x
Senden Sie Ihre Anfrage noch heute
Schnelles Angebot

Daxun is a 17-4 stainless steel sheet supplier in China

As China’s leading stainless steel plate supplier and exporter, Daxun provides 17-4 stainless steel plates to the world.
  • Grade: AISI 17-4PH-630-Precipitation Hardening Steel
  • Manufacturing: cold-rolled plate, hot-rolled plate, forged plate
  • Standard: ASTM, ASME, GB, DIN, JIS, ISO, EN, BS
  • Type: cold-rolled thin plate, hot-rolled thick plate
  • Surface: 2B, NO.1, NO.4, HL, BA, 8K, etc.
  • Length: 2438mm3048mm6000mm can be customized
  • Origin: TISCO, Baosteel, Pohang, Tsingshan, Delong

17-4PH Global leader in stainless steel sheet fabrication services

Type 17-4 PH stainless steel plate is the most widely used of all precipitation hardening stainless steels. Its valuable combination of properties gives designers the opportunity to improve the reliability of their products while simplifying the manufacturing process and reducing costs. Type 17-4 PH is a martensitic precipitation hardening stainless steel that offers exceptional high strength, good corrosion resistance, and good mechanical properties at temperatures up to 600°F (316°C). Its unique combination of properties makes this alloy an effective solution to many design and production problems. Contact Daxun today

17-4PH stainless steel, otherwise known as SAE Type 630, is frequently used with operations demanding high tensile strength and a middling level of corrosion resistance. 17-4 PH is the most-used grade of martensitic precipitation hardenable alloys and is regarded as the most broadly formed precipitation hardening grade. Its intense tensile strength keeps its ductility and hardness at high temperatures while still demonstrating exceptional corrosion resistance in all conditions.Contact Daxun now to obtain the latest technical documents and information.

Weiterlesen

Technical Data

Product Parameters: 17-4PH  Stainless Steel Sheet/Plate
Breite 10mm~2500mm
Dicke 0.2mm~100mm Thickness tolerance +/-0.03mm
Standard ASTM/ASME 240/480,JIS 4305,DIN EN 10088-2
Oberfläche 2B,BA,8K,NO.1,NO.4,NO.3,hairline,checkered,gold ,black ,rose gold,etc
Spezifikation 1000*2000/L,1219*2438/L,1250*2500/L,1500*3000/L1500*6000/L,1800*6000/L,2000*6000/L2200*6000L
 Mühlenursprung TISCO, ZPSS, BAOSTEEL, JISCO, ZSESS, ATI, SMC, HAYNES, VDM, ArcelorMittal, Outokumpu, etc.
Zertifizierung ISO, SGS, BV, TUV,CE etc
Carbon 0.07% (Max)
Silicon 1.00% (Max)
Manganese 1.00% (Max)
Phosphorous 0.040% (Max)
Sulfur 0.030% (Max)
Chromium 15%-17.5%
Molybdenum 0.50% (Max)
Nickel 3%-5%
Copper 3%-5%
Material Type Condition Ultimate Tensile Strength (PSI) 0.2% Yield Strength (PSI) Elongation (% In 2in.) Reduction Of Area (%) Hardness Brinell Hardness Rockwell
17-4 PH H900 190,000 170,000 10 40 388 C40
H1025 155,000 145,000 12 45 331 C35
H1075 145,000 125,000 13 45 311 C32
H1150 135,000 105,000 16 50 277 C28
H1150-M 115,000 75,000 18 55 255 C24
H1150-D 125,000 105,000 16 50 255 min – 311 max C24 – 33
Heat Treated Condition H900
Density, lbs/in3 0.282
Electrical Resistivity, microhm-cm 77
Specific Heat, BTU/lb/°F (32-212°F) 0.1
Thermal Conductivity, BTU/hr/ft2/in/°F
300°F 124
500°F 135
860°F 156
900°F 157
Mean Coefficient of Thermal Expansion, in/in/°F
-100 to 70°F 5.8 x 10^-6
70 – 200°F 6.0 x 10^-6
70 – 400°F 6.0 x 10^-6
70 – 600°F 6.3 x 10^-6
70 – 800°F 6.5 x 10^-6
70 – 900°F
Modulus of Elasticity, ksi 28.5 x 10^3
Modulus of Rigidity, ksi 11.2 x 10^3
Poisson’s Ratio (all conditions) 0.272
Klasse UNS Industry Specifications
17-4 Duplex Stainless Steel UNS 17-4PH UNS: S17400
• AMS: 5604
• ASTM: A693
• ASME: SA693
• W. Nr./EN: 1.4548
UNS 630 UNS: S17400
• AMS: 5604
• ASTM: A693
• ASME: SA693
• W. Nr./EN: 1.4548

Choose Daxun and make your customers satisfied.

