Daxun 347-347H UNS S34700 stainless steel PIPE and TUBE China supplier
As a leading stainless steel supplier and exporter in China, Daxun supplies stainless steel barsRod (Round Bar)to all over the world.
- 등급: AISI 17-4PH-SUS630
- 제조: 열간 압연, 냉간 인발, 단조
- 표준 ASTM, ASME, GB, DIN, JIS, ISO
- 높은 강도
- 높은 경도
- 내마모성
- 열처리 가능
스테인리스 강관 및 튜브 제작 서비스 분야의 글로벌 리더
Global Leader in Stainless Steel Rod and Round Bar Fabrication
Daxun is a trusted global supplier and exporter of SS 17-4PH/630 round bars and rods. We produce high-quality products in a range of surface finishes, end treatments, dimensions, shapes, and sizes to suit your exact requirements.
Why Choose SS 17-4PH?
SS 17-4PH is a martensitic stainless steel that undergoes precipitation hardening for superior mechanical properties. Its alloying elements—nickel, copper, and chromium—contribute to excellent strength, corrosion resistance, and durability. Widely adopted in the aerospace industry, this alloy is ideal for fasteners and other structural components thanks to its refined microstructure, which is developed through a controlled remelting process.
Optimized Properties Through Heat Treatment
UNS S17400, the designation for 17-4PH, responds well to heat treatment and aging. These processes enhance its toughness and ductility, making it suitable for demanding applications. Compared to many high-nickel, non-ferrous alloys, 17-4PH provides a more cost-effective solution without sacrificing performance.
A Versatile Choice for Many Industries
Stainless steel 17-4PH round bars are popular in manufacturing and engineering due to their corrosion resistance, high strength, and ease of production. The “PH” stands for precipitation hardening, a treatment method that further improves the material’s mechanical properties. With its balanced combination of features and value, 17-4PH is an excellent choice for a wide range of industrial projects.
ur network of service centers stock stainless steel bar products for fast, ready supply of bar in common sizes and alloys.We also produce custom-sized stainless steel rods and can arrange inventory schedules for quick turnaround in a timely manner if quantities are below factory minimums.Daxun Alloys stocks stainless steel round bars with diameters ranging from 1/16″ to 26″. Round bars are available in nearly every grade of stainless steel, including 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205, and Alloy 20. Heat treated stainless steel round bars are offered in 17-4PH, H900 temper (on request), H1025, H1150, Double H1150, and H1150M. Other heat-treated tempers can be manufactured upon request. We stock the following 400 series stainless steels: 410, 430, and 416. We also carry 303, 304, and 316/L precision and bearing quality stainless steel round bars. The majority of our inventory consists of our unique machined bar grades: stainless steel round bars that are melted to consistent standards to increase machinability and lower total cost per component. Our stainless steel bar processing machinery allows Daxun Alloys to produce to our customers’ exact specifications.
It performs reliably in high temperature service conditions between 600°F and 800°F.
데이터
- 기술적 매개 변수
- 재료
- 기계적 특성
- 물리적 속성
- 동등한 등급
- 파이프 유형
| Stainless Steel 347 Tube Standards | ASTM A213, ASTM A249, ASTM A269, ASME SA213, ASME SA249, ASME SA269, EN 10216-5 TC1 / TC2, PED 97/23/EC, AD 2000, NACE MR0175/ISO 15156 |
| 347 SEAMLESS Stainless Steel Aerospace Tubing | AMS 5557, AMS 5897 (Canceled & non-current specs include MIL-T-8808, MIL-T-8973) |
