x
오늘 문의 보내기
빠른 견적

310S-310-31008 stainless steel bars and round bars China supplier

중국의 선도적인 스테인리스 스틸 공급업체이자 수출업체인 Daxun은 스테인리스 스틸 바를 공급합니다.로드(원형 막대)를 전 세계로 배송합니다.
  • High temperature resistance
  • 높은 강도
  • 내식성
  • Reliability
  • Grade: 310S-2520
    제조: 열간 압연, 냉간 인발, 단조
    표준 ASTM, ASME, GB, DIN, JIS, ISO

For over 20 years, Daxun Alloys has been the premier supplier of heat resistant, high temperature 310 or 310S stainless steel bar. Contact Daxun to learn more about how 310S SS can best suit your specific application.

310S Global leader in stainless rod and Round Bar fabrication services

Daxun Alloys is a reputable manufacturer of high-quality SS 310 / 310S Round Bars with a variety of characteristics. Stainless Steel 310 / 310S Round Bars are austenitic stainless steel that is based on chromium and nickel. SS310/310S Round Bars/Rods have exceptional properties such as durability, flexibility, workability, machinability, weldability, ductility, fabricability, high strength, and hardness. These rods are mostly useful for industrial chemistry and nut manufacture. These rods are most likely the most popular on the market due to their anti-corrosion qualities. These rods and bars withstand extreme temperatures. These rods may be simply utilized at annealing temperatures without deforming the rod. We supply Stainless Steel Round Bars to our valued clients at market-leading costs. We can customize round bars in a variety of finishes, lengths, and shapes to meet our clients’ specific wants or specifications. We sell circular bars that may be conveniently used in industrial applications.

당사의 서비스 센터 네트워크는 일반적인 크기와 합금의 바를 빠르고 준비된 공급을 위해 스테인리스 스틸 바 제품을 보유하고 있으며, 또한 맞춤형 크기의 스테인리스 스틸 막대를 생산하며 수량이 공장 최소 수량 미만인 경우 적시에 빠른 처리를 위해 재고 일정을 조정할 수 있으며, Daxun Alloys는 직경이 1/16 인치에서 26 인치 범위의 스테인리스 스틸 원형 바를 재고하고 있습니다. 원형 바는 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205 및 Alloy 20을 포함한 거의 모든 등급의 스테인리스 스틸로 제공됩니다. 열처리된 스테인리스 스틸 원형 바는 17-4PH, H900 템퍼(요청 시), H1025, H1150, Double H1150 및 H1150M으로 제공됩니다. 요청 시 다른 열처리된 템퍼도 제조할 수 있습니다. 410, 430, 416 등 400 시리즈 스테인리스 스틸을 보유하고 있습니다. 또한 303, 304, 316/L 정밀 및 베어링 품질의 스테인리스 스틸 원형 바도 보유하고 있습니다. 재고의 대부분은 가공성을 높이고 부품당 총 비용을 낮추기 위해 일관된 표준으로 용융된 스테인리스 스틸 원형 봉강인 당사의 고유한 가공 봉강 등급으로 구성되어 있습니다. 당사의 스테인리스 스틸 바 가공 기계를 통해 Daxun Alloys는 고객의 정확한 사양에 따라 생산할 수 있습니다.