Contact Daxun now

Fast delivery

We provide timely and fast delivery of stainless steel products for customers with urgent needs. Behind the speed is the system support from information flow to logistics and capital flow. For example, in terms of information flow, Daxun’s order data is pushed to the logistics system in real time, and the data is seamlessly connected; in terms of logistics, the processing center is close to highways and rivers and seas, with reasonable scheduling, rapid response, storage and transportation linkage, and efficient loading, ensuring that the task is completed on schedule.

Contact Daxun now

17-4PH stainless steel plate advantages:

• Excellent corrosion resistance
• Provides toughness to both the base metal and the weld.
• Ideal for applications that require ease of fabrication, then increased strength/hardness for increased reliability
• The physical properties of 17-4 PH stainless steel plate are dependent on any tempering process performed on the material. If your application requires specific physical properties, please contact a DAHSUN sales representative to ensure this material meets your needs.

Contact Daxun now

Stainless Steel 17-4PH Applications

• Aerospace applications
• Chemical processing equipment
• Oil and petroleum refining equipment
• Food processing equipment
• General metalworking
• Base plates
• Nuclear components
• Food grade stainless steel for processing equipment
• General metalworking applications that call for precipitation-hardening
stainless steel

Contact Daxun now

Quality, delivery, inspection

  • Daxun also conducts several quality assurance tests. These tests include flattening test, pitting and resistance test, mechanical test, hardness test, material positive identification, expansion test, etc. All these tests ensure that the material is suitable for the required application.
  • During the production process, we measure the diameter, thickness, and surface of the product. Our standard delivery time is 7-15 days, except for some special size products, our delivery time will increase to 20 days.
    Our delivery time is strictly in accordance with the contract.
  • Support customer third-party agencies to go to the factory for inspection
  • Support free samples to customers for testing
  • Support on-site or video factory inspection
Contact Daxun now

Technical Support

If you need any additional technical assistance, our resident metallurgist and knowledgeable staff will be pleased to help. Additionally, Daxun boasts a certified testing laboratory—a first in the multi-metal and plastic inventory industry. This, in our opinion, demonstrates our unwavering dedication to quality and our philosophy as a full-service supplier.

Contact Daxun now

Ordering Information

The purchase order shall include quantity, PSL grade, type or category, API5L reference, diameter, finish, length and any applicable attachments or additional requirements relating to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface finish or end finish. Bars are solution bright annealed.

17-4PH plate stainless steel Features

High strength
Corrosion resistance
Heat resistance
Low temperature resistance
Environmental protection
Welding performance

