CE Certification 2205 Stainless Steel Round Bar
As a leading stainless steel supplier and exporter in China, Daxun supplies stainless steel barsRod (Round Bar)to all over the world.
- Grade: AISI 2205-S32205-S31803
- 제조: 열간 압연, 냉간 인발, 단조
- 표준 ASTM, ASME, GB, DIN, JIS, ISO
- High resistance to stress corrosion cracking, fatigue and erosion
- Higher thermal conductivity and lower thermal expansion than austenitic steels
- Excellent and uniform resistance to pitting and crevice corrosion
- Good resistance to sulfide stress corrosion cracking
스테인리스 봉 및 원형 막대 제작 서비스 분야의 글로벌 리더
Product Specifications
- ASTM A479 UNS S32205 Bar
- ASTM A276 F60 Duplex Round Bar
- ASTM A479 UNS S32205 Round Bar
- UNS S32205 Duplex Round Bar
- Duplex Steel S32205 Bar Manufacturer from China
Overview
Duplex Steel S32205 rods are used in many industries because of their great properties and versatility. S32205 is a duplex stainless steel that has both austenitic and ferritic characteristics. This gives it high strength, excellent corrosion resistance, and cost efficiency.
Composition and Properties
Duplex Steel S32205 has about 22% chromium, 5-6% nickel, 3% molybdenum, and high nitrogen. This combination makes it very resistant to corrosion and very strong. Its structure has both austenite and ferrite, which makes it stronger and better than regular austenitic or ferritic stainless steels.
내식성
One of the main features of S32205 rods is their resistance to different types of corrosion. They are highly resistant to pitting and crevice corrosion in chloride environments, which makes them perfect for use in corrosive areas like chemical processing, marine settings, and the offshore oil and gas industry.
당사의 서비스 센터 네트워크는 일반적인 크기와 합금의 바를 빠르고 준비된 공급을 위해 스테인리스 스틸 바 제품을 보유하고 있으며, 또한 맞춤형 크기의 스테인리스 스틸 막대를 생산하며 수량이 공장 최소 수량 미만인 경우 적시에 빠른 처리를 위해 재고 일정을 조정할 수 있으며, Daxun Alloys는 직경이 1/16 인치에서 26 인치 범위의 스테인리스 스틸 원형 바를 재고하고 있습니다. 원형 바는 302, 303, 304/L, 309/S, 310/S, 316/L, 317/L, 321, 321/H, 347, 347H, 410, 416, 420, 440C, 17-4PH, Duplex 2205 및 Alloy 20을 포함한 거의 모든 등급의 스테인리스 스틸로 제공됩니다. 열처리된 스테인리스 스틸 원형 바는 17-4PH, H900 템퍼(요청 시), H1025, H1150, Double H1150 및 H1150M으로 제공됩니다. 요청 시 다른 열처리된 템퍼도 제조할 수 있습니다. 410, 430, 416 등 400 시리즈 스테인리스 스틸을 보유하고 있습니다. 또한 303, 304, 316/L 정밀 및 베어링 품질의 스테인리스 스틸 원형 바도 보유하고 있습니다. 재고의 대부분은 가공성을 높이고 부품당 총 비용을 낮추기 위해 일관된 표준으로 용융된 스테인리스 스틸 원형 봉강인 당사의 고유한 가공 봉강 등급으로 구성되어 있습니다. 당사의 스테인리스 스틸 바 가공 기계를 통해 Daxun Alloys는 고객의 정확한 사양에 따라 생산할 수 있습니다.
