321-321Hstainless steel bars and round bars China supplier
중국의 선도적인 스테인리스 스틸 공급업체이자 수출업체인 Daxun은 스테인리스 스틸 바를 공급합니다.로드(원형 막대)를 전 세계로 배송합니다.
- Good formability and weldability
- Service temperature up to 900°C
- Acid, alkali and low temperature resistance
- Excellent corrosion resistance
- High creep and stress rupture properties
- Grade: AISI 321-S32100
- 제조: 열간 압연, 냉간 인발, 단조
- 표준 ASTM, ASME, GB, DIN, JIS, ISO
For over 20 years, Daxun Alloys has been the premier supplier of heat resistant, high temperature 321 or 321H stainless steel bar. Contact Daxun to learn more about how 316 SS can best suit your specific application.
스테인리스 봉 및 원형 막대 제작 서비스 분야의 글로벌 리더
Daxun is an ASTM A276 Stainless Steel 321H Bar Exporter, SS 321 Forged Bar, SS 321 Square Bar, SS 321 Bright Bar, SS ASTM A276 321 Round Bar, SS 321H Stainless Steel Bar, ASTM A276 Stainless Steel 321H Hexagonal Bar Supplier, and China SS 321/321H Round Bar Manufacturer. SS 321 Round Bar, commonly known as UNS S32100, is a Titanium Stabilized Austenitic Stainless Steel with top-tier general corrosion resistance. Our SS 321 Rods are highly resistant to intergranular corrosion when exposed to chromium carbide precipitation temperatures ranging from 427 to 816°C. These SS 321 Round Bars, classified as WNR 1.4541, can be produced and treated to meet the 321 Stainless Steel Rod requirements of our customers. Our Stainless Steel 321 Welding Rods are also available in bespoke lengths and shapes, with market-leading costs.
당사의 서비스 센터 네트워크는 일반적인 크기와 합금의 바를 빠르고 준비된 공급을 위해 스테인리스 스틸 바 제품을 보유하고 있으며, 또한 맞춤형 크기의 스테인리스 스틸 막대를 생산하며 수량이 공장 최소 수량 미만인 경우 적시에 빠른 처리를 위해 재고 일정을 조정할 수 있으며, Daxun Alloys는 직경이 1/16 인치에서 26 인치 범위의 스테인리스 스틸 원형 바를 재고하고 있습니다. 원형 바는 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205 및 Alloy 20을 포함한 거의 모든 등급의 스테인리스 스틸로 제공됩니다. 열처리된 스테인리스 스틸 원형 바는 17-4PH, H900 템퍼(요청 시), H1025, H1150, Double H1150 및 H1150M으로 제공됩니다. 요청 시 다른 열처리된 템퍼도 제조할 수 있습니다. 410, 430, 416 등 400 시리즈 스테인리스 스틸을 보유하고 있습니다. 또한 303, 304, 316/L 정밀 및 베어링 품질의 스테인리스 스틸 원형 바도 보유하고 있습니다. 재고의 대부분은 가공성을 높이고 부품당 총 비용을 낮추기 위해 일관된 표준으로 용융된 스테인리스 스틸 원형 봉강인 당사의 고유한 가공 봉강 등급으로 구성되어 있습니다. 당사의 스테인리스 스틸 바 가공 기계를 통해 Daxun Alloys는 고객의 정확한 사양에 따라 생산할 수 있습니다.
