x
أرسل استفسارك اليوم
اقتباس سريع

Daxun is an excellent manufacturer of CP-1-grade titanium rods

As China’s leading supplier of titanium and titanium alloy rods, Daxun provides high-performance titanium rods to the world.
  • Titanium bar grade: CP-1 (grade 1) – UNS R50250-3.7025-TA1
  • Type: hot rolled bar, forged bar, cold drawn bar, extruded bar, etc.
  • Shape: titanium round bar, titanium square bar, titanium hexagonal bar
  • Titanium bar density: Grade 1 titanium bar density is 4.51g/cm3
  • Standard: ASTM B 348, ASME SB348, ASTM F67, ASTM 265
  • Size: GB, GJB, EN, ASTM, JIS, ASME, BS, AISI, DIN, ISO, etc.

————تنتج شركة Daxun قضبان التيتانيوم في الصين لتلبية احتياجات السوق المتنوعة و ——الاحتياجات المتطلبة للعملاء!

الشركة الرائدة عالمياً في خدمات تصنيع قضبان التيتانيوم النقي تجارياً

Titanium round bars are among the most sought-after titanium products offered by Daxun Alloy China. The production of Grade 1 Titanium bars involves a more automated process compared to the manufacturing of blocks and plates. These bars are available in over forty unique grades, including various commercially pure titanium grades, with the most commonly used being Grade 5, Grade 2, and Grade 1. Their diameters can range up to 14 inches, catering to diverse industrial requirements. Each cp grade is categorized based on its composition, purity, and properties.

Pure Titanium Grade 1 stands out for its exceptional ductility and cold formability, making it ideal for deep drawing applications. This grade is highly regarded for its excellent corrosion resistance to general and seawater corrosion, as well as its ability to withstand oxidizing, neutral, and mildly reducing environments, including chloride-containing solutions. Additionally, Grade 1 Titanium has the lowest strength among the commercially pure titanium grades, but its high corrosion resistance and superior ductility make it suitable for various applications. Titanium’s low density—approximately half that of nickel-based alloys—combined with its high strength-to-weight ratio and superior corrosion resistance, makes it an optimal material for use in demanding chemical environments.

Daxun sells both pure titanium and titanium alloy bars to fulfill the needs of aerospace applications. Alloy titanium bars are created only from high-performance materials. Although titanium is an alloy, it can be easily shaped into bars while maintaining its hard, shiny appearance. Alloy titanium bars are frequently utilized because of their high strength-to-weight ratio and the ability to be custom-produced to requirements. Daxun offers round and square titanium bars in a range of lengths, but if you don’t see what you’re looking for, we can tailor our products to your specific needs and requirements. Contact us today to learn more! Our titanium bar supply includes Grades 1, 2, and 5 (Ti 6AL/4V and ELi), as well as Grade 7.

