Daxun is an excellent manufacturer of grade 12 (Ti-0.3Mo-0.8Ni) titanium rods and bars.
- Titanium bar grade: Grade 12-Ti / UNS R53400
- Titanium bar types: rolled bars, drawn bars, forged titanium bars
- Titanium bar density: The density of grade 12 titanium is 4.51 g/cm³
- Main standards: ASTM ASME GB GJB EN JIS DIN ISO ATP BS, etc.
- High corrosion resistance, excellent weldability, superior strength, lightweight, and outstanding performance in aggressive environments.
The global leader in commercially pure titanium rod manufacturing services
Daxun, specializing in the production of alloy titanium rods for extreme environments—Grade 12 titanium alloy rods.
Grade 12 titanium bar (Ti Grade 12 / UNS R53400) is a nickel-molybdenum-enhanced, commercially pure (CP) titanium alloy specifically engineered for superior corrosion resistance in aggressive environments. It consists of titanium (≥99%) with strategic additions of 0.6–0.9% nickel (Ni) and 0.2–0.4% molybdenum (Mo), which significantly enhances its electrochemical properties. This nickel-molybdenum modification substantially improves resistance to reducing acids (e.g., sulfuric, hydrochloric, phosphoric), chloride solutions (including seawater and brines), and crevice corrosion—conditions where standard CP grades like Grade 2 would exhibit accelerated degradation. While maintaining the inherent advantages of titanium—low density (~4.5 g/cm³), high strength-to-weight ratio, excellent weldability, and biocompatibility—Grade 12 offers enhanced performance at elevated temperatures (up to ~315°C/600°F) and in moderately reducing or acidic environments. Its passive oxide layer, reinforced by the nickel-molybdenum combination, provides exceptional protection against chemical attack, making it one of the most cost-effective corrosion-resistant metallic materials available.
Where is Grade 12 titanium bar used?
Grade 12 titanium bar is widely utilized in chemical processing for essential components such as heat exchangers, piping systems, vessel linings, and agitators handling acids, chlorides, or organic compounds. In marine and offshore applications, it serves in seawater desalination plants, condenser tubing, and offshore platform components exposed to high-salinity conditions. The alloy also performs exceptionally well in oil and gas production equipment, pulp and paper processing machinery, and power generation systems due to its durability and corrosion resistance. Despite its moderate premium over standard grades—justified by its alloying elements—Grade 12 delivers outstanding lifecycle value by reducing maintenance requirements, extending service intervals, and minimizing replacement costs in corrosive service. Its reliability in preventing premature failures ensures operational continuity and cost efficiency in applications ranging from chemical processing plants to marine infrastructure, establishing it as an optimal solution for demanding corrosion challenges where budget constraints exist.
Daxun is your trusted titanium alloy rod production company. Daxun produces all grades of titanium alloys, including commercially pure titanium series CP, titanium alloy series, titanium nickel alloy, etc. They have reliable performance and provide high performance for your critical applications. In various industries and applications, you can rely on Daxun titanium alloy rods for high strength, high temperature and corrosive environments. For decades, Daxun Metals has been committed to producing highly engineered titanium alloy solutions to meet the most severe challenges.
Data
- Parameter
- Ingredient
- Mechanical Properties
- Physical Properties
| Specification | Details |
|---|---|
| Material | Titanium rod and bar Grade 12 (UNS R53400) |
| Standard | ASTM B348, ASTM SB348, AMS 4921, AMS 4902 |
| Dimensions | EN, ASTM, JIS, ASME, BS, AISI, GB, GJB, DIN |
| Diameter Range | 0.125″ – 14″ (3.175mm – 355.6mm), custom |
| Length Range | Up to 240″ (6096mm), custom |
| Finish | Cold (bright) drawn, centerless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centerless Ground & Black |
| Oberfläche | Cold drawn, Centerless Ground, Polished, Or Rough Turned, Black, NO.4 Finish, BA Finish, Matt Finish, etc. |
