x
お問い合わせ
クイック見積もり

Daxun is an excellent manufacturer of CP-2-grade titanium rods

中国のチタンおよびチタン合金棒の大手サプライヤーとして、大順は高性能チタン棒を世界に提供しています。.
  • Titanium Rod Grade:CP-2(Grade 2)- UNS R50400-3.7035-TA2
  • Types: Hot rolled rod, forged rod, cold drawn rod, extruded rod etc
  • Shape: Titanium round bar, titanium square bar、Ti  hexagonal bar
  • Density of Titanium Rod: Density of Grade 2 Titanium Rod is 4.51g/cm3
  • Standards: ASTM B 348,ASME SB348,DIN 17862,ASTM F67,ASTM 265
  • Dimensions: GB, GJB, EN, ASTM, JIS, ASME, BS, AISI, DIN, ISO, etc.

純チタン棒製造サービスのグローバルリーダー

Grade 2 Titanium Rod is the workhorse among titanium alloy rods, offering an excellent balance of strength and weight for weight-sensitive applications. As a commercially pure (CP) titanium alloy, it achieves an ideal combination of strength and ductility, making it suitable for a wide range of demanding uses. It provides high impact strength, is easily weldable, and is extremely corrosion-resistant in oxidizing conditions, alkaline media, brine solutions, weakly reducing environments, nitric acid, and wet chlorine. Additionally, its excellent resistance to seawater and saline solutions further enhances its versatility.

The Grade 2 Titanium Rod stands out for its lightweight nature, impressive strength-to-weight ratio, and outstanding resistance to corrosion, making it highly versatile and ideal for numerous industrial uses. From general industrial uses to military and aerospace applications, this material delivers reliable performance in challenging environments.

Daxun Alloys stocks Grade 2 Titanium Rods in a variety of diameters to meet the specific requirements of different projects. Our inventory includes sizes ranging from 1 mm to 300 mm, with the ability to accommodate custom orders for larger dimensions. All rods are certified to ASTM B348 and ASTM B381 standards.

For those seeking reliable suppliers, Daxun Alloys offers a comprehensive range of Grade 2 Titanium products, including ASTM B348 Titanium Grade 2 Round Bars, UNS R50400 Bright Bars, and WERKSTOFF NR. 3.7035 Round Bars. Whether you need round, forged, or square bars, we ensure consistent quality and competitive pricing.

Feel free to contact Daxun Alloys for inquiries or to request a quote. Our team is committed to providing high-quality Grade 2 Titanium Rods and is happy to assist with any questions or project-specific needs.

