x
오늘 문의 보내기
빠른 견적

Daxun is an experienced Ti 6Al 4V Grade 5 Titanium Plate manufacturer

As a leading supplier of titanium in China, Daxun provides high-performance 6-4 titanium plates to the world.

  • Plate Grade: Grade 5-Ti-6Al-4V-USN 56400-TC4
  • Plate Production type: cold rolling, hot rolling, forging.
  • Standard: ASTM B265  AMS 4911、AMS-T-9046、ASTM F1472 etc
  • Features: High strength, Lightweight, High-temperature resistance
  • The density of grade 5 titanium plate is 4.51 g/cm3
  • α-β titanium alloy, aluminum stabilizes the α phase, vanadium stabilizes the beta phase

————Daxun produces titanium sheets in China to meet the diverse and ——고객의 까다로운 요구 사항!

A global leader in high performance Ti-6Al-4V alloy titanium plate manufacturing services

DAXUN, based in China, is a prominent manufacturer and supplier of Ti 6AL 4V (Grade 5, UNS R56400) titanium plates. We are dedicated to providing high-performance, world-class titanium plates, ensuring timely global delivery of ASTM B265 Grade 2 and Grade 5 titanium plates.

We produce Grade 5 titanium plates (UNS R56400) in thicknesses from 0.5mm to 300mm, with specifications for cold rolling (0.5 mm-6.0 mm), hot rolling (6.0–50 mm), and forging (over 50 mm). Grade 5 (Ti-6Al-4V), often referred to as the “workhorse” of titanium alloys, is renowned for its exceptional strength, ductility, and resistance to both corrosion and high temperatures. These qualities make it a top choice for numerous general and military applications. Our products meet various standards such as ASTM, ASME, AMS, GB, GJB, MIL, JIS, and EN.

Titanium Grade 5, also known as Ti-6Al-4V, is composed of 90% titanium, 6% aluminum, and 4% vanadium, making it an α-β titanium alloy. In this alloy, aluminum stabilizes the α phase, while vanadium stabilizes the β phase. Key characteristics of Ti-6Al-4V plates include exceptional overall performance, excellent processability, and outstanding strength at both ambient and elevated temperatures. They also demonstrate excellent creep resistance, thermal stability, fatigue performance in seawater, crack growth resistance, and strong fracture toughness under hot salt stress corrosion. Furthermore, these plates exhibit remarkable plasticity and superplasticity, making them versatile for various processing methods, welding, and machining.

DAXUN is a metal expert focused on small and large pure titanium plate and 6-4 titanium alloy plate projects. DAXUN is your reference point and long-term partner, ready to provide you and your business with grade 5 titanium plates and any technical assistance you may need. You can think of DAXUN not only as your industrial pure titanium plate and titanium alloy plate supplier, but also as your strategic partner to help you meet any challenges and needs you may encounter, ultimately allowing you to achieve your project goals.

DAXUN’s service center in China has 6al 4v titanium plate products in stock and can quickly process orders. Through basic processing, water jet cutting and plate nesting products, we provide added value to our customers, saving them time and costs.

Continuous investment in DAXUN’s production facilities and capacity agreements with partners ensure that DAXUN is at the forefront of titanium plate quality now and in the future.

