CP Grade 3 Titanium Pipe Manufacturer

As a leading supplier of titanium and titanium alloy tubes in China, Daxun provides high-performance titanium tubes to the world.
  • Titanium tube Grade:R50550 / CP TI50A
  • Titanium tube types:Seamless Ti tube, Ti welded tube, forged Ti tube
  • Standards:ASTM B338
  • Softest Ti,High ductility, Very corrosion resistant, good cold formability

————Daxun produces titanium tubes in China to meet the diverse and ——demanding needs of customers!

CP Grade 3 Titanium Pipe Manufacturer

CP Grade 3 titanium pipe is a commercially pure titanium product known for its balanced combination of moderate strength and excellent corrosion resistance. With titanium content of approximately 99.1% and controlled oxygen levels between 0.10-0.27%, Grade 3 offers higher mechanical properties than Grades 1 and 2. This specific oxygen content is the key differentiator, providing increased strength while retaining the inherent corrosion resistance of pure titanium.

In terms of mechanical performance, CP Grade 3 features a tensile strength around 450-485 MPa and a yield strength of 380-415 MPa, all while maintaining good ductility with 20-30% elongation. This makes it stronger than Grade 1 and Grade 2 but less strong than Grade 4 or titanium alloys like Grade 5, positioning it as a versatile “middle-strength” option within the commercially pure titanium series.

Applications of CP Grade 3 titanium

CP Grade 3 titanium pipes find extensive applications across various industries due to their excellent corrosion resistance and moderate strength. In the chemical processing industry, they are widely used for heat exchangers, condensers, and piping systems that handle corrosive chemicals and chlorides. The marine sector relies on these pipes for seawater cooling systems, desalination plants, and offshore platform components where resistance to saltwater corrosion is critical.

The oil and gas industry utilizes CP Grade 3 pipes for downhole tubing and surface equipment exposed to harsh environments. In power generation, particularly in geothermal and coastal plants, these pipes serve in condensers and heat transfer systems. The aerospace industry employs them for hydraulic systems and fuel lines where weight savings and corrosion resistance are priorities.

Medical applications include surgical implants and medical devices that benefit from titanium’s biocompatibility. Additionally, the food processing and pharmaceutical industries use CP Grade 3 pipes for equipment requiring sanitary conditions and resistance to cleaning chemicals. Their combination of weldability, formability, and durability makes them suitable for custom fabrication across these diverse applications.

Comparison of Grade 3 titanium pipes with other pure titanium grades

CP Grade 3 titanium pipe sits in a practical middle ground within the commercially pure titanium series. Think of it as a balance between strength and formability.

Grade 1 is the softest and most easily formed, perfect for complex deep-drawing applications, but it has the lowest strength. Grade 2 is the workhorse of the titanium industry—it’s slightly stronger than Grade 1 while still offering excellent corrosion resistance and weldability, which is why it’s the most commonly used grade.

This is where CP Grade 3 comes in. With a higher oxygen content, it provides significantly more strength than Grade 2, making it suitable for pressure vessels and piping systems where Grade 2 might not be robust enough. However, this extra strength means it’s slightly less formable than the lower grades.

Grade 4 is the strongest of all the commercially pure grades, but it sacrifices much of the ductility that makes the other grades easy to work with.

For most piping applications, the choice often comes down to Grade 2 versus Grade 3. If your project demands higher pressure ratings and mechanical strength, Grade 3 is the superior choice. If you need maximum formability for complex shapes, Grade 2 might be more suitable. Essentially, you choose Grade 3 when strength is a higher priority than ease of fabrication.

Weiterlesen

Data

Element Content (%)
Titanium (Ti)
Balance (~99.1%)
Oxygen (O) 0.10 – 0.27
Iron (Fe) ≤ 0.30
Carbon © ≤ 0.10
Nitrogen (N) ≤ 0.05
Hydrogen (H) ≤ 0.015
Eigentum Wert
Density ~4.51 g/cm³
Melting Point
~1660–1670 °C
Modulus of Elasticity
~103–107 GPa
Thermal Conductivity
~21.9 W/m·K (at 25°C)
Electrical Resistivity ~420 nΩ·m
Eigentum Wert
Zugfestigkeit
~450–485 MPa
Yield Strength
~380–415 MPa
Elongation ~20–30%
Härte (Brinell)
~200–240 HB

Choose Daxun to help your project take off.

