Daxun is an excellent manufacturer of Ti 6Al4V 5 grade titanium rods and bars.
As China’s leading supplier of titanium and titanium alloy rods, Daxun provides high-performance titanium rods to the world.
- Titanium bar grade: Grade 5-Ti6Al 4V- UNS R56400-3.7165-TC4
- Titanium bar types: rolled bars, drawn bars, forged titanium bars
- Titanium bar density The density of grade 5 titanium is 4.51 g/cm3
- Main standards: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
- High strength, high temperature resistance, corrosion resistance, light
- weight, excellent comprehensive performance.
————Daxunは中国でチタン棒を生産し、多様なニーズに応えている。 ——顧客の厳しいニーズ!
純チタン棒製造サービスのグローバルリーダー
Daxun, specializing in the production of alloy titanium rods for extreme environments—Ti6AL-4V titanium alloy rods.
Grade 5 titanium alloy rod (titanium aluminum vanadium alloy) is the most commonly used α-β titanium alloy, accounting for 50% of the total titanium alloy usage worldwide. One of the most notable features of grade 5 titanium alloy is that it is fully heat treatable and can be used at temperatures up to 400°C. It has low density (4.43 kg/dm), excellent corrosion resistance, and high mechanical strength. Grade 5 titanium alloy has high tensile strength at ambient temperature and good creep resistance at temperatures up to 300°C. It also has strong crack resistance and fatigue resistance. The age-hardening ability of 6AL-4V titanium alloy rod makes it an excellent choice for a wide range of applications, including fasteners and components in harsh environments. Its high machinability and weldability make it suitable for a wide range of industrial applications.
大順 is your trusted titanium alloy rod production company. Daxun produces all grades of titanium alloys, including commercially pure titanium series CP, titanium alloy series, titanium nickel alloy, etc. They have reliable performance and provide high performance for your critical applications. In various industries and applications, you can rely on Daxun titanium alloy rods for high strength, high temperature and corrosive environments. For decades, Daxun Metals has been committed to producing highly engineered titanium alloy solutions to meet the most severe challenges.
データ
- パラメータ
- 原材料
- 機械的特性
- 物理的性質
- ホットな検索
| 仕様 | 詳細 |
| 素材 | Titanium rod and bar Grade 5 (UNS R56400) |
| スタンダード | ASMB348、ASMSB348、AMS4921、AMS4902 |
| 寸法 | EN, ASTM, JIS, ASME, BS, AISI , GB,GJB,DIN |
| 直径範囲 | 0.125″~14″(3.175mm~355.6mm)、カスタム |
| 長さの範囲 | 最大240″(6096mm)、カスタム |
| 表面処理 | 冷間(明るい)引かれた、センターレス地面、熱間圧延された、滑らかな回された、皮をむかれた、切り開かれた圧延された端、熱間圧延されたアニールされた、荒い回された、明るい、ポーランド語、粉砕、センターレス地面及び黒 |
| 表面仕上げ | 冷間引抜、センタレス研磨、ポリッシュ、ラフ切削、黒色、NO.4仕上げ、BA仕上げ、マット仕上げ等。. |
| コンディション | 焼入れ、焼戻し、アニール |
| 寛容 | 直径公差:+/- 0.127mm(±0.005)、長さ公差:+/-0.125″(3.175ミリメートル) |
| 様式 | チタン角棒、チタンインゴット、チタン丸棒、チタン角棒、チタン三角棒、鍛造チタン棒、チタン六角棒など。. |
| 物理的性質 | 密度: 0.163 lb/in³ (4.51 g/cm³), 融点: 3,020°F (1,660°C), 伸び: 20-30%, 弾性率: 16.5 x 10⁶ psi (114 GPa) |