| Condition | Hardened & tempered, annealed |
| Tolerance | Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm) |
| Form | Titanium square bars, titanium ingots, titanium round bars, rectangular titanium bars, triangular titanium bars, forged titanium bars, titanium hexagonal bars, etc. |
| Element | Minimum (%) |
Maximum (%)
|
| Titanium (Ti) | Balance | Balance |
| Molybdenum (Mo) | 0.25 | 0.4 |
| Nickel (Ni) | 0.6 | 0.9 |
| Iron (Fe) | — | 0.3 |
| Oxygen (O) | — | 0.25 |
| Carbon © | — | 0.08 |
| Nitrogen (N) | — | 0.03 |
| Hydrogen (H) | — | 0.015 |
| Other Elements | — | 0.40 (total) |
| Eigentum | Minimum Requirement | Typical Value | Unit | Test Method |
| Zugfestigkeit | 483 | 520–620 | MPa |
ASTM E8/E8M
|
| Yield Strength (0.2% offset) | 345 | 380–480 | MPa |
ASTM E8/E8M
|
| Elongation | 18 | 22–30 | % |
ASTM E8/E8M
|
| Hardness | ≤ 200 (HV) | 150–180 (HV) | Vickers | ASTM E10 |
| Impact Toughness | Not specified | 40–60 | J | ASTM E23 |
Elevated Temperature Performance
|
Temperature (°C)
|
Zugfestigkeit (MPa) | Yield Strength (MPa) |
Dehnung (%)
|
| 100 | 450–500 | 320–370 | 20–25 |
| 200 | 400–450 | 280–330 | 18–23 |
| 300 | 350–400 | 240–290 | 15–20 |
| Eigentum | Value/Range | Unit |
| Density | 4.48 | g/cm³ |
| Melting Point | 1650 ± 20 | °C |
| Thermal Conductivity | 7.2 (at 25°C) | W/m·K |
| Specific Heat | 560 (at 25°C) | J/kg·K |
| Electrical Resistivity | 1.7 | μΩ·m |
| Magnetic Susceptibility | Paramagnetic | — |
Choose Daxun to help your project take off.
DAXUN® Grade 12 Titanium Rod Features
DAXUN® Ti Grade 5 is a titanium alloy bar (6al-4v) featuring:
- Good hot formability and weldability;
- Tensile strength can reach 1000MPa;
- Dimensional work at high temperature
- Insensitive to seawater or seawater;
- Not affected by various corrosive media;
- High strength and good toughness;
- Resist crack initiation and crack propagation.
Daxun Factory Advantages
Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.
Grade 12 Titanium Rod Production Method
Daxun produces high-quality titanium bars with high performance, and can also manufacture according to customer’s agreement:
- Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.
Test Reports
The test reports we provide include: Grade 2 Titanium Rod and Grade 2 Titanium Round Bar Factory Test Certificate, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, NABL Approved Laboratory Report, Destructive Test Report, Non-destructive Testing Report. (Daxun will provide according to customer requirements)
Grade 12 Rods Applications and Standards
Grade 12 Titanium Rods are widely used in the following industries under extreme corrosive conditions:
- Aerospace, shipbuilding, oil and gas industry, marine engineering, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, military industry, pharmaceutical and food processing equipment, etc.
- Specifications: AMS 4928,AMS 4967,AMS 4965 ,AMS 6931 ,ASTM B 348
- Standards: ASTM, ASME, EN, JIS, DIN, GB, GJB, API
Quality, delivery, inspection
Daxun performs several quality assurance tests, these tests include mechanical tests like area tensile, chemical analysis, material positive identification – PMI test, micro and macro testing, intergranular corrosion (IGC) test, ultrasonic flaw detection test, pitting and resistance test, hardness test, material positive identification, expansion test etc. All these tests ensure that the Grade 2 Titanium Rod and Grade 2 Titanium Round Bar material is suitable for the required application. During the production process, we measure the diameter, thickness and surface of the product.
- Our delivery time is strictly in accordance with the contract.
- Support customer third-party agencies to go to the factory for inspection
- Support free samples for customer testing
- Support on-site or video factory inspection
Verpackung
Daxun Alloy ensures the best quality of packaging as it plays an important role in international freight where goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
• Boxes and crates
• Shrink wrap
• Wooden pallets
• Wooden boxes
Technical Support
If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.
