier requisito adicional no indicado aquí. | |
| Estado de entrega | |
| Elección del Estado de entrega | Estado de la superficie |
| Laminado en caliente | No.1 |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| En escabeche | |
| Nota: | |
| 1. Si necesita un estado de entrega diferente al indicado anteriormente, confírmelo con nosotros. | |
| 2. En caso de cualquier consulta o pedido, por favor, háganos saber cualquier requisito adicional no indicado aquí. | |
The surface and shape of 201 stainless steel plate (7)
Información disponible para consulta y descarga
Daxun es un fabricante de placas de acero inoxidable de confianza
Como fabricante profesional, Daxun asegura que todos los productos que producimos son de alta calidad. Por lo tanto, nos aseguramos de que todas las placas de acero inoxidable estén certificadas por ISO9001, SGS, CE, OQC y más normas internacionales de calidad.También tenemos un estricto control de calidad para garantizar que las placas de acero inoxidable tengan menos defectos. En Daxun, puede estar seguro de que todos los productos son duraderos, de alta calidad y alto rendimiento.
Proyectos y productos recientes
Productos relacionados (13)
Daxun stainless steel plates are in high demand, have good quality, and are honest and trustworthy.
- Daxun International has been in international business for over ten years. In 2022, its export revenue surpassed $100 million, and its export volume was among the top Chinese stainless steel processing enterprises. To serve abroad markets, we have built three export service facilities in China and collaborated with engineering organisations, steel mills, and international trade companies. We continue to enhance our service capabilities, establishing three export service bases in China, and collaborating with engineering firms, steel mills, and international trading firms to grow into new markets.
- Daxun has long-standing relationships with dozens of well-known steel mills throughout the world, supplying 30,000 tonnes of standard stainless steel plates and 20,000 tonnes of metals such as duplex steel, nickel-based alloys, and heat-resistant steel. Daxun’s stainless steel materials are of consistent quality and never counterfeited. The kinds, specifications, and delivery weights strictly adhere to the standards.
- Daxun has several stainless steel plate processing equipment, a professional physical and chemical testing centre, and “cutting, grinding, forming, beveling, welding, heat treatment, machining, and spraying” production lines. Services are provided in approximately 30 industries, including vehicles, home appliances, lifts, new energy, vacuum semiconductors, food and beverage/biofermentation, petrochemicals, and energy equipment. Collaborate with steel mills, research institutes, and other organisations to offer comprehensive services ranging from project design and material development to processing and manufacturing process optimisation.
Stainless steel materials “more, faster, better, and cheaper” customised services
- First, it refers to Daxun’s stainless steel plate kinds and specifications, as well as its spot inventories.Daxun has strategic resource assistance from many large steel mills at home and abroad, ensuring the stability of the stainless steel plate supply chain and meeting clients’ individualised needs on specific materials.
- Secondly, Daxun’s processing technology is diverse.
processes, including stainless steel plate cutting, grinding, cutting, forming, welding, and machining, to provide customers with “one-stop” service.
Daxun services a large number of consumers in a variety of sectors.
- Daxun’s stainless steel company focuses on the key sectors of equipment manufacture. far, it has served over 30,000 customers, including over 10,000 active customers from more than 30 industries and a big number of major businesses. This demonstrates Daxun’s extensive service experience, as well as its widespread consumer recognition across industries.
Customers with urgent needs can rest assured that we will supply stainless steel plate products on time and quickly.
- Behind the speed is the support of the system, including information flow, logistics, and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, seamlessly connected; in terms of logistics, the processing center is close to ports, rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading to ensure that the task is completed on time.
We provide excellent quality and high-quality services.
- Quality is belief, and integrity is a business card. Daxun pioneered the concept of “excellent performance management” and promoted the “PDCA+Lean” management model, making “Daxun = assured quality” the company’s business card. In terms of materials, Daxun Stainless Steel has achieved full traceability of each steel plate from the ERP system, including varieties, specifications, and origins, and advocated and encouraged industry anti-counterfeiting.
- Daxun Stainless Steel relies on technology for processing, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, closely monitors during sales, and provides worry-free service guarantees after sales.
We save our customers time, materials and energy, and ultimately save them money.
Daxun’s professional advantages enable us to provide the most cost-effective material recommendations based on customer needs, and minimize costs for customers through methods such as continuous processing and nesting processing.
Our innovative nesting processing methods optimize material and cutting utilization.
At the same time, Daxun achieves continuous cost reduction and efficiency improvement by promoting lean improvement activities and passing the benefits to customers. Daxun also has a complete product traceability system and timely quality objection handling, which relieves customers’ concerns.
Leading Stainless Steel Sheet Suppliers in China
Contact the top suppliers in China for stainless steel sheets (steel plates) in a variety of finishes. You need no other stainless steel sheet supplier than Daxun Alloys, who offer free cutting services and delivery times as short as 5-7 days.
201 Stainless Steel Plate in a Variety of Finishes
Our stainless steel sheets (sometimes called steel sheets) are available in a range of beautiful finishes: brushed finish, 2B smooth finish or 8K mirror finish.
The finished side of each stainless steel sheet we supply is coated with a film. This film is easily peeled off after fabrication or installation and protects the surface of the material from wear and marks. The back side is unfinished.
201 Stainless Steel Plate is the most commonly used variety. It is easily weldable, formable, and has good corrosion resistance.
We can assist in providing stainless steel sheets in any required size.
To meet your specific requirements, our stainless steel sheets are available in three finishes and a variety of sizes. We can readily provide any custom size you may need with our free unlimited cutting service.
We are able to meet any size needs between 0.3 and 30 mm in thickness and between 50 x 50 mm and 2500 x 1250 mm in size. In addition, we provide free unlimited cutting with every order, using a state-of-the-art cutting machine to precisely meet your requirements.
Order Stainless Steel Sheets by Phone or Online.
There has never been an easier way to get stainless steel sheets. Simply refer to the simple and detailed instructions on our website. Alternatively, our sales staff will be happy to take your order or answer any questions when you call +86 13382898899 or email [email protected].
Our delivery time is only one to two days.
Characteristics:
This grade is more resistant to corrosion and pitting than 304 and offers higher strength at elevated temperatures. In addition, 316L is an extra low carbon variation that helps avoid carbide precipitation due to welding.
Important Safety Note:
The edges of the metal sheets we sell are not polished, ground or finished, so they may be sharp, just like the edges of any stainless steel sheet. We remind users to use, install and handle these devices with care.
Podemos proporcionarle muestras de chapa de acero inoxidable para que compruebe la calidad. La muestra es gratuita y usted sólo paga el flete.
Hemos exportado a más de 42 países, como Canadá, Chile, Kuwait, Alemania, Corea del Sur, Arabia Saudí, Singapur, etc.
Nuestro MOQ es de 1 tonelada de chapa de acero inoxidable.
Los pedidos de prueba pueden entregarse en una semana. Los pedidos normales tardan unas dos semanas.