x
오늘 문의 보내기
빠른 견적

Daxun is an experienced carbon steel plate manufacturer

As a leading carbon steel plate supplier and exporter in China, Daxun supplies carbon steel plates to the world.
  • 제조: 냉연 판재, 열연 판재, 단조 판재
  • Standards: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Thickness: 0.8mm-60mm
  • Width: 1000mm-1200mm-1500mm-2000mm-2500mm etc.
  • Length: 2438mm-3048mm-6000mm-8000mm etc.
  • Origin: Baosteel, Shagang, Angang, Shandong Steel, Shougang etc.

A global leader in carbon steel plate fabrication services

Carbon steel plates are among the most widely used materials across a wide range of industries. Composed primarily of iron and carbon, these alloys are produced by rolling carbon steel ingots or continuously cast slabs to meet customers’ specific requirements for size or chemical composition.

Available in the “as rolled” or heat treated state, these plates are supplied in standard sizes or custom cut sizes to specific design profiles. High-grade carbon steel plates are integral components in numerous applications, including steel frame buildings, storage tanks, welded structures, freight containers, chimneys, bridges, heat exchangers, pipelines, cranes and a wide range of industrial machinery parts.

Daxun offers a comprehensive range of carbon steel plates and sheets, available in a variety of lengths, widths, thicknesses and diameters to suit varying project specifications. Our inventory includes products that meet ASTM standards, ensuring precise dimensions and weights (in kilograms) to meet stringent industry requirements.

The weight and thickness of a carbon steel plate are key factors in determining its suitability for a particular application, affecting aspects such as structural integrity and load-bearing capacity. By offering a wide range of options, Daxun ensures that customers are able to select the right material to achieve optimal performance in their respective projects.

데이터

AISI AISI 1020, 1045, 4130, 4140
ASTM/ASME (Structural Grades) A36, A572, A588 (CorTen), A656 , A709-36, (36W, 36WT, 36WF), A709-50, A709-HPS70W, A514 (grades B, S, F, H, Q), 100XF, A871
ASTM/ASME (Pressure Vessel Grades) A285-C, A387, A455, A516(N), A517, A612(N)
CSA G40.21 (Structural Grades) 38W-38WT/260W-260WT, 44W-44WT/300W-300WT, 50W-50WT/350W-350WT, 50A-50AT/350A-350AT, 60W-60WT/400W-400WT
ABRASIVE RESISTANT GRADES AR200, AR235, AR400F, AR450F, AR500
SHIPBUILDING AND OFFSHORE GRADES ABS, Lloyds, DNV, A131, API 2H Grade 50
EURONORM EN10025 (Available by special request) S235, S275, S355, S420, S460, S500, S690
MILITARY GRADES MIL-A-12560, MIL-A-46100, MIL-DTL-46177C
두께 3/16″ to 8″
Master Width 72″ to 154″

 

중국 America 일본 Germany England France ISO
GB ASTM JIS DIN, DINEN BS, BSEN NF, NFEN ISO 630
Q195 Cr.B SS330; SPHC; SPHD S185 040;A10;S185 S185
Q215A Cr.C; Cr.58 SS330; SPHC
Q235A Cr.D SS440; SM400A E235B
Q235B Cr.D SS440; SM400A S235JR; S235JRG1; S235JRG2 S235JR; S235JRG1; S235JRG2 S235JR; S235JRG1; S235JRG2 E235B
Q255A SS440; SM400A
Q275 SS490 E275A

Daxun을 선택하고 고객을 만족시키세요.

지금 Daxun에 문의

Stock Carbon Steel Plate Types

Low carbon steel plate
Medium carbon steel plate
High carbon steel plate
Structural steel plate
Wear-resistant steel plate
Pressure vessel plate
Armor and ship plate

지금 Daxun에 문의

Advanced machining

As one of the largest processors and distributors of carbon plate products in China, we offer a large supply of high-quality, competitively priced products through our network of metal service centers. We leverage our industry expertise, extensive experience and investment in innovative technologies to provide an unparalleled supply of carbon steel plate.

지금 Daxun에 문의

Advantages of Buying Carbon Steel Plates in China

High quality and innovation:
Cost effectiveness:
Diverse product range and customization:
Government support and policy stability:
Combined with these factors, China becomes a strong sourcing source for carbon steel plates, offering a balance of quality, price and reliability.

지금 Daxun에 문의

Please contact DAXUN experts when deciding on steel grade

Here are the international grades for carbon steel plates: ASTM Standards: A36, A283 (Grade A, B, C, D), A572 (Grade 42, 50, 55, 60, 65), A516 (Grade 55, 60, 65, 70), A1011 (CS Type A, B, C), A1008 (CS Type A, B, C); EN Standards: S235JR, S275JR, S355JR, S355J2, S460NL; JIS Standards: SS330, SS400, SS490, SPHC, SPHD, SPHE; GB/T Standards: Q195, Q235, Q275, Q345; Other International Grades: DIN 17100 (St37-2, St52-3), ISO 630 (Fe360A, Fe430B).