続きを読む

データ

仕様 詳細
素材 Titanium rod and bar Grade 2 (UNS R50400)
スタンダード ASMB348、ASMSB348、AMS4921、AMS4902
寸法 EN、ASM、JIS、ASME、BS、AISI
直径範囲 0.125″~14″(3.175mm~355.6mm)、カスタム
長さの範囲 最大240″(6096mm)、カスタム
表面処理 冷間(明るい)引かれた、センターレス地面、熱間圧延された、滑らかな回された、皮をむかれた、切り開かれた圧延された端、熱間圧延されたアニールされた、荒い回された、明るい、ポーランド語、粉砕、センターレス地面及び黒
表面仕上げ 冷間引抜、センタレス研磨、ポリッシュ、ラフ切削、黒色、NO.4仕上げ、BA仕上げ、マット仕上げ等。.
コンディション 焼入れ、焼戻し、アニール
寛容 直径公差:+/- 0.127mm(±0.005)、長さ公差:+/-0.125″(3.175ミリメートル)
様式 チタン角棒、チタンインゴット、チタン丸棒、チタン角棒、チタン三角棒、鍛造チタン棒、チタン六角棒など。.
物理的性質 密度: 0.163 lb/in³ (4.51 g/cm³), 融点: 3,020°F (1,660°C), 伸び: 20-30%, 弾性率: 16.5 x 10⁶ psi (114 GPa)
化学組成 チタン(最小):99.2%、酸素(最大):0.25%、炭素(最大):0.08%、鉄(最大):0.30%、窒素(最大):0.03%、水素(最大):0.015%
エレメント Weight %
C ≤0.08
O ≤0.25
N ≤0.03
H ≤0.015
フェ ≤0.30
*OEE ≤0.10
*OET ≤0.40
ティ Remaining
硬度、ヌープ 170 170
硬度、ロックウェルB 80 80
硬度、ヴィッカース 145 145
引張強さ、極限 344 MPa 49900 psi
引張強さ、降伏点 275 – 410 MPa 39900 – 59500 psi
破断伸び 20 % 20 %
面積の縮小 35 % 35 %
弾性係数 105 GPa 15200 ksi  In Tension
圧縮弾性率 110 GPa 16000キロ・シー
ポアソン比 0.37 0.37
Izod Impact 114 – 171 J 84.1 – 126 ft-lb
Fatigue Strength 300 MPa 43500 psi  1E+7 cycles, Unnotched
Fatigue Strength 425 MPa 61600 psi  30,000 cycles, Unnotched
Fracture Toughness 66 MPa-m½ 60.1 ksi-in½  K(Q); annealed
せん断弾性率 45 GPa 6530キロ・シー
密度 Melting Range Modulus of Elasticity (Tension) Specific Heat Mean Coefficient of Expansion 熱伝導率 電気抵抗率
kg/m3 °C GPa J/kg. °C x10 -6 / °C W / m. °C micro-ohm.m
4,507 1668± 10 103 519 8.41 11.4 0.42
ASTM B348 Alloy Gr 2 Hex Bar Polished grade 2 titanium Hexagonal Bar
ASTM B348 Alloy Gr 2 Rectangular Bar Titanium WERKSTOFF NR. 3.7035 Threaded Bar Black
Titanium UNS R50400 Round Bar grade 2 titanium Din 3.7035 Flat Bar
Titanium Grade 2 Bar Alloy grade 2 titanium Flat Bar Black
Alloy Gr 2 Rounds ASME SB 338 gr 2 Flat Bar Bright
Titanium Alloy Grade 2 Bright Bar Alloy Gr 2 Flat Bar Polished
Alloy grade 2 titanium Hex Bar Annealed Titanium WERKSTOFF NR. 3.7035 Cold Drawn Round Bar
ASTM B348 grade 2 titanium Round Bars Titanium Grade 2 Flat Bar stock
Titanium WERKSTOFF NR. 3.7035 Hex Bar Alloy Gr 2 Threaded Bar
Titanium Grade 2 Square Bar Polished Titanium UNS R50400 Bright Bar Hot Rolled
3.7035 grade 2 titanium Hex Bar Bright Alloy Gr 2 Alloy Hollow Bar
Gr 2 Titanium Rectangular Bar Annealed Alloy grade 2 titanium Polished Hex Bar
ASME SB 338 gr 2 Forged Bar Gr 2 Titanium Polished Bar
Alloy Gr 2 Alloy Rods UNS R50400 Titanium Flat Bar Cold Drawn
Alloy Gr 2 Square Bar Cold Drawn Titanium Grade 2 Bright Bar material
grade 2 titanium Rod Titanium UNS R50400 Flat Bar Annealed

Daxunを選んで、あなたのプロジェクトを成功に導きましょう。.

DAXUN® Grade 2 Titanium Rod Features

DAXUN® Ti Grade 2 is a commercially pure (CP) titanium bar known for its standout features:

  • Excellent general corrosion resistance in seawater
  • Resistant to stress corrosion cracking in chloride and sour gas environments
  • Excellent resistance to pitting, crevice, and erosion-corrosion
  • 高い熱伝達効率
  • Good formability and weldability
  • Extremely low thermal expansion
  • Moderate strength

Daxun Factory Advantages

Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

Grade 2 Titanium Rod Production Method

Daxun specializes in producing high-quality titanium bars known for their exceptional performance. Additionally, we offer customized manufacturing services to meet specific requirements as outlined in the customer’s agreement.

  • Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.