| 347 WELDED & DRAWN Stainless Steel Aerospace Tubing | AMS 5556, AMS 5575 (Canceled & non-current specs include MIL-T-6737, MIL-T-8606, MIL-T-8808) |
| Stainless Steel 347 Seamless Tube Size | 1.2 mm OD To 630 mm OD |
| Stainless Steel 347 Welded Tube Size | 1.2 mm OD To 1219 mm OD |
| Swg & Bwg | 10 스와지, 12 스와지, 14 스와지, 16 스와지, 18 스와지, 20 스와지. |
| Stainless Steel 347 tubing wall thickness | 0.020″ -0.220″, (특수 벽 두께 사용 가능) |
| SS 347 tube Length | 싱글 랜덤, 더블 랜덤, 표준 및 컷 길이 |
| 347 Stainless Steel Tube Finish | 광택, AP(어닐링 및 절임), BA(브라이트 및 어닐링), MF |
| Stainless Steel 347 tube Form | Round, Coil, Square, Rectangular, Boiler, Hydraulic, Straight or ‘U’ bent Tubes, Hollow, LSAW Tubes Etc. |
| Stainless Steel 347 Tube Type | 심리스, ERW, EFW, 용접, 제작 |
| Electropolished | (EP) Electropolished for Ultra High Purity Systems |
| Non-Electropolished | (BA) Bright Annealed or (AP) Annealed & Pickled for High-Purity, (CFOS) Cleaned for Oxygen Grade Service or Corrosive Systems |
| I.D. Surface Finish Options | 5, 7 & 10 µin. Ra |
| JIS | 8A to 250A |
| 허용 오차 | In accordance with: ASTM: A269 & A632, JIS: G 3459 |
| 347 stainless steel tubing End | Plain End, Beveled End, Treaded, Ends are suitable for orbital welding |
| 마킹 | All 347 Stainless Steel tubes are marked as follows: Standard, Grade, OD, Thickness, Length, Heat No. (Or according to the customer’s request.) |
| 347 stainless steel tubing Application | 오일 튜브, 가스 튜브, 유체 튜브, 보일러 및 열교환기 |
| 부가 가치 서비스 | 필요한 크기 및 길이에 따라 드로잉 및 확장, 광택 (전기 및 상업용) 어닐링 및 절임 굽힘, 기계 가공 등. |
| 전문 분야 | Stainless Steel 347 Capillary Tube & Other Odd Size |
| Stainless Steel 347 Heat Exchanger & Condenser Tubes | |
| Stainless Steel 347 Hydraulic tubing with OD up to 50.8 mm (2.0 in.) are delivered in bright annealed condition | |
| Stainless Steel 347 hydraulic tube with OD larger than 50.8 mm are supplied in the annealed and pickled condition, Or in polished condition | |
| Marking & Traceability | Each Stainless Steel 347 Tubing is traceable to its producing mill and heat by an identification number etched within 24″ (610mm) of one end. |
| 347 stainless steel tubing Test Certificate | Manufacturer Test Certificate according to EN 10204 3.1 B |
| 정부 승인 연구소에서 발급한 실험실 테스트 인증서. | |
| 타사 검사 중 | |
| 347 stainless steel tubing Testing & Inspection | Visual inspection • Surface roughness measurement • Helium-leak testing • Scanning Electron Microscopy (SEM) • Auger Electron Microscopy (AES) • Election Spectroscopy for Chemical Analysis (ESCA or XPS) • Particle testing • Moisture testing |
| We can also cut, thread, and groove Stainless Steel 347 Tubes to meet your specifications | |
| Composition of 347/347H Pipe and Tubing | ||
| 등급 | 347 | 347H |
| 유엔 지정 | S34700 | S34709 |
| 탄소(C) 최대. | 0.08 | 0.04–0.10 |
| 망간(Mn) 최대. | 2 | 2 |
| 인(P) 최대. | 0.04 | 0.04 |
| 황(S) 최대. | 0.03 | 0.03 |
| 실리콘(Si) 최대. | 0.75 | 0.75 |
| 크롬(Cr) | 17.0–20.0 | 17.0–20.0 |
| 니켈(Ni) | 9.0–13.0 | 9.0–13.0 |
| 몰리브덴(Mo) | — | — |
| 질소(N) | — | — |
| 철(Fe) | Bal. | Bal. |
| 기타 요소 | Cb+Ta=10xC-1.0 | Cb+Ta=8xC-1.0 |
| Physical Properties of 347/347H Alloys in the Annealed Condition at -20°F to +100°F | ||||||||||||||
| 인장 강도 | 수율 강도 | |||||||||||||
| 합금 | 유엔 지정 | 사양. | psi | MPa | ksi | psi | MPa | ksi | Elongation in 2 inches (min.) % | 입자 크기 요구 사항. | Maximum Harndess | 탄성 계수(x106 psi) | 평균 열팽창 계수(IN./IN./°F x 10-6) | Thermal Conductivity (BTU-in/ft2-h-°F) |
| 347 | S34700 | — | 75,000 | 515 | — | 30,000 | 205 | — | 35 | — | — | 29 | 9.2 | — |
| 347H | S34709 | — | 75,000 | 515 | — | 30,000 | 205 | — | 35 | 7 or coarser | — | 29 | 9.2 | — |