데이터
- 매개변수
- 재료
- 기계적 특성
- 물리적 속성
- 모두 동일
- 유형
| 제품 매개변수: 스테인리스 스틸 로드 | |
| 사양 | ASTM A276, ASME SA276 / ASTM A479 ASME SA479 |
| 치수 | EN, DIN, JIS, ASTM, BS, ASME, AISI |
| SS 321/321H Round Bars | 4mm ~ 500mm 범위의 외경 |
| SS 321/321H Bright Bars | 4mm~100mm 범위의 외경 |
| SS 321/321H Hex Bars | 18mm - 57mm(11/16인치 ~ 2-3/4인치) |
| 완료 | 블랙, 밝은 광택, 러프 턴, NO.4 마감, 무광 마감, BA 마감 |
| 길이 | 1~6미터, 맞춤형 절단 길이 |
| 양식 | 원형, 정사각형, 육각(A/F), 직사각형, 빌렛, 잉곳, 단조 등. |
| Composition 321/321H | ||
| 등급 | 321 | 321H |
| 유엔 지정 | S32100 | S32109 |
| 탄소(C) 최대. | 0.08 | 0.04–0.10 |
| 망간(Mn) 최대. | 2 | 2 |
| 인(P) 최대. | 0.04 | 0.04 |
| 황(S) 최대. | 0.03 | 0.03 |
| 실리콘(Si) 최대. | 0.75 | 0.75 |
| 크롬(Cr) | 17.0–20.0 | 17.0–20.0 |
| 니켈(Ni) | 9.0–12.0 | 9.0–12.0 |
| 몰리브덴(Mo) | — | — |
| 질소(N) | 0.1 Max. | 0.1 Max. |
| 철(Fe) | Bal. | Bal. |
| 기타 요소 | Ti=5(C) to 0.70% | Ti=4(C) to 0.60% |
| 인장 강도 | 수율 강도 | |||||||||||||
| 합금 | 유엔 지정 | 사양. | psi | MPa | ksi | psi | MPa | ksi | Elongation in 2 inches (min.) % | 입자 크기 요구 사항. | Maximum Harndess | 탄성 계수(x106 psi) | 평균 열팽창 계수(IN./IN./°F x 10-6) | Thermal Conductivity (BTU-in/ft2-h-°F) |
| 321 | S32100 | — | 75,000 | 515 | — | 30,000 | 205 | — | 35 | — | — | 29 | 9.2 | — |
| 321H | S32109 | — | 75,000 | 515 | — | 30,000 | 205 | — | 35 | 7 or coarser | — | 29 | 9.2 | — |
| ade | Density (kg/m3) | Elastic Modulus (GPa) | Mean Coefficient of Thermal Expansion (m/m/0C) | Thermal Conductivity (W/m.K) | Specific Heat 0-1000C (J/kg.K) | Electrical Resistivity (n.m) | |||
| 0-1000C | 0-3150C | 0-5380C | at 1000C | at 5000C | |||||
| 321/321H | 8027 | 193 | 16.6 | 17.2 | 18.6 | 16.1 | 22.2 | 500 | 720 |
| rade | 유엔 아니요 | 올드 브리티시 | 유로노름 | Swedish SS | Japanese JIS | ||
| BS | En | 아니요 | 이름 | ||||
| 321 | S32100 | 321S31 | 58B, 58C | 1.4541 | X6CrNiTi18-10 | 2337 | SUS 321 |
| 321H | S32109 | 321S51 | – | 1.4878 | X10CrNiTi18-10 | – | SUS 321H |
| Stainless Steel 321/321H Bright Bar | SS 321/321H Bright Bar |
| 321/321H SS Bright Bar | |
| Stainless Steel 321/321H Bright Bar | |
| UNS S321/321H00 SS Bright Bar | |
| WERKSTOFF NR. 1.4541 Bright Bar | |
| ASTM A276 321/321H Stainless Steel Bright Bar | |
| Stainless Steel 321/321H Hex Bar | SS 321/321H Hex Bar |
| 321/321H SS Hexagonal Bar | |
| 321/321H Stainless Steel Hex Bar | |
| UNS S321/321H00 SS Hexagonal Bar | |
| ASTM A276 321/321H Stainless Steel Hex Bar | |
| Stainless Steel 321/321H Square Bar | SS 321/321H Square Bar |
| 321/321H SS Square Bars | |
| 321/321H Stainless Steel Square Bar | |
| UNS S321/321H00 SS Square Bar | |
| WERKSTOFF NR. 1.4541 Square Bar | |
| ASTM A479 321/321H Stainless Steel Square Bars | |
| Stainless Steel 321/321H Rectangular Bar | SS 321/321H Rectangular Bar |
| 321/321H SS Rectangular Bars | |
| 321/321H Stainless Steel Rectangular Bar | |
| UNS S321/321H00 SS Rectangular Bars | |
| WERKSTOFF NR. 1.4541 Rectangular Bar | |
| ASTM A276 321/321H Stainless Steel Rectangular Bar | |
| Stainless Steel 321/321H Flat Bars | SS 321/321H Flat Bar |
| 321/321H SS Flat Bars | |
| 321/321H Stainless Steel Flat Bars | |
| UNS S321/321H00 SS Flat Bars | |
| WERKSTOFF NR. 1.4541 Flat Bars | |
| ASTM A276 321/321H Stainless Steel Flat Bars | |
| Stainless Steel 321/321H Polished Bar | SS 321/321H Polished Bar |
| 321/321H SS Polished Bars | |
| 321/321H Stainless Steel Polished Bar | |
| UNS S321/321H00 SS Polished Bars | |
| WERKSTOFF NR. 1.4541 Polished Bar | |
| ASTM A476 321/321H Stainless Steel Polished Bar | |
| Stainless Steel 321/321H Threaded Bar | SS 321/321H Threaded Bar |
| 321/321H SS Threaded Bars | |
| 321/321H Stainless Steel Threaded Bar | |
| UNS S321/321H00 SS Threaded Bar | |
| WERKSTOFF NR. 1.4541 Threaded Bar | |
| ASTM A276 321/321H Stainless Steel Threaded Bar |
Daxun을 선택하고 고객을 만족시키세요.