자세히 보기

데이터

제품 매개변수: 스테인리스 스틸 로드
사양 ASTM A276, ASME SA276 / ASTM A479 ASME SA479
치수 EN, DIN, JIS, ASTM, BS, ASME, AISI
SS 310/310S Round Bars 4mm ~ 500mm 범위의 외경
SS 310/310S Bright Bars 4mm~100mm 범위의 외경
SS 310/310S Hex Bars 18mm - 57mm(11/16인치 ~ 2-3/4인치)
완료 블랙, 밝은 광택, 러프 턴, NO.4 마감, 무광 마감, BA 마감
길이 1~6미터, 맞춤형 절단 길이
양식 원형, 정사각형, 육각(A/F), 직사각형, 빌렛, 잉곳, 단조 등.
등급 C Mn Si P S Cr Mo Ni Fe
SS 310 0.015 max 2.0 max 최대 0.15 0.020 max 0.015 max 24.00 – 26.00 0.10 max 19.00 – 21.00 54.7 min
SS 310S 0.08 max 2.0 max 1.00 max 0.045 max 0.030 max 24.00 – 26.00 0.75 max 19.00 – 21.00 53.095 min
밀도 녹는점 인장 강도 Yield Strength (0.2%Offset) 신장
7.9 g/cm3 1402 °C (2555 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 40%
속성 에서 가치 unit
밀도 8,000 kg/m³
Melting Range 1400 – 1450 °C
탄성 계수 20°C 200 GPa
전단 계수 20°C 77 GPa
푸아송 비율 20°C 0.3
열 전도성 100°C 14.2 W / m. °C
전기 저항 25°C 0.78 micro-ohm . m
Electrical Conductivity 25°C 1.25 % IACS
Specific Heat 500 J/kg. °C
Relative Magnetic Permeability 1.02
확장 계수 0 – 100°C 15.9 /°C
0 – 315°C 16.2 /°C
0 – 540°C 17 /°C
등급 중국 유엔 아니요 올드 브리티시 유로노름 Swedish SS Japanese JIS GOST
BS En 아니요 이름
310S 00Cr25Ni20 S31008 304S31 58E 1.4845 X5CrNi18-10 2332 SUS 310S 20Ch23N18
Stainless Steel 310/310S Bright Bar SS 310/310S Bright Bar
310/310S SS Bright Bar
Stainless Steel 310/310S Bright Bar
UNS S310/310S00 SS Bright Bar
WERKSTOFF NR. 1.4845 Bright Bar
ASTM A276 310/310S Stainless Steel Bright Bar
Stainless Steel 310/310S Hex Bar SS 310/310S Hex Bar
310/310S SS Hexagonal Bar
310/310S Stainless Steel Hex Bar
UNS S310/310S00 SS Hexagonal Bar
ASTM A276 310/310S Stainless Steel Hex Bar
Stainless Steel 310/310S Square Bar SS 310/310S Square Bar
310/310S SS Square Bars
310/310S Stainless Steel Square Bar
UNS S310/310S00 SS Square Bar
WERKSTOFF NR. 1.4845 Square Bar
ASTM A479 310/310S Stainless Steel Square Bars
Stainless Steel 310/310S Rectangular Bar SS 310/310S Rectangular Bar
310/310S SS Rectangular Bars
310/310S Stainless Steel Rectangular Bar
UNS S310/310S00 SS Rectangular Bars
WERKSTOFF NR. 1.4845 Rectangular Bar
ASTM A276 310/310S Stainless Steel Rectangular Bar
Stainless Steel 310/310S Flat Bars SS 310/310S Flat Bar
310/310S SS Flat Bars
310/310S Stainless Steel Flat Bars
UNS S310/310S00 SS Flat Bars
WERKSTOFF NR. 1.4845 Flat Bars
ASTM A276 310/310S Stainless Steel Flat Bars
Stainless Steel 310/310S Polished Bar SS 310/310S Polished Bar
310/310S SS Polished Bars
310/310S Stainless Steel Polished Bar
UNS S310/310S00 SS Polished Bars
WERKSTOFF NR. 1.4845 Polished Bar
ASTM A476 310/310S Stainless Steel Polished Bar
Stainless Steel 310/310S Threaded Bar SS 310/310S Threaded Bar
310/310S SS Threaded Bars
310/310S Stainless Steel Threaded Bar
UNS S310/310S00 SS Threaded Bar
WERKSTOFF NR. 1.4845 Threaded Bar
ASTM A276 310/310S Stainless Steel Threaded Bar

Daxun을 선택하고 고객을 만족시키세요.

지금 Daxun에 문의

Quick response-310S Stainless Steel Rod

We provide timely and fast delivery of stainless steel rod products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on time.

지금 Daxun에 문의

닥순의 장점

  • 종류: 300 시리즈, 400 시리즈, 600 시리즈 등 다양한 크기와 등급을 제공합니다.
  • 유연성: 열간 압연 또는 냉간 압연 바가 필요하든, 당사의 스테인리스 스틸 바 길이는 특정 프로젝트 요구 사항을 충족하도록 설계되었습니다.
  • Quality Standards: Our 310S Stainless Steel Rod meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
  • 맞춤 주문: 특별한 사이즈의 스테인리스 스틸 바를 찾고 계신가요? 경쟁력 있는 가격과 편리한 온라인 주문으로 다양한 스테인리스 스틸 바 맞춤 제작 옵션을 제공합니다.
지금 Daxun에 문의

310S Stainless Steel Rod packaging

We focus on every procedure to assure quality, the package we usually take is pack Stainless Steel Round Bar with environmental poly bags, and then in free fumigation wooden cases or wooden palte. Also can accept customized package such as OEM by negotiation. We offers just about everything to meet your  Round Bar pack requirements. Lot of emphasis is placed on the packing and packaging. The  Round Bar are packed in wooden corrugated boxes foiled in plastic wraps and bubble wraps.