| 등급 | Density (kg/m3) | Elastic Modulus (GPa) | Mean Coefficient of Thermal Expansion (m/m/0C) | Thermal Conductivity (W/m.K) | Specific Heat 0-1000C (J/kg.K) | Electrical Resistivity (n.m) | |||
| 0-1000C | 0-3150C | 0-5380C | at 1000C | at 5000C | |||||
| 347 | 8000 | 193 | 15.9 | 16.2 | 17 | 14.2 | 18.7 | 500 | 740 |
| 347H | 8000 | 193 | 15.9 | 16.2 | 17 | 14.2 | 18.7 | 500 | 740 |
| 등급 | 중국 | 유엔 아니요 | 올드 브리티시 | 유로노름 | Swedish SS | Japanese JIS | ||
| BS | En | 아니요 | 이름 | |||||
| 347 | 0Cr18Ni11Nb | S34700 | – | X6CrNiNb18-10 | 1.455 | – | – | – |
| 347H | 07Cr18Ni11Nb | S34709 | – | – | 1.4961 | – | – | – |
| Stainless Steel ASTM A213 TP347H/347 Condenser Tube | Stainless Steel 347H/347 Welded Pipe |
| ASTM A269 TP347H/347 straight tube | 347H/347 Stainless Steel Welded Tube |
| ASTM A249 TP347H/347 Mirror Tube | Jis 347H/347 Stainless Steel Tubing |
| JIS SUS347H/347 Seamless Tubes | Din 1.4550 Stainless Steel Tube |
| Stainless Steel SA312 TP347H/347 Welded Tubes | Stainless Steel AISI 347H/347 Seamless Tube |
| ASTM A312 TP347H/347 Coiled Tubing | Stainless Steel Inox 347H/347 Capillary Tubing |
| ASTM A312 gr TP 347H/347 Aerospace tubes | ASTM A632 TP347H/347 Electric Fusion Welding Pipes |
| Stainless Steel 347H/347 Grade Pipe | Type 347H/347 Stainless Steel Polished Pipes |
| ASTM A312 TP347H/347 Elliptical Tubes | ASTM A213 SS TP 347H/347 Stainless Steel Rectangular Tube |
| 347H/347 Stainless Steel Oval Tubing | SS 347H/347 Needle Tube |
| Din 1.4550 Stainless Steel Welded Pipes | ASTM A358 TP347H/347 Coil Tubing Heat Exchanger |
| SAE J405 Uns S347H/34700 Thin Wall Tubing | 347H/347 Stainless Steel Metric Tubing |
| 347H/347 Stainless Steel Seamless Square Tubing | Large Diameter 347H/347 Stainless Steel Tube |
| SS 347H/347 Erw Pipe | 347H/347 Stainless Steel Instrumentation Tubing |
| High-pressure 347H/347 Stainless Steel Water Pipe | Stainless Steel 347H/347 Hexagonal Pipe |
| Din W.-Nr. 1.4550 Aisi 347H/347 Corrugated Tube | Stainless Steel 347H/347 Round Tube |
| UNS S347H/34700 Seamless Pipes | Stainless Steel 347H/347 Seamless Round Tubing |
| ASTM A358 TP347H/347 Polished Tubing | 347H/347 Stainless Steel Ornamental Tube |
| Stainless Steel ASTM A312 TP347H/347 erw | 347H/347 Stainless Steel Spiral Pipe |
| ASME SA213 TP347H/347 Perforated Tube | Din 1.4550 Material Tube |
| Stainless Steel SA 688 TP347H/347 Finned Tube | SA312 TP347H/347 Dom Tube |
| Din 1.4550 AISI 347H/347 Perforated Exhaust Tube | Stainless Steel 347H/347 Hypodermic Tubing |
| Material 1.4550 Aisi 347H/347 Slotted Handrail Tube | SA312 TP347H/347 Thin Wall Tube |
| SA213 TP 347H/347 Thick Wall Tube | En 1.4550 / Aisi 347H/347 Hydraulic Tubing |
| Stainless Steel 347H/347 Ornamental Pipe | Stainless Steel 347H/347 Fin Tube / Finned Tube |
| S347H/34700 Stainless Steel U Shaped Tube | 347H/347 Stainless Steel Square Tube Mirror Finish |
| Din 1.4550 Material Seamless Tubing | Stainless Steel WERKSTOFF NR. 1.4550 Coaxial Tube |
| 347H/347 Stainless Steel Rectangular Pipe | 347H/347 Stainless Steel Hypodermic Tubing for Medical Needle |
| 1.4550 Instrument Tubing | 347H/347 Stainless Steel Square Tubing |
| Ultra-High Purity Electropolished Stainless Steel 347H/347 Tube | Thin Wall S347H/34700 Stainless Steel Pipe |
| 347H/347 Stainless Steel ERW Pipes | Corrugated 347H/347 Stainless Steel Tube (CSST) for Gas |
| Jis 347H/347 Stainless Steel Coil Tubing | Stainless Steel 347H/347 Seamless Pipe |
| Schedule 10 Type 347H/347 Stainless Steel Pipe | Schedule 40 Type 347H/347 Stainless Steel Pipe |