قراءة المزيد

البيانات

المواصفات التفاصيل
المواد Titanium rod and bar Grade 1 (UNS R50250)
قياسي astm b348، astm sb348، ams 4921، ams 4902
الأبعاد EN, ASTM, JIS, ASME, BS, AISI
نطاق القطر 0.125″ – 14″ (3.175mm – 355.6mm), custom
نطاق الطول Up to 240″ (6096mm), custom
الإنهاء Cold (bright) drawn, centreless ground, hot rolled, smooth turned, peeled, slit rolled edge, hot rolled annealed, Rough Turned, Bright, Polish, Grinding, Centreless Ground & Black
تشطيب السطح مسحوب على البارد، أو مسحوب على البارد، أو أرضي بدون مركز، أو مصقول، أو خشن، أو أسود، أو تشطيب رقم 4، أو تشطيب BA، أو تشطيب غير لامع، إلخ.
الحالة Hardened & tempered, annealed
التسامح Diameter tolerance: +/- 0.005″ (0.127mm), length tolerance: +/- 0.125″ (3.175mm)
الاستمارة قضبان التيتانيوم المربعة، وسبائك التيتانيوم، وقضبان التيتانيوم المستديرة، وقضبان التيتانيوم المستطيلة، وقضبان التيتانيوم المثلثة، وقضبان التيتانيوم المطروقة، وقضبان التيتانيوم السداسية الشكل، إلخ.
الخصائص الفيزيائية Density: 0.163 lb/in³ (4.51 g/cm³), Melting Point: 3,020°F (1,660°C), Elongation: 20-30%, Modulus of Elasticity: 16.5 x 10⁶ psi (114 GPa)
التركيب الكيميائي Titanium (min): 99.2%, Oxygen (max): 0.25%, Carbon (max): 0.08%, Iron (max): 0.30%, Nitrogen (max): 0.03%, Hydrogen (max): 0.015%
العنصر Minimum (weight %) Maximum (weight %) Typical (weight %)
في 0.2
O 0.18
C 0.08
N 0.03
H 0.015
تي الرصيد
الخصائص الفيزيائية Metric English Comments
الكثافة 4.50 g/cc 0.163 lb/in³
a Lattice Constant 2.95 Å @Temperature 25.0 °C 2.95 Å @Temperature 77.0 °F alpha phase
3.29 Å @Temperature 900 °C 3.29 Å @Temperature 1650 °F beta phase
c Lattice Constant 4.683 Å 4.683 Å @Temperature 77.0 °F c/a = 1.587
Chemical Properties Metric English Comments
Thermal Neutron Cross Section 5.6 barns/atom 5.6 barns/atom Average for naturally occurring Ti
الخواص الميكانيكية Metric English Comments
Hardness, Brinell 120 120 annealed
Hardness, Knoop 132 132 Estimated from Brinell.
Hardness, Rockwell B 70 70 annealed
Hardness, Vickers 122 122 Estimated from Brinell.
قوة الشد 124 – 138 MPa @Temperature 427 °C 18000 – 20000 psi @Temperature 801 °F
152 – 179 MPa @Temperature 316 °C 22000 – 26000 psi @Temperature 601 °F
193 – 207 MPa @Temperature 204 °C 28000 – 30000 psi @Temperature 399 °F
Tensile Strength, Ultimate 240 MPa 34800 psi
Tensile Strength, Yield 170 – 310 MPa 24700 – 45000 psi
76.0 – 90.0 MPa @Temperature 427 °C 11000 – 13100 psi @Temperature 801 °F 0.2% offset
83.0 – 103 MPa @Temperature 316 °C 12000 – 14900 psi @Temperature 601 °F 0.2% offset
110 – 124 MPa @Temperature 204 °C 16000 – 18000 psi @Temperature 399 °F 0.2% offset
Elongation at Break 24% 24%
25 – 30 % @Temperature 427 °C 25 – 30 % @Temperature 801 °F
30 – 35 % @Temperature 316 °C 30 – 35 % @Temperature 601 °F
40 – 50 % @Temperature 204 °C 40 – 50 % @Temperature 399 °F
Reduction of Area 35% 35%
Tensile Modulus 103 GPa 14900 ksi
Compressive Modulus 110 GPa 16000 ksi
Poissons Ratio 0.37 0.37
Shear Modulus 45.0 GPa 6530 ksi
Charpy Impact 310 J 229 ft-lb V-notch
Impact Test 136 J 100 ft-lb Impact Strength
Coefficient of Friction, Dynamic 0.68 0.68 Ti sliding on Ti; 300 m/min
0.8 0.8 Ti sliding on Ti; 40 m/min
Electrical Properties Metric English Comments
المقاوماتية الكهربائية 0.0000420 ohm-cm 0.0000420 ohm-cm
Magnetic Permeability 1.00005 1.00005 at 1.6 kA/m
Magnetic Susceptibility 3.98E-08 3.98E-08 1/kg; Paramagnetic
Thermal Properties Metric English Comments
Heat of Fusion 325 J/g 140 BTU/lb High Purity Ti.
CTE, linear 8.35 µm/m-°C @Temperature 15.0 °C 4.64 µin/in-°F @Temperature 59.0 °F
8.70 µm/m-°C @Temperature 100 °C 4.83 µin/in-°F @Temperature 212 °F
9.50 µm/m-°C @Temperature 300 °C 5.28 µin/in-°F @Temperature 572 °F
9.70 µm/m-°C @Temperature 0.000 – 540 °C 5.39 µin/in-°F @Temperature 32.0 – 1000 °F perpendicular to the c-axis
Specific Heat Capacity 0.520 J/g-°C 0.124 BTU/lb-°F
0.560 J/g-°C @Temperature 200 °C 0.134 BTU/lb-°F @Temperature 392 °F
0.620 J/g-°C @Temperature 400 °C 0.148 BTU/lb-°F @Temperature 752 °F
0.690 J/g-°C @Temperature 600 °C 0.165 BTU/lb-°F @Temperature 1110 °F
التوصيل الحراري 16.0 W/m-K 111 BTU-in/hr-ft²-°F annealed
نقطة الانصهار <= 1670 °C <= 3040 °F
Liquidus 1670 °C 3040 °F
Beta Transus 882 °C 1620 °F
Optical Properties Metric English Comments
Emissivity (0-1) 0.3 @Temperature 710 °C 0.3 @Temperature 1310 °F High purity Ti
Reflection Coefficient, Visible (0-1) 0.56 0.56 High purity Ti; visible light.
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 % <= 0.10 %
Hydrogen, H <= 0.015 % <= 0.015 %
Iron, Fe <= 0.20 % <= 0.20 %
Nitrogen, N <= 0.030 % <= 0.030 %
Other, total <= 0.30 % <= 0.30 %
Oxygen, O <= 0.18 % <= 0.18 %
Titanium, Ti >= 99.175 % >= 99.175 %
Descriptive Properties
Alpha Phase Crystal Structure cph, below 882°C
Beta Phase Crystal Structure bcc, above 882°C
Gr 1 Titanium Industrial Bars & Rods  ASTM B348 Titanium Grade 1 Rod and Bar
 Titanium Gr 1 Rods in china  Titanium UNS R50250 Hollow Bar
 Grade 1 Titanium Half Round Bars  Titanium Gr.1 Cold Drawn Round bar
 Titanium Grade 1 Bar Stock  Titanium Grade 1 ASME SB348 Bars
 Titanium Gr 1 Solid Bar  Titanium Gr 1 Black Bar
 Titanium Grade 1 Bar Suppliers  ASTM B348 Ti Grade 1 Forged Rods
 Polished Titanium Grade 1 Rod  SB 348 Titanium Grade 1 Triangle Bar
 Ti Alloy Grade 1 Hexagon Bars  Titanium Alloy Gr 1 Threaded Bar
 Titanium R50250 Hollow Bar  Grade 1 Titanium Alloy Round Bar
 ASTM B348 UNS R50250 Bar  Titanium Grade 1 Round Bar Supplier
 Titanium Gr1 Rods  SB348 Titanium Grade 1 Alloy Bars
 Titanium 3.7025 Rectangle Bar  ASTM B348 Titanium Grade 1 Solid Rod
 Titanium Alloy Grade 1 Round Rods  Titanium Grade 1 Polish Bar

