| Produktparameter: Edelstahlblech/-platte | |||
| Klasse | 201,304,304L,316,316L,317,321,309,310S,2205,2507,904L,409,410,420,430,436,444,441,17-4 etc. | ||
| Breite | 10mm~2500mm | ||
| Dicke | 0.2mm~100mm | Thickness tolerance | +/-0.03mm |
| Standard | ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2 | ||
| Oberfläche | 2B,BA,8K,NO.1,NO.4,NO.3,hairline,checkered,gold ,black ,rose gold,etc | ||
| Spezifikation | 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L | ||
| Mühlenursprung | TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc. | ||
| Zertifizierung | ISO, SGS, BV, TUV,CE etc | ||
Eine breite Palette an Stahlsorten
Daxun Alloy bietet eine breite Palette an Edelstahlblechen an.
Um Ihren Anwendungsanforderungen gerecht zu werden, bieten wir kaltgewalzte und warmgewalzte Produkte (funktionaler Edelstahl) an.
Große Auswahl an Produkten, verschiedene Produktkategorien oder ganze Produktkategorien
Hervorragende Ebenheit und Dickengenauigkeit
Die Produkte von Daixun Alloy zeichnen sich durch eine hervorragende Ebenheit und Dickengenauigkeit aus.
Wir fertigen äußerst gleichmäßige Edelstahlbleche mit ausgezeichneter Formbarkeit und Korrosionsbeständigkeit, die alle auf einem konstanten Qualitätskontrollsystem basieren.
Oberflächenveredelung
Mit modernster automatischer Steuerungstechnik sind wir stets bestrebt, die Präzision in allen Bereichen zu verbessern und Stahl unter idealen Bedingungen zu walzen.
Dadurch weisen alle unsere Edelstahlbleche eine fein bearbeitete Oberfläche auf. Der hervorragende Oberflächenglanz unserer Produkte wird von unseren Kunden sehr geschätzt.
Edelstahlblech ist ein Edelstahlprodukt, das in einer Vielzahl von Legierungen und Oberflächenausführungen erhältlich ist. Daxun liefert Edelstahlblechprodukte nach den genauen Spezifikationen jedes Kunden. Wir stellen Ihnen unser komplettes Sortiment an Daxun-Edelstahlprodukten vor – der Inbegriff von Zuverlässigkeit, Langlebigkeit und hoher Leistung. Wir sind stolz darauf, eine große Auswahl an Güten und Typen anbieten zu können, um den vielfältigen Anforderungen von Industrie- und Bauanwendungen gerecht zu werden. Von austenitischen Serien bis hin zu Spezialkategorien wie ferritischen Serien sind unsere Edelstahlprodukte für ihre hervorragende Leistung und vielfältigen Spezifikationen bekannt. Die austenitische Serie umfasst 201/304/304L/304J1, 321, 316/316L/317L/316Ti, die unterschiedliche Anforderungen an die Dicke erfüllen und verschiedene Oberflächenbehandlungen wie 2B, BA, NO.4, 8K, SB, HL usw., NO. 1 usw. bieten.
Edelstahlblech-Güten und Eigenschaften
Jedes Edelstahlplattenmaterial hat seine eigenen unterschiedlichen Anwendungsszenarien.
201 Edelstahlblech ist kostengünstig und eignet sich für Baumaterialien, Geräte und Maschinengehäuse usw.
Korrosionsbeständig, geeignet für Gebäudedekoration, Lebensmittel und Medizin, Maschinen und Anlagen usw.
Korrosionsbeständig, geeignet für chemische Anlagen, Lebensmittel und Medizin, mechanische Anlagen
Corrosion resistant,Suitable for chemical energy, marine engineering, mechanical equipment
Korrosionsbeständig, geeignet für chemische Energie, Meerestechnik, mechanische Ausrüstung usw.
Korrosionsbeständig, hochtemperaturbeständig, geeignet für chemische Energie, Meerestechnik, mechanische Ausrüstung.
Korrosionsbeständig, hochtemperaturbeständig, geeignet für Kesselanlagen, hitzebeständige Anlagen, mechanische Anlagen.
Hohe Festigkeit, geeignet für die Raffinerieindustrie, die petrochemische Industrie und die Schifffahrtsindustrie.
Edelstahlplattenformtypen
Wenn die von Ihnen benötigte Form hier nicht verfügbar ist, kontaktieren Sie uns bitte.
Die Dicke von Edelstahlplatten variiert je nach Verwendungszweck zwischen 0,3 mm und 50 mm. Sie eignen sich ideal für den Einsatz im Bauwesen, Maschinenbau, für Industrieanlagen und als Dekorationsmaterial.