| SA 312 TP347H/347 Seamless Tubing | Polished 347H/347 Stainless Steel Tubing |
| 347H/347 Stainless Steel Threaded Pipe | SAE 347H/347 Stainless Steel Rectangular Tube |
| Stainless Steel 347H/347 EFW Pipe | SS 347H/347 Electropolish Pipe |
| Stainless Steel 347H/347 Pipe | SS UNS S347H/34700 Heat exchager Pipe |
| DIN 1.4550 SS 347H/347 Pipe | Stainless Steel WERKSTOFF NR. 1.4550 Pipe |
| Stainless Steel UNS S347H/34700 Welded Pipe | ASTM A249 TP 347H/347 Stainless Steel High Pressure Pipe |
| ASTM A312 TP 347H/347 SS Seamless Pipe | Stainless Steel WERKSTOFF NR.1.4550 |
| 347H/347 SS Electropolished Pipe | SS UNS S347H/34700 Heat exchager Pipe |
| Stainless Steel 347H/347 Seamless Pipe | 347H/347 SS Decorative Pipe |
| SS 347H/347 Pipe | ASTM A249 TP 347H/347 Stainless Steel High Pressure Pipe |
| Stainless Steel 347H/347 Round Pipe | SS 347H/347 Cold Rolled Coiled Tubing |
| Austenitic Stainless Steel 347H/347 Pipe | SS 347H/347 Polish Pipe |
| ASTM A312 Stainless Steel Pipe | Stainless Steel 347H/347 Instrumentation Pipe |
| WERKSTOFF NR. 1.4550 SS 347H/347 Pipe | Stainless Steel 347H/347 Bright Annealed Pipe |
| 347H/347 Stainless Steel Seamless Pipe | TP347H/347 SS Welded Pipe |
| Stainless Steel 347H/347 Seamless Pipe | Stainless Steel 347H/347 Seamless Pipe |
| Stainless Steel GOST 08Ch18N12B Pipe | SS 347H/347 Santiary Pipe |
| WERKSTOFF NR.1.4449 SS 347H/347 Pipe | Stainless Steel 347H/347 Pipe |
| SS 347H/347 Welded Pipe | Stainless Steel 347H/347 Welded tubing |
| Stainless Steel 347H/347 Welded Pipe | SS TP347H/347 Seamless Tubing |
| SS TP347H/347 Seamless Pipe | 347H/347 Stainless Steel Seamless Pipe |
| 347H/347 SS Hollow Pipe | SCH40 347H/347 Stainless Steel pipe |
| TP347H/347 SS Welded Pipe | 347H/347 Stainless Steel erw Pipe |
| ASTM A213 Stainless Steel Tubing | 347H/347 Seamless Stainless Steel Pipe |
| Stainless Steel 347H/347 Electropolish Pipe | 347H/347 Stainless Steel erw Pipe |
| 347H/347 Stainless Steel Seamless Pipe | SS 347H/347 Cold Rolled Coiled Tubing |
| Stainless Steel WERKSTOFF NR. 1.4550 Pipe | ASTM A249 TP 347H/347 SS Seamless Pipe |
| TP 347H/347 SS ERW Pipe | SS 347H/347 Pipe |
| Stainless Steel 347H/347 Pipe | Stainless Steel UNS S347H/34700 Square Pipe |
| ASTM A312 TP347H/347 Stainless Steel Pipe | SS DIN 1.4550 Rectangular Welded Pipe |
Daxun을 선택하고 고객을 만족시키세요.

- Higher creep stress and rupture performance
- Excellent for high temperature service
- Can be used in ASME boilers and pressure vessels
- The material has better overall corrosion resistance
- Excellent mechanical properties
- High carbon version (347H) has good high temperature creep performance
- Used for heavy welding equipment where annealing is not possible
- 우수한 내산화성
- Prevents harmful carbide precipitation in the heat affected zone (HAZ) of the weld area
- Imparts substantial immunity to intergranular corrosion
- Reduces embrittlement in the heat affected zone of the weld are
—347 Stainless Steel pipe and tube
닥순의 장점
- 종류: 300 시리즈, 400 시리즈, 600 시리즈 등 다양한 크기와 등급을 제공합니다.
- 유연성: 열간 압연 또는 냉간 압연 바가 필요하든, 당사의 스테인리스 스틸 바 길이는 특정 프로젝트 요구 사항을 충족하도록 설계되었습니다.
- 품질 표준: 17-4 스테인리스 스틸 막대는 엄격한 ASTM, ISO9001, GB, NSF/ANSI 표준을 충족하여 신뢰성과 성능을 보장합니다.
- 맞춤 주문: 특별한 사이즈의 스테인리스 스틸 바를 찾고 계신가요? 경쟁력 있는 가격과 편리한 온라인 주문으로 다양한 스테인리스 스틸 바 맞춤 제작 옵션을 제공합니다.


17-4 스테인리스 스틸 로드 포장
우리는 품질을 보장하기 위해 모든 공정에주의를 기울이고 있으며, 일반적으로 채택하는 17-4 원형 강철 포장은 스테인리스 스틸 원형 막대를 친환경 비닐 봉지로 포장 한 다음 훈증없는 목재 상자 또는 목재 팔레트에 넣는 것입니다. OEM과 같은 맞춤형 포장도 협상할 수 있습니다. 로즈 플라스틱은 고객의 원형 바 포장 요구 사항을 충족하기 위해 거의 모든 것을 제공합니다. 우리는 포장을 매우 중요하게 생각합니다. 원형 바는 나무 골판지 상자에 포장하고 외부는 플라스틱 포장과 버블 필름으로 감쌉니다.