자세히 보기

데이터

Ti 6Al-4V Titanium Plate and sheet Type 플레이트, 시트, 스트립, 코일, 포일, 플랫, 클래드 플레이트, 일반 시트, 롤링 시트, 롤링 플레이트, 플랫 심, 플랫 시트, 심 시트, 롤, 블랭크(원형), 전단, 어닐링, 연질 어닐링, 스케일 제거, 트레드 플레이트, 체커 플레이트
등급 ASME SB265, AMS 4911, AMS 4919, AMS 4914, ASTM F67, ASTM F136, MSRR, AMS, BS
Titanium Alloy Gr 5 Plate Length 1000mm-13000mm 또는 필요에 따라
Gr 5 Titanium Plate Width 1000mm-1219mm-1500mm-1800mm-2000mm-2500mm 또는 필요한 경우
UNS R56400 Plate Thickness 0.3~120mm 또는 필요에 따라
ASTM B265 Titanium Alloy Gr 5 Plate Process 열간/냉간 압연/단조
UNS R56400 Plate surface No.1, No. 2D, No. 2B, BA, No.3, No.4, No.6, No.7, 2B, 2D, BA NO(8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled ASTM B265 Titanium Alloy Gr 5 Plate, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc.
ASTM B265 Titanium Alloy Gr 5 Plate, Sheet and Strip JIS: N0, N2, N1, NW2200, NW2201, NW4400, NW5500, NW6002 등
Titanium Grade 5 Sheet ASTM ASTM B265
Titanium Grade 5 Sheet AMS AMS 4902
너비 및 두께 공차 EN 10258 (formerly DIN 59381),EN 10151 ASTM B265 Titanium Alloy Gr 5 strip for springs,EN 10088 ASTM B265 Titanium Alloy Gr 5 strip (general)
Ti 6Al 4v Grade 5 Titanium Plate standards and approvals EN ISO 18286 EN 10051 EN 10088-1 ISO 15510 EN ISO 9445 ASTM A 480 ASTM A 959 ASME IID
Standard Ti-6Al-4V ALLOY Plate & Sheet Sizes 1000 x 2000mm, 1220 x 2440mm, 1500 x 3000mm, 2000 x 2000mm, 2000 x 4000mm
Cold rolled Gr 5 Titanium Plate 0.5-6.4 mm
Hot rolled Gr 5 Titanium Plate 3.0–60.0 mm
UNS R56400 Plate Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard ASTM B265 Titanium Alloy Gr 5 Sheet suppliers
Availability of Titanium Alloy Gr 5 Foil sizes 두께: 8-100미크론(0.00031-0.004인치)
폭: 최대 500mm(19.5인치)
무게(롤 단위) : 최대 50kg(110파운드)(예: 8미크론에서 약 1400m, 100미크론에서 약 112m).
절단 포괄적인 서비스를 제공하기 위해 다음과 같은 다양한 절단 방법을 사용합니다:
레이저 플레이트 절단, 플라즈마 플레이트 절단, 옥시-프로판 화염 절단
플라즈마 프로파일 고객의 도면에 따라
Value added services for Cp Grade 5 Titanium Plate 레이저 절단, 워터젯 절단, 플라즈마 절단, 굽힘 및 기계 가공, 가장자리 준비, 용접, 톱질 및 전단.
China Grade 5 Titanium Plate Manufacturer ASTM B265 Titanium Alloy Gr 5 Plate: material 3/16″ [5.00 mm] and over in thickness and over 10″ [250 mm] in width;Gr 5 Titanium Sheet: material under 3/16″ [5.00 mm] in thickness and 24″ [600 mm] and over in width;Alloy Titanium Grade 5 Clad plate: Alloy Titanium Grade 5 Clad plate is a composite steel plate made by bonding UNS R56400 Titanium Grade 5 Plate, etc.ASTM B265 Titanium Alloy Gr 5 Strip: cold-rolled material under 3/16″ [5.00 mm] in thickness and under 24″ [600 mm] in width.
UNS R56400 Plate Origin 중국
Packing of Ti-6Al-4V plate 외부 방수 천 또는 합판 상자와 함께 번들 제공
테스트 UT, SGS 테스트, TUV 등
Why buy UNS R56400 Sheet from DAXUN? 무료 견적、무료 샘플、EN 10204 3.1、밀 테스트 인증서 배송과 함께 제공、NABL 승인 실험실 보고서、모든 타사 검사 허용、 ASTM A923 방법 “C” 또는 ASTM G48 방법 “A”로 테스트 최소 질소 함량 및 페라이트 개수 테스트
Chemical Composition:
기호 요소 Min % Max %
Al Aluminum 5.50% 6.75%
V Vanadium 3.50% 4.50%
Fe Iron 0.30%
O 산소 0.20%
C 탄소 0.08%
N 질소 0.05%
H 수소 0.01%
Y Yttrium 0.01%
Other, each 0.10%
Other, total 0.40%
Ti 티타늄 Remainder
물리적 속성 Metric English Comments
밀도 4.43 g/cc 0.16 lb/in³
기계적 특성
Hardness, Brinell 334 334  Estimated from Rockwell C.
Hardness, Knoop 363 363  Estimated from Rockwell C.
Hardness, Rockwell C 36 36
Hardness, Vickers 349 349  Estimated from Rockwell C.
Tensile strength min. 895MPa 129810 psi
수율 강도 min. 828MPa 120090 psi
Elongation at Break min.10 % 10 %
Reduction of Area min.25 % 25 %
탄성 계수 113.8 GPa 16500 ksi
Compressive Yield Strength 970 MPa 141000 psi
Notched Tensile Strength 1450 MPa 210000 psi  Kt (stress concentration factor) = 6.7
Ultimate Bearing Strength 1860 MPa 270000 psi  e/D = 2
Bearing Yield Strength 1480 MPa 215000 psi  e/D = 2
Poisson’s Ratio 0.342 0.342
Charpy Impact 17 J 12.5 ft-lb  V-notch
Fatigue Strength 240 MPa 34800 psi  at 1E+7 cycles. Kt (stress concentration factor) = 3.3
Fatigue Strength 510 MPa 74000 psi  Unnotched 10,000,000 Cycles
Fracture Toughness 75 MPa-m½ 68.3 ksi-in½
전단 계수 44 GPa 6380 ksi
전단 강도 550 MPa 79800 psi  Ultimate shear strength
Electrical Properties
전기 저항 0.000178 ohm-cm 0.000178 ohm-cm
자기 투과성 1.00005 1.00005  at 1.6kA/m
Magnetic Susceptibility 3.30E-06 3.30E-06  cgs/g
열 속성
CTE, linear 20°C 8.6 µm/m-°C 4.78 µin/in-°F  20-100ºC
CTE, linear 250°C 9.2 µm/m-°C 5.11 µin/in-°F  Average over the range 20-315ºC
CTE, linear 500°C 9.7 µm/m-°C 5.39 µin/in-°F  Average over the range 20-650ºC
비열 용량 0.5263 J/g-°C 0.126 BTU/lb-°F
열 전도성 6.7 W/m-K 46.5 BTU-in/hr-ft²-°F
녹는점 1604 – 1660 °C 2920 – 3020 °F
Solidus 1604 °C 2920 °F
Liquidus 1660 °C 3020 °F
Beta Transus 980 °C 1800 °F