Carbon steel plate characteristics

높은 강도
내식성
내열성
저온 저항
환경 보호
용접 성능

Let your brand improve rapidly

Cold rolled sheet tolerances

크기 허용 오차 순위
그룹 1 그룹 2 그룹 3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
Hot rolled plate tolerance
크기 허용 오차 순위
그룹 1 그룹 2 그룹 3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
등급 유형 두께 Surface
오스테나이트 304/304H/304L/304J1 0.25-150mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0.4-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0.3-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
페라이트 430 0.4-3.0mm 2B/BA/NO.4/8K/SB/HL
울트라 퓨어 페라이트 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
등급 유형 두께 원본
내열성 강철 309S 0.5-40mm CHN
310S 0.5-40mm CHN
듀플렉스 스틸 2101 1.5-50mm CHN
2304 3.0-50mm CHN
2205 0.5-60mm CHN
2507 1.0-60mm 스웨덴/일본/중국
슈퍼 오스테나이트강 N08904 0.6-50mm 스웨덴/일본/중국
S31254 0.5-50mm 스웨덴/일본/중국
N08926 0.5-50mm 스웨덴/일본/중국
N08367 0.5-50mm 스웨덴/일본/중국
니켈 베이스 합금 N08031 1.0-50mm 미국/일본/독일
N08810/N08800 0.8-50mm 미국/일본/중국
N08028 1.0-20mm US / 독일 / 일본
N08020 1.0-20mm US / 독일 / 일본
N08825 0.8-40mm 미국 / 독일 / 스웨덴 / 일본 / 중국
N10276 0.5-50mm US / 독일 / 일본
N06022 1.0-50mm US / 독일 / 일본
N06625 0.8-20mm US / GER / CHN
N04400 1.0-20mm US / 독일 / 일본
N06600 1.0-50mm US / 독일 / 일본 / 중국
N02201 0.5-20mm 미국/일본
티타늄 TA1/Gr1 0.5-50mm 일본/중국
TA2/Gr2 0.5-50mm 일본/중국
용접 재료 ERNiCrMo-13 1.2, 2.4mm GER
ERNiCrMo-3 2.4mm GER
ERNiCrMo-4 2.4mm US

참조 및 다운로드 가능한 정보

Daxun 합금
Daxun provides all the carbon steel plate data required by customers

Daxun is a trustworthy steel plate manufacturer

As a carbon steel plate manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all carbon steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the carbon steel plates have less defects.

Q1: What is carbon steel?

A1: Carbon steel is a type of steel where the primary alloying element is carbon. It is commonly used in construction, automotive, and manufacturing industries due to its strength, durability, and versatility.

Q2: What are the different types of carbon steel plates?

A2: Carbon steel plates are generally classified into three types based on carbon content: low carbon steel (0.05% – 0.25% carbon), medium carbon steel (0.25% – 0.60% carbon), and high carbon steel (0.60% – 1.00% carbon).

Q3: What are the common grades of carbon steel plates?

A3: Common grades include ASTM A36, ASTM A572, ASTM A516, S235JR, S275JR, S355JR, and JIS SS400, among others.

Q4: What are the uses of carbon steel plates?

A4: Carbon steel plates are used in construction, shipbuilding, automotive manufacturing, machinery, pressure vessels, and structural components due to their strength and versatility.

Q5: What is the difference between low carbon and high carbon steel plates?

A5: Low carbon steel has higher ductility and is easier to weld and form, while high carbon steel has greater hardness and strength but is less ductile and more prone to cracking during welding.

Q6: Can carbon steel plates be welded?

A6: Yes, carbon steel plates can be welded, though the specific welding process and techniques may vary depending on the carbon content and plate thickness.

Q7: How do you prevent carbon steel plates from rusting?

A7: To prevent rusting, carbon steel plates should be properly coated with paint, oil, or other protective coatings. In some cases, galvanizing or applying corrosion-resistant alloys can also help protect the steel.

Q8: What are the advantages of using carbon steel plates?

A8: The main advantages include high strength, durability, low cost, and ease of fabrication. Carbon steel plates are also widely available and can be heat-treated to meet various requirements.

Q9: What are the disadvantages of carbon steel plates?

A9: The main disadvantages include susceptibility to corrosion, especially in harsh environments, and lower resistance to wear compared to other materials like stainless steel.

Q10: How do you select the right grade of carbon steel plate?

A10: Selection depends on factors such as the intended application, required strength, welding capability, environmental conditions, and cost considerations. It is important to choose the grade that meets both mechanical and chemical property requirements for the specific use case.

If you need more details or have other questions, please contact Daxun’s sales team and experts, we will serve you quickly!

오늘 문의 보내기
빠른 견적