| 化学組成 | チタン(最小):99.2%、酸素(最大):0.25%、炭素(最大):0.08%、鉄(最大):0.30%、窒素(最大):0.03%、水素(最大):0.015% |
| Chemical Composition: | |||
| シンボル | エレメント | Min % | Max % |
| アル | Aluminum | 5.50% | 6.75% |
| V | Vanadium | 3.50% | 4.50% |
| フェ | 鉄 | 0.30% | |
| O | 酸素 | 0.20% | |
| C | カーボン | 0.08% | |
| N | 窒素 | 0.05% | |
| H | 水素 | 0.01% | |
| Y | Yttrium | 0.01% | |
| Other, each | 0.10% | ||
| Other, total | 0.40% | ||
| ティ | チタン | Remainder | |
| 物理的性質 | メートル | 英語 | コメント |
| 密度 | 4.43 g/cc | 0.16 lb/in³ | |
| 機械的特性 | |||
| 硬度、ブリネル | 334 | 334 | Estimated from Rockwell C. |
| 硬度、ヌープ | 363 | 363 | Estimated from Rockwell C. |
| Hardness, Rockwell C | 36 | 36 | |
| 硬度、ヴィッカース | 349 | 349 | Estimated from Rockwell C. |
| 引張強さ | min. 895MPa | 129810 psi | |
| 降伏強度 | min. 828MPa | 120090 psi | |
| 破断伸び | min.10 % | 10 % | |
| 面積の縮小 | min.25 % | 25 % | |
| 弾性係数 | 113.8 GPa | 16500 ksi | |
| Compressive Yield Strength | 970 MPa | 141000 psi | |
| Notched Tensile Strength | 1450 MPa | 210000 psi | Kt (stress concentration factor) = 6.7 |
| Ultimate Bearing Strength | 1860 MPa | 270000 psi | e/D = 2 |
| Bearing Yield Strength | 1480 MPa | 215000 psi | e/D = 2 |
| Poisson’s Ratio | 0.342 | 0.342 | |
| シャルピー衝撃 | 17 J | 12.5 ft-lb | Vノッチ |
| Fatigue Strength | 240 MPa | 34800 psi | at 1E+7 cycles. Kt (stress concentration factor) = 3.3 |
| Fatigue Strength | 510 MPa | 74000 psi | Unnotched 10,000,000 Cycles |
| Fracture Toughness | 75 MPa-m½ | 68.3 ksi-in½ | |
| せん断弾性率 | 44 GPa | 6380 ksi | |
| Shear Strength | 550 MPa | 79800 psi | Ultimate shear strength |
| 電気的特性 | |||
| 電気抵抗率 | 0.000178 ohm-cm | 0.000178 ohm-cm | |
| 透磁率 | 1.00005 | 1.00005 | at 1.6kA/m |
| 磁気感受性 | 3.30E-06 | 3.30E-06 | cgs/g |
| 熱特性 | |||
| CTE, linear 20°C | 8.6 µm/m-°C | 4.78 µin/in-°F | 20-100ºC |
| CTE, linear 250°C | 9.2 µm/m-°C | 5.11 µin/in-°F | Average over the range 20-315ºC |
| CTE, linear 500°C | 9.7 µm/m-°C | 5.39 µin/in-°F | Average over the range 20-650ºC |
| 比熱容量 | 0.5263 J/g-°C | 0.126 BTU/lb-°F | |
| 熱伝導率 | 6.7 W/m-K | 46.5 BTU-in/hr-ft²-°F | |
| 融点 | 1604 – 1660 °C | 2920 – 3020 °F | |
| Solidus | 1604 °C | 2920 °F | |
| リクイダス | 1660 °C | 3020 °F | |
| ベータ・トランサス | 980 °C | 1800 °F | |
| Beta Transus (F ± 25) | 1830 | ||||
| Coefficient of Thermal Expansion (10-6in./in./F) | 32-212 | 5 | |||
| 32-600 | 5.3 | ||||
| 32-1000 | 5.6 | ||||
| 32-1200 | 5.9 | ||||
| 32-1500 | 6.1 | ||||
| Density (lbs./cu. in.) | 0.16 | ||||
| Melting Point, Approx (F) | 3200 | ||||
| Electrical Resistivity at Room Temp. (Microhms cm) | 171 | ||||
| Modulus Elasticity – Tension (106 psi) | 16.5 | ||||
| Modulus Elasticity – Torsion (106 psi) | 6.1 | ||||
| 熱伝導率 | 3.9 at Room Temperature | ||||
| (Btu/hr/sq. ft./F/ft.) | |||||
| Specific Heat (Btu/lb./F) at Room Temp. | 0.135 | ||||
| 溶接性 | Fair | ||||
| Annealing Temp. (F) | Full | 1300 – 1525°/15 Min. – 2 Hrs,; Air Cool | |||
| Stress Relief | 900 – 1200°/1 -4 Hrs.; Air Cool | ||||
| Forging* Temp. (F) | Blocking | 1750 – 1800° | |||