지금 Daxun에 문의

품질, 배송, 검사

  • Daxun은 또한 여러 가지 품질 보증 테스트를 수행합니다. 이러한 테스트에는 평탄화 테스트, 피팅 및 저항 테스트, 기계적 테스트, 경도 테스트, 재료 양성 식별, 팽창 테스트 등이 포함됩니다. 이러한 모든 테스트를 통해 재료가 필요한 용도에 적합한지 확인합니다.
  • 생산 과정에서 제품의 직경, 두께, 표면을 측정합니다. 표준 배송 기간은 7~15일이며, 일부 특수 사이즈 제품을 제외하고는 배송 기간이 20일로 늘어납니다.
    배송 시간은 엄격하게 계약에 따릅니다.
  • 고객 타사 대행사가 공장에 가서 검사할 수 있도록 지원
  • 고객에게 테스트용 무료 샘플 지원
  • 현장 또는 비디오 공장 검사 지원
지금 Daxun에 문의

기술 지원

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.Stainless Steel rods

지금 Daxun에 문의

310S Stainless Steel Rod Ordering Information

Stainless Steel rods The purchase order shall include quantity, PSL grade, type or category, API5L reference, diameter, finish, length and any applicable attachments or additional requirements relating to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish or end finish. Bars are solution bright annealed.

310-310S Stainless Steel Rod Features

높은 강도
내식성
내열성
저온 저항
환경 보호
용접 성능

Daxun 합금으로 브랜드를 빠르게 향상 시키십시오.

배송 상태 선택 표면 상태
Forged 블랙
광택
열간 압연 블랙
광택
밝음
피클
콜드 드로잉 광택
밝음
참고:
1. 위에 나열된 것과 다른 배송 상태가 필요한 경우 당사에 문의해 주시기 바랍니다.
2. 문의 또는 주문 시 여기에 표시되지 않은 추가 요구 사항이 있으면 친절하게 알려주시기 바랍니다.
용액 어닐링 상태의 재료는 다음과 같이 숙성될 수 있습니다.-*두 배 숙성을 나타냅니다.
조건 H900(H480) H925(H495) H1025(H550) H1075(H580) H1100(H595) H1150(H620) H1150M(H620M)* 플러스 H1150D(H620D)* 플러스
로 가열합니다. ±15oF 900oF 925 oF 1025oF 1075oF 1100oF 1150oF 1400oF 1150oF 1150oF 1150oF
±9oC 480oC 495oC 550oC 580oC 595oC 620oC 760oC 620oC 620oC 620oC
몇 시간 동안 보류 1 4 4 4 4 4 2 4 4 4
아래로 냉각 Air Air Air Air Air Air Air Air Air Air
90oF(32oC)

Types of 310-310S Stainless Steel Rods (3)

참조 및 다운로드 가능한 정보

Daxun은 신뢰할 수 있는 스테인리스 스틸 막대 및 바 제조업체입니다.

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless ros  are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 310S Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

최근 인기 있는 사례 프로젝트 및 제품

스테인리스 스틸 로드
대구경 스테인리스 스틸 로드
310-310S stainless steel rod
스테인리스 스틸 광택 막대
스테인리스 스틸 로드
스테인리스 스틸 로드
스테인리스 스틸 로드
310-310S stainless rod
스테인리스 스틸 정밀 로드
스테인리스 스틸 로드
샘플을 받을 수 있나요?

We can provide 310S Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.

이미 수출한 국가는 어디인가요?

캐나다, 칠레, 쿠웨이트, 독일, 한국, 사우디아라비아, 싱가포르 등 42개 이상의 국가에 수출하고 있습니다.

MOQ는 얼마인가요?

Our MOQ is 1 ton for 310S Stainless Steel Rod.

배송 시간은 얼마나 걸리나요?

체험판 주문은 일주일 이내에 배송됩니다. 일반 주문의 경우 대략 2주 정도 소요됩니다.

오늘 문의 보내기