Daxun is a 310S stainless steel sheet supplier from China
As China’s leading stainless steel plate supplier and exporter, Daxun provides 310S stainless steel plates to the world.
- Grade: AISI 310-310S-S31008
- 제조: 냉연 판재, 열연 판재, 단조 판재
- 표준 ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
- 유형: 냉간 압연 박판, 열간 압연 후판
- 표면: 2B, NO.1, NO.4, HL, BA, 8K 등.
- 길이: 2438mm3048mm6000mm 사용자 정의 가능
- 원산지: TISCO, 바오스틸, 포항, 칭산, 델롱
The global leader in stainless steel sheet fabrication services
S31008 (310S) Sheet and Plate, Austenitic stainless steel alloy 310S (UNS S31008) is designed for applications requiring high-temperature corrosion resistance. The alloy resists oxidation up to 2010°F (1100°C) with room temperature cycling. Alloy 310 can be used in moderate carburizing environments and is resistant to sulfidation due to its high chromium content and moderate nickel content. More severe carburizing environments in heat-treating equipment typically require a nickel alloy such as 330 (UNS N08330). Alloy 310S can be used in bonding, nitriding, mild oxidation, and thermal cycling processes; however, a reduced maximum service temperature is required. Alloy 310 can also be used in cryogenic applications because it has low magnetic permeability and remains strong down to -450°F (-268°C). When heated to 1202–1742, the alloy precipitates the sigma phase (650–950°C). Hardness is partially restored by solution annealing at 2012–2102°F (1100–1150°C). This alloy is also available as a low-carbon alloy, 310S (UNS S31008). It is easily fabricated. A high carbon modification, 310H (UNS S31009), is designed to improve creep resistance. In most cases, the grain size and carbon content of the plate can meet both 310S and 310H standards. Standard shop fabrication procedures can be used to easily weld and process alloy 310.
Stainless Steel 310S Plate has trace amounts of silicon, sulfur, phosphorus, manganese, and up to 24% chromium, 19% nickel, and up to 0.08% carbon. Heat resistance, corrosion resistance, strength, and even high-temperature oxidation resistance are just a few of the many benefits of this popular stainless steel alloy. It can be utilized in many different applications, including burners, oil burners, and evaporator pipes and tubes. Because of its affordability, it’s perfect for a range of applications requiring low-cost maintenance supplies.
Because of its exceptional resilience to high temperatures, the 310S stainless steel plate is a great option for a wide range of industries, including petrochemical and chemical production, food processing, power plants, dairy farms, sugar mills, breweries, and energy generation. 310S Stainless Steel Plate is capable of withstanding oxidizing environments up to 2100°F (1149°C) due to its high chromium concentration. Its ductility, toughness, and weldability are all excellent. Its exceptional low-temperature performance, even down to -20°F (-29°C), combined with its resistance to heat and corrosion make it the perfect material for cryogenic applications. In conclusion, it is an excellent option for high-temperature industrial applications due to its strong resistance to oxidation and ability to prevent scaling at temperatures as high as 2000°F (1093°C).
기술 데이터
- 매개변수
- 요소
- 기계적 특성
- 표준
| Product Parameters: 310(UNS S31008) Stainless Steel Sheet/Plate | |||
| 너비 | 10mm~2500mm | ||
| 두께 | 0.2mm~100mm | 두께 허용 오차 | +/-0.03mm |
| 표준 | ASTM/ASME 240/480, JIS 4305, DIN EN 10088-2 | ||
| Surface | 2B,BA,8K,NO.1,NO.4,NO.3,헤어라인,체크무늬,골드,블랙,로즈골드 등 | ||
| 사양 | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
| 밀 원산지 | TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu 등. | ||
| 인증 | ISO, SGS, BV, TUV, CE 등 | ||
| 요소 | % Present (in product form) | |
| C, H, P, L | TW* / TS* | |
| 탄소(C) | ≤0.10 | ≤0.15 |
| 실리콘(Si) | ≤1.50 | ≤0.75 |
| 망간(Mn) | ≤2.00 | ≤2.00 |
| Phosphorous (P) | ≤0.045 | ≤0.045 |
| Sulfur (S) | ≤0.015 | ≤0.030 |
| 크롬(Cr) | 24.00 – 26.00 | 24.00 – 26.00 |
| 니켈(Ni) | 19.00 – 22.00 | 19.00 – 22.00 |
| 질소(N) | ≤0.11 | - |
| 철(Fe) | 잔액 | 잔액 |
| Product Form | |||||
| C, H, P | L | TW* / TS* | |||
| Thickness a or diamter d (mm) | a ≤ 12 | d ≤ 25 | - | ||
| Hardness HB max. 1) 2) 3) | 192 | 192 | - | ||
| Proof Strength3) | Rp0.2 N/mm2 | 210 | 210 | 230 | |
| Rp1.0 N/mm2 | 230 | 230 | 270 | ||
| 인장 강도 | Rm N/mm2 | 500 – 700 | 500 – 700 | min. 500 | |
| Elongation min. in % | Long Products | 351) | 351) | 334) / 355) | |
| Flat Products | 0.5 ≤ a/d < 3 | 334)5) | 334)5) | 354)5)6) | |
| 3 ≤ a/d | 354)5) | 354)5) | 354)5)6) | ||
| 310 | 310S | 310H |
|---|---|---|
| UNS S31000 | UNS S31008 | UNS S31009 |
| ASTM A240 | ASTM A240 | ASTM A240 |
| ASTM A480 | ASTM A480 | ASTM A480 |
| ASME SA240 | ASME SA240 | ASME SA240 |
| AMS 5521 | AMS 5521 | AMS 5521 |
Daxun을 선택하고 고객을 만족시키세요.