빠른 응답
We provide timely and fast delivery of stainless steel rod products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
닥순의 장점
- 종류: 300 시리즈, 400 시리즈, 600 시리즈 등 다양한 크기와 등급을 제공합니다.
- 유연성: 열간 압연 또는 냉간 압연 바가 필요하든, 당사의 스테인리스 스틸 바 길이는 특정 프로젝트 요구 사항을 충족하도록 설계되었습니다.
- Quality Standards: 321 Stainless Steel Rod meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
- 맞춤 주문: 특별한 사이즈의 스테인리스 스틸 바를 찾고 계신가요? 경쟁력 있는 가격과 편리한 온라인 주문으로 다양한 스테인리스 스틸 바 맞춤 제작 옵션을 제공합니다.
321 Stainless Steel Rod packaging
We pay attention to every process to ensure quality. The packaging we usually use for stainless steel rods is to pack the stainless steel round rods in environmentally friendly plastic bags and then put them into fumigation-free wooden boxes or wooden pallets. Customized packaging, such as OEM, can also be negotiated. We provide almost everything to meet your round rod packaging requirements. We attach great importance to packaging. The round rods are packed in wooden corrugated boxes, wrapped with plastic packaging and bubble film on the outside.
품질, 배송, 검사
- Daxun은 또한 여러 가지 품질 보증 테스트를 수행합니다. 이러한 테스트에는 평탄화 테스트, 피팅 및 저항 테스트, 기계적 테스트, 경도 테스트, 재료 양성 식별, 팽창 테스트 등이 포함됩니다. 이러한 모든 테스트를 통해 재료가 필요한 용도에 적합한지 확인합니다.
- 생산 과정에서 제품의 직경, 두께, 표면을 측정합니다. 표준 배송 기간은 7~15일이며, 일부 특수 사이즈 제품을 제외하고는 배송 기간이 20일로 늘어납니다.
배송 시간은 엄격하게 계약에 따릅니다. - 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
- 고객에게 테스트용 무료 샘플 지원
- 현장 또는 비디오 공장 검사 지원
기술 지원
If you require any additional technical assistance with 321 stainless steel bar, our resident metallurgist and knowledgeable staff will be happy to assist you. In addition, Daxun has a certified testing laboratory – a first in the multi-metal and plastic stock industry. We believe this reflects our relentless pursuit of quality and our philosophy as a full-service supplier.
321 Stainless Steel Rod Ordering Information
Purchase orders for 321 stainless steel bars shall include quantity, PSL grade, type or category, API5L reference, diameter, surface finish, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish, or end treatment. Bars are solution bright annealed.
321-321H Stainless Steel Rod Features
Daxun 합금으로 브랜드를 빠르게 향상 시키십시오.
- 갤러리
- 배송 상태
- 나이 경화
| 배송 상태 선택 | 표면 상태 |
| Forged | 블랙 |
| 광택 | |
| 열간 압연 | 블랙 |
| 광택 | |
| 밝음 | |
| 피클 | |
| 콜드 드로잉 | 광택 |
| 밝음 | |
| 참고: | |
| 1. 위에 나열된 것과 다른 배송 상태가 필요한 경우 당사에 문의해 주시기 바랍니다. | |
| 2. 문의 또는 주문 시 여기에 표시되지 않은 추가 요구 사항이 있으면 친절하게 알려주시기 바랍니다. | |
| 용액 어닐링 상태의 재료는 다음과 같이 숙성될 수 있습니다.-*두 배 숙성을 나타냅니다. | ||||||||||||
| 조건 | H900(H480) | H925(H495) | H1025(H550) | H1075(H580) | H1100(H595) | H1150(H620) | H1150M(H620M)* | 플러스 | H1150D(H620D)* | 플러스 | ||
| 로 가열합니다. | ±15oF | 900oF | 925 oF | 1025oF | 1075oF | 1100oF | 1150oF | 1400oF | 1150oF | 1150oF | 1150oF | |
| ±9oC | 480oC | 495oC | 550oC | 580oC | 595oC | 620oC | 760oC | 620oC | 620oC | 620oC | ||
| 몇 시간 동안 보류 | 1 | 4 | 4 | 4 | 4 | 4 | 2 | 4 | 4 | 4 | ||
| 아래로 냉각 | Air | Air | Air | Air | Air | Air | Air | Air | Air | Air | ||
| 90oF(32oC) | ||||||||||||
Types of 321 Stainless Steel Rods (6)
참조 및 다운로드 가능한 정보
Daxun은 신뢰할 수 있는 스테인리스 스틸 막대 및 바 제조업체입니다.
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel rod are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 321 Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
최근 인기 있는 사례 프로젝트 및 제품
관련 제품 (11)
We can provide 321 Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.
캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.
Our MOQ is 1 ton for 321 Stainless Steel Rod.
체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.