| Finishing | 1650 – 1750° | ||||
| Typical Application | Compressor blades, discs, aircraft components, pressure vessels, rocket engine cases; | ||||
| the most versatile titanium alloy. | |||||
| ASTM B348 Gr5 Titanium Round Bar | ASTM B348 GR 5 Cold Rolled Rods |
| Titanium Alloy Grade 5 Bright Bars | ASTM B348 Gr 5 Titanium Polish Bars |
| B348 Grade 5 Titanium Forged Round Bars | Titanium Alloy ASTM B348 Grade 5 Spring Steel Bars |
| Grade 5 Ti Alloy Hexagon Bars | Titanium Alloy Werkstoff Nr. 3.7165 Square Bars |
| Titanium Alloy UNS R56400 Rods | B348 Grade 5 Titanium Alloy Hex Bars |
| Ti Alloy GR5 Cold Drawn & Polished Square Bars | Titanium Alloy Grade5 Hollow Bars |
| ASTM B348 Grade 5 Titanium Threaded Bars | Titanium ASTM B348 Grade 5 Flat Bars |
| Top Quality B348 Grade 5 Titanium Cold Drawn Bars | AS ASTM B348 Gr 5 Black Bars |
Daxunを選んで、あなたのプロジェクトを成功に導きましょう。.
DAXUN® Grade 5 Titanium Rod Features
DAXUN® Ti Grade 5 is a titanium alloy bar (6al-4v) featuring:
- Good hot formability and weldability;
- Tensile strength can reach 1000MPa;
- Dimensional work at high temperature
- Insensitive to seawater or seawater;
- Not affected by various corrosive media;
- High strength and good toughness;
- Resist crack initiation and crack propagation.
Daxun Factory Advantages
Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.
Grade 5 Titanium Rod Production Method
Daxun produces high-quality titanium bars with high performance, and can also manufacture according to customer’s agreement:
- Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
試験報告書
The test reports we provide include: Grade 2 Titanium Rod and Grade 2 Titanium Round Bar Factory Test Certificate, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, NABL Approved Laboratory Report, Destructive Test Report, Non-destructive Testing Report. (Daxun will provide according to customer requirements)
Grade 5 Rods Applications and Standards
Grade 5 Titanium Rods are widely used in the following industries under extreme corrosive conditions:
- Aerospace, shipbuilding, oil and gas industry, marine engineering, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, military industry, pharmaceutical and food processing equipment, etc.
- Specifications: AMS 4928,AMS 4967,AMS 4965 ,AMS 6931 ,ASTM B 348
- Standards: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
品質、納期、検査
Daxun performs several quality assurance tests, these tests include mechanical tests like area tensile, chemical analysis, material positive identification – PMI test, micro and macro testing, intergranular corrosion (IGC) test, ultrasonic flaw detection test, pitting and resistance test, hardness test, material positive identification, expansion test etc. All these tests ensure that the Grade 2 Titanium Rod and Grade 2 Titanium Round Bar material is suitable for the required application. During the production process, we measure the diameter, thickness and surface of the product.