Wellbleche aus Edelstahl werden häufig in Baumaterialien verwendet, beispielsweise in Dachplatten für Fabrikgebäude. Sie zeichnen sich durch hervorragende Korrosionsbeständigkeit aus, haben eine lange Lebensdauer und sind besonders strapazierfähig.
Polierte Edelstahlplatten können verschiedene Oberflächen verarbeiten, wie z. B. gebürstete Edelstahlplatten, spiegelnde Edelstahlplatten und matte Edelstahlplatten. Eine Vielzahl von Optionen stehen Ihnen zur Auswahl.
Edelstahl-Musterplatten eignen sich für Konstruktionen, rutschfeste Böden, Dekorplatten usw. Sie werden im Warm- und Kaltwalzverfahren hergestellt. Diese Stahlplatten sind auf Anfrage in Naturfarbe erhältlich.
Oberfläche aus Edelstahlblech
Mit unseren zuverlässigen Edelstahlplatten kann die Oberfläche an Ihre Anwendung angepasst werden.
Leistung von Edelstahlblech
Die chemische Zusammensetzung von Edelstahlblechen schützt sie vor Rost. Ihre Korrosionsbeständigkeit wird durch die notwendige Politur noch erhöht, was sie perfekt für Küchengeräte macht.
Da SS-Bleche einen niedrigeren Schmelzpunkt haben, sind keine Spezialwerkzeuge erforderlich. Außerdem sind sie langlebig und strapazierfähig, wodurch Unternehmen Arbeits- und Wartungskosten einsparen können.
Die intelligentere Option: SS-Bleche haben weitaus weniger Nachteile als andere Legierungen. Sie bieten ein hervorragendes Preis-Leistungs-Verhältnis, Wirtschaftlichkeit und Langlebigkeit. SS ist ein leicht zu reinigendes Metallmaterial.
Edelstahlbleche eignen sich hervorragend für verschiedene Anwendungen, beispielsweise für Fertigungszwecke. Sie sind einfach zu verarbeiten und ideal für den massiven industriellen und komplexen Einsatz.
Riesige Auswahl an Materialien
Von Anfang an bieten wir Ihnen eine große Auswahl an Materialien für unsere hochwertigen Edelstahlprodukte. Daxun verfügt über Edelstahlbestände in gängigen Qualitäten und Größen, um schnell auf die Anforderungen unserer Kunden reagieren zu können.
Oberflächenausführungen für Edelstahlbleche
- Gebürstete Oberfläche: Oberflächenausführungen für Edelstahlbleche
- Sandgestrahlt: Die sandgestrahlte Oberfläche ergibt eine perlgestrahlte Blechoberfläche mit einer gleichmäßigen matten Oberfläche.
- Spiegelglanz: Es wird auch als spiegelpolierte Platte bezeichnet. Diese Oberfläche wird hochglänzend und richtungsunabhängig poliert.
- Geätztes Finish: Dieses Finish wird durch elektrochemische Verfahren erzielt. Es handelt sich um ein dauerhaftes Ätzmuster mit hoher Genauigkeit.
- Geprägte Oberfläche: Diese Oberfläche zeichnet sich durch einzigartige und atemberaubende Designs aus, die konkave und konvexe Strukturen bilden.
Strenge Qualitätskontrolle
Daxun schneidet und verarbeitet hochwertigen Edelstahl genau nach Ihren Maßvorgaben. Edelstahlbleche sind vollständig zertifiziert. Als stolzes Mitglied der BSSA und nach ISO 9001 zertifiziert, stammen alle unsere Edelstahlbleche aus zuverlässigen Fabriken und müssen vor der Lieferung an unser Lager unsere strengen Qualitätskontrollverfahren durchlaufen. Wir führen von Anfang bis Ende eine strenge Qualitätskontrolle für jede Produktion durch, um sicherzustellen, dass die erhaltenen Waren Sie voll und ganz zufriedenstellen.
Stainless steel plate processing and customization
We have laser cutting machines, water jet cutting machines, CNC bending machines, CNC shearing machines. We can provide customized processing services for stainless steel plate cutting and bending. You just need to provide us with the drawings and we can customize it according to the size of your stainless steel plate.
Packaging of Stainless Plates
At Daxun, we choose different packaging for different stainless steel products, including: kraft paper, wooden boxes, woven bags, wooden pallets, based on the highest industry standards to ensure that the goods arrive in your hands in good condition.
All our stainless steel materials are certified by different industry standards such as ISO9001:2008, ISO14001:2014, AAA Certification, CQGC Certifications, and more. Our company also have certifications from ISO9001:2015 quality management system.
At Daxun, we have testing laboratory and equipment to ensure that our stainless steel materials are in actual weight and good quality before shipment. Our strict quality control team also performs strict and 100% inspection on all production stages.
Our support and services are not only limited from the beginning of our transactions. Even if you have received your orders, TuoLian will continue to provide excellent after-sales services. We will continue providing assistance and warranty to your orders.
