x
Senden Sie Ihre Anfrage noch heute
Schnelles Angebot

Daxun is an experienced manufacturer of CP-Grade 1 titanium plates

As China’s leading supplier of titanium and titanium alloy plates, Daxun provides high-performance titanium plates to the world.
  • Titanium plate Grade:CP-1(Klasse 1)- UNS R50250
  • Titanium plate production types: cold rolling, hot rolling, forging.
  • Titanium plate density The density of grade 1 titanium is 4.51 g/cm3
  • Standards: ASTM B265 Gr 1, ASME SB265, ASTM F67 AMS 4919
  • Features: high specific strength, light weight, corrosion resistance
  • Processing: high ductility, easy to form, easy to process

——Daxun produces titanium sheets in China to meet the diverse and demanding needs of customers!

A global leader in commercially pure titanium sheet fabrication services

DAXUN Alloys is a top global supplier of premium Grade 1 titanium plates. Grade 1 titanium offers great ductility and cold formability, perfect for deep drawing. It is also highly resistant to seawater and various solutions, including chlorides, making it a reliable choice for different environments.

Titanium’s low density, high strength-to-weight ratio, and corrosion resistance make it ideal for tough chemical environments. Commercially pure Grade 1 titanium is the softest and most ductile, offering great cold formability and top-notch corrosion resistance. It also welds easily and has good impact strength. Grade 1 titanium is also used in the aerospace industry for manufacturing airframe components due to its excellent properties.

DAXUN specializes in large and small titanium plate projects. We are your trusted partner, dedicated to providing high-quality titanium plates and ongoing technical support for your business. Our focus is on building long-term relationships through reliability and expertise.

Weiterlesen

Technical Data Sheet

Alvac Grade ASTM B348 Grade # Chemistry N C HA HB O Fe Pd Other Elements Each Total Other Elements Ti
30 1 Weight %, maximum 0.03 0.10 0.010 0.0125 0.18 0.20 0.05 0.30 Bal.

Unalloyed CP titanium (Grades 1, 2, 3, and 4) generally resist crevice corrosion at temperatures below 80°C (175°F) in any pH-treated solution.

Our technical datasheet pdf provides more information about mechanical properties. If you have any concerns or need more details about our product, please contact us.

Physical Properties & Specifications

ASTM Grades I (ATI 30)

ATI 30: 1,630°F ± 25°F (888°C ± 4°C)

ASTM F 67 – Unalloyed Titanium

ISO 5832-2 – Unalloyed Titanium

Wärmebehandlung

Commercially pure titanium can be annealed by heating to 1,000 – 1,300°F (538 – 704°C) for 1/2 to 2 hours and air cooling.

Choose Daxun to help your project take off.

Contact Daxun now

Custom Cutting

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • Water jet cutting
  • Laser cutting
  • Plasma cutting
  • Wire cutting
  • Bending
  • Slitting
  • Sawing
Contact Daxun now

Grade1 TItanium sheet FINISHES

#1 – Hot rolled, annealed, and descaled for applications that do not require a smooth decorative finish. #2D – Dull finish achieved through cold rolling, annealing, and descaling. Used for deep-drawn pieces and parts requiring lubricants to be kept during the shaping process.

#2B – Smooth finish achieved through cold rolling, annealing, and descaling. A light, cold rolling pass following annealing results in a brighter finish than 2D.

#BA – Cold rolled, brilliant annealed

#CBA: Coarse bright annealed cold rolled matte finish and bright annealed.

Contact Daxun now

Advanced Production

The cold-rolled thickness range for Grade 1 Titanium Plates is 0.3 mm to 6.0 mm, while the hot-rolled range is 4.76 mm to 155 mm. These plates are produced through longitudinal and transverse rolling and are available in hot-rolled or heat-treated conditions. Over 70% of all alloy grades melted are variants of Titanium 6Al-2Sn-4Zr-6Mo, showcasing its significant application in various industries. We also offer cut blanks, allowing complex shapes to be cut from the parent plate as needed.

Contact Daxun now

Quality, Inspection

Daxun performs a variety of quality assurance tests, including flattening, pitting resistance, mechanical, hardness, material identification, and expansion tests. These tests guarantee that the material meets the required standards for its intended application.

During the production process, we measure the diameter, thickness and surface of the product.

  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples for customer testing
  • Support on-site or video factory inspection
Contact Daxun now

Technical Support

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Contact Daxun now

Fast Delivery

We ensure timely delivery of Grade 1 titanium plates, supported by our strong production capacity, seamless information flow, and efficient logistics. Daxun’s order data is instantly integrated with our logistics system, enabling smooth coordination. Our processing center is strategically located near highways, rivers, and ports, allowing for quick scheduling, storage, and transportation. With efficient loading, we guarantee that your goods arrive on time.

We provide different way to ship our product, including FOB, CFR, CIF, DDP and DAP.

Our delivery time is strictly in accordance with the contract.