프로젝트의 성공을 위해 Daxun을 선택하세요.

빠른 배송

Daxun provides customers with timely and fast delivery of grade 5 titanium plate products. Behind the speed is the system support from professional production capacity, and information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected.

주요 기능

Grade 5 titanium alloy plate is the most commercially available of all titanium alloys. It combines high strength and toughness. Grade 5 can be cold drawn and extruded, but this process is generally limited to smaller industrial facilities and is more commonly applied to commercially pure grades.

Ti-6Al-4V Grade 5 titanium alloy has good comprehensive properties:

  • 높은 강도
  • Creep resistance
  • Fatigue resistance
  • 열처리 가능
  • Good ductility
  • Good plasticity
  • 우수한 용접성
  • Suitable for service temperatures -196°C-450°C

Common applications

Ti-6AL-4V titanium plates and sheets are primarily used for components that demand superior corrosion resistance, high strength at elevated temperatures (400-450°C), as well as good ductility and lateral strength.

1. Applications include jet engine compressor blades, disks, and rings, fuselage components like wings and doors, turbine disks, bulkheads, military aircraft parts, engine nozzles, landing gear doors, and fuselage superplastic forming components.

2. Military applications include armor, guidance, shell casings, etc.

3. Spacecraft components, including rocket engines and heat shields, etc.

4. Medical and surgical instruments.

5. Sports equipment, including bicycle frames and golf clubs.

맞춤 커팅

Daxun Alloy provides customers with customized cutting solutions of various sizes to help you control the size loss of titanium plates, thereby saving your processing costs and time. Our cutting methods include:

  • 워터젯 절단
  • 레이저 커팅
  • Plasma cutting
  • Wire cutting
  • Bending
  • Slitting
  • 톱질

패키징

We pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
- 상자 및 상자
• Shrinkwrap
- 목재 팔레트
- 나무 상자

기술 지원

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry.