Daxun Let your brand improve rapidly

Tolerance for 2B Sheet
Size Tolerance Rank
Group 1 Group 2 Group 3
0.4 0.3 ~ 0.32 0.33 ~ 0.37 0.37 ~ 0.39
0.5 0.4 ~ 0.42 0.43 ~ 0.47 0.47 ~ 0.49
0.6 0.5 ~ 0.52 0.53 ~ 0.56 0.57 ~ 0.59
0.7 0.6 ~ 0.62 0.63 ~ 0.67 0.67 ~ 0.69
0.8 0.7 ~ 0.72 0.73 ~ 0.77 0.74 ~ 0.79
0.9 0.8 ~ 0.82 0.83 ~ 0.87 0.87 ~ 0.89
1 0.89 ~ 0.9 0.91 ~ 0.94 0.94 ~ 0.99
1.2 1.02 ~ 1.08 1.09 ~ 1.15 1.16 ~ 1.18
1.5 1.32 ~ 1.38 1.39 ~ 1.45 1.46 ~ 1.48
2 1.72 ~ 1.79 1.8 ~ 1.86 1.87 ~ 1.9
2.5 2.23 ~ 2.36 2.32 ~ 2.42 1.42 ~ 1.47
3 2.7 ~ 2.77 2.78 ~ 2.82 2.85 ~ 2.9
Tolerance for No.1 Hot Rolled Plate
Size Tolerance Rank
Group 1 Group 2 Group 3
3 2.6 ~ 2.75 2.75 ~ 2.85 2.86 ~ 2.9
4 3.5 ~ 3.6 3.6 ~ 3.75 3.76 ~ 3.95
5 4.5 ~ 4.6 4.6 ~ 4.75 4.75 ~ 4.95
6 5.4 ~ 5.6 5.6 ~ 5.75 5.75 ~ 5.85
8 7.3 ~ 7.5 7.5 ~ 7.65 7.65 ~ 7.85
10 9.2 ~ 9.3 9.3 ~ 9.6 9.6 ~ 9.85
12 11.1 ~ 11.2 11.2 ~ 11.6 11.6 ~ 11.85
14 13.1 ~ 13.2 13.2 ~ 13.6 13.6 ~ 13.85
16 15.2~ 15.5 15.5~ 15.7 15.7~ 16.1
18 17.2~ 17.5 17.5~ 17.7 17.7~ 18.1
20 19.2~ 19.5 19.5~ 19.7 19.7~ 20.1
30 29.2~ 29.5 29.5~ 29.7 29.7-30.1
40 39.2~ 39.5 39.5~ 39.7 39.7~ 40.1
50 49.2~ 49.5 49.5~ 49.7 49.7~ 50.1
60 59.2~ 59.5 59.5~ 59.7 59.7~ 60.1
Delivery State Choice Surface Condition
Cold Rolled 2B
2D
BA
Hairline
No.3
No.4
6K
8K
Note:
1. If you require different deliver state than the above listed, kindly confirm with us.
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here.
Delivery State
Delivery State Choice Surface Condition
Hot Rolled No.1
No.3
No.4
6K
8K
Pickled
Note:
1. If you require different deliver state than the above listed, kindly confirm with us.
2. In case of any enquiry or order, please kindly let us know any extra requirement not indicated here.
Klasse Typ Dicke Oberfläche
Austenitisch 304/304H/304L/304J1 0.25-150mm 2B/BA/NO.4/8K/SB/HL/NO.1
321 0.4-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
316/316L/317L/316Ti 0.3-80mm 2B/BA/NO.4/8K/SB/HL/NO.1
Ferrite 430 0.4-3.0mm 2B/BA/NO.4/8K/SB/HL
Ultra Pure Ferrite 443 0.4-2.0mm 2B
436L/439/444/441 0.5-3.0mm 2B、2D
409L 0.4-2.5mm 2B、2D
Klasse Typ Dicke Original
Heat-resistant Steel 309S 0.5-40mm CHN
310S Edelstahlplatte 0.5-40mm CHN
Duplex Steel 2101 1.5-50mm CHN
2304 3.0-50mm CHN
2205 0.5-60mm CHN
2507 1.0-60mm SWE / JPN / CHN
Super Austenitic Steel N08904 0.6-50mm SWE / JPN / CHN
S31254 0.5-50mm SWE / JPN / CHN
N08926 0.5-50mm SWE / JPN / CHN
N08367 0.5-50mm SWE / JPN / CHN
Nickel Base Alloy N08031 1.0-50mm US / JPN / GER
N08810/N08800 0.8-50mm US / JPN / CHN
N08028 1.0-20mm US / GER / JPN
N08020 1.0-20mm US / GER / JPN
N08825 0.8-40mm US / GER / SWE / JPN / CHN
N10276 0.5-50mm US / GER / JPN
N06022 1.0-50mm US / GER / JPN
N06625 0.8-20mm US / GER / CHN
N04400 1.0-20mm US / GER / JPN
N06600 1.0-50mm US / GER / JPN / CHN
N02201 0.5-20mm US / JPN
Titan TA1/Gr1 0.5-50mm JPN / CHN
TA2/Gr2 0.5-50mm JPN / CHN
Welding Material ERNiCrMo-13 1.2、2.4mm GER
ERNiCrMo-3 2.4mm GER
ERNiCrMo-4 2.4mm US

The surface and shape of 17-4PH stainless steel plate (7)

Daxun is a trustworthy stainless steel plate manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all stainless steel plates are certified by ISO9001, SGS, CE, OQC and more international quality standards.We also have strict quality control to ensure that the stainless steel plates have less defects. At Daxun, rest assured that all products are durable, high quality and high performance.

Recent hot case projects and products

17-4PH plate stainless steel
astm a240 17-4PH stainless steel plate
17-4PH flat stainless steel plate
17-4PH stainless steel sheet suppliers
17-4PH 2b stainless steel sheet
17-4PH stainless steel sheet

Leading Stainless Steel Sheet Suppliers in China

Daxun can provide upon request: Alloy 17-4 (H900, UNS S17400) plates.

 

CORROSION RESISTANCE:

  • Withstands corrosive attacks better than any of the standard hardenable stainless steels.
  • Comparable to Alloy 304 in most media.
  • Corrosion resistant in some chemical, petroleum, dairy, and food process industries.
  • Subject to crevice or pitting attack if exposed to stagnant sea water for any length of time.