اختر Daxun لمساعدة مشروعك على الانطلاق.

DAXUN® Grade 1 Titanium Rod Features

DAXUN® Ti Grade 1 is a commercially pure (CP) titanium bar, known for its distinct characteristics, including:

  • Excellent general corrosion resistance
  • Excellent resistance to pitting, crevice and erosion-corrosion
  • Very good ductility
  • High heat transfer efficiency
  • Good formability and weldability
  • Extremely low thermal expansion
  • Ideal for chemical processing applications due to its corrosion resistance

These properties are critical for applications in demanding environments.

مزايا مصنع داكسن

Daxun’s “Performance Excellence Management” concept promotes the “PDCA + Lean” management model. The company’s business card says “Daxun = Reliable Quality”. Daxun uses the ERP system to achieve full traceability of the variety, specification, and origin of each titanium rod, and advocates and encourages industry anti-counterfeiting. Daxun relies on technology for processing and customization, and high precision and high quality are the industry benchmarks; in terms of service, it promotes product life cycle management, provides professional material selection and processing solutions before sales, strictly monitors during sales, and provides worry-free service guarantees after sales.

اتصل بـ Daxun الآن

Grade 1 Titanium Rod Production Method

Daxun manufactures premium-quality titanium bars known for their exceptional performance. Additionally, the company is capable of producing titanium bars tailored to meet specific customer requirements, as per individual agreements:

  • Titanium ingots need to go through heat treatment and machining, immersion ultrasonic testing, mechanical properties testing, macroscopic and microscopic structural inspection and other processes. Production process: hot-rolled titanium bars – high efficiency, stable performance, forged titanium bars – flexible size, multi-fire forging, improve the comprehensive performance of titanium bars, cold-drawn titanium bars – usually small-sized high-precision titanium bars; the above titanium bars are all delivered with bright surface.