Stainless Steel plate application cases in different industries
Stainless steel plates are widely used in the construction field and can be used for exterior wall decoration, interior decoration, roofing materials, building structures, etc. Stainless steel plates have beautiful appearance and high strength, and can meet the design needs of different buildings.
Stainless steel plates have the advantages of corrosion resistance, no rust, no discoloration, easy removal of attached food, and good high and low temperature mechanical properties. They are widely used in food machinery, such as sanitation systems, fluid pipe troughs, food storage tanks, thermal Exchangers, vacuum vessels, etc.
Stainless steel plates have good strength, toughness and corrosion resistance and are widely used in aircraft structural parts. For example, the wing structure, fuselage supports, seats and other parts are all made of stainless steel.
The manufacturing and maintenance of petroleum refining equipment also uses 321-316L and other brands of medium-thick plates and cold-rolled stainless steel sheets for petrochemical containers (usually 0.3-0.6mm, 1219-1520mm, SUS316, surface condition is NO.2B/2D)
Main application parts: wing skin, wing stringers, upper and lower edge strips of wing spar, web, fuselage stringers, seat rails, keel beam, side frames, fuselage skin, lower fuselage wall panels, Main floor stringers, etc.
Stainless steel plates are widely used in the shipbuilding industry. The stainless steel plates supplied by Daxun are used in the shipbuilding and petroleum industries. They have high strength, good toughness, and are resistant to seawater corrosion, fatigue, and wear resistance.
SS316L is the primary austenitic stainless steel grade used in offshore installations, where it enhances strength at high temperatures and protects structures from severe acidic environments.There are also duplex stainless steels, which offer an excellent combination of mechanical properties and resistance to stress corrosion cracking, making them ideal for offshore applications. UNS S32205 steel is the most commonly used duplex stainless steel grade for offshore installations.
The application of stainless steel in electricity is mainly for the processing and manufacturing of large turbine units in power stations. Stainless steel’s excellent corrosion resistance and high strength make it the preferred material for power generation components.
Our stainless steel plate stock sizes
- Data Sheet
- Tolerances and Delivery State
- Surface finishes
- Production Process
| Thickness (mm) | Width (mm) | Länge (mm) | Kommentar |
| 0.5 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 0.8 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 1.0 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 1.5 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 2.5 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 3.0 | 1000/1219/1500 | 2000/2438/3000 | AAA |
| 5.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 6-8.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 1.0-20.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 20.0-50.0 | 1500/1800/2000 | 3000/6000/8000 | AAA |
| 50.0+ | 1500/1800/2000 | 3000/6000/8000 | AAA |
| Tolerances | |||||
| Tolerance Rank | |||||
| Size | Group 1 | Group 2 | Group 3 | Delivery State | Surface Condition |
| 0.4 | 0.3 ~ 0.32 | 0.33 ~ 0.37 | 0.37 ~ 0.39 | Cold Rolled | 2B 2D BA Hairline No.3 No.4 6K 8K |
| 0.5 | 0.4 ~ 0.42 | 0.43 ~ 0.47 | 0.47 ~ 0.49 | ||
| 0.6 | 0.5 ~ 0.52 | 0.53 ~ 0.56 | 0.57 ~ 0.59 | ||
| 0.7 | 0.6 ~ 0.62 | 0.63 ~ 0.67 | 0.67 ~ 0.69 | ||
| 0.8 | 0.7 ~ 0.72 | 0.73 ~ 0.77 | 0.74 ~ 0.79 | ||
| 0.9 | 0.8 ~ 0.82 | 0.83 ~ 0.87 | 0.87 ~ 0.89 | ||
| 1 | 0.89 ~ 0.9 | 0.91 ~ 0.94 | 0.94 ~ 0.99 | ||
| 1.2 | 1.02 ~ 1.08 | 1.09 ~ 1.15 | 1.16 ~ 1.18 | ||
| 1.5 | 1.32 ~ 1.38 | 1.39 ~ 1.45 | 1.46 ~ 1.48 | ||
| 2 | 1.72 ~ 1.79 | 1.8 ~ 1.86 | 1.87 ~ 1.9 | ||
| 2.5 | 2.23 ~ 2.36 | 2.32 ~ 2.42 | 1.42 ~ 1.47 | ||
| 3 | 2.7 ~ 2.77 | 2.78 ~ 2.82 | 2.85 ~ 2.9 | ||
| 3 | 2.6 ~ 2.75 | 2.75 ~ 2.85 | 2.86 ~ 2.9 | Delivery State | No.1 No.3 No.4 6K 8K Pickled |
| 4 | 3.5 ~ 3.6 | 3.6 ~ 3.75 | 3.76 ~ 3.95 | ||
| 5 | 4.5 ~ 4.6 | 4.6 ~ 4.75 | 4.75 ~ 4.95 | ||
| 6 | 5.4 ~ 5.6 | 5.6 ~ 5.75 | 5.75 ~ 5.85 | ||
| 8 | 7.3 ~ 7.5 | 7.5 ~ 7.65 | 7.65 ~ 7.85 | ||
| 10 | 9.2 ~ 9.3 | 9.3 ~ 9.6 | 9.6 ~ 9.85 | ||
| 12 | 11.1 ~ 11.2 | 11.2 ~ 11.6 | 11.6 ~ 11.85 | ||
| 14 | 13.1 ~ 13.2 | 13.2 ~ 13.6 | 13.6 ~ 13.85 | ||
| Note: 1. If you require different deliver state than the above listed, kindly confirm with us. 2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here. |