WELDABILITY:

  • Successfully welded by most common fusion and resistance methods.
  • Should not be joined by oxyacetylene welding.
  • Generally no pre-heating required.
  • Inter-pass temperature must be limited to 248°F.
  • Better toughness is obtained in the weld after a complete heat treatment.

ELEVATED TEMPERATURE USE:

  • Excellent resistance to oxidation to approximately 1100°F.
  • Long-term exposure to elevated temperature can result in reduced toughness in the precipitation hardened conditions.

PROCESSING – HOT FORMING:

  • To forge, heat uniformly to 2150 / 2200°F and hold for half hour per inch.
  • Preferred temperature range for hot forming is at 650-900°F, while the steel is still austenitic.
  • To ensure the best condition for the hardening operations, the forgings must be re-heat treated at 1875-1925°F.
  • Cool forgings to below 90°F to ensure grain refinement.

PROCESSING – COLD FORMING:

  • Alloy 17-4 is limited to mild operations since in the annealed (solution treated) condition the material is hard.
  • For severe cold working the material should be heat treated to condition H1150. This will help prevent possible cracking.
  • Bend radius in excess of 7T is often required.
  • To improve stress corrosion resistance after cold forming, re-aging at the precipitation-hardening temperature is recommended.

MACHINABILITY:

  • Can be machined in both solution-treated and precipitation-hardening conditions.

Mechanical Properties

  • Type 17-4PH stainless steel has excellent mechanical properties. For applications requiring high strength and hardness as well as corrosion resistance, Type 17-4PH stainless is an outstanding choice, and it is more cost effective than many high nickel non-ferrous alloys.

17-4PH Grade Stainless Steel Sheets in a Variety of Finishes

Our stainless steel sheets (sometimes called steel sheets) are available in a range of beautiful finishes: brushed finish, 2B smooth finish or 8K mirror finish.

The finished side of each stainless steel sheet we supply is coated with a film. This film is easily peeled off after fabrication or installation and protects the surface of the material from wear and marks. The back side is unfinished.

17-4ph Grade Stainless Steel Sheet is the most commonly used variety. It is easily weldable, formable, and has good corrosion resistance.

We can assist in providing stainless steel sheets in any required size.

To meet your specific requirements, our stainless steel sheets are available in three finishes and a variety of sizes. We can readily provide any custom size you may need with our free unlimited cutting service.

We are able to meet any size needs between 0.3 and 30 mm in thickness and between 50 x 50 mm and 2500 x 1250 mm in size. In addition, we provide free unlimited cutting with every order, using a state-of-the-art cutting machine to precisely meet your requirements.

Order Stainless Steel Sheets by Phone or Online.

There has never been an easier way to get stainless steel sheets. Simply refer to the simple and detailed instructions on our website. Alternatively, our sales staff will be happy to take your order or answer any questions when you call +86 13382898899 or email [email protected].

Our delivery time is only one to two days.

Important Safety Note:

The edges of the metal sheets we sell are not polished, ground or finished, so they may be sharp, just like the edges of any stainless steel sheet. We remind users to use, install and handle these devices with care.

How Does 17-4 Steel Stack Up Against Other Metals?

17-4 stainless steel may not be the only choice for the job. At Daxun Alloys, we offer a wide variety of materials suitable for your job.

Is 17-4 Stainless Steel Magnetic?

Like all alloy steels, when 17-4 stainless steel is hardened, it becomes magnetic.

Does 17-4 Stainless Steel Rust?

The alloy is considered to be highly resistant to rust, particularly in comparison to other types of stainless steel. However, 17-4 stainless steel can still rust in certain conditions if it is exposed to harsh environments for long periods of time and not properly maintained.

How Much Is 17-4 Stainless Steel?

Prices will vary depending on your project, so the best way to get accurate pricing is to contact Daxun for a custom quote.

Kann ich ein paar Muster bekommen?

Wir können Ihnen Muster aus Edelstahlblech zur Qualitätsprüfung zur Verfügung stellen. Das Muster ist kostenlos, Sie zahlen lediglich die Versandkosten.

Which countries have you already exported?

We’ve exported to more than 42 countries, such as Canada, Chile, Kuwait, Germany, South Korea, Saudi Arabia, Singapore etc.

What is your MOQ?

Our MOQ is 1 ton for stainless steel sheet.

How long is your delivery time?

Trial orders can be delivered within a week. For regular orders, it takes two weeks roughly.

Senden Sie Ihre Anfrage noch heute
Schnelles Angebot