تقارير الاختبار

The test reports we provide include: Grade 1 Titanium Rod and Grade 1 Titanium Round Bar Factory Test Certificate, EN 10204 3.1, Chemical Report, Mechanical Report, PMI Test Report, Visual Inspection Report, Third Party Inspection Report, NABL Approved Laboratory Report, Destructive Test Report, Non-destructive Testing Report. (DaXun will provide according to customer requirements)

Grade 1 Rods Applications and Standards

Grade 1 Titanium Rods are widely used in the following industries under extreme corrosive conditions:

  • Aerospace, military, oil and gas industry, marine engineering, marine hardware, chemical plants, industrial machinery, power industry, paper and pulp industry, food processing industry, refineries, pharmaceutical and food processing equipment, etc.
  • Specifications: ASTM B861, B862, B338 / ASME SB861, SB862, SB338
  • المعايير: Astm, asme, asme, en, jis, din, gb, gjb, gjb, api

Titanium, particularly Grade 1 Titanium, is categorized among metals known for their excellent corrosion resistance and versatility in various applications, including marine and aerospace industries.

الجودة والتسليم والتفتيش

Daxun conducts a comprehensive range of quality assurance tests to ensure the highest standards of its titanium products. These tests include mechanical assessments such as area tensile testing, yield strength classification, chemical analysis, and material positive identification (PMI). Additionally, micro and macro testing, intergranular corrosion (IGC) testing, ultrasonic flaw detection, pitting and resistance testing, hardness testing, and expansion testing are performed. These procedures guarantee that the Grade 2 Titanium Rod and Grade 2 Titanium Round Bar meet the specific requirements of their intended applications. Throughout the production process, we carefully measure the diameter, thickness, and surface quality of each product.

  • وقت التسليم لدينا يتوافق تمامًا مع العقد.
  • دعم الوكالات الخارجية للعملاء للذهاب إلى المصنع للفحص
  • دعم العينات المجانية لاختبار العملاء
  • دعم الفحص الموقعي أو فحص المصنع بالفيديو

التعبئة والتغليف

تضمن شركة Daxun Alloy أفضل جودة للتغليف لأنها تلعب دورًا مهمًا في الشحن الدولي حيث تمر البضائع عبر قنوات مختلفة للوصول إلى الوجهة النهائية، لذلك نولي اهتمامًا خاصًا بالتغليف. نقوم بتغليف بضائعنا بعدة طرق حسب المنتج. نقوم بتغليف منتجاتنا بعدة طرق مثل:
- الصناديق والصناديق
- الغلاف المنكمش
- منصات خشبية
- صناديق خشبية

الدعم الفني

If you require any additional technical support, our experienced metallurgist and knowledgeable staff are always available to assist. Furthermore, Daxun is proud to feature a certified testing laboratory—the first of its kind in the multi-metal and plastic inventory industry. We believe this reinforces our strong commitment to quality and aligns with our philosophy of being a full-service supplier.

Grade 1 bar and rod features

قوة عالية
مقاومة التآكل
مقاومة الحرارة
مقاومة درجات الحرارة المنخفضة
حماية البيئة
خفيف الوزن