Grade 5 Titanium Plate Features

높은 강도
내식성
내열성
저온 저항
환경 보호
경량

Daxun Grade 5 Titanium sheet Let your brand improve rapidly

아래 나열된 제품 외에 사용 가능한 다른 금속 제품은 여기에 나열되어 있지 않습니다. DAXUN이 제조 및 공급할 수 있는 기타 금속 제품으로는 탄탈륨, 니오븀, 지르코늄, 하프늄, 니켈, 구리 등이 있으며 주로 판재, 바, 튜브 형태입니다.
제품/처리 표준 등급/크기
티타늄 플레이트, 시트, 코일- ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23, Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(두께:( 0.0197”-6”)최대 폭: 12피트, 최대 길이: 50피트)
AMS-T-9046
티타늄 및 티타늄 합금 시트, 플레이트
상업적으로 순수한 티타늄(CP)
코드 지정 수율 강도
최소, KSI 1 /
CP-1 Gr1 70
CP-2 Gr2 55
CP-3 Gr3 40
CP-4 Gr4 25
알파 티타늄 합금(A)
코드 지정 구성
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
알파-베타 티타늄 합금(AB)
코드 지정 구성
AB-1 Gr5 6A1-4V
AB-2 Gr5 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
베타 티타늄 합금(B)
코드 지정 구성
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
처리 중입니다:
열간 압연 냉간 압연
사용 가능한 성적:
CP 1등급 6Al-2Sn-4Zr-2Mo(6-2-4-2) 등급
CP 2등급 6Al-4V ELI 등급(이전 23등급)
7학년 6Al-6V-2Sn(6-62) 등급
19학년 8알-1모-1V 등급(8-1-1)
5등급(6Al-4V) 9등급(3Al-2.5V)
6등급(5Al-2.5Sn) CP 3등급
애플리케이션
화학 산업 해수 담수화
석유화학 산업 항공우주
기계 가공 분야, 자동차 분야 휴대폰 구성 요소 필드.

참조 및 다운로드 가능한 정보

Daxun is a trustworthy titanium plate manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium plates are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the titanium plates have fewer defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

최근 인기 있는 사례 프로젝트 및 제품

2등급 티타늄 플레이트 및 시트
2등급 티타늄 플레이트 및 시트
티타늄 플레이트 및 시트
티타늄 플레이트 및 시트
티타늄 플레이트 및 시트
티타늄 플레이트 및 시트
티타늄 플레이트 및 시트
티타늄 플레이트 및 시트
티타늄 플레이트 및 시트
티타늄 플레이트 및 시트 등급 2 / UNS R50400

Titanium plate and sheet Grade 5 

  • Our expertise includes the provision of products in the form of titanium sheets for industrial and aerospace applications, whereby we make sure our customers trust us to meet their product specifications. We are flexible to change over to meet the specifications, or requirements, of each project—planning and budgeting the process down to the preparation of raw materials, inspection, and delivery of the finished product. Ever since the very beginning of DAXUN’s history, we have established excellent relations with consumers from other parts of the world and forged very important relationships with key international partners in the world market of titanium.
  • Our technological strengths guarantee high-level material provision for tightly fulfilling the needs of your project. We also nurture robust company chains, research facilities, and subsidiaries to see that each order meets top-tier standards of production and delivery. Customer service is one of the cornerstones at DAXUN.
  • We provide clear communication, and detailed pricing that covers the whole process of production. Besides, we answer technical questions related to our products. When you work with us, you get nothing but high-quality raw materials supplied with great service and professional technical support.

설명 

  • DAXUN ALLOYS is a global supplier and manufacturer of metal titanium to the aerospace, oilfield, biomedical, military, and other critical industries in China. With an inventory of comprehensive titanium mill products, we are able to offer quick delivery requirements through an advanced mill capability.
  • At DAXUN, we have quality, customer outstanding service, and overall customer satisfaction. With a large stock of titanium ingots and billets, DAXUN produces Ti-6AL-4V plates, sheets, forged titanium plates, and 6-4 titanium plate forgings. Our product price is competitive, with no requirement for a factory minimum quantity, thus delivery times are faster than ordering directly from a factory.
  • Third-party inspection reports can also be provided, in which the key items such as mechanical properties and chemical composition are called out to ensure compliance with the material standards for both room temperature and high-temperature performance.
  • The added value services extended by DAXUN also include heat treatment, hole drilling, water jet cutting, ultrasonic inspection, and mechanical testing.

Properties of Grade 5 titanium alloy

       Titanium 6al-4v has a density of 4.43 g/cc.