Contact Daxun now

Verpackung

Daxun pays special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
• Boxes and crates
• Shrinkwrap
• Wooden pallets
• Wooden boxes

Grade 1 Titanium Plate Features

High strength
Corrosion resistance
Heat resistance
Low temperature resistance
Environmental protection
Leichtgewicht

Daxun Grade 1 Titanium sheet Let your brand improve rapidly

Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube.
Products/Processing Standard Grade/Size
Titanium Plate, Sheet, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Thickness:( 0.0197”-6”)Max Width: 12 feet,Max Length: 50 feet)
AMS-T-9046
Titanium and Titanium alloy sheet, plate
Commercially pure titanium (CP)
Code designation Yield strength
minimum, ksi 1 /
CP-1 70
CP-2 55
CP-3 40
CP-4 25
Alpha titanium alloys(A)
Code designation Zusammensetzung
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
Alpha-beta titanium alloys(AB)
Code designation Zusammensetzung
AB-1 6A1-4V
AB-2 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
Beta titanium alloys(B)
Code designation Zusammensetzung
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
Processing:
Warmwalzen Kaltwalzen
Available Grades:
CP Grade 1 Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CP Grade 2 Grade 6Al-4V ELI (Formerly Grade 23)
Grade 7 Grade 6Al-6V-2Sn (6-62)
Grade 19 Grade 8Al-1Mo-1V (8-1-1)
Grade 5 (6Al-4V) Grade 9 (3Al-2.5V)
Grade 6 (5Al-2.5Sn) CP Grade 3
Anwendung
Chemische Industrie Desalination Of Sea Water
Petrochemical Industry Luft- und Raumfahrt
Machining Field, Automobile Field Mobile Phone Component Field.

Daxun ist ein professioneller Hersteller, der sich für hochwertige Produkte einsetzt. Wir stellen sicher, dass alle unsere Titanplatten internationalen Standards entsprechen. Dazu gehören certifications from ISO9001, SGS, CE, and OQC. Our strict quality control process minimizes defects.

Recent hot case projects and products

Grade 1 Titanium Plate and sheet
Nuclear electricity
Grade 1 Titanium Plate and sheet
Luft- und Raumfahrt
Titanium Plate and sheet
Chemicals
Titanium Plate and sheet
Pressure Vessels
Titanium Plate and sheet
New energy industry
Titanium Plate and sheet
Schiffstechnik
Titanium Plate and sheet
Desalination
Titanium Plate and sheet
Power Industry
Titanium Plate and sheet
Photovoltaic Energy
Titanium plate and sheet Grade 1 

We specialize in pure titanium plates. Our products serve both the industrial and aerospace sectors. We excel in meeting customer needs. Our clients trust our capabilities. We consistently deliver the products they require.

DAXUN has always worked with overseas clients. We have strong ties to global titanium industry leaders. Our technology ensures high-quality materials. We meet specific project needs.

We have established supply chains and maintain research laboratories. Alpha-beta alloys, such as Ti 6Al-4V, are heat-treatable and extensively used in various industries, including aerospace and marine applications. We operate through subsidiaries to ensure top-quality production. We adapt to any specific product request. Every order receives our full attention. Quality is our priority from start to finish.

DAXUN values customer service highly. It’s a key part of our business. We provide clear information to customers. Our pricing is comprehensive. We interact closely with our customers and answer their technical questions. Our support goes beyond the product itself.

When you buy from us, you get more. You receive raw materials, of course. But you also get excellent service.

Titanium Plate and sheet Grade 1 Data sheet

ASTM B265 | ASME SB265 | ASTM F67 | ISO 5832-2 | 3.7025 | UNS R50250

Grade 1 pure titanium sheet is highly ductile. It has excellent cold formability, making it ideal for deep drawing. Grade 1 titanium resists corrosion well. It stands up to general corrosion. It also withstands seawater corrosion. The material resists oxidizing media. It handles neutral solutions too. Even mildly reducing media, like chlorides.

Titanium has a low density. It’s about half as dense as nickel-based alloys. Titanium offers a high strength-to-weight ratio. Its corrosion resistance is remarkable.

These properties make titanium versatile. It performs well in harsh chemical conditions. Many industries choose it for demanding applications.

Grade 1 Titanium Plate Features and Corrosion Resistance

High ductility;
Good cold formability and impact strength;
Medium strength;
High corrosion resistance and notched impact strength;
Excellent biocompatibility;
Very easy to weld and not magnetic.

Welche Titanlegierung ist die beste?

Die von Ihnen benötigte Titanlegierung hängt von Ihrem Projekt ab, da jede Legierung unterschiedliche Vorteile bietet.

Alle Titanlegierungen sind extrem fest und korrosionsbeständig, sodass sie auch unter härtesten Bedingungen weiterhin einwandfrei funktionieren.

Die höheren Güteklassen der Titanlegierungen (5-12) sind Legierungen, die für bestimmte Vorteile entwickelt wurden. Sie sind auch als Beta-Legierungen für verschiedene Verwendungszwecke bekannt, beispielsweise als Metallstütze im menschlichen Körper. Die Titanlegierung der Güteklasse 12 verfügt beispielsweise über eine ausgezeichnete Hitzebeständigkeit und ist daher die perfekte Wahl für Rohrbündelwärmetauscher, Hydraulikleitungen und Anlagen für die chemische Industrie.