빠른 배송
We provide timely and fast delivery of 310S stainless steel plate products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real-time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.
Benefits of Stainless Steel 310S Plates :
- Corrosion resistance: The main benefit of 310S stainless steel plates is their excellent corrosion resistance. They resist corrosion from a wide range of environments, including acidic and alkaline solutions, making them suitable for a wide range of applications.
- High-temperature strength: 310S stainless steel plates exhibit excellent strength at elevated temperatures. This property is critical in applications that are frequently exposed to high temperatures, ensuring structural integrity and performance in demanding conditions.
- Durability and lifespan: The durability of 310S stainless steel plates gives them a long service life, making them an affordable choice for many applications. The material is resistant to wear and tear, minimizing the need for frequent replacement.

Benefits of Stainless Steel 310S Plates :
310S/2520 Plate Features:
- High-temperature resistance
- Excellent oxidation resistance
- Improved creep/rupture properties
- Excellent corrosion resistance
- Not susceptible to thermal fatigue and cyclic heating
- Good strength at temperatures up to 2100°F
품질, 배송, 검사
- Daxun strictly controls product quality. Before placing an order, we will send you the product warranty, or if you need samples for testing, we can also send samples for free.
- During the production process, we carefully measure the diameter, thickness, and surface quality of each product to ensure it meets exacting standards. Our standard delivery time is typically 7 to 15 days. However, for special-sized products, the delivery time may be extended to 20 days to accommodate the additional customization and processing required.
배송 시간은 엄격하게 계약에 따릅니다. - 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
- 고객에게 테스트용 무료 샘플 지원
- 현장 또는 비디오 공장 검사 지원

애플리케이션
- Cryogenic Components: Designed to withstand extremely low temperatures, ensuring optimal performance in critical applications.
- Food Processing: Reliable materials and components tailored for hygienic and efficient food production systems.
- Furnaces: Durable solutions for burners, doors, fans, ducting, and liners, supporting high-temperature industrial processes.
- Fluidized Bed Furnaces: Robust components including coal burners, grates, ducting, and bellows for enhanced operational efficiency.
- Ore Processing and Steel Mills: High-performance equipment for smelting, steelmaking, and continuous casting operations.
- Petroleum Refining: Specialized systems such as catalytic recovery units, flares, heat exchangers, and tube hangers for maximum efficiency in refining processes.
- Power Generation: Precision-engineered components like gas furnace internals, pulverized coal burners, and tube hangers to support energy production.
- Sintering and Cement Plants: Reliable burners, burner hoods, feed and discharge systems, and bellows for seamless operation in harsh environments.
- Heat Treating: Advanced solutions, including annealing covers and boxes, burner grates, doors, fans, muffle furnaces, retorts, heat exchangers, and walking beams for consistent performance in thermal processing.
SS 310S Plate Surface Treatment
1D: The surface is matte with a discontinuous particle shape.
2D: 은빛 톤의 흰색.
2B: Silver gray with better gloss and flatness than the 2D surface.
Ba: 거울에 가까운 표면으로 광택과 반사율이 우수합니다.
3번: 광택이 좋고 표면이 거칠다.
4번: 표면에 잔주름이 있고 광택이 좋습니다.
HL: 은회색에 황금빛 머리카락.
8K: 거울 표면.