Contact Daxun now

Advanced Production:Titanium seamless pipe

  • CP Grade 3 titanium pipes are typically manufactured according to major international standards such as ASTM B338, ASME SB338, ASTM B861 (for seamless pipes), and ASTM B862 (for welded pipes). They are readily available in a variety of sizes, with diameters ranging from 3.35mm to 152mm and wall thicknesses from 0.020″ to 0.220″, accommodating diverse project requirements.
Contact Daxun now

CP Grade 3 Titanium Tube Features

  • Balanced Properties: As a commercially pure titanium, it offers a great balance of moderate strength and excellent corrosion resistance, stronger than Grade 1 and 2.
  • Superior Corrosion Resistance: Exceptionally resistant to chloride and seawater environments, making it ideal for marine and chemical processing applications.
  • Good Fabricability: It is well-suited for forming, welding, and machining, allowing for easy manufacturing of complex components.
  • Biocompatible: Safe for use in medical implants and food processing equipment due to its non-toxic and hypoallergenic nature.
  • Cost-Effective: Provides better performance than lower grades without the high cost of titanium alloys, offering a practical solution for many industrial uses.
Contact Daxun now

Advanced Production: Titanium Welded Tube

Titanium Welded Tube: Diameter ranges from 6.0mm to 1219mm, wall thickness ranges from 0.3mm to 30mm (depending on diameter), length up to 25000mm, made from Gr1 titanium tube. Welded tubes are made from flat rolled billets (tube blanks) on electric tube welding machines using automatic tungsten inert gas (argon) welding, and heat treated on the mill line. Mechanical tests, geometric measurements, 100% ultrasonic and eddy current testing, pneumatic or hydrostatic testing are performed before the finished titanium welded tubes are packaged according to customer specifications. Manufacturing technology as well as inspection and testing equipment ensure that thin wall welded tubes meet ASTM B 338 and ASME SB 338 specifications.

Contact Daxun now

Test Reports

The test reports we provide include: Factory test certificate for CP Grade 3 titanium welded pipe and CP Grade 3 titanium seamless pipe, EN 10204 3.1, Chemical report, Mechanical report, PMI test report, Visual inspection report, Third-party inspection report, NABL approved laboratory report, Destructive test report, Non-destructive test report. (Daxun will provide according to customer’s requirements)

Contact Daxun now

Applications and standards

CP Grade 3 Pipes and Tubing are extensively applied in extremely corrosive conditions in the below Industries:

  • Chemical processing parts such as heat exchangers, reaction vessels, evaporators and delivery pipelines, automotive exhaust, oil and gas industry, petrochemical plants, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications : ASTM B861, B862, B338 / ASME SB861, SB862, SB338
    Standard : ASTM, ASME and API
Contact Daxun now

Quality, delivery, inspection

Daxun performs several quality assurance tests, these tests include flattening test, flaring test, ultrasonic flaw detection test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the Titanium Welded Pipe and  Titanium Seamless Pipe materials are suitable for the required application. During the production process, we measure the diameter, thickness and surface of the products. Our standard delivery time is 5-7 days and the delivery time for special size products is 15-20 days.

  • Our delivery time is strictly in accordance with the contract.
  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples for customer testing
  • Support on-site or video factory inspection
Contact Daxun now

Verpackung

Daxun Alloy ensures the best quality of packaging as it plays an important role in international freight where goods go through various channels to reach the final destination, so we pay special attention to packaging. We pack our goods in many ways depending on the product. We pack our products in many ways such as:
• Boxes and crates
• Shrink wrap
• Wooden pallets
• Wooden boxes

Contact Daxun now

Technical Support

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Daxun CP Grade 3 Titanium TUBE Let your brand improve rapidly

CP Grade 3 titanium tube form (4)

  • Titanium seamless tubes are made by piercing and drawing solid titanium bars, and the hollow part of the tube is made by piercing or hot extrusion. Titanium seamless tubes are ideal for very large diameter to wall thickness ratios and have very good external dimensional tolerances.