품질, 배송, 검사
- Daxun은 또한 여러 가지 품질 보증 테스트를 수행합니다. 이러한 테스트에는 평탄화 테스트, 피팅 및 저항 테스트, 기계적 테스트, 경도 테스트, 재료 양성 식별, 팽창 테스트 등이 포함됩니다. 이러한 모든 테스트를 통해 재료가 필요한 용도에 적합한지 확인합니다.
- During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days. Our delivery time is strictly in accordance with the contract.
- 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
- 고객에게 테스트용 무료 샘플 지원
- 현장 또는 비디오 공장 검사 지원


기술 지원
-
추가 기술 지원이 필요한 경우 금속 전문가와 지식이 풍부한 직원이 기꺼이 도와드릴 것입니다. 또한 Daxun은 다중 금속 및 플라스틱 재고 업계 최초로 인증된 테스트 실험실을 보유하고 있습니다. 이는 품질에 대한 변함없는 헌신과 풀서비스 공급업체로서의 철학을 보여주는 것이라고 생각합니다.
기술 지원
17-4 stainless steel rod The purchase order shall include quantity, PSL grade, type or category, API5L reference, diameter, finish, length and any applicable attachments or additional requirements relating to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish or end finish. Bars are solution bright annealed.

347-347H UNS S34700 Stainless Steel pipe and tube Features
Daxun 합금으로 브랜드를 빠르게 향상 시키십시오.
- 갤러리
- 347-347H UNS S34700 STEEL PIPE DATA TUBE
- 압력 등급
- 크기
- 표면 마감
| NPS | 외경 | 벽 두께 | 무게 | 무게 | |||
| in | mm | in | mm | Sched | kg/Mtr | 파운드/피트 | |
| 1/2″ | 0.84 | 21 | 0.109 | 2.769 | 40 STD | 1.268 | 0.851 |
| 0.147 | 3.734 | 80 STD | 1.621 | 1.088 | |||
| 3/4″ | 1.05 | 27 | 0.113 | 2.87 | 40 STD | 1.684 | 1.131 |
| 0.154 | 3.912 | 80 STD | 2.195 | 1.474 | |||
| 1″ | 1.315 | 33 | 0.133 | 3.378 | 40 STD | 2.501 | 1.679 |
| 0.179 | 4.547 | 80 STD | 3.325 | 2.172 | |||
| 1 1/4″ | 1.66 | 42 | 0.14 | 3.556 | 40 STD | 3.385 | 2.273 |
| 0.191 | 4.851 | 80 STD | 4.464 | 2.997 | |||
| 1 1/2″ | 1.9 | 48 | 0.145 | 3.683 | 40 STD | 4.048 | 2.718 |
| 0.2 | 5.08 | 80 STD | 5.409 | 3.361 | |||
| 2″ | 2.375 | 60 | 0.154 | 3.912 | 40 STD | 5.441 | 3.653 |
| 0.218 | 5.537 | 80 STD | 7.48 | 5.022 | |||
| 2 1/2″ | 2.875 | 73 | 0.203 | 5.516 | 40 STD | 8.629 | 5.793 |
| 0.276 | 7.01 | 80 STD | 11.411 | 7.661 | |||
| 3″ | 3.5 | 89 | 0.216 | 5.486 | 40 STD | 11.284 | 7.576 |
| 0.3 | 7.62 | 80 STD | 15.272 | 10.253 | |||
| 4″ | 4.5 | 114 | 0.237 | 6.02 | 16.073 | 10.79 | |
| 0.337 | 8.56 | 22.318 | 14.983 | ||||
| 6″ | 6.625 | 168 | 0.188 | 4.775 | 19.252 | 12.924 | |
| 0.203 | 5.516 | 20.739 | 13.923 | ||||
| 0.219 | 5.563 | 22.318 | 14.983 | ||||
| 0.25 | 6.35 | 25.354 | 17.021 | ||||
| 0.28 | 7.112 | 40 STD | 58.263 | 18.974 | |||
| 0.312 | 7.925 | 31.334 | 21.036 | ||||
| 0.375 | 9.525 | 37.285 | 25.031 | ||||
| 0.432 | 10.973 | 80 XHY | 42.561 | 28.573 | |||
| 0.5 | 12.7 | 48.719 | 32.708 | ||||
| 8″ | 8.625 | 219 | 0.188 | 4.775 | 25.233 | 16.94 | |
| 0.203 | 5.156 | 27.198 | 18.259 | ||||
| 0.219 | 5.563 | 29.286 | 19.661 | ||||
| 0.25 | 6.35 | 20 | 33.308 | 22.361 | |||
| 0.277 | 7.036 | 30 | 36.786 | 24.696 | |||