Daxun Grade 1 Titanium Rods help your brand improve quickly

Apart from the products listed below, other available metal products are not listed here. Other metal products DAXUN can manufacture and supply include Tantalum, Niobium, Zirconium, Hafnium, Nickel, Copper etc., which are mainly in the form of Plate, Bar and Tube.
Products/Processing Standard Grade/Size
Titanium rod/bar— ASME SB265, AMS 4911, AMS 4919, AMS 4914,ASTM F67, ASTM F136  GR1, GR2, GR3, GR4, GR5, GR7,GR9, GR12, GR16, GR17, GR23,Ti-6Al-4V ELI, Ti-6-2-4-2, Ti-15-3-3-3(Thickness:( 0.0197”-6”)Max Width: 12 feet,Max Length: 50 feet)
AMS-T-9046
Titanium and Titanium alloy rod/bar
Commercially pure titanium (CP)
Code designation Yield strength
minimum, ksi 1 /
CP-1 70
CP-2 55
CP-3 40
CP-4 25
Alpha titanium alloys(A)
Code designation Composition
A-1 5A1-2.5Sn
A-2 5A1-2.5Sn(ELI) 2 /
A-3 6A1-2Cb-1Ta-0.8Mo
A-4 8A1-1Mo-1V
Alpha-beta titanium alloys(AB)
Code designation Composition
AB-1 6A1-4V
AB-2 6A1-4V(ELI)
AB-3 6A1-6V-2Sn
AB-4 6A1-2Sn-4Zr-2Mo
AB-5 3A1-2.5V
AB-6 8Mn
Beta titanium alloys(B)
Code designation Composition
B-1 13V-11Cr-3A1
B-2 11.5Mo-6Zr-4.5Sn
B-3 3A1-8V-6Cr-4Mo-4Zr
B-4 8Mo-8V-2Fe-3A1
Processing:
الدرفلة على الساخن الدرفلة على البارد
Available Grades:
الصف الأول الابتدائي Grade 6Al-2Sn-4Zr-2Mo (6-2-4-2)
الصف الثاني الابتدائي Grade 6Al-4V ELI (Formerly Grade 23)
Grade 7 Grade 6Al-6V-2Sn (6-62)
Grade 19 Grade 8Al-1Mo-1V (8-1-1)
Grade 5 (6Al-4V) Grade 9 (3Al-2.5V)
Grade 6 (5Al-2.5Sn) الصف الثالث الابتدائي
Application
الصناعة الكيميائية Desalination Of Sea Water
Petrochemical Industry الطيران والفضاء
Machining Field, Automobile Field Mobile Phone Component Field.
Titanium Grade 1 Bright Bar Titanium Grade 1 Bright Bar
Grade 1 Titanium Alloy Bright Bar
Titanium Gr 1 Bright Bar
UNS R50250 Titanium Bright Bar
WERKSTOFF NR. 3.7035 Bright Bar
ASTM B348 Gr 1 Titanium Bright Bar
Titanium Grade 1 Hex Bar Titanium Gr 1 Hex Bar
Grade 1 Titanium Hexagonal Bar
Gr 1 Titanium Alloy Hex Bar
UNS R50250 Titanium Hexagonal Bar
ASTM B348 Grade 1 Titanium Hex Bar
Titanium Alloy Grade 1 Square Bar Titanium Grade 1 Square Bar
Grade 1 Titanium Square Bars
Gr 1Titanium Alloy Square Bar
UNS R50250 Titanium Square Bar
WERKSTOFF NR. 3.7035 Square Bar
ASTM B348 Gr 1 Titanium Square Bars
Titanium Grade 1 Rectangular Bar Titanium Grade 1 Rectangular Bar
Ti. Alloy Gr2 Rectangular Bars
Gr 1 Titanium Alloy Rectangular Bar
UNS R50250 Titanium Rectangular Bars
WERKSTOFF NR. 3.7035 Rectangular Bar
ASTM B348 Gr 1 Titanium Rectangular Bar
Titanium Grade 1 Flat Bars Titanium Grade 1 Flat Bar
Gr 1Titanium Alloy Flat Bars
Titanium Gr 1Flat Bars
UNS R50250 Titanium Flat Bars
WERKSTOFF NR. 3.7035 Flat Bars
ASTM B348 Gr 1 Titanium Flat Bars
Titanium Grade 1 Polished Bar Titanium Grade 1 Polished Bar
Grade 1Titanium Polished Bars
Gr 1Titanium Alloy Polished Bar
UNS R50250 Titanium Polished Bars
WERKSTOFF NR. 3.7035 Polished Bar
ASTM B348 Gr 1 Titanium Polished Bar
Titanium Grade 1 Threaded Bar Titanium Gr 1 Threaded Bar
Grade 1Titanium Threaded Bars
Ti. Alloy Grade 1 Threaded Bar
UNS R50250 Titanium Threaded Bar
WERKSTOFF NR. 3.7035 Threaded Bar
ASTM B348 Gr 1 Titanium Threaded Bar
الحجم الاسمي h5 h6 h7 h8 h9 H10 H11 h12
القطر مم
~ إلى 3 +0.004/0 +0.006/0 +0.01/0 +0.014/0 +0.025/0 +0.04/0 +0.06/0 +0.1/0
أكثر من 3 إلى 6 +0.005/0 +0.008/0 +0.012/0 +0.018/0 +0.03/0 +0.048/0 +0.075/0 +0.12/0
أكثر من 6 إلى 10 +0.006/0 +0.009/0 +0.015/0 +0.022/0 +0.036/0 +0.058/0 +0.09/0 +0.15/0
فوق 10 إلى 18 سنة +0.008/0 +0.011/0 +0.018/0 +0.027/0 +0.043/0 +0.07/0 +0.11/0 +0.18/0
فوق 18 إلى 30 سنة +0.009/0 +0.013/0 +0.021/0 +0.033/0 +0.052/0 +0.084/0 +0.13/0 +0.21/0
أكثر من 30 إلى 50 +0.011/0 +0.016/0 +0.025/0 +0.039/0 +0.062/0 +0.1/0 +0.16/0 +0.25/0
أكثر من 50 إلى 80 +0.013/0 +0.019/0 +0.03/0 +0.046/0 +0.074/0 +0.12/0 +0.19/0 +0.3/0
أكثر من 80 إلى 120 +0.015/0 +0.022/0 +0.035/0 +0.054/0 +0.087/0 +0.14/0 +0.22/0 +0.35/0
أكثر من 120 إلى 180 +0.018/0 +0.025/0 +0.04/0 +0.063/0 +0.1/0 +0.16/0 +0.25/0 +0.4/0
أكثر من 180 إلى 250 +0.02/0 +0.029/0 +0.046/0 +0.072/0 +0.115/0 +0.185/0 +0.29/0 +0.46/0