Daxun Grade 12 Titanium Rods help your brand improve quickly
- Tolerances for Grade 12 Titanium Round Bars (BS EN ISO 286-2)
| NOMINAL SIZE | h5 | h6 | h7 | h8 | h9 | H10 | H11 | h12 |
|---|---|---|---|---|---|---|---|---|
| DIAMETER mm | ||||||||
| ~ to 3 | +0.004/0 | +0.006/0 | +0.01/0 | +0.014/0 | +0.025/0 | +0.04/0 | +0.06/0 | +0.1/0 |
| over 3 to 6 | +0.005/0 | +0.008/0 | +0.012/0 | +0.018/0 | +0.03/0 | +0.048/0 | +0.075/0 | +0.12/0 |
| over 6 to 10 | +0.006/0 | +0.009/0 | +0.015/0 | +0.022/0 | +0.036/0 | +0.058/0 | +0.09/0 | +0.15/0 |
| over 10 to 18 | +0.008/0 | +0.011/0 | +0.018/0 | +0.027/0 | +0.043/0 | +0.07/0 | +0.11/0 | +0.18/0 |
| over 18 to 30 | +0.009/0 | +0.013/0 | +0.021/0 | +0.033/0 | +0.052/0 | +0.084/0 | +0.13/0 | +0.21/0 |
| over 30 to 50 | +0.011/0 | +0.016/0 | +0.025/0 | +0.039/0 | +0.062/0 | +0.1/0 | +0.16/0 | +0.25/0 |
| over 50 to 80 | +0.013/0 | +0.019/0 | +0.03/0 | +0.046/0 | +0.074/0 | +0.12/0 | +0.19/0 | +0.3/0 |
| over 80 to 120 | +0.015/0 | +0.022/0 | +0.035/0 | +0.054/0 | +0.087/0 | +0.14/0 | +0.22/0 | +0.35/0 |
| over 120 to 180 | +0.018/0 | +0.025/0 | +0.04/0 | +0.063/0 | +0.1/0 | +0.16/0 | +0.25/0 | +0.4/0 |
| over 180 to 250 | +0.02/0 | +0.029/0 | +0.046/0 | +0.072/0 | +0.115/0 | +0.185/0 | +0.29/0 | +0.46/0 |
Types of Grade 12 Titanium Rods (3)
Titanstab
Recent hot case projects and products
Verwandte Produkte (8)
Daxun has a state-of-the-art production facility in China that produces highly competitive, high-precision Grade 12 titanium bars. Excellent surface, tolerance, straightness and material quality provide you with technological leadership and consistent production processes. These advantages apply to a wide range of diameters and materials. In addition, our comprehensive stock program at our service center enables just-in-time delivery.
SPEZIFIKATIONEN
ASTM B348 – Titanium and Titanium Alloy Bars and Billets
ASTM SB348 – Specification for Titanium and Titanium Alloy Bars and Billets
AMS 4921 – Titanium Alloy Bars, Wire, and Forgings
AMS 4924 – Titanium Alloy Bars and Billets, Grade 12
HEAT TREATMENT
When enhanced corrosion resistance and mechanical properties are required, annealing can be performed at 1,200-1,400°F (649-760°C).
DAXUN Grade 12 alloy can be heat treated in a variety of ways:
- Anneal: 1,200-1,400°F (649-760°C), 1 to 2 hours, air cool
- Stress Relief Anneal: 900-1,100°F (482-593°C), 1 to 4 hours, air cool
HARDNESS
Typical hardness in the annealed condition is Rockwell B 70-80, providing excellent machinability while maintaining superior corrosion resistance.
Forgeability / Formability
Grade 12 titanium alloy bar is forged at 1,650-1,750°F (899-954°C) with a final forging temperature of 1,450°F (788°C). A minimum of 30% reduction is recommended for optimum properties.
Grade 12 alloy bar exhibits good formability in the annealed condition. For severe forming operations such as bending or stretching, these can be performed at temperatures up to 1,200°F (649°C) without affecting mechanical properties. Hot sizing or forming can be accomplished by creep forming in the range of 1,000-1,200°F (538-649°C).
Machinability
Grade 12 titanium alloy bar can be machined using austenitic stainless steel machining methods with slow machining speeds, high feeds, rigid tools, and the use of large amounts of non-chlorinated cutting fluids. The nickel-molybdenum content does not significantly affect machinability compared to other CP titanium grades.
Schweißeignung
Grade 12 titanium rod is readily weldable in the annealed condition. Precautions must be taken to prevent contamination with oxygen, nitrogen, and hydrogen. Fusion welding may be performed in an inert gas filled chamber or with inert gas to weld the molten metal and adjacent heated zones, with a tail shield. The nickel-molybdenum addition enhances weld integrity in corrosive environments.
Special Considerations
Grade 12 titanium alloy rod may be contaminated with hydrogen from improper pickling, and with oxygen, nitrogen, and carbon during forging, heat treating, brazing, etc. This contamination may result in a loss of ductility, which may adversely affect notch sensitivity and forming characteristics. The nickel-molybdenum content provides additional protection against corrosion in contaminated conditions.
Size Range
Grade 12 Titanium Bar Dimensions
Ø 0.7 – 30 mm (drawn, ground)
Ø 16 – 400 mm (hot rolled, peeled)
Tolerances: h11–h5 (ISO 286-2)
Tighter or different tolerances available on request
Lengths up to 9,000 mm long, depending on diameter
For larger diameters, other bar lengths and tolerances can be agreed upon request
Availability Grade 7 Titanium Rods
Processing options include:
- Drawing, straightening
- Drawing, straightening, polishing
- Drawing, grinding, polishing
- Drawing, straightening, grinding, polishing
- Drawing, annealing, straightening
- Drawing, annealing, polishing
- Drawing, annealing, grinding, polishing
- Drawing, annealing, straightening, grinding, polishing
We produce bars according to your requirements.