| 0.322 | 8.179 | 40 | 42.352 | 28.554 | |||
| 0.375 | 9.525 | 49.216 | 33.041 | ||||
| 0.406 | 10.312 | 60 | 53.085 | 35.638 | |||
| 0.5 | 12.7 | 80 XHY | 64.627 | 43.388 | |||
| 10″ | 10.75 | 273 | 0.188 | 4.775 | 31.588 | 21.207 | |
| 0.219 | 5.563 | 36.689 | 24.631 | ||||
| 0.25 | 6.35 | 20 | 41.759 | 28.035 | |||
| 0.307 | 7.798 | 30 | 51.002 | 34.24 | |||
| 0.344 | 8.738 | 56.946 | 38.231 | ||||
| 0.365 | 9.271 | 40 STD | 63.301 | 40.483 | |||
| 0.438 | 11.125 | 71.852 | 48.238 | ||||
| 0.5 | 12.7 | 60 XHY | 81.53 | 54.735 | |||
| 0.594 | 15.088 | 80 | 95.969 | 64.429 | |||
| 12″ | 12.75 | 324 | 0.188 | 4.775 | 37.57 | 25.222 | |
| 0.219 | 5.563 | 43.657 | 29.309 | ||||
| 0.25 | 6.35 | 49.713 | 33.375 | ||||
| 0.281 | 7.137 | 55.739 | 37.42 | ||||
| 0.312 | 7.925 | 61.735 | 41.445 | ||||
| 0.375 | 9.525 | 73.824 | 49.562 | ||||
| 0.406 | 10.312 | 79.727 | 53.525 | ||||
| 0.5 | 12.7 | 97.438 | 65.415 | ||||
| 0.562 | 14.275 | 108.966 | 73.154 | ||||
| 14″ | 14 | 356 | 0.188 | 4.775 | 41.308 | 27.732 | |
| 0.219 | 5.563 | 48.012 | 32.233 | ||||
| 0.25 | 6.35 | 20 | 54.685 | 36.713 | |||
| 0.281 | 7.137 | 61.327 | 41.172 | ||||
| 0.312 | 7.925 | 67.939 | 45.611 | ||||
| 0.375 | 9.525 | STD | 81.281 | 54.568 | |||
| 0.438 | 11.125 | 40 | 94.498 | 63.441 | |||
| 0.5 | 12.7 | XHY | 107.381 | 72.09 | |||
| 0.625 | 15.875 | 132.983 | 89.278 | ||||
| 16” | 16 | 406 | 0.188 | 4.775 | 47.29 | 21.748 | |
| 0.219 | 5.563 | 54.98 | 36.91 | ||||
| 0.25 | 6.35 | 10 | 62.639 | 42.053 | |||
| 0.281 | 7.137 | 70.268 | 47.174 | ||||
| 0.312 | 7.925 | 20 | 77.866 | 52.275 | |||
| 0.344 | 8.738 | 85.677 | 57.519 | ||||
| 0.375 | 9.525 | 30 | 93.213 | 62.578 | |||
| STD | |||||||
| 0.438 | 11.125 | 108.433 | 72.797 | ||||
| 0.5 | 12.7 | 40 | 123.289 | 82.77 | |||
| XHY | |||||||
| 18″ | 18 | 457 | 0.219 | 5.563 | 61.948 | 41.588 | |
| 0.25 | 6.35 | 70.593 | 47.393 | ||||
| 0.281 | 7.137 | 79.208 | 53.176 | ||||
| 0.312 | 7.925 | 20 | 87.792 | 58.939 | |||
| 0.375 | 9.525 | STD | 105.144 | 70.588 | |||
| 0.438 | 11.125 | 30 | 122.369 | 82.152 | |||
| 0.5 | 12.7 | XHY | 139.198 | 93.45 | |||
| 0.562 | 14.275 | 40 | 155.904 | 104.666 | |||
| 0.625 | 15.875 | 172.754 | 115.978 | ||||
| 20″ | 20 | 508 | 0.25 | 6.35 | 78.547 | 52.733 | |
| 0.282 | 7.163 | 88.458 | 59.386 | ||||
| 0.312 | 7.925 | 97.719 | 65.604 | ||||
| 0.375 | 9.525 | 20 STD | 117.075 | 78.598 | |||
| 0.438 | 11.125 | 136.305 | 91.508 | ||||
| 0.5 | 12.7 | 30 XHY | 155.106 | 104.13 | |||
| 0.594 | 15.088 | 40 | 183.378 | 123.11 | |||
| 0.625 | 15.875 | 192.64 | 129.328 | ||||
| 0.688 | 17.475 | 211.368 | 141.901 | ||||
| 24″ | 24 | 610 | 0.25 | 6.35 | 94.456 | 63.413 | |