- 当社の納期は、契約に厳密に従います。.
- 顧客の第三者機関が工場に検査に行くのをサポートする。
- 顧客テストのための無料サンプルをサポート
- 現場検査またはビデオ工場検査をサポート
パッケージング
国際貨物は様々な経路を経て最終目的地に到着するため、梱包は重要な役割を担っています。商品によって、様々な方法で梱包しています。当社では、以下のような様々な方法で商品を梱包しています:
- 箱と木箱
- シュリンクラップ
- 木製パレット
- 木製ボックス
テクニカルサポート
さらに技術的なサポートが必要な場合は、常駐の冶金学者と知識豊富なスタッフが喜んでお手伝いいたします。さらに、Daxunは、マルチメタルおよびプラスチック在庫業界初の認定試験所を誇っています。これは、当社の品質への揺るぎないこだわりと、フルサービスサプライヤーとしての理念を示すものだと考えています。.
You can trust it Daxun Alloy
Daxun Grade 5 Titanium Rods help your brand improve quickly
- チタン棒
- Types of Grade 5 Titanium Rods
- Tolerances for Grade 5 Titanium Round Bars (BS EN ISO 286-2)
| 以下に記載されている製品とは別に、他の利用可能な金属製品はここに記載されていません。DAXUNが製造・供給できるその他の金属製品には、タンタル、ニオブ、ジルコニウム、ハフニウム、ニッケル、銅などがあり、これらは主に板、棒、管の形をしています。. | |
| 製品/加工基準 | グレード/サイズ |
| Titanium Plate, rod, Coil— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136 | GR1,GR2,GR3,GR4,GR5,GR7,GR9,GR12,GR16,GR17,GR23,Ti-6Al-4V ELI,Ti-6-2-4-2,Ti-15-3-3(厚さ:( 0.0197”-6”)最大幅:12フィート,最大長:50フィート) |
| AMS-T-9046 | |
| Titanium and Titanium alloy rod, plate | |
| 商業用純チタン(CP) | |
| コード指定 | 降伏強度 |
| 最小値、ksi 1 | |
| CP-1 | 70 |
| CP-2 | 55 |
| CP-3 | 40 |
| CP-4 | 25 |
| アルファチタン合金(A) | |
| コード指定 | 構成 |
| A-1 | 5A1-2.5Sn |
| A-2 | 5A1-2.5Sn(ELI)2・・・。 |
| A-3 | 6A1-2Cb-1Ta-0.8Mo |
| A-4 | 8A1-1Mo-1V |
| α-βチタン合金(AB) | |
| コード指定 | 構成 |
| AB-1 | 6A1-4V |
| AB-2 | 6A1-4V(ELI) |
| AB-3 | 6A1-6V-2Sn |
| AB-4 | 6A1-2Sn-4Zr-2Mo |
| AB-5 | 3A1-2.5V |
| AB-6 | 8Mn |
| ベータチタン合金(B) | |
| コード指定 | 構成 |
| B-1 | 13V-11Cr-3A1 |
| B-2 | 11.5Mo-6Zr-4.5Sn |
| B-3 | 3A1-8V-6Cr-4Mo-4Zr |
| B-4 | 8Mo-8V-2Fe-3A1 |
| 処理: | |
| 熱間圧延 | 冷間圧延 |
| 利用可能なグレード | |
| CPグレード1 | グレード 6Al-2Sn-4Zr-2Mo (6-2-4-2) |
| CPグレード2 | グレード6Al-4V ELI(旧グレード23) |
| グレード7 | グレード 6Al-6V-2Sn (6-62) |
| 19年生 | グレード 8Al-1Mo-1V (8-1-1) |
| グレード 5 (6Al-4V) | グレード9(3Al-2.5V) |
| グレード 6 (5Al-2.5Sn) | CPグレード3 |
| 申し込み | |
| 化学工業 | 海水の脱塩 |
| 石油化学産業 | 航空宇宙 |
| 機械加工分野、自動車分野 | 携帯電話のコンポーネント分野。. |
| Titanium Grade 5 Bright Bar | Titanium Grade 5 Bright Bar |
| Grade 5 Titanium Alloy Bright Bar | |
| Titanium Gr 5 Bright Bar | |
| UNS R56400 Titanium Bright Bar | |
| WERKSTOFF NR. 3.7035 Bright Bar | |
| ASTM B348 Gr 5 Titanium Bright Bar | |
| Titanium Grade 5 Hex Bar | Titanium Gr 5 Hex Bar |
| Grade 5 Titanium Hexagonal Bar | |
| Gr 5 Titanium Alloy Hex Bar | |
| UNS R56400 Titanium Hexagonal Bar | |
| ASTM B348 Grade 5 Titanium Hex Bar | |
| Titanium Alloy Grade 5 Square Bar | Titanium Grade 5 Square Bar |
| Grade 5 Titanium Square Bars | |