310 plate stainless steel Features
Daxun 브랜드가 빠르게 향상되도록 하세요
- 갤러리
- 허용 오차
- 배송 상태
- 기타 제품 시리즈
| 2B 시트 허용 오차 | |||
| 크기 | 허용 오차 순위 | ||
| 그룹 1 | 그룹 2 | 그룹 3 | |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 |
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 |
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 |
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 |
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 |
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 |
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 |
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 |
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 |
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 |
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 |
| No.1 열연 판재 공차 | |||
| 크기 | 허용 오차 순위 | ||
| 그룹 1 | 그룹 2 | 그룹 3 | |
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 |
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 |
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 |
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 |
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 |
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 |
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 |
| 16 | 15.2~ 15.5 | 15.5~ 15.7 | 15.7~ 16.1 |
| 18 | 17.2~ 17.5 | 17.5~ 17.7 | 17.7~ 18.1 |
| 20 | 19.2~ 19.5 | 19.5~ 19.7 | 19.7~ 20.1 |
| 30 | 29.2~ 29.5 | 29.5~ 29.7 | 29.7-30.1 |
| 40 | 39.2~ 39.5 | 39.5~ 39.7 | 39.7~ 40.1 |
| 50 | 49.2~ 49.5 | 49.5~ 49.7 | 49.7~ 50.1 |
| 60 | 59.2~ 59.5 | 59.5~ 59.7 | 59.7~ 60.1 |
| 배송 상태 선택 | 표면 상태 |
| 냉간 압연 | 2B |
| 2D | |
| BA | |
| 헤어라인 | |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| 참고: | |
| 1. 위에 나열된 것과 다른 배송 상태가 필요한 경우 당사에 문의해 주시기 바랍니다. | |
| 2. 문의 또는 주문 시 여기에 표시되지 않은 추가 요구 사항이 있으면 친절하게 알려주시기 바랍니다. | |
| 배송 상태 | |
| 배송 상태 선택 | 표면 상태 |
| 열간 압연 | No.1 |
| No.3 | |
| No.4 | |
| 6K | |
| 8K | |
| 피클 | |
| 참고: | |
| 1. 위에 나열된 것과 다른 배송 상태가 필요한 경우 당사에 문의해 주시기 바랍니다. | |
| 2. 문의 또는 주문 시 여기에 표시되지 않은 추가 요구 사항이 있으면 친절하게 알려주시기 바랍니다. | |
| 등급 | 유형 | 두께 | Surface |
| 오스테나이트 | 304/304H/304L/304J1 | 0.25-150mm | 2B/BA/NO.4/8K/SB/HL/NO.1 |
| 321 | 0.4-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 316/316L/317L/316Ti | 0.3-80mm | 2B/BA/NO.4/8K/SB/HL/NO.1 | |
| 페라이트 | 430 | 0.4-3.0mm | 2B/BA/NO.4/8K/SB/HL |
| 울트라 퓨어 페라이트 | 443 | 0.4-2.0mm | 2B |
| 436L/439/444/441 | 0.5-3.0mm | 2B、2D | |
| 409L | 0.4-2.5mm | 2B、2D | |
| 등급 | 유형 | 두께 | 원본 |
| 내열성 강철 | 309S | 0.5-40mm | CHN |
| 310S | 0.5-40mm | CHN | |
| 듀플렉스 스틸 | 2101 | 1.5-50mm | CHN |
| 2304 | 3.0-50mm | CHN | |
| 2205 | 0.5-60mm | CHN | |
| 2507 | 1.0-60mm | 스웨덴/일본/중국 | |
| 슈퍼 오스테나이트강 | N08904 | 0.6-50mm | 스웨덴/일본/중국 |
| S31254 | 0.5-50mm | 스웨덴/일본/중국 | |
| N08926 | 0.5-50mm | 스웨덴/일본/중국 | |
| N08367 | 0.5-50mm | 스웨덴/일본/중국 | |
| 니켈 베이스 합금 | N08031 | 1.0-50mm | 미국/일본/독일 |
| N08810/N08800 | 0.8-50mm | 미국/일본/중국 | |
| N08028 | 1.0-20mm | US / 독일 / 일본 | |
| N08020 | 1.0-20mm | US / 독일 / 일본 | |
| N08825 | 0.8-40mm | 미국 / 독일 / 스웨덴 / 일본 / 중국 | |
| N10276 | 0.5-50mm | US / 독일 / 일본 | |
| N06022 | 1.0-50mm | US / 독일 / 일본 | |
| N06625 | 0.8-20mm | US / GER / CHN | |
| N04400 | 1.0-20mm | US / 독일 / 일본 | |
| N06600 | 1.0-50mm | US / 독일 / 일본 / 중국 | |
| N02201 | 0.5-20mm | 미국/일본 | |
| 티타늄 | TA1/Gr1 | 0.5-50mm | 일본/중국 |
| TA2/Gr2 | 0.5-50mm | 일본/중국 | |
| 용접 재료 | ERNiCrMo-13 | 1.2, 2.4mm | GER |
| ERNiCrMo-3 | 2.4mm | GER | |
| ERNiCrMo-4 | 2.4mm | US |
The surface and shape of 310S stainless steel plate (7)
참조 및 다운로드 가능한 정보
Daxun은 신뢰할 수 있는 스테인리스 강판 제조업체입니다.
전문 제조업체로서 Daxun은 우리가 생산하는 모든 제품의 고품질을 보장합니다. 따라서 모든 스테인리스 강판은 ISO9001, SGS, CE, OQC 및 기타 국제 품질 표준 인증을 받았으며 스테인리스 강판의 결함이 적도록 엄격한 품질 관리를 실시하고 있습니다. Daxun에서는 모든 제품이 내구성, 고품질 및 고성능이므로 안심하십시오.
최근 인기 있는 사례 프로젝트 및 제품
관련 제품 (13)
품질을 확인할 수 있도록 스테인리스 강판 샘플을 제공할 수 있습니다. 샘플은 무료이며 운임만 지불하면 됩니다.
캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.
당사의 MOQ는 스테인리스 강판의 경우 1톤입니다.
체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.