試験報告書

The test reports we provide include: Grade 2 Titanium Rod and Grade 2 Titanium Round Bar Factory Test Certificate, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, NABL Approved Laboratory Report, Destructive Test Report, Non-destructive Testing Report. (Daxun will provide according to customer requirements)

今すぐDaxunに連絡する

Grade 2 Rods Applications and Standards

Grade 2 Titanium Rods are widely used in the following industries under extreme corrosive conditions:

  • Aerospace, military, oil and gas industry, marine engineering, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications: ASTM B861, B862, B338 / ASME SB861, SB862, SB338
  • Standards: ASTM, ASME, EN, JIS, DIN, GB, GJB, API

品質、納期、検査

Daxun ensures the reliability of Grade 2 Titanium Rods and Round Bars through rigorous quality assurance tests. These include tensile testing, chemical analysis, PMI for material consistency, micro and macro testing, IGC testing for corrosion resistance, ultrasonic flaw detection, and hardness and expansion evaluations.

Throughout production, Daxun carefully measures diameter, thickness, and surface quality, guaranteeing materials meet the highest standards and application requirements.

  • 当社の納期は、契約に厳密に従います。.
  • 顧客の第三者機関が工場に検査に行くのをサポートする。
  • 顧客テストのための無料サンプルをサポート
  • 現場検査またはビデオ工場検査をサポート

パッケージング

国際貨物は様々な経路を経て最終目的地に到着するため、梱包は重要な役割を担っています。商品によって、様々な方法で梱包しています。当社では、以下のような様々な方法で商品を梱包しています:
- 箱と木箱
- シュリンクラップ
- 木製パレット
- 木製ボックス

テクニカルサポート

If you require additional technical assistance, our resident metallurgist and knowledgeable staff are ready to support you. At Daxun, we take pride in our certified testing laboratory, a first in the multi-metal and plastic inventory industry. This reflects our unwavering commitment to quality and reinforces our philosophy as a full-service supplier dedicated to meeting your needs.

Grade 2 bar and rod features

高強度
耐食性
耐熱性
低温耐性
環境保護
軽量

Daxun Grade 2 Titanium Rods help your brand improve quickly

Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of rod/bar, Bar and Tube.
製品/加工基準 グレード/サイズ
Titanium rod/bar— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1,GR2,GR3,GR4,GR5,GR7,GR9,GR12,GR16,GR17,GR23,Ti-6Al-4V ELI,Ti-6-2-4-2,Ti-15-3-3(厚さ:( 0.0197”-6”)最大幅:12フィート,最大長:50フィート)
AMS-T-9046
Titanium and Titanium alloy rod/bar
商業用純チタン(CP)
コード指定 降伏強度
最小値、ksi 1
CP-1 70
CP-2 55
CP-3 40
CP-4 25
アルファチタン合金(A)
コード指定 構成
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI)2・・・。
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
α-βチタン合金(AB)
コード指定 構成
AB-1 6A1-4V
AB-2 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
ベータチタン合金(B)
コード指定 構成
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
処理:
熱間圧延 冷間圧延
利用可能なグレード
CPグレード1 グレード 6Al-2Sn-4Zr-2Mo (6-2-4-2)
CPグレード2 グレード6Al-4V ELI(旧グレード23)
グレード7 グレード 6Al-6V-2Sn (6-62)
19年生 グレード 8Al-1Mo-1V (8-1-1)
グレード 5 (6Al-4V) グレード9(3Al-2.5V)
グレード 6 (5Al-2.5Sn) CPグレード3
申し込み
化学工業 海水の脱塩
石油化学産業 航空宇宙
機械加工分野、自動車分野 携帯電話のコンポーネント分野。.
Titanium Grade 2 Hex Bar Titanium Gr 2 Hex Bar
Grade 2 Titanium Hexagonal Bar
Gr 2 Titanium Alloy Hex Bar
UNS R50400 Titanium Hexagonal Bar
ASTM B348 Grade 2 Titanium Hex Bar
Titanium Alloy Grade 2 Square Bar Titanium Grade 2 Square Bar
Grade 2 Titanium Square Bars
Gr 2Titanium Alloy Square Bar
UNS R50400 Titanium Square Bar
WERKSTOFF NR. 3.7035 Square Bar
ASTM B348 Gr 2 Titanium Square Bars
Titanium Grade 2 Rectangular Bar Titanium Grade 2 Rectangular Bar
Ti. Alloy Gr2 Rectangular Bars
Gr 2 Titanium Alloy Rectangular Bar
UNS R50400 Titanium Rectangular Bars
WERKSTOFF NR. 3.7035 Rectangular Bar
ASTM B348 Gr 2 Titanium Rectangular Bar
Titanium Grade 2 Flat Bars Titanium Grade 2 Flat Bar
Gr 2Titanium Alloy Flat Bars
Titanium Gr 2Flat Bars
UNS R50400 Titanium Flat Bars
WERKSTOFF NR. 3.7035 Flat Bars
ASTM B348 Gr 2 Titanium Flat Bars
Titanium Grade 2 Polished Bar Titanium Grade 2 Polished Bar
Grade 2Titanium Polished Bars
Gr 2Titanium Alloy Polished Bar
UNS R50400 Titanium Polished Bars
WERKSTOFF NR. 3.7035 Polished Bar
ASTM B348 Gr 2 Titanium Polished Bar
Titanium Grade 2 Threaded Bar Titanium Gr 2 Threaded Bar
Grade 2Titanium Threaded Bars
Ti. Alloy Grade 2 Threaded Bar
UNS R50400 Titanium Threaded Bar
WERKSTOFF NR. 3.7035 Threaded Bar
ASTM B348 Gr 2 Titanium Threaded Bar
NOMINAL SIZE h5 h6 h7 h8 h9 H10 H11 h12
DIAMETER mm
~ to 3 +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
over 3 to 6 +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
over 6 to 10 +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
over 10 to 18 +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
over 18 to 30 +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
over 30 to 50 +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
over 50 to 80 +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
over 80 to 120 +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
over 120 to 180 +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
over 180 to 250 +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

