x
Envie hoje o seu pedido de informação
Orçamento rápido

  • Tubo de Hastelloy
  • Tubo de Hastelloy
  • Tubo de Hastelloy
  • Tubo de Hastelloy
  • Tubo de Hastelloy
  • Tubo de Hastelloy
  • Tubo de Hastelloy
  • Tubo de Hastelloy
  • Tubo de Hastelloy
  • Tubo de Hastelloy

Daxun Alloy - Hastelloy C-22 pipe made in China

As a leading supplier of Hastelloy C-22 pipes in China, Daxun provides high-performance alloy tubes to the world.
  • Hastelloy C-22 types: Seamless tube,  welded tube, forged tube
  • Certification : ASTM,SGS,ISO,CE
  • Prazo de entrega: 7-15 dias
  • Surface finish: Annealed, polished etc.
  • MOQ : ≥300kg

————Daxun produces hastelloy pipe in China to meet the diverse and ——necessidades exigentes dos clientes!

Caraterísticas e propriedades do Hastelloy C-22

A liga Hastelloy C-22 (UNS N06022) é uma liga completa de níquel-crómio-molibdénio-tungsténio com melhor resistência global à corrosão do que outras ligas de níquel-crómio-molibdénio existentes, incluindo a liga Hastelloy C-276, a liga C-4 e a liga 625. A liga Hastelloy C-22 tem boa resistência à corrosão por pite, à corrosão em fendas e à fissuração por corrosão sob tensão. Tem uma excelente resistência a meios aquosos oxidantes, incluindo cloro húmido, ácido nítrico ou ácidos mistos contendo ácidos oxidantes com iões cloreto. Ao mesmo tempo, a liga Hastelloy C-22 também tem uma resistência ideal a ambientes redutores e oxidantes encontrados no processo. Com base neste desempenho versátil, pode ser utilizada em alguns ambientes problemáticos ou em fábricas com múltiplos objectivos de produção. A liga Hastelloy C-22 tem uma resistência excecional a vários ambientes químicos, incluindo substâncias oxidantes fortes, tais como cloreto férrico, cloreto cúprico, cloro, soluções contaminadas a quente (orgânicas e inorgânicas), ácido fórmico, ácido acético, anidrido acético, água do mar e soluções salinas. A liga Hastelloy C-22 tem a capacidade de resistir à formação de precipitação no limite do grão na zona afetada pelo calor da soldadura, pelo que também pode ser utilizada em muitos processos químicos no estado soldado.

Corrosion resistance
The corrosion resistance of Hastelloy C-22 is its most outstanding feature, and it is suitable for a variety of corrosive environments:
Oxidizing media: such as nitric acid, chromic acid, hypochlorite, etc.
Reducing media: such as sulfuric acid, hydrochloric acid, phosphoric acid, etc.
Local corrosion: It has strong resistance to pitting, crevice corrosion and stress corrosion cracking (SCC).
Mixed acid environment: complex media such as sulfuric acid + hydrochloric acid, nitric acid + hydrofluoric acid.
High temperature corrosion: It can still maintain good corrosion resistance at high temperatures.

Comparison with other alloys
Compared with Hastelloy C-276, C-22 has a higher chromium content and stronger oxidation resistance.
Compared with stainless steel, C-22 has significantly better pitting and crevice corrosion resistance in chloride environments.

Processing performance
Hastelloy C-22 has good processing performance, but its high strength and work hardening tendency should be noted:
Cold processing: It can be processed by cold rolling, cold drawing, etc., but attention should be paid to work hardening.
Hot working: The hot working temperature range is 950-1200°C, and overheating should be avoided.
Welding: TIG (tungsten inert gas shielded welding), MIG (metal inert gas shielded welding), plasma arc welding and other methods can be used. Heat treatment is usually not required after welding, but heat input needs to be controlled to avoid intergranular corrosion.
Application areas
Hastelloy C-22 is widely used in the following fields:
Chemical industry: used to manufacture reactors, heat exchangers, pipelines, valves and other equipment, especially in strong acid, strong alkali and mixed acid environments.
Oil and gas: used for downhole tools, valves, pumps, pipelines, etc., to resist corrosion from hydrogen sulfide, carbon dioxide and chlorides.
Environmental protection field: used for flue gas desulfurization (FGD) systems, wastewater treatment equipment, etc.
Pharmaceutical industry: used for high-purity equipment to resist corrosive media.
Nuclear industry: used for nuclear waste treatment equipment to resist corrosion from radioactive media.