| Gr 5Titanium Alloy Square Bar | |
| UNS R56400 Titanium Square Bar | |
| WERKSTOFF NR. 3.7035 Square Bar | |
| ASTM B348 Gr 5 Titanium Square Bars | |
| Titanium Grade 5 Rectangular Bar | Titanium Grade 5 Rectangular Bar |
| Ti. Alloy Gr2 Rectangular Bars | |
| Gr 5 Titanium Alloy Rectangular Bar | |
| UNS R56400 Titanium Rectangular Bars | |
| WERKSTOFF NR. 3.7035 Rectangular Bar | |
| ASTM B348 Gr 5 Titanium Rectangular Bar | |
| Titanium Grade 5 Flat Bars | Titanium Grade 5 Flat Bar |
| Gr 5Titanium Alloy Flat Bars | |
| Titanium Gr 5Flat Bars | |
| UNS R56400 Titanium Flat Bars | |
| WERKSTOFF NR. 3.7035 Flat Bars | |
| ASTM B348 Gr 5 Titanium Flat Bars | |
| Titanium Grade 5 Polished Bar | Titanium Grade 5 Polished Bar |
| Grade 5Titanium Polished Bars | |
| Gr 5Titanium Alloy Polished Bar | |
| UNS R56400 Titanium Polished Bars | |
| WERKSTOFF NR. 3.7035 Polished Bar | |
| ASTM B348 Gr 5 Titanium Polished Bar | |
| Titanium Grade 5 Threaded Bar | Titanium Gr 5 Threaded Bar |
| Grade 5Titanium Threaded Bars | |
| Ti. Alloy Grade 5 Threaded Bar | |
| UNS R56400 Titanium Threaded Bar | |
| WERKSTOFF NR. 3.7035 Threaded Bar | |
| ASTM B348 Gr 5 Titanium Threaded Bar |
| NOMINAL SIZE | h5 | h6 | h7 | h8 | h9 | H10 | H11 | h12 |
|---|---|---|---|---|---|---|---|---|
| DIAMETER mm | ||||||||
| ~ to 3 | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| over 3 to 6 | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| over 6 to 10 | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| over 10 to 18 | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| over 18 to 30 | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| over 30 to 50 | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| over 50 to 80 | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| over 80 to 120 | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| over 120 to 180 | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| over 180 to 250 | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
Types of Ti-6AL-4V Grade 5 Titanium Rods (3)
参照およびダウンロード可能な情報
チタン棒
Daxun is a reliable manufacturer of grade 5 titanium rods
As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium bars are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the titanium rod have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.
最近の注目プロジェクトと製品
関連商品 (8)
大順 has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 5 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.