参照およびダウンロード可能な情報

チタン棒

Daxun is a trustworthy titanium rod and bar manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium bars are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the Titanium rod have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

Commercially Pure Titanium Rod Grade 2/UNS R50400

What are Grade 2 Titanium rods?

Ti CP Grade 2 has greater tolerated levels of iron and oxygen and is frequently utilized due to its outstanding formability, moderate strength, and superior corrosion resistance. It has a minimum yield strength of 275 Mpa (40 ksi) and relatively low amounts of impurity elements, placing it in the strength range of Grades 1 to 3.

Grade 2 Titanium Rod Equivalent Grade

nation name usually
Russia VT1-0 (VT1-0) Gorst 19807-91
ドイツ 3.7035 Job Number (3.7035)
Europe Titanium Grade 2 ZH-10204 3.1
日本 Titanium Grade 2 JIS H 4600
People’s Republic of China TA2 GB/T 3621-2007 / GB/T 13810-2007
USA Titanium Grade 2 ASTM B348 / B265 / B337,UNS R50400

耐食性

Commercially pure (CP) titanium offers remarkable resistance to crevice corrosion in salt solutions, outperforming stainless steel. It retains its integrity against crevice corrosion at temperatures under 80 °C (176 °F), regardless of pH levels, even in environments with high chlorine concentrations.

Stress Corrosion Cracking (SCC)
Grade 2 titanium exhibits remarkable resistance to stress corrosion cracking. It performs exceptionally well in hot chloride solutions and is entirely immune to SCC in seawater, making it a dependable material for harsh environments.

Erosion Corrosion
Titanium exhibits exceptional durability in flowing seawater, withstanding velocities as high as 130 ft/sec (40 m/sec) without significant degradation. Even in the presence of abrasive particles like sand, its corrosion resistance remains largely unaffected, highlighting its reliability in demanding environments.

Hydrogen Embrittlement
When exposed to seawater, titanium absorbs minimal hydrogen, even at higher temperatures. However, absorption typically takes place only under certain specific conditions:

  • pH levels below 3 or above 12
  • Temperatures exceeding 80 °C (176 °F)
  • A mechanism for hydrogen generation, such as galvanic coupling or an impressed current.