المعلومات المتاحة للرجوع إليها وتنزيلها

Daxun is a trustworthy Titanium rod and bar rod manufacturer

As a professional manufacturer, Daxun ensures that all the products we produce are of high quality. Therefore, we ensure that all titanium bars are certified by ISO9001, SGS, CE, OQC and more international quality standards. We also conduct strict quality control to ensure that the titanium rods have less defects. At Daxun, you can rest assured that all products are durable, high quality and excellent in performance.

أحدث مشاريع ومنتجات الحالة الساخنة

قضيب وقضيب التيتانيوم
قضيب وقضيب التيتانيوم
قضيب وقضيب التيتانيوم
قضيب وقضيب التيتانيوم
قضيب وقضيب التيتانيوم
قضيب وقضيب التيتانيوم
قضيب وقضيب التيتانيوم
قضيب وقضيب التيتانيوم
Commercially Pure Titanium Rod Grade 1

Daxun manufactures highly competitive, high-precision Grade 1 titanium bars at our advanced production facilities in China. Our products are known for their excellent surface finish, precise tolerances, straightness, and superior material quality, providing you with both technological leadership and consistent production processes. These benefits extend across a wide range of diameters and materials. Additionally, our extensive stocking program at our service center ensures reliable, just-in-time delivery for your needs.

Size range

  • Grade 1 Titanium Bar Dimensions
  • Ø 0,7 – 30 mm (drawn, ground)
  • Ø 16 – 400 mm (hot rolled, peeled)
  • h11-h5 possible
  • Tighter or different tolerances are available on request
  • Lengths up to 9,000 mm long, depending on diameter
  • For larger diameters, other bar lengths and tolerances can be agreed upon request

Availability Grade 1 Titanium rods

  • Drawing, straightening
  • Drawing, straightening, polishing
  • Drawing, grinding, polishing
  • الرسم، والتقويم، والطحن، والتلميع، والصقل
  • Drawing, annealing, straightening
  • Drawing, annealing, polishing
  • Drawing, annealing, grinding, polishing
  • Drawing, annealing, straightening, grinding, polishing

Processing

We produce bars according to your requirements.

Our titanium bars feature an excellent surface finish, superior straightness, perfect roundness, and the tightest diameter tolerances, adhering to ISO 286-2 standards (up to h5). These bars are available in various conditions, including straightened, ground, and polished.

For sawing, we utilize high-performance band saws, capable of handling diameters up to Ø510 mm. Our bench band saws can accommodate larger sizes, with cutting capacities of up to 6,000 x 3,000 x 400 mm. These advanced sawing machines ensure precise and efficient cutting, meeting the most exacting specifications.