仕様
AMS 4928 – Bars, Forgings, and Forging Stock (Annealed)
AMS 4965 – Bars, Forgings (Solution treated and aged)
AMS 4967 – Bars, Forgings (Annealed, Heat Treatable)
HEAT TREATMENT
- When high hardness, tensile strength, and fatigue strength are required, annealing can be performed at 1,700-1,900°F (927 – 1,038°C).
DAXUN 6-4™ Grade 5 alloy can be heat treated in a variety of ways. - 1. Anneal: 1,275 -1,400°F; (691 – 760°C), ½ to 2 hours, air or furnace cool
- 2. Stress Relief Anneal: 1,000 -1,200°F; (538 – 649°C), 1 to 8 hours, air or furnace cool
- 3. Solution Heat Treat: 1,675 -1,750°F; (913 – 954°C), 1 hour, water quench
- 4. Aging: 975 -1,025°F; (524 – 552°C), 4 to 8 hours – air cool
In the solution treated and aged condition, rapid quenching of small sections yields optimum properties. Larger section sizes and/or delayed quenching may result in less than optimum properties.
HARDNESS
Typical hardness in the annealed condition is Rockwell C 30-34, and about Rockwell C 35-39 in the solution and aged condition.
Forgeability/Formability
- Ti-6Al-4V, Grade 5 alloy bar is forged at 1,750°F; (954°C) with a final forging temperature of 1,450°F; (788°C). A minimum of 35% reduction is recommended for optimum properties.
- Ti-6Al-4V, Grade 5 alloy bar is difficult to form at room temperature, even in the annealed condition. Therefore, severe forming operations such as bending or stretching can be performed on annealed material at temperatures up to 1,200°F; (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000 – 1,200°F; (538 – 649°C).
加工性
Ti-6Al-4V, Grade 5 alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids.
溶接性
Ti-6Al-4V, Grade 5 alloy rod is readily weldable in the annealed condition or in the solution and partially aged condition, with aging being accomplished during post weld heat treatment. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. Spot, seam, and flash welding may be performed without the aid of a protective atmosphere.
Special Considerations
Ti-6Al-4V, Grade 5 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics.
Size range
- Grade 1 Titanium Bar Dimensions
- Ø 0,7 – 30 mm (drawn, ground)
- Ø 16 – 400 mm (hot rolled, peeled)
- h11-h5 possible
- Tighter or different tolerances available on request
- Lengths up to 9,000 mm long, depending on diameter
- For larger diameters, other bar lengths and tolerances can be agreed upon request
Availability Grade 5 Titanium rods
- Drawing, straightening
- Drawing, straightening, polishing
- Drawing, grinding, polishing
- Drawing, straightening, grinding, polishing
- Drawing, annealing, straightening
- Drawing, annealing, polishing
- Drawing, annealing, grinding, polishing
- Drawing, annealing, straightening, grinding, polishing
Processing
We produce bars according to your requirements.
Excellent surface and straightness, perfect roundness and tightest diameter tolerances (according to ISO 286-2 up to h5). Available in straightened, ground, polished conditions.
製材
Band saws (up to Ø510 mm)
Bench band saws (up to 6,000 x 3,000 x 400 mm)
High-performance sawing machines for precise sawing
Titanium Bar end machining
Single or double sided
Chamfer 90° (45°)
Point 60° (30°)
Flat end
Centered
Delivery form
ASTM American Society for Testing and Materials Standards
AMS American Aerospace Materials Standards
NACE American Association of Corrosion Engineers International Standards
ASME American Society of Mechanical Engineers Standards
GB Chinese National Standards
GJB Chinese National Military Standards
ISO International Standards
DIN German Standards
EN European Standards
API American Petroleum Institute Standards
Detection method
Non-destructive testing > 100% testing
Testing methods
Eddy current testing/eddy current crack testing
Defect-free surface (level 4)
Flat bottom hole diameter 0.7 mm and 0.4 mm
Blind area can be cut off according to fixed length >Test to the end of the bar
Full diameter ultrasonic testing
Our Titanium Bar Material Services
- As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.