Bio-Corrosion
Titanium alloys exhibit complete immunity to microbiologically influenced corrosion. However, because they are non-toxic to marine organisms, biofouling can develop in seawater. This can be effectively managed through chlorination or by increasing the flow rate of water through heat exchangers.

Corrosion Fatigue
Unlike many materials, titanium maintains its fatigue performance in seawater. Fatigue endurance limits and crack growth rates are consistent, whether tested in air or seawater, making it a reliable choice for marine applications.

Galvanic Corrosion
Titanium ranks among the noble materials in the galvanic series, positioned near stainless steels, and generally serves as the cathode when paired with other metals. As a result, titanium remains resistant to galvanic corrosion but can increase corrosion in less noble metals. When paired with more noble substances, such as graphite, its passive properties become even stronger.

Fatigue Properties

Grade 2 Titanium Rod maintains its exceptional fatigue properties even in seawater. Its fatigue endurance limits and crack growth rates remain unchanged regardless of whether testing occurs in air or seawater, highlighting its consistent performance under varied conditions.

溶接性

CP2 Grade Titanium Rod is highly weldable when appropriate precautions are observed. Given its reactive nature, an inert gas shield must protect both the outer diameter (OD) and inner diameter (ID) during welding. Additionally, the rod should be completely free of grease or oil to ensure optimal weld integrity.

Grade 2 Titanium Rod is most often welded using either manual or automatic TIG methods, with or without filler wire. A low heat input is advised to limit the size of the heat-affected zone. Post-weld heat treatment is generally not required, simplifying the process while maintaining the rod’s key properties.

This revised version maintains the technical depth and original structure while improving clarity, readability, and flow. Let me know if you’d like further refinements!

Working material: 3.7035 / UNS R50400
Diameter: 3 – 400 mm
Lengths: 2.000 – 4.000 mm
Versions: Rolled, forged, annealed
Surfaces: Turned, peeled, polished
Standards: ASTM B 348, ASME SB 348, DIN 17862, ASTM F 67, NACE MR 0175, ISO 1515156-3, ISO 5832-2

Buy Grade 2 Titanium Rods/Rounds at Daxun

Are you in need of round rod material made from Grade 2 Titanium Alloy Rod-3.7035? At Daxun, we specialize in providing customized titanium rods tailored to your project’s specifications. As an experienced supplier, we are committed to supporting your needs with precision and reliability.

Our Grade 2 Titanium bars are available in diameters ranging from 2.0 mm to 400 mm. Tolerances and execution may vary based on the size of the bar. Smaller diameters are provided centerless ground with h7 tolerances, while larger sizes come with h9 or h11 tolerances. Contact Daxun to discuss your requirements or to request a customized project quote.

Buy Grade 2 Titanium Bars: Features and Specifications.

  • Forged bars can be peeled or pre-machined. The material is available in a variety of specifications depending on the application and market needs.
  • Our titanium bars typically meet various requirements and certifications, including ASTM B348 and ASTM F 67, DIN 17860, VD TÜV Table 230-3, and Nace MR 0175.
  • Titanium round bars are often used where they have excellent corrosion resistance and good mechanical properties.
  • Grade 2 titanium bars (3,7035) are therefore suitable for use as a construction material for equipment and devices, as they are easy to process.

Our Titanium Bar Material Services

  • As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.
  • We will be happy to provide you with a consultation and explain everything you need to know about obtaining titanium bar material, including which standards require greater attention for the components to be manufactured.
  • If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.
  • Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about the Grade 2 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.

ご注文について

When placing a purchase order, make sure to include the quantity, grade, type or category, API5L reference, as well as the thickness, width, and length of the product. If you have any specific requirements, like chemical composition, mechanical properties, heat treatment, additional testing, manufacturing methods, surface coatings, or end finishes, let us know so we can meet your needs.

Feel free to contact Daxun with your order details. We are committed to responding to your inquiry promptly.

どのグレードのチタンが最適ですか?