데이터
- 매개변수
- 재료
- 기계적 특성
- 물리적 속성
- 모두 동일
- 유형
| 제품 매개변수: 스테인리스 스틸 로드 | |
| 사양 | ASTM A276, ASME SA276 / ASTM A479 ASME SA479 |
| 치수 | EN, DIN, JIS, ASTM, BS, ASME, AISI |
| SS 2205/S32205 Round Bars | 4mm ~ 500mm 범위의 외경 |
| SS 2205/S32205 Bright Bars | 4mm~100mm 범위의 외경 |
| SS 2205/S32205 Hex Bars | 18mm - 57mm(11/16인치 ~ 2-3/4인치) |
| 완료 | 블랙, 밝은 광택, 러프 턴, NO.4 마감, 무광 마감, BA 마감 |
| 길이 | 1~6미터, 맞춤형 절단 길이 |
| 양식 | 원형, 정사각형, 육각(A/F), 직사각형, 빌렛, 잉곳, 단조 등. |
| 등급 | C | Mn | Si | P | S | Cr | Mo | Ni | N |
| 2205 | 0.03 | 2 | 1 | 0.03 | 0.02 | min: 21.0 | min: 2.5 | min: 4.5 | min: 0.08 |
| (S31803) | max | max | max | max | max | max: 23.0 | max: 3.5 | max: 6.5 | max: 0.20 |
| 2205 | 0.03 | 2 | 1 | 0.03 | 0.02 | min: 22.0 | min: 3.0 | min: 4.5 | min: 0.14 |
| (S32205) | max | max | max | max | max | max: 23.0 | max: 3.5 | max: 6.5 | max: 0.20 |
| 등급 | 인장 강도 | 수율 강도 | 신장 | 경도 | |
| (MPa) min | 0.2% Proof | (% in 50mm) min | |||
| (MPa) min | Rockwell C (HR C) | Brinell (HB) | |||
| UNS S31803 / 2205 | 621 | 448 | 25 | 31 max | 293 max |
| UNS S32205 / 2205 | 621 | 448 | 25 | 31 max | 293 max |
| Grade 2205 | 밀도 | Elastic | Mean Co-eff of Thermal | Thermal | Specific | Electrical | |||
| (kg/m3) | Modulus(GPa) | Expansion (μm/m/°C) | Conductivity (W/m.K) | Heat | Resistivity | ||||
| 0-100°C | 0-315°C | 0-538°C | at 100°C | at 500°C | 0-100°C( J/kg.K) | (nΩ.m) | |||
| UNS S32205 / UNS S31803 | 782 | 190 | 13.7 | 14.2 | – | 19 | – | 418 | 850 |
| 등급 | 중국 | UNS | 올드 브리티시 | 유로노름 | 스웨덴어 SS | 일본어 JIS | ||
| 아니요 | BS | En | 아니요 | 이름 | ||||
| 2205 | 022Cr23Ni5Mo3N | S31803/S32205 | 318S13 | – | 1.4462 | X2CrNiMoN22-5-3 | 2377 | SUS 329J3L |
| Stainless Steel 2205/S32205/S31803 Bright Bar | SS 2205/S32205/S31803 Bright Bar |
| 2205/S32205/S31803 SS Bright Bar | |
| Stainless Steel 2205/S32205/S31803 Bright Bar | |
| UNS S2205/S32205/S3180300 SS Bright Bar | |
| WERKSTOFF NR. 1.4462 Bright Bar | |
| ASTM A276 2205/S32205/S31803 Stainless Steel Bright Bar | |
| Stainless Steel 2205/S32205/S31803 Hex Bar | SS 2205/S32205/S31803 Hex Bar |
| 2205/S32205/S31803 SS Hexagonal Bar | |
| 2205/S32205/S31803 Stainless Steel Hex Bar | |
| UNS S2205/S32205/S3180300 SS Hexagonal Bar | |
| ASTM A276 2205/S32205/S31803 Stainless Steel Hex Bar | |
| Stainless Steel 2205/S32205/S31803 Square Bar | SS 2205/S32205/S31803 Square Bar |
| 2205/S32205/S31803 SS Square Bars | |
| 2205/S32205/S31803 Stainless Steel Square Bar | |
| UNS S2205/S32205/S3180300 SS Square Bar | |
| WERKSTOFF NR. 1.4462 Square Bar | |
| ASTM A479 2205/S32205/S31803 Stainless Steel Square Bars | |
| Stainless Steel 2205/S32205/S31803 Rectangular Bar | SS 2205/S32205/S31803 Rectangular Bar |
| 2205/S32205/S31803 SS Rectangular Bars | |
| 2205/S32205/S31803 Stainless Steel Rectangular Bar | |
| UNS S2205/S32205/S3180300 SS Rectangular Bars | |
| WERKSTOFF NR. 1.4462 Rectangular Bar | |
| ASTM A276 2205/S32205/S31803 Stainless Steel Rectangular Bar | |
| Stainless Steel 2205/S32205/S31803 Flat Bars | SS 2205/S32205/S31803 Flat Bar |
| 2205/S32205/S31803 SS Flat Bars | |
| 2205/S32205/S31803 Stainless Steel Flat Bars | |
| UNS S2205/S32205/S3180300 SS Flat Bars | |
| WERKSTOFF NR. 1.4462 Flat Bars | |
| ASTM A276 2205/S32205/S31803 Stainless Steel Flat Bars | |
| Stainless Steel 2205/S32205/S31803 Polished Bar | SS 2205/S32205/S31803 Polished Bar |
| 2205/S32205/S31803 SS Polished Bars | |
| 2205/S32205/S31803 Stainless Steel Polished Bar | |
| UNS S2205/S32205/S3180300 SS Polished Bars | |
| WERKSTOFF NR. 1.4462 Polished Bar | |
| ASTM A476 2205/S32205/S31803 Stainless Steel Polished Bar | |
| Stainless Steel 2205/S32205/S31803 Threaded Bar | SS 2205/S32205/S31803 Threaded Bar |
| 2205/S32205/S31803 SS Threaded Bars | |
| 2205/S32205/S31803 Stainless Steel Threaded Bar | |
| UNS S2205/S32205/S3180300 SS Threaded Bar | |
| WERKSTOFF NR. 1.4462 Threaded Bar | |
| ASTM A276 2205/S32205/S31803 Stainless Steel Threaded Bar |
Daxun을 선택하고 고객을 만족시키세요.