Die Sorten 1 bis 4 sind reine Titansorten und die perfekte Wahl, wenn Sie ein schweißbares, duktiles Material für Rohrleitungssysteme und Rohre benötigen.

Bei der Auswahl von Titanlegierungen sind die üblichen physikalischen Eigenschaften wie Wärmebehandlung, Bruchzähigkeit, Wärmeleitfähigkeit, mechanische Eigenschaften, Zugfestigkeit und Streckgrenze zu berücksichtigen. Außerdem müssen wir die Anwendung verstehen, um Ihnen bei der Erreichung Ihres Ziels zu helfen.

Wenn Sie ein Projekt starten und sich nicht sicher sind, welche Sorte für Sie am besten geeignet ist, kontaktieren Sie uns jetzt. Wir helfen Ihnen gerne weiter.

Wie unterscheiden sich höhere Titanqualitäten von niedrigeren Qualitäten?

Titan-Gerades, auch bekannt als kommerziell reines Titan und Titanlegierungen.

Bei DAXUN bieten wir eine breite Palette an Titanlegierungen von Grad 1 bis Grad 18 an.

Die Güteklassen 1 bis 4 bestehen aus reinem Titan, während höhere Güteklassen Legierungen sind. Legierungen sind aufgrund ihres hohen Verhältnisses von Festigkeit zu Gewicht beliebt.

Die am häufigsten verwendete Titanlegierung ist die Legierung der Güteklasse 5 (Ti 6Al 4V). Ausgehend von der Güteklasse 5 wird sie mit verschiedenen Metallen wie Aluminium und Eisen kombiniert. Diese hervorragende Kombination erweitert die ausgezeichnete Schweißbarkeit und die hohe Temperaturkriechfestigkeit.

Höhere Güteklassen werden aufgrund ihrer Verschleiß- und Korrosionsbeständigkeit von Branchen wie der Luft- und Raumfahrtindustrie und der Schifffahrtsindustrie bevorzugt.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

Does the grade of titanium affect the cost?

While the grade of titanium does increase the cost slightly, the total cost is primarily determined by the shape and form of titanium you require.

At DAXUN, we offer all sorts of titanium products, including plates, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

It is difficult to offer a price online without knowing much about your project and what the metal will be used for.

But don’t worry. Our team is always here to help with your titanium needs. By sending an email to us, we will be able to get back to you with some advice and an accurate quote. Make sure to include as much information as possible about your needs.

Where can I learn more about the grades of titanium?

Das Team von DAXUN ist erfahren, kompetent und freundlich. Dank ihrer langjährigen Erfahrung in der Branche wissen sie alles über Titan, einschließlich seiner Verwendungsmöglichkeiten, Vorteile und Güteklassen.

Regelmäßige Updates zu Titan, seinen Verwendungszwecken und seinen Anwendungen in verschiedenen Branchen finden Sie in unserem Blog. Unsere Experten haben leicht verständliche Beiträge verfasst, die Sie jederzeit nachlesen können.

By sending an email to [email protected], you’ll receive a quick response.

Wie kann man schnellstmöglich ein Angebot einholen oder Marktinformationen verstehen?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email ([email protected]) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week.

Kann ich ein paar Muster bekommen?

We can provide Titanium sheet samples for you to check the quality. The sample is free and you just pay the freight. Contact us for more details and we are happy to make you a special offer.

What is your MOQ?

MOQ is 1 ton for the Titanium sheet.

Übersicht über Titanlegierungen

Titanlegierungen sind eine Mischung aus Titan und anderen chemischen Elementen, die selbst unter extremen Temperaturen eine außergewöhnliche Zugfestigkeit und Zähigkeit bieten. Diese Legierungen sind leicht, weisen eine außergewöhnliche Korrosionsbeständigkeit auf und halten hohen Temperaturen stand, wodurch sie in verschiedenen Branchen unverzichtbar sind. Von der Luft- und Raumfahrt über Flugzeuge bis hin zu medizinischen Geräten und Schmuck sind Titanlegierungen aus vielen Anwendungen mit hoher Beanspruchung nicht mehr wegzudenken.

Kommerziell reines Titan, das für seine akzeptablen mechanischen Eigenschaften bekannt ist, wird häufig in orthopädischen und zahnmedizinischen Implantaten verwendet. Die gängigste Titanlegierung, Ti 6Al 4V, enthält geringe Mengen an Aluminium und Vanadium (6 % bzw. 4 % des Gewichts). Diese Kombination ermöglicht eine Ausscheidungshärtung, wodurch die mechanischen Eigenschaften der Legierung verbessert werden. Ob in Form von Alpha-Legierungen, Beta-Legierungen oder Alpha-Beta-Legierungen – Titanlegierungen sind nach wie vor ein wichtiger Bestandteil in Branchen, in denen Materialien benötigt werden, die sowohl Festigkeit als auch Korrosionsbeständigkeit bieten.

Schnelles Angebot