Titanium Bar end machining

Single or double-sided
Chamfer 90° (45°)
Point 60° (30°)
Flat end
Centered

Delivery form

  • ASTM: American Society for Testing and Materials Standards
  • AMS: American Aerospace Materials Standards
  • NACE: American Association of Corrosion Engineers International Standards
  • ASME: American Society of Mechanical Engineers Standards
  • GB: Chinese National Standards
  • GJB: Chinese National Military Standards
  • ISO: International Standards
  • DIN: German Standards
  • EN: European Standards
  • API: American Petroleum Institute Standards

Detection method

Non-destructive testing > 100% testing

  • Eddy Current Testing/Eddy Current Crack Testing: This method is used to detect surface cracks and discontinuities, ensuring defect-free surfaces (level 4).
  • Flat Bottom Hole Diameter Testing: We use flat bottom hole diameters of 0.7 mm and 0.4 mm to accurately assess material integrity.
  • Blind Area Testing: The blind area of the material can be cut off according to a fixed length, with testing conducted all the way to the end of the bar.
  • Full Diameter Ultrasonic Testing: This technique is used to inspect the entire diameter of the bar, ensuring it meets rigorous standards for quality and performance.

Our Titanium Bar Material

الخدمات

  • As an experienced service center, we can tailor your titanium bar material to your specifications, work with various certification bodies such as TÜV Rheinland or DNV to approve the specifications, and initiate the upgrading of titanium semi-finished products to meet appropriate applications.
  • We will be happy to provide you with a consultation and explain everything you need to know about obtaining titanium bar material, including which standards require greater attention for the components to be manufactured.
  • If you have a long-term supply commitment, you can establish a framework agreement with Daxun. We guarantee prices and quantities for a specified period.
  • Benefit from our extensive experience in the global market. We have been helping businesses around the world since 2003. If you need any additional information about the Grade 2 Titanium Bar, our professionals will be happy to help you. We look forward to hearing from you.

معلومات الطلب

When placing a purchase order, please ensure it includes the following details: quantity, grade, type or category, API 5L reference, thickness, width, length, and any relevant attachments or specific requirements related to chemical composition, mechanical properties, heat treatment, additional testing, manufacturing process, surface coating, or end finish.

ما هي درجة التيتانيوم الأفضل؟

تعتمد درجة سبيكة التيتانيوم التي تحتاجها على المشروع الذي تعمل عليه، حيث أن لكل درجة فوائد مختلفة.

إنّ جميع درجات سبائك التيتانيوم قوية للغاية ومقاومة للتآكل، مما يعني أنها ستستمر في العمل بشكل جيد في أقسى الظروف.

إن الدرجات الأعلى من سبائك التيتانيوم (5-12) هي سبائك مصممة لفوائد محددة. على سبيل المثال، تتميز سبائك التيتانيوم من الدرجة 12 بمقاومة ممتازة للحرارة، مما يجعلها خياراً مثالياً للمبادلات الحرارية الصدفية والأنبوبية والأنابيب الهيدروليكية ومعدات الصناعة الكيميائية.

الدرجات من 1-4 هي سبائك التيتانيوم النقي، وهي خيار مثالي إذا كنت بحاجة إلى مادة قابلة للحام وقابلة للسحب لأنظمة الأنابيب والأنابيب. ستجد درجات أقل تستخدم في الصناعات البحرية والصناعية.

إذا كنت تبدأ مشروعاً ولست متأكداً من درجة سبيكة التيتانيوم الأفضل لك، اتصل بنا اليوم؛ فنحن سعداء للغاية بمساعدتك.

كيف تختلف الدرجات الأعلى من التيتانيوم عن الدرجات الأدنى؟

نقدم في DAXUN مجموعة واسعة من درجات سبائك التيتانيوم من الدرجة 1 إلى الدرجة 12.

الدرجات من 1 إلى 4 هي التيتانيوم النقي، بينما الدرجات الأعلى هي السبائك.

تحظى درجات السبائك بشعبية كبيرة بسبب نسبة قوتها إلى وزنها العالية.