| 0.281 | 7.137 | 106.029 | 71.183 | ||||
| 0.312 | 7.925 | 117.573 | 18.932 | ||||
| 0.375 | 9.525 | 20 STD | 140.938 | 64.618 | |||
| 0.438 | 11.125 | 164.176 | 110.219 | ||||
| 0.5 | 12.7 | XHY | 186.923 | 125.49 | |||
| 0.625 | 15.875 | 232.41 | 156.028 | ||||
| 0.688 | 17.475 | 40 | 255.148 | 171.293 | |||
| 0.75 | 19.05 | 277.401 | 186.233 | ||||
| 30″ | 30 | 762 | 0.25 | 6.35 | 118.318 | 79.433 | |
| 0.281 | 7.137 | 132.851 | 89.189 | ||||
| 0.312 | 7.925 | 10 | 147.353 | 98.925 | |||
| 0.375 | 9.525 | STD | 176.731 | 118.648 | |||
| 0.438 | 11.125 | 205.983 | 138.286 | ||||
| 0.5 | 12.7 | 20 XHY | 234.647 | 157.53 | |||
| 0.625 | 15.875 | 30 | 292.066 | 196.078 | |||
| 0.688 | 17.475 | 320.817 | 215.38 | ||||
| 0.75 | 19.05 | 348.988 | 234.293 | ||||
| 36″ | 36 | 914 | 0.25 | 6.35 | 142.18 | 95.453 | |
| 0.281 | 7.137 | 159.672 | 107.196 | ||||
| 0.312 | 7.925 | 10 | 177.133 | 118.918 | |||
| 0.375 | 9.525 | STD | 215.525 | 142.678 | |||
| 0.438 | 11.125 | 247.79 | 166.353 | ||||
| 0.5 | 12.7 | 20 XHY | 282.372 | 198.57 | |||
| 0.625 | 15.875 | 351.723 | 236.128 | ||||
| 0.688 | 17.475 | 386.487 | 259.467 | ||||
| 0.75 | 19.05 | 420.576 | 282.353 | ||||
| 42″ | 42 | 1067 | 0.312 | 7.925 | 206.914 | 138.911 | |
| 0.375 | 9.525 | STD | 248.319 | 166.708 | |||
| 0.5 | 12.7 | XHY | 33.097 | 221.61 | |||
| 0.75 | 19.05 | 492.163 | 330.413 | ||||
| 48″ | 48 | 1219 | 0.375 | 9.525 | STD | 284.112 | 190.738 |
| 0.438 | 11.125 | 331.404 | 222.487 | ||||
| 0.5 | 12.7 | XHY | 377.822 | 253.65 | |||
| 0.75 | 19.05 | 563.75 | 378.473 | ||||
| 0.875 | 22.225 | 655.969 | 440.383 | ||||
| ASTM A312 SS TP347 이음매 없는 파이프 압력 등급 | ||||||||||
| SS 파이프 압력 등급(psig) | ||||||||||
| SS 파이프 크기(인치) | SS 파이프 일정 | 온도(F) | ||||||||
| 100 | 200 | 300 | 400 | 500 | 600 | 650 | 700 | 750 | ||
| 1″ | 40 | 3048 | 2629 | 2362 | 2171 | 2019 | 1924 | 1867 | 1824 | 1810 |
| 80 | 4213 | 3634 | 3265 | 3002 | 2791 | 2659 | 2580 | 2528 | 2501 | |
| 160 | 6140 | 5296 | 4759 | 4375 | 4068 | 3876 | 3761 | 3684 | 3646 | |
| 1 1/2″ | 40 | 2257 | 1947 | 1750 | 1608 | 1496 | 1425 | 1383 | 1354 | 1340 |
| 80 | 3182 | 2744 | 2466 | 2267 | 2108 | 2009 | 1949 | 1909 | 1889 | |
| 160 | 4619 | 3984 | 3580 | 3291 | 3060 | 2916 | 2829 | 2772 | 2743 | |
| 2″ | 40 | 1902 | 1640 | 1474 | 1355 | 1260 | 1201 | 1165 | 1141 | 1129 |
| 80 | 2747 | 2369 | 2129 | 1957 | 1820 | 1734 | 1682 | 1648 | 1631 | |
| 160 | 4499 | 3880 | 3486 | 3205 | 2980 | 2840 | 2755 | 2699 | 2671 | |
| 3″ | 40 | 1806 | 1558 | 1400 | 1287 | 1196 | 1140 | 1106 | 1084 | 1072 |
| 80 | 2553 | 2202 | 1979 | 1819 | 1691 | 1612 | 1564 | 1532 | 1516 | |
| 160 | 3840 | 3312 | 2976 | 2736 | 2544 | 2424 | 2352 | 2304 | 2280 | |