- We will be happy to provide you with a consultation and explain everything you need to know about obtaining titanium bar material, including which standards require greater attention for the components to be manufactured.
- If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.
- Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 2 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.
ご注文について
Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.
必要なチタン合金のグレードは、取り組んでいるプロジェクトによって異なります。各グレードには異なる利点があるためです。
すべてのグレードのチタン合金は極めて強靭で耐食性に優れており、過酷な環境下でも良好な性能を維持し続けます。
チタン合金の高グレード品(5~12)は、特定の利点を目的として設計された合金である。例えば、グレード12チタン合金は優れた耐熱性を有し、シェルアンドチューブ式熱交換器、油圧配管、化学工業用機器に最適な選択肢となる。
グレード1~4は純チタン合金であり、配管システムやチューブ用に溶接可能で延性のある材料が必要な場合に最適な選択肢です。低グレード品は船舶産業や工業分野で使用されています。
プロジェクトを開始するにあたり、どのグレードのチタン合金が最適かお悩みでしたら、ぜひ当社までご連絡ください。喜んでご支援いたします。
大迅では、グレード1からグレード12まで幅広いチタン合金グレードを提供しています。
グレード1~4は純チタンであり、それより上のグレードは合金である。
合金グレードは、高い強度重量比で人気がある。
最も一般的に使用されるチタン合金グレードはグレード5です。チタン含有量は依然として高いものの、このグレードは600°F(約315℃)までの高温に耐え、過酷な条件にも耐えられるため、最も信頼性の高いグレードの一つです。
航空宇宙産業や海洋産業などの業界では、耐摩耗性と耐食性に優れていることから、より高品位のグレードが好まれている。
逆に、低品位の鋼材は強度が低いため、主に溶接用として使用される。
各種チタン合金のグレードの違いについて詳しく知りたい方は、本日+86 13382898899までお電話ください。専門家が直接ご説明いたします。
チタンのグレードはコストをわずかに増加させますが、総コストは主に必要なチタンの形状と形態によって決定されます。
At DAXUN, we offer a wide range of titanium products, including plates, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.
残念ながら、プロジェクトの詳細やチタニウムの使用目的がわからないと、オンラインで価格をお見積もりするのは難しいです。
幸いなことに、当社の専門家チームが常に皆様のチタンに関するご要望にお応えし、アドバイスを提供いたします。[email protected] までメールをお送りいただければ、アドバイスと正確な見積もりをご案内いたします。
ご要望のチタニウムのグレード、形状、数量について、可能な限り詳細な情報をご提供ください。これにより、お客様のニーズをより正確に把握できます。
DAXUNのチームは経験豊富で知識が深く、親しみやすいです。業界での長年の経験から、チタンの用途、利点、グレードに至るまで、あらゆることを熟知しています。
チタニウムの最新情報、用途、および産業分野における応用事例については、当社のブログをぜひご覧ください。専門家による分かりやすいガイドを掲載しており、疑問が生じた際にはいつでもご参照いただけます。
もし問題が解決しない場合は、お気軽にお問い合わせください。喜んでお手伝いいたします。
[email protected] 宛にメールをお送りいただければ、迅速なご返答を差し上げます。お問い合わせの際は、可能な限り詳細な情報をご記載ください。そうすることで、適切な解決策をご提案できます。
お問い合わせ “ページのフォームにご記入いただくか、”+86 13382898899 “までお電話ください。WhatsAppはオンライン、Eメール([email protected])は6時間以内に確認いたします。すべてのお問い合わせやメッセージに迅速に対応させていただきます。また、毎週お客様と市場情報を共有しています。
We can provide titanium rod samples for you to check the quality. Sample is free and you just pay the freight.
カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.
Our MOQ is 1 ton for titanium rod.
トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.