Excellent surface and straightness, perfect roundness and tightest diameter tolerances (according to ISO 286-2 up to h5). Available in straightened, ground, polished conditions.
Sawing
- Band saws (up to Ø510 mm)
- Bench band saws (up to 6,000 x 3,000 x 400 mm)
- High-performance sawing machines for precise sawing
Titanium Bar End Machining
- Single or double sided
- Chamfer 90° (45°)
- Point 60° (30°)
- Flat end
- Centered
Delivery Form
- ASTM American Society for Testing and Materials Standards
- AMS American Aerospace Materials Standards
- NACE American Association of Corrosion Engineers International Standards
- ASME American Society of Mechanical Engineers Standards
- GB Chinese National Standards
- GJB Chinese National Military Standards
- ISO International Standards
- DIN German Standards
- EN European Standards
- API American Petroleum Institute Standards
Detection Method
Non-destructive testing > 100% testing
Testing methods:
- Eddy current testing / eddy current crack testing
- Defect-free surface (level 4)
- Flat bottom hole diameter 0.7 mm and 0.4 mm
- Blind area can be cut off according to fixed length > Test to the end of the bar
- Full diameter ultrasonic testing
Our Titanium Bar Material Services
As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.
We will be happy to provide you with a consultation and explain everything you need to know about obtaining Grade 7 titanium bar material, including which standards require greater attention for the components to be manufactured.
If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.
Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about Grade 12 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.
Ordering Information
Purchase orders should include quantity, grade, type or category, API5L reference, thickness, width, length, and any applicable attachments or additional requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating or end finish. Contact Daxun now, we will reply to your email as soon as possible.
Die von Ihnen benötigte Titanlegierung hängt von Ihrem Projekt ab, da jede Legierung unterschiedliche Vorteile bietet.
All grades of titanium alloy are extremely strong and corrosion resistant, which means they will continue to work well in the harshest conditions.
The higher grades of titanium alloy (5-12) are alloys designed for specific benefits. For example, grade 12 titanium alloy has excellent heat resistance, making it a perfect choice for shell and tube heat exchangers, hydraulic piping, and chemical industry equipment.
Grades 1-4 are pure titanium alloys, and they are a perfect choice if you need a weldable, ductile material for piping systems and tubing. You will find lower grades used in the marine and industrial industries.
If you are starting a project and are unsure which grade of titanium alloy is best for you, contact us today; we are more than happy to help you.
At DAXUN, we offer a wide range of titanium alloy grades from grade 1 to grade 12.
Grades 1-4 are pure titanium, while higher grades are alloys.
Alloy grades are popular for their high strength-to-weight ratio.
The most commonly used titanium alloy grade we find is grade 5. While still high in titanium, this grade is one of the most reliable because it can withstand temperatures up to 600°F and withstand extreme conditions.
Höhere Güteklassen werden aufgrund ihrer Verschleiß- und Korrosionsbeständigkeit von Branchen wie der Luft- und Raumfahrtindustrie und der Schifffahrtsindustrie bevorzugt.
Conversely, lower grades are primarily used for welding due to their lower strength.
To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.
While the grade of titanium does increase the cost slightly, the total cost is primarily determined by the shape and form of titanium you require.
At DAXUN, we offer a wide range of titanium products, including plates, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.
Unfortunately, it is difficult to come up with a price online without knowing much about your project and what the titanium will be used for.
Fortunately, our team of experts are always here to help and advise you on your titanium needs. By sending an email to [email protected], we will be able to get back to you with some advice and an accurate quote.
Make sure to include as much information as possible about the grade, shape and quantity of titanium you require to get a better understanding of your needs.
Das Team von DAXUN ist erfahren, kompetent und freundlich. Dank ihrer langjährigen Erfahrung in der Branche wissen sie alles über Titan, einschließlich seiner Verwendungsmöglichkeiten, Vorteile und Güteklassen.
For regular updates on titanium, its uses, and its applications across industries, be sure to check out our blog. Our experts have written easy-to-follow guides that you can always refer to when you have questions.
If you’re still having trouble, feel free to contact us; we’ll be happy to help.
By sending an email to [email protected], you’ll receive a quick response. Make sure to include as much detail as possible in your question so we can recommend a suitable solution.
Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email ([email protected]) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week
We can provide titanium rod samples for you to check the quality. Sample is free and you just pay the freight.
We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.
Our MOQ is 300 Kg for titanium rod.
Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.