빠른 응답
We provide timely and fast delivery of 2205 stainless steel bar products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading to ensure that the task is completed on time.
닥순의 장점
- 종류: 300 시리즈, 400 시리즈, 600 시리즈 등 다양한 크기와 등급을 제공합니다.
- 유연성: 열간 압연 또는 냉간 압연 바가 필요하든, 당사의 스테인리스 스틸 바 길이는 특정 프로젝트 요구 사항을 충족하도록 설계되었습니다.
- Quality Standards: Our stainless steel tubes meet strict ASTM, ISO9001, GB, NSF/ANSI standards to ensure reliability and performance.
- 맞춤 주문: 특별한 사이즈의 스테인리스 스틸 바를 찾고 계신가요? 경쟁력 있는 가격과 편리한 온라인 주문으로 다양한 스테인리스 스틸 바 맞춤 제작 옵션을 제공합니다.
2205 Stainless Steel Rod packaging
We pay attention to every process to ensure quality. The packaging we usually adopt is to pack 2205 stainless steel round bars in environmentally friendly plastic bags and then put them into fumigation-free wooden boxes or wooden pallets. Customized packaging, such as OEM, can also be negotiated. We provide almost everything to meet your round bar packaging requirements. We attach great importance to packaging. The round bars are packed in wooden corrugated boxes, wrapped with plastic packaging and bubble film on the outside.
품질, 배송, 검사
- Daxun conducts several quality assurance tests, including flattening tests, pitting resistance tests, mechanical tests, hardness tests, material identification, and expansion tests. These tests ensure that the materials meet all required standards for their intended applications.
- We support customer inspections by third-party agencies, provide free samples for testing, and offer both on-site and video factory inspections.
기술 지원
추가 기술 지원이 필요한 경우 금속 전문가와 지식이 풍부한 직원이 기꺼이 도와드릴 것입니다. 또한 Daxun은 다중 금속 및 플라스틱 재고 업계 최초로 인증된 테스트 실험실을 보유하고 있습니다. 이는 품질에 대한 변함없는 헌신과 풀서비스 공급업체로서의 철학을 보여주는 것이라고 생각합니다.
2205 Stainless Steel Rod Ordering Information
When placing an order for 2205 Stainless Steel Round Bars, please include the following details:
- Quantity
- PSL grade
- Type or category
- API5L reference
- 지름
- 표면 마감
- 길이
- Any other specific requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish, or end treatment.
- Payment terms, including deposit requirements and available options such as T/T and L/C.
All bars are solution bright annealed.
2205-S32205-S31803 Stainless Steel Rod Features
Daxun 합금으로 브랜드를 빠르게 향상 시키십시오.
- 갤러리
- 배송 상태
- 나이 경화
| 배송 상태 선택 | 표면 상태 |
| Forged | 블랙 |
| 광택 | |
| 열간 압연 | 블랙 |
| 광택 | |
| 밝음 | |
| 피클 | |
| 콜드 드로잉 | 광택 |
| 밝음 | |
| 참고: | |
| 1. 위에 나열된 것과 다른 배송 상태가 필요한 경우 당사에 문의해 주시기 바랍니다. | |
| 2. 문의 또는 주문 시 여기에 표시되지 않은 추가 요구 사항이 있으면 친절하게 알려주시기 바랍니다. | |
| 용액 어닐링 상태의 재료는 다음과 같이 숙성될 수 있습니다.-*두 배 숙성을 나타냅니다. | ||||||||||||
| 조건 | H900(H480) | H925(H495) | H1025(H550) | H1075(H580) | H1100(H595) | H1150(H620) | H1150M(H620M)* | 플러스 | H1150D(H620D)* | 플러스 | ||
| 로 가열합니다. | ±15oF | 900oF | 925 oF | 1025oF | 1075oF | 1100oF | 1150oF | 1400oF | 1150oF | 1150oF | 1150oF | |
| ±9oC | 480oC | 495oC | 550oC | 580oC | 595oC | 620oC | 760oC | 620oC | 620oC | 620oC | ||
| 몇 시간 동안 보류 | 1 | 4 | 4 | 4 | 4 | 4 | 2 | 4 | 4 | 4 | ||
| 아래로 냉각 | Air | Air | Air | Air | Air | Air | Air | Air | Air | Air | ||
| 90oF(32oC) | ||||||||||||
참조 및 다운로드 가능한 정보
스테인리스 스틸 로드 생산
Daxun은 신뢰할 수 있는 스테인리스 스틸 막대 및 바 제조업체입니다.