| 4″ | 40 | 1531 | 1321 | 1187 | 1091 | 1014 | 967 | 938 | 919 | 909 |
| 80 | 2213 | 1909 | 1715 | 1577 | 1466 | 1397 | 1355 | 1328 | 1314 | |
| 160 | 3601 | 3106 | 2791 | 2566 | 2386 | 2273 | 2206 | 2161 | 2138 | |
| 5″ | 40 | 1342 | 1158 | 1040 | 956 | 889 | 847 | 822 | 805 | 797 |
| 80 | 1981 | 1709 | 1535 | 1411 | 1312 | 1250 | 1213 | 1189 | 1176 | |
| 160 | 3414 | 2945 | 2646 | 2433 | 2262 | 2155 | 2091 | 2049 | 2027 | |
| 6 | 40 | 1219 | 1052 | 945 | 869 | 808 | 770 | 747 | 732 | 724 |
| 80 | 1913 | 1650 | 1483 | 1363 | 1267 | 1208 | 1172 | 1148 | 1136 | |
| 160 | 3289 | 2836 | 2549 | 2343 | 2179 | 2076 | 2014 | 1973 | 1953 | |
| 8″ | 40 | 1073 | 926 | 832 | 765 | 711 | 678 | 657 | 644 | 637 |
| 80 | 1692 | 1459 | 1311 | 1205 | 1121 | 1068 | 1036 | 1015 | 1005 | |
| 160 | 3175 | 2738 | 2460 | 2262 | 2103 | 2004 | 1944 | 1905 | 1885 | |
| 10″ | 40 | 974 | 840 | 755 | 694 | 645 | 615 | 596 | 584 | 578 |
| 80 | 1609 | 1388 | 1247 | 1147 | 1066 | 1016 | 986 | 966 | 56 | |
| 160 | 3147 | 2714 | 2439 | 2242 | 2085 | 1986 | 1927 | 1880 | 1868 | |
| 1 psi(lb/in2) = 6,894.8 Pa(N/m2) = 6.895×10-2 bar | ||||||||||
| 참고: 최대 안전 작동 압력은 ASME B 31.3-2012, 304.1.2 단락(공식 3a)에 따라 계산됩니다. 계산은 최대 허용 O.D. 및 최소 허용 벽 두께(최악의 시나리오)를 가정합니다. |
||||||||||
| 재질: ASTM A269 및 A632에 따른 TP 304L 또는 TP 316L. | ||||||||||
| 온도 범위 = -20°F ~ +300°F, -28.8°C ~ 148.9°C | ||||||||||
| 유형 | 외경 | 크기 | 길이 |
| NB 사이즈(재고 있음) | .0035” ~ 20” | 1/8″, 1/4″, 3/8″, 1/2″, 5/8″, 3/4″, 1″, 1.25″, 1.5″, 2″, 2.5″, 3″, 4″, 5″, 6″ 등 | 길이에 맞게 자르기 |
| Stainless Steel 347-347H UNS S34700 Seamless Tube (Custom Sizes) | 6.35mm OD ~ 508mm OD | 요구 사항에 따라 | 길이에 맞게 자르기 |
| Stainless Steel 347-347H UNS S34700 Welded Tube (ERW Tube) (in Stock + Custom Sizes) | 6.35mm OD ~ 1219mm OD | 요구 사항에 따라 | 길이에 맞게 자르기 |
| 표면 마감 | 내부 표면(ID) | 외부 표면(OD) | |||
| 거칠기 평균(RA) | 거칠기 평균(RA) | ||||
| μ 인치 | μm | μ 인치 | μm | ||
| AP | 절임 & 절임 | 정의되지 않음 | 정의되지 않음 | 40 또는 정의되지 않음 | 1.0 또는 정의되지 않음 |
| BA | 베이트 어닐링 | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| MP | 기계식 광택 | 40,32,25,20 | 1.0,0.8,0.6,0.5 | 32 | 0.8 |
| EP | 일렉트로 폴리쉬 | 15,10,7,5 | 0.38,0.25,0.20;0.13 | 32 | 0.8 |
The surface and shape of 347-347H UNS S34700 stainless steel tube (6)
참조 및 다운로드 가능한 정보
Daxun은 신뢰할 수 있는 스테인리스 스틸 막대 및 바 제조업체입니다.
전문 제조업체로서 Daxun은 우리가 생산하는 모든 제품의 고품질을 보장합니다. 따라서 모든 스테인리스 막대가 ISO9001, SGS, CE, OQC 및 기타 국제 품질 표준의 인증을 받았으며 17-4 스테인리스 스틸로드의 결함이 적도록 엄격한 품질 관리를 실시하고 있습니다. Daxun에서는 모든 제품이 내구성, 고품질 및 고성능이므로 안심하십시오.
최근 인기 있는 사례 프로젝트 및 제품
관련 제품 (10)
품질을 확인하기 위해 17-4 스테인레스 스틸로드 샘플을 제공 할 수 있습니다. 샘플은 무료이며 운임만 지불하면 됩니다.
We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.
당사의 MOQ는 17-4 스테인리스 스틸 막대의 경우 1톤입니다.
체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.