Ler mais

Hastelloy C-22 Parâmetros

Ni Cr Mo W Fe Co
56% 20-22.5% 12.5-14.5% 2.5-3.5% 2-6% ≤2.5%
Mn Si C P S
≤0,5% ≤0,08% ≤0,015% ≤0,02% ≤0,02%

 

Imóveis Densidade Ponto de fusão Coeficiente de expansão térmica Condutividade térmica Resistividade eléctrica Módulo de elasticidade
Valor 8,69 g/cm³ 1325-1370°C 12,8 μm/m-°C 10,1 W/m-K 1,25 μΩ-m 206 GPa

 

Imóveis Temperatura ambiente (20°C) Alta temperatura (600°C) Norma de ensaio/Notas
Resistência à tração ≥690 MPa ≥380 MPa ASTM E8/E8M
Resistência ao escoamento (0.2%) ≥310 MPa ≥220 MPa ASTM E8/E8M
Alongamento ≥45% ≥30% 50 mm de comprimento do calibre
Dureza (Brinell) ≤220 HB ASTM E10

 

Escolha a Daxun para ajudar o seu projeto a arrancar.

Contactar a Daxun agora

Advanced Production:Hastelloy alloy pipe

Hastelloy C22 alloy is an all-around nickel-chromium-molybdenum-tungsten alloy with good resistance to pitting, crevice corrosion and stress corrosion cracking. It has excellent resistance to oxidative aqueous media, including wet chlorine, nitric acid or mixed acids of oxidizing acids containing chloride ions. At the same time, Hastelloy C22 alloy also has ideal resistance to reducing and oxidizing environments encountered in the process. Relying on this versatile performance, it can be used in some troublesome environments or in factories for a variety of production purposes.

Contactar a Daxun agora

Hastelloy C-22 Pipe Features

Hastelloy C22 alloy has an exceptional resistance to various chemical environments, including strong oxidizing substances, such as ferric chloride, cupric chloride, chlorine, thermally contaminated solutions (organic and inorganic), formic acid, acetic acid, acetic anhydride, seawater and salt solutions, etc. Hastelloy C22 alloy has the ability to resist the formation of grain boundary precipitation in the heat affected zone of welding, so that it can also be used in many chemical processes in the welding state.

Contactar a Daxun agora

Qualidade, entrega, inspeção

Daxun conducts a series of quality assurance tests on Hastelloy C-22 pipes. These tests include flattening test, flaring test, ultrasonic flaw detection, crevice corrosion resistance test, mechanical property test, hardness test, material positive identification, and expansion test, etc. All these tests are designed to ensure that the Hastelloy C-22 pipes meet the requirements of the intended applications. During the production process, we meticulously measure the outer diameter, wall thickness, and surface quality of the products. Our standard delivery time is 5 – 7 days, and for special sizes, it is 15 – 20 days.

  • O nosso prazo de entrega está estritamente de acordo com o contrato.
  • Apoio a agências terceiras do cliente para se deslocarem à fábrica para inspeção
  • Apoio a amostras gratuitas para teste do cliente
  • Apoio à inspeção de fábrica no local ou por vídeo
Contactar a Daxun agora

Embalagem

A Daxun Alloy assegura a melhor qualidade de embalagem, uma vez que esta desempenha um papel importante no transporte internacional de mercadorias, onde as mercadorias passam por vários canais para chegar ao destino final, pelo que prestamos especial atenção à embalagem. Embalamos os nossos produtos de várias formas, consoante o produto. Embalamos os nossos produtos de várias formas, tais como:
- Caixas e caixotes
- Película retrátil
- Paletes de madeira
- Caixas de madeira

Contactar a Daxun agora

Apoio técnico

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. [Contacte-nos agora]Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Daxun is a trustworthy stainless steel tube manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium tubes are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the stainless steel tubes have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

Como obter uma cotação OU compreender a informação de mercado o mais rapidamente possível?

Preencha o formulário na página “Contacte-nos” ou ligue para o nosso gestor de vendas através do número “+86 13382898899” e entraremos em contacto consigo o mais rapidamente possível. O nosso WhatsApp está online e o e-mail ([email protected]) será verificado no prazo de 6 horas. Todas as perguntas ou mensagens serão respondidas prontamente. Além disso, todas as semanas partilhamos informações de mercado com os nossos clientes

Podem dar-me algumas amostras?

Podemos fornecer amostras de chapas de aço inoxidável para que possa verificar a qualidade. A amostra é grátis e o cliente só paga o frete.

Para que países já exportou?

Exportámos para mais de 42 países, como o Canadá, Chile, Kuwait, Alemanha, Coreia do Sul, Arábia Saudita, Singapura, etc.

Qual é o vosso MOQ?

The minimum order quantity for our Hastelloy products is 300kg

Qual é o prazo de entrega?

As encomendas de teste podem ser entregues no prazo de uma semana. Para as encomendas normais, são necessárias cerca de duas semanas.

Envie hoje o seu pedido de informação
Orçamento rápido