|||||
| Finish Designation | Method and degree of finish |
| No.1 | After hot rolling, heat treatment, pickling or other equivalent treatment is applied. |
| No.2D | Annealing and pickling are performed after cold rolling; material is soft with surface of silver-white luster; used for general applications and deep drawing. |
| No.2B | After 2D finish, skin pass rolling is performed to obtain a more suitable luster; the surface becomes very exquisite; used for general applications. |
| No.3 | Intermediate 100-120 grit finish; used for applications in which surface polishing is performed after shaping. |
| No.4 | General 150-180 grit finish; used for restaurants and kitchen equipment and tools. |
| #240 | 240 grit finish; used when a finer finish than No. 4 is required; typically for restaurants and kitchen equipment and tools. |
| #320 | 320 grit finish polished product. |
| HL | This finish is performed by continuous linear polishing using an abrasive of appropriate grain size; mainly used for architectural applications. |
| BA | Achieved by performing bright annealing after cold rolling and then skin pass rolling to obtain even greater reflectance; provides excellent corrosion resistance; used for household appliances, kitchen equipment, and automobiles. |
| 8K | Through multiple grinding, it achieves very high brightness and smoothness, like a mirror. |

Verwandtes Produkt
Daxun-Legierung
Regarding stainless steel plates, we can handle any type of inquiry. Please feel free to ask us. We will make recommendations based on each client’s needs.
Stainless Steel Sheets from Well-Known Suppliers in China.
Buy stainless steel sheets (also known as steel sheets) with various finishes from well-known suppliers in China. You only need to look once for a stainless steel sheet supplier, because Daxun offers free cutting and fast delivery, as fast as 1-2 days.
All stainless steel sheets have a variety of different finishes.
Our stainless steel sheets come in a variety of different beautiful finishes: brushed, 2B smooth, 8K mirror and round polished, etc.
Each of our stainless steel sheet metal products comes with a film covering the final surface. After installation or fabrication, it can be easily torn off to protect the surface of the material from wear and marks. The back part is not filmed.
The most commonly used type of stainless steel is 300 series stainless steel sheet. It has good formability, good corrosion resistance and easy welding.
We can provide you with any size of stainless steel sheet you need.
Our stainless steel sheets are available in three coatings and a wide range of sizes to meet your specific needs. In addition, since we provide free unlimited cutting services, we can easily meet any unique size you may need.
We can meet any size requirement, ranging from 0.3mm to 30mm in thickness, and from 50mm x 50mm to 2500mm x 1250mm in size. In addition, we offer free unlimited cutting with every transaction, using first-class cutting machines to precisely meet your needs.
Buy stainless steel plates by phone or online.
Ordering stainless steel plates has never been easier. Just follow the simple step-by-step instructions on our website. You can also contact our sales team by email at [email protected] or phone +8613382898899. They will be happy to accept your purchase and answer any questions you may have.
We have three shipping methods for you to choose from, including ship, land and air. Daxun hopes to deliver the goods to you quickly and safely every time.
Important Safety Note:
The edges of the metal plates we sell are not polished, ground or finished, so they may be sharp like any other stainless steel plates. We advise customers to handle, install and use these products with care.
Ja, wir verfügen über vollständige Spezifikationen und Lagerbestände und können Ihre Anforderungen schnell erfüllen.
Ja, es kann individuell angepasst werden. Sie können uns kontaktieren und uns die individuellen Spezifikationen und die gewünschte Menge mitteilen.
Unsere Transportmethoden umfassen im Allgemeinen Seetransport, Landtransport und Seetransport. Wir erreichen Sie schnell und sicher.
Da unsere Produktionsmenge hoch ist, sind die Kosten deutlich geringer, sodass der Preis niedrig ist.
Wir können Ihnen Muster aus Edelstahlblech zur Qualitätsprüfung zur Verfügung stellen. Das Muster ist kostenlos, Sie zahlen lediglich die Versandkosten.
Wir legen großen Wert auf Produktqualität und haben verschiedene Qualitätssystemtests bestanden.