  • Titanium welded pipe is a tubular product made of strip titanium that is roll formed and fusion welded along the longitudinal seam. The welding process used by Daxun Alloy does not use any filler metal during the welding process.

  • Titanium square tubes are drawn from round tubes or round tube billets and can be formed into right angles or rounded corners. They can also be cold extruded, which is efficient and low cost. The only disadvantage is that the tolerance will gradually increase.

  • Tubular products are welded and then re-drawn to final size. Welding and drawing is ideal for producing thick walled, large diameter tubes that cannot be welded directly to size but still offer cost savings over seamless tubes. All Daxun welded and drawn tubes are bright annealed.

Recent hot case projects and products

CP Grade 3 Titanium pipe and tube
CP Grade 3 Titanium pipe and tube
Titanium Titanium pipe and tube
Rohre und Schläuche aus Titan
Titanium Titanium pipe and tube
Titanium Titanium pipe and tube
What is the main difference between CP Grade 3 and CP Grade 2 titanium pipe?

The primary difference is the oxygen content, which directly impacts strength. CP Grade 3 has a higher oxygen content (0.10-0.27%) than Grade 2, giving it approximately 20-30% higher tensile and yield strength. This makes Grade 3 suitable for applications requiring more robust pressure handling and mechanical performance, while Grade 2 is often chosen for its superior formability.

Is CP Grade 3 titanium pipe weldable?

Yes, CP Grade 3 has excellent weldability using standard titanium welding procedures, most commonly TIG (GTAW) and MIG (GMAW) welding. It requires proper inert gas shielding (argon or helium) to prevent contamination of the weld pool, but it can be reliably welded to itself or other CP titanium grades.

When should I choose CP Grade 3 over a titanium alloy like Grade 5 (Ti-6Al-4V)?

You should choose CP Grade 3 when excellent corrosion resistance is your primary concern and the mechanical demands are moderate. Titanium alloys like Grade 5 offer much higher strength and are better for high-stress structural applications. CP Grade 3 is more cost-effective than titanium alloys and provides superior corrosion resistance in many environments, making it the ideal choice for piping, heat exchangers, and chemical processing equipment.

How does CP Grade 3 titanium compare to 316L stainless steel?

CP Grade 3 offers vastly superior corrosion resistance, especially in chloride environments like seawater, where 316L is prone to pitting and crevice corrosion. Titanium is also about 40% lighter than steel and has a much longer service life in aggressive environments. However, 316L has a lower initial material cost. The choice depends on whether long-term durability and corrosion resistance outweigh upfront cost.

Does the grade of titanium affect the cost?

While the grade of titanium does increase the cost slightly, the total cost is primarily determined by the shape and form of titanium you require.

At DAXUN, we offer a wide range of titanium products, including tubes, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

Unfortunately, it is difficult to come up with a price online without knowing much about your project and what the titanium will be used for.

Fortunately, our team of experts are always here to help and advise you on your titanium needs. By sending an email to [email protected], we will be able to get back to you with some advice and an accurate quote.

Make sure to include as much information as possible about the grade, shape and quantity of titanium you require to get a better understanding of your needs.

How to get a quote OR understand the market information ASAP?

Please fill in the form on the “Contact Us” page, or call our sales manager at “+86 13382898899”, we will contact you as soon as possible. Our WhatsApp is online, and email ([email protected]) will be checked within 6 hours. Every inquiry or message will be responded to promptly. In addition, we share market information with our customers every week

Kann ich ein paar Muster bekommen?

Wir können Ihnen Muster aus Edelstahlblech zur Qualitätsprüfung zur Verfügung stellen. Das Muster ist kostenlos, Sie zahlen lediglich die Versandkosten.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.

Senden Sie Ihre Anfrage noch heute
Schnelles Angebot