درجة سبائك التيتانيوم الأكثر استخداماً لدينا هي الدرجة 5. وعلى الرغم من أنها لا تزال تحتوي على نسبة عالية من التيتانيوم، إلا أن هذه الدرجة هي الأكثر موثوقية لأنها تتحمل درجات حرارة تصل إلى 600 درجة فهرنهايت وتتحمل الظروف القاسية.

وتفضل الصناعات مثل صناعات الطيران والصناعات البحرية الدرجات الأعلى لمقاومتها للتآكل والتآكل.

وعلى العكس من ذلك، تُستخدم الدرجات الأقل في المقام الأول في اللحام نظرًا لانخفاض قوتها.

To learn more about the differences between different grades of titanium alloy, call +86 13382898899 today to speak directly with our experts.

هل تؤثر درجة التيتانيوم على التكلفة؟

على الرغم من أن درجة التيتانيوم تزيد من التكلفة قليلاً، إلا أن التكلفة الإجمالية تتحدد في المقام الأول حسب شكل وشكل التيتانيوم الذي تحتاجه.

At DAXUN, we offer a wide range of titanium products, including rods, tubes, coils and bars. The length, width and quantity of each item you require will affect the amount you pay at checkout.

لسوء الحظ، من الصعب التوصل إلى سعر عبر الإنترنت دون معرفة الكثير عن مشروعك وما سيُستخدم التيتانيوم من أجله.

لحسن الحظ، فريق خبرائنا موجود دائماً لمساعدتك وتقديم المشورة لك بشأن احتياجاتك من التيتانيوم. من خلال إرسال بريد إلكتروني إلى [email protected]، سنكون قادرين على الرد عليك ببعض النصائح وعرض أسعار دقيق.

احرص على تضمين أكبر قدر ممكن من المعلومات حول درجة وشكل وكمية التيتانيوم التي تحتاجها للحصول على فهم أفضل لاحتياجاتك.

أين يمكنني معرفة المزيد عن درجات التيتانيوم؟

يتمتع فريق العمل في DAXUN بالخبرة والمعرفة والود. وبفضل سنوات خبرتهم الطويلة في هذا المجال، فهم يعرفون كل شيء عن التيتانيوم، بما في ذلك استخداماته وفوائده ودرجاته.

للحصول على تحديثات منتظمة عن التيتانيوم واستخداماته وتطبيقاته في مختلف الصناعات، احرص على الاطلاع على مدونتنا. لقد كتب خبراؤنا أدلة سهلة المتابعة يمكنك الرجوع إليها دائماً عندما تكون لديك أسئلة.

إذا كنت لا تزال تواجه مشكلة، فلا تتردد في الاتصال بنا؛ يسعدنا تقديم المساعدة.

من خلال إرسال بريد إلكتروني إلى [email protected]، ستتلقى رداً سريعاً. تأكد من تضمين أكبر قدر ممكن من التفاصيل في سؤالك حتى نتمكن من التوصية بالحل المناسب.

كيف تحصل على عرض أسعار أو تفهم معلومات السوق في أسرع وقت ممكن؟

يُرجى ملء النموذج الموجود في صفحة “اتصل بنا”، أو الاتصال بمدير المبيعات لدينا على “+86 13382898899”، وسوف نتصل بك في أقرب وقت ممكن. واتسابنا على الإنترنت، وسيتم التحقق من البريد الإلكتروني ([email protected]) في غضون 6 ساعات. سيتم الرد على كل استفسار أو رسالة على الفور. بالإضافة إلى ذلك، نشارك معلومات السوق مع عملائنا كل أسبوع

هل يمكنني الحصول على بعض العينات؟

يمكننا تقديم عينات من قضبان التيتانيوم لك للتحقق من الجودة. العينة مجانية وما عليك سوى دفع أجرة الشحن.

ما هي الدول التي قمت بتصديرها بالفعل؟

لقد قمنا بالتصدير إلى أكثر من 42 دولة، مثل كندا، وتشيلي، والكويت، وألمانيا، وكوريا الجنوبية، والمملكة العربية السعودية، وسنغافورة، وغيرها.

ما هو موك الخاص بك؟

Our MOQ is 1 ton for titanium rod.

ما هي مدة التوصيل؟

يمكن تسليم الطلبات التجريبية في غضون أسبوع. بالنسبة للطلبات العادية، يستغرق الأمر أسبوعين تقريباً.

أرسل استفسارك اليوم
اقتباس سريع