  • 열 속성Melting Point: 1604 – 1660 °C Solidus: 1604 °C Liquidus: 1660 °C Beta Transus: 980 °C
  • 기계적 특성Tensile Strength, Ultimate: 1170 Mpa Tensile Strength, Yield: 1100 Mpa Elongation at Break: 10% Modulus of Elasticity: 114 Gpa
  • 경도Brinell: 334 Rockwell: C 363 Vickers: 36
  • 경도

    Brinell: 334
    Rockwell: C 363
    Vickers: 36

열처리

  • Ti 6Al 4V alloy titanium plate is commonly heat treated to increase its characteristics. Usually, rolling annealing, solution treatment, or aging treatment are widely used. Stress relief is utilized for shaping and welding pieces, whereas beta annealing is used to increase the strength of an alloy.

Excellent Corrosion resistance

  • The Ti 6Al 4V Plate quickly forms a ceramic oxide layer on its surface, safeguarding it against degradation in all but the toughest situations. Because of this, the Grade 5 Titanium Plate is extensively utilized in saltwater and humid conditions. It also has a modest tolerance to very acidic conditions, but titanium alloys incorporating palladium are superior.

Thermal processing

  • Ti 6Al 4V Plate is usually hot worked using a recrystallization process to obtain the proper microstructure. This allows the alloy’s yield strength and hardness to remain low while maintaining its ductility. In Grade 5, this process is performed at temperatures between 870°C and 980°C to prevent excessive alpha phase growth.

Cold Working

  • Ti 6AL 4V Titanium Plate is not easily cold-worked due to its low elastic modulus, which causes it to return to its original shape. Grade 5 can be cold drawn and extruded, but this is generally limited to small industrial processing facilities using commercially pure titanium grades.

Weldability of Ti-6Al-4V Titanium Alloy Plate

  • Ti 6Al-4V can be welded with filler metal. The metal must be shielded with an inert gas to avoid oxygen absorption in the weld area, which can cause embrittlement and failure. Gas tungsten arc welding is the most popular welding method for the alloy, but gas metal arc welding can be widely used to weld larger components.
  • Ti 6Al-4V can be successfully welded by plasma arc welding, spot welding, electron beam, laser beam, resistance welding, and diffusion welding.

Machinability of Ti-6Al4V Grade 5 Plate

  • Unlike other metals, the Ti6Al4V parts are easy to machine and can be used as standard parts. The following elements contribute to the efficient machining of Ti6Al4V parts: low cutting speeds, high feed rates, suitable cutting fluids, sharp tools, and a solid setup. Learn more on Daxun’s machining page.

Equivalent Grade

  • 6-4 Titanium
  • Ti 6-4
  • 6Al4V Titanium
  • Alpha Beta Titanium
  • Grade 5 Titanium
  • Ti-Grade 5
  • 6%Al-4%V Titanium
  • Titan Grade 5 (6Al-4V) EN Designation
  • TC4
  • Ti64
  • ASTM Grade 5
  • DIN 3.7165

Get in touch with your preferred grade 5 titanium plate supplier

  • Contact Daxun for the latest prices on Grade 2 Titanium Plates. It couldn’t be easier to buy the Titanium Plates you need, as well as all our other products, through our website. Alternatively, you can call our China sales team at +86 13382898899 to place your order and they will be happy to process your order. If you have any questions, you can even send an email to [email protected] and our team will get back to you as soon as possible. If you have any technical questions about Titanium Plates, you can also submit your details using the Contact Us form.
견적을 받거나 시장 정보를 최대한 빨리 파악하려면 어떻게 해야 하나요?

“문의하기” 페이지의 양식을 작성하거나 영업 관리자(+86 13382898899)에게 전화하시면 최대한 빨리 연락드리겠습니다. WhatsApp은 온라인 상태이며 이메일([email protected])은 6시간 이내에 확인합니다. 모든 문의나 메시지는 신속하게 답변해 드립니다. 또한 매주 고객과 시장 정보를 공유합니다.

샘플을 받을 수 있나요?

We can provide titanium sheet samples for you to check the quality. Sample is free and you just pay the freight.

이미 수출한 국가는 어디인가요?

캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.

MOQ는 얼마인가요?

티타늄 시트의 경우 MOQ는 1톤입니다.

배송 시간은 얼마나 걸리나요?

체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.

오늘 문의 보내기
빠른 견적