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless rod are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the 2205 Stainless Steel Rod have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.
최근 인기 있는 사례 프로젝트 및 제품





관련 제품 (12)
2205 Duplex Stainless Steel Round Bar is a strong type of steel that contains 22% chromium, 3% molybdenum, and 5-6% nickel. It has both ferritic and austenitic properties, which makes it stronger than regular stainless steels. 2205 has twice the yield strength of standard stainless steels and is very resistant to corrosion in tough environments. It also has good fatigue strength and resists stress cracking, pitting, crevice corrosion, and erosion, making it useful for challenging applications.
- 화학 처리, 운송 및 보관 - 압력 용기, 탱크, 배관 및 열교환기
- 석유 및 가스 탐사 및 처리 장비 - 배관, 튜브 및 열교환기
- 해양 및 기타 염화물이 많은 환경
- 폐수 스크러빙 시스템
- 펄프 및 제지 산업 - 소화기, 표백 장비 및 재고 처리 시스템
- 선박 및 트럭용 화물 탱크
- 식품 가공 장비
- 바이오 연료 플랜트
- ASTM/ASME: 240 UNS S32205/S31803
- EURONORM: 1.4462 X2CrNiMoN 22.5.3
- AFNOR: Z3 CrNi 22.05 AZ
- DIN: W.Nr 1.4462
We can provide 2205 Stainless Steel Rod samples for you to check the quality. Sample is free and you just pay the freight.
내식성
- High amounts of chromium, molybdenum, and nitrogen make Duplex 2205 Stainless Steel more corrosion-resistant than 316 and 316L grades.
- Provides protection against pitting and crevice corrosion, even in tough or acidic environments.
- Resistant to chloride stress corrosion cracking.
- Handles temperatures up to 302°F (150°C).
- Ferrite in its structure helps it work well in caustic conditions.
- Suitable for challenging environments.
내열성
- Duplex 2205 has good oxidation resistance at high temperatures, similar to other duplex stainless steels.
- Becomes brittle when exposed to temperatures above 572°F (300°C), even for short periods.
- Not recommended for use at temperatures above 572°F (300°C).
Welding Characteristics
- Duplex 2205 has good weldability.
- Should not be welded without filler metal, as this can lead to excessive ferrite content.
열처리
- Annealing temperature range is between 1868 to 2012°F (1020 to 1100°C).
- Cannot be hardened by heat treatment but does work-harden.
- Special attention is needed to handle a higher thermal expansion rate to avoid warping and distortion.
가공 - 열간 성형
Most producers suggest keeping the hot forming temperature for Duplex 2205 between 2010 and 2100°F (1100 to 1150°C). If the shape isn’t compact, the edges can cool faster than the center, which might cause cracking.
가공 - 냉간 성형
Duplex 2205 can be formed in different ways, but its high strength makes it more challenging. Even with strong equipment, you need to account for extra spring-back because of its strength.
기계성
Duplex 2205 stainless steel is a bit harder to machine than 300 series stainless steels. It needs more cutting force, which makes tools wear out faster. Here are some machining tips:
- Use a strong, rigid machine with solid tool and workpiece mounts.
- Keep tool extensions short to reduce vibration.
- Avoid a large tool nose radius to keep the carbide sharp but strong.
- Plan the machining so the cut depth stays below the hardened layer from previous passes.
테스트
- Here are the tests we conduct for Duplex 2205 Stainless Steel:
- Positive material identification test
- Intergranular corrosion test
- Pitting resistance test
- Mechanical test
- Chemical test
- Macro/micro test
- Flattening/flaring test
Documents provided
- Heart treatment chart, quality assurance plan, commercial invoice, certificate of origin, raw material test report, material traceability report etc are a few essential documents provided to the buyers. Additionally, the other documents like MTC as per EN 10204/3.1B, TC like radiography test report and the third party test report are provided.
2205-s32205-S31803 grade stainless steel round bars
We provide important documents such as:
- Heat treatment chart
- Quality assurance plan
- Commercial invoice
- Certificate of origin
- Raw material test report
- Material traceability report
Documents Provided
We provide important documents such as:
- Heat treatment chart
- Quality assurance plan
- Commercial invoice
- Certificate of origin
- Raw material test report
- Material traceability report
We also provide other documents like Material Test Certificate (MTC) according to EN 10204/3.1B, radiography test report, and third-party test report.
Our stainless steel round bars come in many sizes. You can choose the grade you need, with lengths from 500mm to 6 meters and diameters from 3mm to 500mm. We offer both metric and imperial sizes. If you need custom sizes, we provide free cuts using advanced bandsaws to make sure it’s done right.
Our MOQ is 1 ton for 2205 Stainless Steel Rod.