必要なチタン合金のグレードは、取り組んでいるプロジェクトによって異なります。各グレードには異なる利点があるためです。

すべてのグレードのチタン合金は極めて強靭で耐食性に優れており、過酷な環境下でも良好な性能を維持し続けます。

チタン合金の高グレード品(5~12)は、特定の利点を目的として設計された合金である。例えば、グレード12チタン合金は優れた耐熱性を有し、シェルアンドチューブ式熱交換器、油圧配管、化学工業用機器に最適な選択肢となる。

グレード1~4は純チタン合金であり、配管システムやチューブ用に溶接可能で延性のある材料が必要な場合に最適な選択肢です。低グレード品は船舶産業や工業分野で使用されています。

プロジェクトを開始するにあたり、どのグレードのチタン合金が最適かお悩みでしたら、ぜひ当社までご連絡ください。喜んでご支援いたします。

高品位チタンと低品位チタンはどのように異なるのですか?

大迅では、グレード1からグレード12まで幅広いチタン合金グレードを提供しています。

グレード1~4は純チタンであり、それより上のグレードは合金である。

合金グレードは、高い強度重量比で人気がある。

最も一般的に使用されるチタン合金グレードはグレード5です。チタン含有量は依然として高いものの、このグレードは600°F(約315℃)までの高温に耐え、過酷な条件にも耐えられるため、最も信頼性の高いグレードの一つです。

航空宇宙産業や海洋産業などの業界では、耐摩耗性と耐食性に優れていることから、より高品位のグレードが好まれている。

逆に、低品位の鋼材は強度が低いため、主に溶接用として使用される。

各種チタン合金のグレードの違いについて詳しく知りたい方は、本日+86 13382898899までお電話ください。専門家が直接ご説明いたします。

チタンのグレードはコストに影響しますか?

チタンのグレードはコストをわずかに増加させますが、総コストは主に必要なチタンの形状と形態によって決定されます。

At DAXUN, we offer a wide range of titanium products, including rod/bars, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

残念ながら、プロジェクトの詳細やチタニウムの使用目的がわからないと、オンラインで価格をお見積もりするのは難しいです。

幸いなことに、当社の専門家チームが常に皆様のチタンに関するご要望にお応えし、アドバイスを提供いたします。[email protected] までメールをお送りいただければ、アドバイスと正確な見積もりをご案内いたします。

ご要望のチタニウムのグレード、形状、数量について、可能な限り詳細な情報をご提供ください。これにより、お客様のニーズをより正確に把握できます。

チタンのグレードについて、どこで詳しく学べますか?

DAXUNのチームは経験豊富で知識が深く、親しみやすいです。業界での長年の経験から、チタンの用途、利点、グレードに至るまで、あらゆることを熟知しています。

チタニウムの最新情報、用途、および産業分野における応用事例については、当社のブログをぜひご覧ください。専門家による分かりやすいガイドを掲載しており、疑問が生じた際にはいつでもご参照いただけます。

もし問題が解決しない場合は、お気軽にお問い合わせください。喜んでお手伝いいたします。

[email protected] 宛にメールをお送りいただければ、迅速なご返答を差し上げます。お問い合わせの際は、可能な限り詳細な情報をご記載ください。そうすることで、適切な解決策をご提案できます。

早急に見積もりを取る、あるいはマーケット情報を理解するには?

お問い合わせ “ページのフォームにご記入いただくか、”+86 13382898899 “までお電話ください。WhatsAppはオンライン、Eメール([email protected])は6時間以内に確認いたします。すべてのお問い合わせやメッセージに迅速に対応させていただきます。また、毎週お客様と市場情報を共有しています。

サンプルをいただけますか?

We can provide Titanium rod. samples for you to check the quality. Sample is free and you just pay the freight.

すでに輸出した国は?

カナダ、チリ、クウェート、ドイツ、韓国、サウジアラビア、シンガポールなど42カ国以上に輸出しています。.

MOQはいくらですか?

Our MOQ is 1 ton for Titanium rod.

納期はどのくらいですか?

トライアル・オーダーは1週間以内にお届けできます。通常のご注文の場合、おおよそ2週間かかります。.

お問い合わせ
クイック見積もり